IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 764 documents. Displaying 25 entries per page.


Combined effects of thermal modification and ACQ-D impregnation on properties of southern yellow pine wood
2013 - IRG/WP 13-40637
In this study, samples of southern yellow pine sapwood were first thermally modified and then treated by the alkaline copper quat-type D (ACQ-D) wood preservative. Two heating temperature (180℃ and 220℃) and two concentrations of ACQ-D solution (0.9% and 1.35%) were used in the experiments. The combined effects of thermal modification and ACQ-D on leaching performance, mechanical prope...
Wang Wang, Yuan Zhu, Jinzhen Cao


Durability of alternatives to CCA-treated wood - Results from field tests after 11 years exposure
2013 - IRG/WP 13-30633
The present study was initiated as a consequence of restrictions against the use of CCA-type wood preservatives in Sweden in the 1990s. New copper-based formulations were introduced on the market and to some extent, also alternatives to preservative-treated wood, such as thermally and chemically modified and linseed oil treated wood as well as heartwood of non-tropical naturally durable wood s...
P Larsson Brelid, M-L Edlund


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Estimation of service life of treated wood in ground contact based on early indicators
2013 - IRG/WP 13-20536
A well-known problem with field testing is that it takes a long time before meaningful and reliable results are achieved. Only when a trial has come to an end the so called average life for the samples in a group can be calculated and compared with other samples. The aim of the present study was to investigate if it is possible to get a reasonable and good estimation of the average life long befor...
M Hansson, J Jermer, P Larsson Brelid, N Terziev


Moisture dynamics of wood – An approach to implement wetting ability of wood into a resistance classification concept
2014 - IRG/WP 14-20557
Within the research programmes WoodBuild and PerformWOOD, wetting ability tests have been conducted with 25 wood-based materials. A first attempt has been made to establish factors for calculating the material resistance of wood materials to be implemented into a design guideline for timber structures. The approach looks promising, but further studies are needed to establish more reliable relation...
C Brischke, C Hesse, L Meyer, S Bardage, J Jermer, T Isaksson


An Overview of Western Red Cedar as a Wood Pole Species
2014 - IRG/WP 14-10815
This paper reviews the characteristics of western red cedar, with particular emphasis on its use in utility poles. Western red cedar naturally grows primarily in British Columbia, Alaska, Washington, Oregon, California, Idaho and Montana. Compared to other commercial softwoods it has low density, increased corrosivity, weaker mechanical properties, high dimensional stability, and high natural dura...
M H Freeman, R Stirling


Performance of recent and old Sweet chestnut (Castanea sativa) wood
2014 - IRG/WP 14-10816
Sweet chestnut (Castanea sativa) hardwood is one of the most durable European wood species. In the present research, various aspects that could potentially influence the durability were elucidated, namely: presence of extractives, ring width, and weathering. Simultaneously, properties of wood, which was in outdoor use for 35 years, were elucidated as well. The results indicate that ring width and ...
M Humar, M Žlahtič, N Thaler


Natural durability of plantation-grown coast redwood (Sequoia sempervirens) in New Zealand
2014 - IRG/WP 14-10817
There is wide variation in the wood properties of plantation-grown coast redwood in New Zealand. Contributing factors are the seed source, silviculture, growth and age of the trees in the plantation forests. Little is known about how these factors affect the variation of wood properties among and within the trees of New Zealand’s coast redwood forests. Heartwood of plantation-grown coast redwood...
D O’Callahan, T Jones, C Low, C Chittenden


Durability and Wood Protection for Historic Covered Bridges in the United States
2014 - IRG/WP 14-10829
A majority of the covered wooden bridges in United States were built in the mid -1800’s. These structures represent a unique cultural and technological heritage from that era. Over time, these bridges have been deteriorated by microorganisms and insects or damaged by acts of vandalism and arson. The National Historic Covered Bridge Preservation (NHCBP) Program sponsored by the Federal Highway Ad...
V W Yang, C A Clausen


Variability in durability of some selected South-American wood species
2014 - IRG/WP 14-10831
Within the scope of sustainable forest management one wants to encourage the proper use of lesser known wood species. Therefore the market has to shift from a demand-driven towards a supply-driven market without loss of wood quality. It is generally known that the durability from pith to bark varies thus, affecting the overall durability of wood species. Consequently, a detailed analysis is necess...
I De Windt, P ’t Hooft, J Van den Bulcke, J Van Acker


Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
Different methods are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring local or global moisture content (MC). Furthermore each measuring metho...
L Meyer, C Brischke, M Kasselmann, C Rösmann


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of wood. The moisture performance of wood and wood-based products has been recognized as key...
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Critical parameters on moisture dynamics in relation to time of wetness as factor in service life prediction
2014 - IRG/WP 14-20555
The concept of natural durability or enhanced durability based on the presence of active ingredients having an impact on both fungi and insects is not the only parameter steering the material resistance. Complementary resistance to getting wet (wetting ability) and consequently the ease of drying afterwards will lead to a parameter related to the time a piece of wood will remain under such wet con...
J Van Acker, I De Windt, W Li, J Van den Bulcke


