TRU-CORE Process for Treatment of Refractory Species and Engineered Wood Products
2011 - IRG/WP 11-40573
The TRU-CORE Process is a novel, chemically-based technology for rapidly delivering globally accepted wood preservatives and insecticides deep into the core of wood and wood-based composites in a waterborne carrier. Protectant materials which can be utilized with the TRU-CORE Process include a variety of carbon-based fungicides and insecticides. An important feature of the TRU-CORE Process is it...
A S Ross


In-situ experimental treatment and consolidation of degraded timber elements from a XIX century building
2012 - IRG/WP 12-10767
This paper presents the in situ experimental conservation work performed on three timber structural elements from a XIX century building: two floor beams and one roof beam. The palace was built in 1877 in the centre of Lisbon initially with residential purposes. It has four floors, with timber structural horizontal elements, stairs and roof beams (generally of Pinus sylvestris L.). The exterior wa...
D F Henriques, J de Brito, L Nunes


Effects of oil types and treatment temperature on the properties of wood subjected to thermal modification in oil medium
2012 - IRG/WP 12-40574
The effect of the use of oil as a medium of heat transfer during thermal modification of different species of wood has been widely investigated with different results accruing with regards to the various end-use properties of the materials. However very little have been done on the effect of oil types as well as its interaction with treatment temperature on the resultant properties of the material...
L Awoyemi, M M Apetogbor, A A Oteng-Amoako


Effect of preservative treatment on dimensional stability of plywood made of treated simul (Bombax ceiba) veneer
2012 - IRG/WP 12-40575
The dimensional stability such as thickness swelling and water absorption of plywood made of treated simul (Bombax ceiba) veneers were investigated after 2 hours and 24 hours soaking under water. The veneers were treated with hot water and cold water solution of borax-boric acid (1:1), neem leaves and mahogany seeds of different concentration (1:10, 1:20, and 1:40) at different treatment duration....
K Akhter, M Mahabubur Rahaman, A Ara


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Relationships between heat treatment intensity and some conferred properties of different European softwood and hardwood species
2012 - IRG/WP 12-40593
Effect of treatment intensity on conferred properties like elemental composition, durability, anti swelling efficiency (ASE) and equilibrium moisture content (EMC) of different European softwood and hardwood species subjected to mild pyrolysis at 230°C under nitrogen for different durations has been investigated. Independently of the wood species studied, elemental composition is strongly correl...
M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Post-Manufacture Biocide Treatment of Engineered Wood I-Joists
2012 - IRG/WP 12-40596
Engineered wood I-joists, fabricated from laminated veneer lumber (LVL) flanges and oriented strand board (OSB) webs, offer many advantages over solid sawn lumber joists in residential and light commercial construction. With the expanded use of these products has come an increasing need to be able to treat them with biocides to prevent attack from decay fungi and termites during service. Historic...
A S Ross, R W Clawson


Mechanical Properties of Hydrothermally Treated Beech Wood in Buffered Mediums
2012 - IRG/WP 12-40597
Hydrothermal treatment of beech wood in buffered mediums was carried out by aim of controlling the destructive effect of acids formed by degradation of carbohydrates on strength properties. Different mediums (water, buffer5, 7 and 8) and temperatures (160 and 180 °C) were used. Mechanical properties of specimens including modulus of rupture (MOR), modulus of elasticity (MOE) and toughness were de...
A Talaei A Karimi, K Yaghoobi, A Talaei


The Effects of Industrial-Scale Heat Treatment and Impregnation with Boron Compounds on Water Uptake and Tangential Swelling of Some Wood Species
2012 - IRG/WP 12-40599
This study evaluated the effects of boron impregnation and heat treatment on water uptake and tangential swelling of spruce (Picea orientalis), pine (Pinus nigra), beech (Fagus orientalis) and poplar (Populus deltoides) wood species. The samples (10 x 5 x 40 - tangential x radial x longitudinal cm) were impregnated with 4 % boric acid and 4 % borax according to the ASTM D-1413 standard method. Aft...
A Can, S Yildiz, Ü C Yildiz


Corrosion of fasteners in heat-treated wood – progress report after nine years’ exposure outdoors
2012 - IRG/WP 12-40601
The corrosion of common fastener materials now in use - mild steel, zinc-coated steel, aluminium and Sanbond Z-coated steel – has been evaluated after nine years’ exposure outdoors in untreated and heat-treated (thermally modified) spruce (Picea abies). Spruce from south-western Sweden was used. The heat-treatment was carried out in Finland by Stora-Enso Oy according to the ThermoWood process ...
J Jermer, B-L Andersson


Chemical Analysis of Hydrothermally Treated Beech Wood in Buffered Mediums
2012 - IRG/WP 12-40604
Hydrothermal treatment of beech wood in buffered mediums was carried out to study the effect of different mediums of heat treatment on crystallinity index of treated specimens due to degradation of carbohydrates. Different mediums (water, buffer5, 7 and 8) and temperatures (160 and 180 °C) were used. ATR spectra focusing on indexes of carbohydrates degradation obtained and analyzed. Results showe...
A Talaei, A Karimi


