IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 237 documents. Displaying 25 entries per page.


Production of exraxellular hydrogen peroxide and oxalic acid by brown-rot fungus Poria placenta
1995 - IRG/WP 95-10112
Hydrogen peroxide and oxalic acid have been suggested to be essential in the degradation of wood carbohydrates by brown-rot fungi. Hydrogen peroxide has been suggested to be one of the diffusible low molecular weight agents produced by brown-rot fungi for the degradation of wood carbohydrates by generating highly active radicals. The production of hydrogen peroxide and oxalic acid by Poria placent...
A-C Ritschkoff, M Rättö, J Buchert, L Viikari


Microbial decomposition of salt treated wood
1993 - IRG/WP 93-50001-22
Specialized microorganisms which are able to convert fixed inorganic preservatives from treated wood into water soluble components are investigated. A number of brown rot fungi like Antrodia vaillantii have been isolated from cases of damage and examined under unsterile conditions with CCA-, CCB-, CCF- and CC-treated wood at retention levels of at least 50% higher than recommended for wood in grou...
R-D Peek, I Stephan, H Leithoff


Degradation of lignin model compounds with coordinated copper in the presence of peroxide
1998 - IRG/WP 98-10282
A novel diffusible system capable of decomposing lignin model compounds with copper, coordinators and peroxides has been proposed. When pyridine was used as a copper coordinator, two synthetic dyes, Poly-R and RBBR were intensively decolorized with Cu(II) and H2O2 in aqueous solutions at room temperature. Although reactions with Cu(II) and H2O2 produce a strong oxidant, hydroxyl radical, via a Fen...
K Koller, K Messner, T Watanabe


Environmental risk assessment of treated wood - A mesocosm study
2005 - IRG/WP 05-50224-8
In order to evaluate the environmental impact of treated poles, we have developed physical models (mesocosms) containing around 250 kg of natural soil and a treated pole. On the top of each mesocosm, a spraying mechanism, which can distribute ultrapure water through several nozzles, was built. On the lower part of each mesocosm, a small tank, which can contain some litres of leachate, was placed...
P Marchal, F Poly


Degradation features of waterlogged archaeological compression wood
1998 - IRG/WP 98-10258
The degradation characteristics of waterlogged archaeological compression wood excavated in South Korea were examined by transmission electron microscopy (TEM) and confocal laser scanning microscopy (CLSM). Degradation of Pinus compression wood occurred mainly in the inner part of S2 layer. In contrast, the outer part of S2 layer remained relatively intact. CLSM and TEM showed the erosion type of ...
Yoon Soo Kim, A P Singh


The rôle of lignin in the nutrition of several Australian termites
1983 - IRG/WP 1191
The ability of Nasutitermes exitiosus (Hill), Coptotermes acinaciformis (Frogatt), Coptotermes lacteus (Froggatt) and Mastotermes darwiniensis (Froggatt) to degrade 14C-lignin preparations was examined. The lower termites were unable to degrade lignin. Nasutitermes exitiosus was able to cause a 5-8% degradation of hardwood lignins and a synthetic lignin. It failed to degrade the lignin of Pinus ra...
L J Cookson


A technique for the rapid assessment of wood surface degradation during weathering
1987 - IRG/WP 2281
Radiate pine (Pinus radiata D. Don) sapwood samples taken from four trees were converted into thin strips 100 x 10 x 0.085 (85 µm) mm³, (longitudinal x radial x tangential) in size and exposed in preweighed hatches to the weather inclined at 45° facing equatorially for 10, 20, 40, 60, 80 and 100 days. Significant (P < 0.001) weight losses occurred with time over the exposure period. Differen...
P D Evans, D Abbott, S Thein


The degradation of wood by metal fastenings and fittings
1972 - IRG/WP 302
As well as the hazards of biological decay, timber used in boat building is subject to the effects of chemical decay associated with the corrosion of metallic fastenings. The title has been deliberately chosen to emphasize that in wooden construction the troubles are not just those of corrosion of the fastenings, but also the destructive secondary effects on the wood caused by the products of the ...
L C Pinion


