The biological natural durability of timber in ground contact
1994 - IRG/WP 94-20051
The BRE ground contact field trials for the determination of the biological natural durability of different timber species have recently been reviewed. The data obtained from these trials have been used to appraise the different ways in which natural durability may be expressed. It is concluded that the use of the mean as a method of assigning the timber to one of five durability classes may be ac...
G A Smith, R J Orsler


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Regulatory and Consumer Challenges Facing Timber Preservation and Durability Interests in New Zealand and Australia
2003 - IRG/WP 03-20282
Timber preservation and durability interests in Australia and New Zealand are facing many challenges and threats arising from regulation and standards changes, to direct competition from competitive materials producers. Industry can address these challenges by pro-active initiation of sound, holistic, research, that addresses the performance needs of the regulators and specifiers and the expectati...
C MacKenzie


Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer


Results of field tests on the natural durability of timber (1932-1975)
1976 - IRG/WP 3105
This paper describes a continuing field stake trial to determine the natural resistance of different species of timber to decay. Data are presented for about 180 timbers, covering over 6000 stakes, and the results are discussed in terms of a natural durability classification....
D W Purslow


Recycling of impregnated timber: Part 2: Combustion trial
1999 - IRG/WP 99-50132
Totally 270 m3 (61,3 t) of CCA impregnated wood was chipped and incinerated at the combustion plant of Jalasjärvi. After the normal gas cleaning venture scrubbers were tested. After the trial a metal balance was calculated. Ash was treated at the copper smelter of Outokumpu Harjavalta Metals Oy. Condensate waters were transfered to the Outokumpu's CCA production plant and utilized by the...
L Lindroos


Final report on world survey of sap displacement impregnation of timber
1975 - IRG/WP 345
The present contribution to the World Survey of Sap Displacement Impregnation of Timber covers the information received since the presentation of the interim report to the 6th Annual Meeting of the International Research Group on Wood Preservation held in Vienna, 20th June 1974....
F B Shorland, C G W Mason


Termite field test results of preservative treated and modified woods in Kumamoto, Japan
2001 - IRG/WP 01-30275
Various preservative treated or modified wood stakes other than CCA, were buried in the soil, maximum for six years in Kumamoto, south west side of Japan. In this area, two main termite species, Coptotermes formosanus and Reticulitermes speratus, are distributed. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservativ...
K Suzuki


Physical and mechanical properties of a suitable constructional timber of Bangladesh
1997 - IRG/WP 97-40102
The study of physical and mechanical properties of lohasirish timber (Derris robusta Roxb.) grown in Bangladesh revealed that the sapwood is whitish to yellowish white, heartwood is dark grey to blackish in colour; the texture is moderately fine, the grain in mostly straight and coarse with whitish rings of parenchyma; shrinkage is moderate; the EMC ranges from 12% to 16%; fuelwood colorific value...
A K Lahiry


A field test with anti-sapstain chemicals on sawn pine timber in Finland
1986 - IRG/WP 3368
Fourteen formulations, each in two concentrations, were tested for effectiveness against sapstain, mould and decay on Scots pine (Pinus sylvestris L.) in a field test in South-Finland. The trial was commenced in June 1985 and finished in October 1985. During the test the boards were infected mainly by mould fungi. In kiln dried boards the protective effects of nine and in green boards of four trea...
L Paajanen


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


The potential for accelerated ageing to determine the persistence of active ingredients in timber
2006 - IRG/WP 06-20323
Fast screening methods for evaluating the persistence of active ingredients in timber are proposed. This is an outline proposal which is intended to provoke discussion and further development of the methods. Reliable and accurate analytical methods are key to these tests....
L D A Saunders, M R Powell


Developments in wood preservation processing techniques in New Zealand
1980 - IRG/WP 3143
P Vinden, A J McQuire


Japanese Classification of Wooden Building Members for ISO Use Classes according to the Building Code in Japan.
2006 - IRG/WP 06-20337
Because of the international approve of use class system for the biological degradation of wood by ISO/DIS 21887 and ISO/DIS 21892, Japanese committee of ISO/TC165/SC1 asked to the JWPA for classify the wooden commodities by use class of these draft ISO. The JWPA was prepared a draft use class model in Japan. Japanese building code systems are described and Japanese draft use class system is also ...
K Suzuki