Environmental safeness of 60% and 72% concentrated CCA-C solution and paste for wood treatment
2012 - IRG/WP 12-50284
In this study 30-years practical and observational experience of the present author about using of 72% concentrated CCA-C paste for preparing treating solutions and for treating wooden poles, anchor logs and cross arms has revealed that the 60% concentrated CCA-C solution is superior to the 72% concentrated CCA-C paste regarding solubility, homogeneity, cleanliness, treatability, sludge formation,...
A K Lahiry


Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Copper naphthenate treatment for wood pols - a review and update
2012 - IRG/WP 12-30600
This paper reviews copper naphthenate (CuNap) and its utility as a treatment for wooden utility poles. One of the principal reasons that CuNap has gained market acceptance, in addition to its efficacy against decay fungi and wood-destroying insects, is its low mammalian toxicity. CuNap is a well-proven non-restricted use preservative, used extensively and specified for environmental reasons by ut...
J A Brient, M H Freeman


Study of the use of organosolv lignin as bio-preservative of wood
2012 - IRG/WP 12-30603
The service life of wood depends on the species, use and environmental conditions of exposure. The treatment of wood protects it against degradation by xylophagous agents, enhancing the durability of material up to 10 times, and reducing the deforestation around 12.5%. In this way, the use of treatments is necessary because increases the service life of material and protect against xylophagous age...
P S B dos Santos, A Garcia, P H G de Cademartori, D A Gatto, J Labidi


Treating Bambusa vulgaris with neem seed oil against basidiomycetic biodegradation
2012 - IRG/WP 12-30608
Realising maximum benefits from bamboo stems/culms in Nigeria are presently constrained by their almost non-acceptance for applications in most structural and construction purposes, except in comparatively low quality and some temporary applications, such as scaffolding, owing to their susceptibility to easy destruction by agents of biodegradation as a result of their poor inherent natural durabil...
A A Erakhrumen


Microwave Treatment of Frozen Wood Packaging Material
2012 - IRG/WP 12-40609
As part of the wood packaging material (WPM) regulation in international trade, the dielectric heating (DH) is soon to be included in ISPM15 (IPPC 2009) as an approved phytosanitary treatment. It has been considered that when using dielectric radiation (i.e. microwaves or radio-frequencies), reaching 60°C or more throughout the entire profile of the wood during at least 60s (i.e. 60°C/60s) ensur...
J-M Henin, A Bauduin, V Leemans, M Leyman, B Jourez, J Hébert


Development of a quality control assessment method to predict properties of heat treated wood
2012 - IRG/WP 12-40611
Heat treatment has been used to improve properties of non durable European species. Chemical modification of some of the wood components provides improved dimensional stability and biological performance against decay fungi while mechanical properties such as modulus of rupture are reduced. Quality control of commercially made thermally treated wood is one of the major challenges to allow its indu...
M Chaouch, K Candelier, S Dumarcay, A Pétrissans, M Pétrissans, P Gérardin


Effect of preservative treatment on mechanical performance of round and square poles made of small diameter Scots pine
2012 - IRG/WP 12-40612
A growing proportion of harvested Scots pine (Pinus sylvestris L.) timber originates from the first or second commercial thinning stands. There is a need to find economically viable and high quality wood products that can be manufactured from this raw material. Small log volume means not only demands of increased efficiency for material handling in logistics and manufacturing processes, but also c...
V Möttönen, R Stöd, K Heikkilä, H Heräjärvi


Differences between heat treated Pinus pinaster heartwood and sapwood
2012 - IRG/WP 12-40617
Heat treatment is a well known process to improve the durability and dimensional stability of less noble woods. The treatment can be applied for heartwood unlike the traditional treatments based on impregnation due to the difficulty of impregnating heartwood. Pure sapwood and pure heartwood samples were treated in an oven at 190ºC and 200ºC for 2h, 4h and 6h. Dimensional stability, measured a...
B Esteves, L Nunes, I Domingos, H Pereira


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


Pre-treatment decay and strength loss of railroad ties, and their prevention
2013 - IRG/WP 13-30610
Evidence of fungal decay in air-drying, untreated railway crossties is referred to as ‘stack burn’ in the industry. The deleterious consequences of stack burn on tie mechanical properties was confirmed by evaluating the impact bending toughness of wood samples taken from untreated tie stock air dried in the southern United States. These results suggest that careful consideration should be give...
A M Taylor, B Jordan, J D Lloyd


Methylene Chloride compared with white spirit as a treatment solvent for wood preservation – results from decay and termite studies
2013 - IRG/WP 13-30611
Non-aqueous solvents have a long history in the treatment of wood products in various parts of the world. The most familiar solvent treatment is the ‘light organic solvent preservative’ (LOSP) treatment based on low density solvents such as white sprit. Until recently white spirit was the only non-aqueous solvent approved for use in wood preservation in New Zealand. Australia also permitted...