Microbial fouling of 10-40% naphthalene in creosote treated and untreated wooden pilings in the marine environment - A progress report
1980 - IRG/WP 455
In June 1978, Document No: IRG/WP/442 entitled &apos;Microbial Biofouling of 10-40% Naphthalene in Creosote Treated and Untreated Wooden Pilings in the Marine Environment" was released to the IRG members as a report on the early results of a long term (about 5 years) study of whether the naphthalene content of creosote was importart in protecting wood pilings in the marine environment from bor...
R R Colwell, A J Emery


Bacteria are important degraders of cooling tower timbers: New Zealand experience
1995 - IRG/WP 95-10128
Microscopic examinations of CCA-treated Pinus radiata timbers in industrial cooling towers in New Zealand showed bacteria and soft rot fungi to be primarily responsible for the decay of these timbers. Of these micro-organisms, erosion bacteria appeared to be most widespread, attacking wood cell walls independently as well as together with tunnelling bacteria and soft rot fungi. Tunnelling bacteria...
A P Singh, R N Wakeling


New approaches to practical evaluation method of bio-degradation of wooden construction - Non-destructive detection of defects using radar technique
2000 - IRG/WP 00-20214
There have been a number of researches and developments on the techniques and apparatus for the nondestructive evaluation of the biological deterioration in wood and wooden constructions, such as decay or insect attack in house, public buildings or in historically important architectures. As for the detection of the decay in wood, techniques using sound in audible or in ultrasonic frequency ranges...
Y Fujii, Y Komatsu, Y Yanase, S Okumura, Y Imamura, M Tarumi, H Takiuchi, A Inai


Lignin degradation by a non-enzymatic system supposed to be active in white rot fungi
2000 - IRG/WP 00-10340
Electron microscopic investigations have shown that ligninolytic enzymes of white-rot fungi are only able to penetrate the wood cell wall in late stages of degradation. Thus, the selective degradation of lignin of certain white-rot fungi can only be explained on the basis of a low molecular weight, highly diffusible system. A system, consisting of copper, a coordination compound and either H2O2 or...
P Lamaipis, W Gindl, T Watanabe, K Messner


Aspects of leaching
1976 - IRG/WP 267
With respect to Document No: IRG/WP/246, and the recommendation that an economic leaching test can be based on a non-changing volume of water (500 ml/block), I would like to relate our experiences with this suggestion. Following 14 days of continuous immersion in de-ionized water it was found that blocks treated with moderate and above concentrations of a preservative gave no problems, but those b...
R S Smith


Permanence of permethrin and bifenthrin in framing timbers subjected to hazard class 3 exposure
2005 - IRG/WP 05-30383
End-sealed Pinus radiata specimens measuring 235 x 90 x 35 mm were treated using a modified Lowry schedule with permethrin or bifenthrin in white spirit to Hazard Class 2 (H2) retentions. After conditioning, the specimens were exposed at 45o on north facing racks near Melbourne (Australia). Samples of the specimens were taken before installation, and after three and six months exposure. Analyses o...
A C Hunt, D G Humphrey, R Wearne, L J Cookson


Aspects of the fungal degradation of quaternary ammonium compounds in liquid culture
1997 - IRG/WP 97-30160
Didecyldimethylammonium chloride (DDAC) is a quaternary ammonium compound (QAC) that has found use as an anti-sapstain preservative for the transportation of softwood lumber from Canada to overseas markets. However, its use is limited by the knowledge that certain mould fungi seem capable of degrading it. The aim of this research was to gain knowledge about the fungal degradation of DDAC. The effe...
J W Dubois, J N R Ruddick


Immuno-electron microscopic localization of extracellular metabolites in spruce wood decayed by brown-rot fungus Postia placenta
1990 - IRG/WP 1441
Degradation by Postia placenta in spruce and birch wood was shown to occur not only in the wood cell wall but also in the middle lamellae region. Middle lamellae was often found to be degraded along the centerline so that cells could separate along this line. Extracellular membrane structures were found surrounding the hyphae and this matrix labelled positively with antisera produced to Postia pla...
Y S Kim, B Goodell, J Jellison


Respiration measurement of dry-rot
1995 - IRG/WP 95-10095
Methods for measuring the production of carbondioxide from wood infected with the dry-rot fungus were evaluated. By enclosing whole wood blocks and measuring the concentration of gas in the headspace by gas chromatography, an exponential increase in the concentration of CO2 was observed for at least 2 months. This technique could therefore present a method for evaluating various treatments of dry-...
L Toft