Dynamic mechanical analysis (DMA) of nano cupric oxide (CuO) modified aqueous phenol formaldehyde (PF) resin
2014 - IRG/WP 14-40654
Phenol formaldehyde (PF) resins, modified by nano CuO incorporating alkane surfactant and polyvinyl alcohol (PVA) 17-99, were analyzed by dynamic mechanical analysis (DMA). The mechanical properties of its bonded plywood including tensile strength, modulus of rupture (MOR), modulus of elasticity (MOE) and shear strength under five test conditions were evaluated. Results indicated that the incorpor...
Wei Gao, Guanben Du


Thermal durability and biodegradation of tannin lignin adhesives
2014 - IRG/WP 14-40657
Mimosa tannins and lignosulfonates were used in wood adhesives formulation to substitute resins based on formaldehyde. Mimosa tannins were mixed with either glyoxalated sodium lignosulfonates or glyoxalated ammonium lignosulfonates. The ratios of mimosa tannins and sodium lignosulfonates varied from 20% tannins to 60% tannins. The thermal durability of the adhesives were analysed by thermogravimet...
L Chupin, B Charrier, A Pizzi, F Charrier


Development of new wood treatments combining boron impregnation and thermo modification - Effect on decay and termites durability
2014 - IRG/WP 14-40666
Environmental pressures appeared in most European countries during the last decade has lead to the development of more environmentally acceptable preservation methods. In this context, wood heat treatment has been one of the most investigated alternative methods during the last years. Treated at temperatures ranging between 180 and 220°C, wood components undergo more or less important chemical mo...
S Salman, A Pétrissans, M-F Thévenon, S Dumarçay, B Pollier, P Gérardin


Possible targets of wood modification in brown rot degradation
2014 - IRG/WP 14-40676
Wood modification protects wood from fungal degradation in a non-toxic manner. However, the mechanisms behind the decay resistance in modified wood are currently unknown. The aim of this study was to discuss the i) colonisation, ii) nutrient recognition, iii) transcription, iv) depolymerisation and v) hydrolysis steps in the brown rot degradation progress and explore whether they are inhibited by ...
R Ringman, A Pilgård, G Alfredsen, B Goodell, K Richter


The Physical Properties of Heat Treated Fir Wood and Outdoor Durability
2014 - IRG/WP 14-40677
Wood might be easily susceptible to degrade by biotic and abiotic factors. Therefore, wood should be protected from fungi, insects and other degradation factors by applying treatment methods. Especially, for the wood have used in the external environment. Chemical treatment methods have some disadvantages such as use of toxic chemicals (Arsenic and chromium) and treatability of refractory wood spe...
O E Özkan, H Vurdu, A Temiz, G Köse


Biological durability of natural fibre reinforced composites
2014 - IRG/WP 14-40681
Composite materials reinforced with wood or non-wood natural fibres have the potential to be a lighter and lower-cost alternative construction material. Until better availability and properties and a lower cost price of degradable polymers makes their use more prevalent, the application of natural fibre reinforcements in synthetic polymers is an intermediate step towards products that are complete...
N Defoirdt, I De Windt, J Van den Bulcke, J Van Acker


Influence of the moon phase on durability against wood decay fungi of Larix kaempferi and Pseudotsuga menziesii wood species
2015 - IRG/WP 15-10836
The analysis of the natural durability of wood is essential when establishing the level of protection required, depending on the designated end use of timber. On the other hand, there is a popular belief based on the influence of the moon phase in felling timber, recommending the waning moon as the optimum for felling trees. In fact, some companies now offer among their products, sawn timber felle...
M T Troya, M Conde, M J Barriola, F Llinares, V Dorronsoro


Field Performance of Old-Growth and Second-Growth Western Red Cedar Fence Posts with and without Barrier Wraps
2015 - IRG/WP 15-10838
Many authors have suggested natural durability may be lower in second-growth western redcedar than in old-growth. One potential means of offsetting a decline in durability is use of physical barriers to separate the wood from soil. In the present work we compared the durability of old-growth and second-growth western red cedar posts, with and without barrier wraps, in a field test. After ten year...
P I Morris, J K Ingram, R Stirling


Interpretation of moisture monitoring data - Relevance of moisture content thresholds for fungal decay
2015 - IRG/WP 15-10839
It is widely accepted that besides temperature wood moisture content (MC) is the key factor when it comes to durability of wooden structures exposed to weathering. Many approaches to predict the service life of wooden structures have therefore been based on using wood MC as one major input-variable to develop dose-response relationships between material climate and decay response. However, to impr...
L Meyer, C Brischke


Investigations on the durability of several Congo basin wood species
2015 - IRG/WP 15-10840
The sawdust of ten wood species was studied to assess their natural resistance to decay. The extractives and lignin contents were primarily determined (between 2.7-16.0% and 26.8-35.9% respectively) to give an overview of the chemical distribution. Then, a phytochemical screening (colorimetric methods) characterized the different chemical functional groups in all extracts studied. Antioxidant act...
S Mounguengui, J-B Tchinda Saha, M Kor Ndikontar, S Dumarçay, C Attéké, D Perrin, E Gelhaye,


Previous Page | Next Page