Timber Preservation and Sustainable Construction in Australia
2005 - IRG/WP 05-50224-14
Sustainable development has been described as meeting the needs of the present without compromising the ability of future generations to meeting their own needs. (Bruntland 1987) To achieve the sustainable development goal therefore, the maximum performance has to be obtained from existing resources (timber) so that the remaining resource is protected from over-exploitation. Clearly, wood preserva...
J Norton


A laboratory evaluation of the susceptibility to biological attack of glued laminated pine timber
1991 - IRG/WP 2387
In the scope of a research programme concerning the use of maritime pine (Pinus pinaster) to produce glued laminated timber structures in Portugal, the natural durability of this material was checked by using laboratory test methods. An European standard, EN 113, was used to test durability against basidiomycetes and a test method developed at LNEC for termites was adapted for this purpose. From t...
L Nunes, H Cruz


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


Wood preservation in Spain
1983 - IRG/WP 3266
This report includes some statistical data on the potential of Spanish forests and the country's timber consumption as well as detailing the extent of development of the wood products industries, and will help to give a better understanding of the use of this raw material in Spain. The main biological deteriorating organisms which damage wood are given and the capacity of the industrial t...
A Lopez de Roma, R Cockcroft


An Open Letter to Proponents of CLT/Massive Timber
2016 - IRG/WP 16-40755
We present an Open Letter that discusses the need to address the potential for biodeterioration in CLT/Massive timber structure. We invite members to review and sign the document. We also welcome suggestions for potential recipients....
A Taylor, J Lloyd, T Shelton


An Historical Roof Timber System in the Old Town of Berlin-Spandau
2019 - IRG/WP 19-10949
In Europe the “Charter of Venice” was enacted on the 31st of May 1964. It is the international directive for the preservation of historic buildings and monuments. All countries in Europe now involve professional wood scientists and engineers in maintaining and preserving historical buildings. Here we discuss a restoration project involving 17th century roof timbering. This project may be used ...
M Luke, W Unger, D Nellessen


Natural durability of some commercial timbers of Sarawak, Malaysia in tropical marine environment
2005 - IRG/WP 05-10561
The abundant supply of timber resources in Sarawak makes timber an ideal choice to be used for marine construction. The natural durability of the main commercial timber species of Sarawak in ground contact is well established but the same is not available for marine environment. This study was conducted to assess the natural durability of 28 commercial timber species in tropical marine environmen...
K Jenang, Wang Choon Ling


Heat treated timber in Finland
2000 - IRG/WP 00-40158
Heat treatment permanently changes the physical and chemical properties of wood by means of high temperatures (150 - 240°C). Heat treatment darkens the colour of the wood. Heat treatment improves the equilibrium moisture content of the wood and the shrinkage and swelling of the wood is reduced. Very high temperatures improve the resistance to rot and also reduce the susceptibility to fungal decay...
T Syrjänen, E Kangas


The leachability and specificity of the biological protection of timber using Scytalidium sp. and Trichoderma spp
1986 - IRG/WP 1302
The results of field experiments, using biological control against internal decay of creosoted poles, are briefly reviewed and the evidence concerning the leachability of the antibiotics produced by these species is presented. A pure culture miniblock decay test on biological control treated pine sapwood is described and the results compared to previously published data. The protection against Len...
P I Morris, N A Summers, D J Dickinson


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 3rd Interim Report
1983 - IRG/WP 4101
This paper updates the results of microbiological examination and marine borer assessment of untreated wood samples (15 x 2 x 2 cm³) and samples treated with 3, 6 and 10% CCA and CCB preservatives. Three reference species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were used at all the test sites in addition to local species chosen by participants in the test....
R A Eaton


Decay patterns observed in butylene oxide modified ponderosa pine after exposure in unsterile soil
1982 - IRG/WP 3211
Small blocks of ponderosa pine (Pinus ponderosa Laws) chemically modified with butylene oxide to three different weight gains were exposed for 6 weeks in unsterile soil. Severe surface decay caused by soft rot fungi and tunnelling bacteria was observed in blocks with 8 weight percent gain. The soft rot attack was restricted to the outer parts of the radial walls in the latewood tracheids. Bacteria...
T Nilsson, R M Rowell