Susceptibility of painted wood to discolouring fungi - influence of binder, solvent and surfactant
1992 - IRG/WP 92-3714
Previous studies have shown that the basic composition of paints, without fungicide addition, can significantly contribute to the varying microbial susceptibility of painted wood. Previously, non-weathered water-borne acrylic paints applied to wood without a primer were shown to be more susceptible to mould attack than solvent-borne alkyd paints. The present study was initiated to reveal if this d...
J Bjurman, C Herder


Microbial tolerance and biodetoxification of organic and organometallic biocides
1990 - IRG/WP 1464
Ten organic and organometallic biocides were assessed for toxicity towards a range of wood decay and spoilage fungi. Minimum inhibitory concentrations indicated selective toxicity of biocides towards particular fungal types. Certain species of fungi demonstrated tolerance to a range of biocides. Further tests using the biocides in soil and wood enrichment cultures resulted in isolation of highly t...
P A Briscoe, G R Williams, D G Anderson, G M Gadd


Aboveground Microbial Decay Test of Biocide Treated and Untreated Wood Exposed to Danish and Humid Tropical Climates
2004 - IRG/WP 04-20306
A co-operative study was initiated to compare the aboveground field decay test of untreated and preservative-treated timbers under Nordic (Danish) and a representative humid tropical (Malaysian) environment according to CEN standard method. Matched specimens of untreated and both preservative-impregnated and surface-treated wood were simultaneously exposed at The Danish Technological Institute (DT...
A H H Wong, N Morsing, K H Henriksen, S Ujang


Alternative technologies for wood wastes recycling - Part A: Supercritical extraction of PAH compounds from wood wastes
1998 - IRG/WP 98-50101-18 a
Alternative technologies have been investigated to detoxify treated wood. Two classes of organic compounds are studied. Creosote-treated wood are classified in France as dangerous wood wastes. A conventional incineration could be provided for these wood wastes but the cost of this elimination could be very high (> 2000 FFR/ton). For these reasons, we have tested two kinds of new processes as al...
L Schrive, C Perre, G Labat


Extracellular substance from the white rot basidiomycete Irpex lacteus involved in wood degradation
1992 - IRG/WP 92-1571
Cellulases, phenol oxidase, and a substance that both produced and reduced H2O2 were isolated from cultures containing wood or glucose on which the white-rot fungus Irpex lacteus was growing. The rate of wood degradation by the fungus with different amounts of glucose in the medium was measured. More of the substance that produced and reduced H2O2 was found extracellularly in cultures containing w...
H Tanaka, T Hirano, G Fuse, A Enoki


Premature failure of CCA treated vineyard posts from brown rot
1993 - IRG/WP 93-10016
A survey of CCA (AWPA Type C) treated posts used as grape vine trellis supports, to determine the extent and type of decay was carried out at a terraced vineyard in the Hawkes Bay region of the North Island of New Zealand. Of 357 posts examined out of a total of 970 in the vineyard, 47% had moderate to severe decay or had failed, 20% had established decay, 10% had a trace of decay and 23% had no s...
R N Wakeling, A P Singh


Relationship between degradation of wood, cellulose or lignin-related compounds and production of hydroxyl radical or accumulation of oxalic acid in cultures of brown-rot fungi
1994 - IRG/WP 94-10062
The degradation activities of brown rot fungi against wood, cellulose, and lignin-related compounds were measured in cultures containing glucose or wood as a carbon source. Also the activities of one-electron oxidation and hydroxyl radical production and the amount of oxalic acid present in the cultures were measured. The degradation activities of the fungi against wood, crystalline cellulose and ...
S Itakura, T Hirano, H Tanaka, A Enoki


An investigation of the factors influencing the rate of deterioration of timber samples due to microfungi in laboratory tests
1997 - IRG/WP 97-20116
An investigation was performed into the comparative performances of test 1 (vermiculite burial) and test 2 (soil burial) as described in ENV 807. Two test preservatives were used - copper naphthenate and propiconazole. Copper chromate was included as a reference preservative. The wood species used was beech (Fagus sylvatica). Test 1 was performed using both a mixed inoculation of the five stipulat...
I J Herring, D J Dickinson, S M Gray, J K Carey