Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Biological and mechanical performances of particleboard panels made from maritime pine (Pinus pinaster) and glued with cornstarch-mimosa tannin-urea formaldehyde adhesive
2011 - IRG/WP 11-40542
The objective of this work was to demonstrate the utility of cornstarch-mimosa tannin-based resins designed for application as an adhesive in the particleboard production. Bond qualities of cornstarch-mimosa tannin- urea formaldehyde (UF) (10:4:86, weight ratios) resins and commercial UF resin were assessed by using an automatic bonding evaluation system, prior to production of particleboard panel...
A Moubarik, F Charrier, A Pizzi, A Allal, B Charrier


Study of properties and application of Paulownia in wood industries
2011 - IRG/WP 11-40560
Important of required raw material supply regarding constraint in harvesting, increasingly population, change in consumption pattern and increasingly focus on wood products and per capita in consumption is obvious for anyone. Paulownia is a marvelous tree species with its characteristics of fast-growing, good Wood quality, multiple uses, wide-ranged distribution, easy propagation, deep root system...
M Akhtari


Effects of nano-silver on brittleness of heat-treated solid woods
2011 - IRG/WP 11-40572
The present study is aimed at the effect of heat-treatment of normal as well as nano-silver-impregnated Populus nigra, Populus deltoides, and Fagus orientalis on brittleness. Specimens were impregnated with 200 ppm water-based solution of nano-silver particles under 3 bars in a pressure vessel using empty-cell process. For heat treatment, both nano-silver-impregnated and normal specimens were kept...
H Reza Taghiyari, B Moradi Malek, A Karimi


Determination of Izod Impact Strength on Wood: A Suitable Method to Detect Fungal Decay in Protective Effectiveness-Screenings of Wood Preservatives
2012 - IRG/WP 12-20484
For testing a large number of different substances regarding fungicide properties, the reduction of the decay test duration is advantageous. In the present paper the suitability of a method for testing plastics using an impact testing machine was examined. The results clearly show that the fungal attack of European beech by the white-rot fungus Trametes versicolor leads to a decrease of izod imp...
H Delenk, M Zauer, A Wagenführ


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Effects Of Wood Preservative On Mechanical Properties Of Glulam Manufactured From Lower Density Malaysian Tropical Timber
2012 - IRG/WP 12-40590
This study is to investigate the effect of wood preservative on the mechanical properties of glulam timbers made from low density Malaysian hardwood timbers. Utilization of lower density Malaysian tropical timber for structural applications have not exploited extensively due to their inferior strength. By converting into treated glued laminated (glulam) timbers it could offer the possibility of th...
L Francis, Z Ahmad


Mechanical Properties of Hydrothermally Treated Beech Wood in Buffered Mediums
2012 - IRG/WP 12-40597
Hydrothermal treatment of beech wood in buffered mediums was carried out by aim of controlling the destructive effect of acids formed by degradation of carbohydrates on strength properties. Different mediums (water, buffer5, 7 and 8) and temperatures (160 and 180 °C) were used. Mechanical properties of specimens including modulus of rupture (MOR), modulus of elasticity (MOE) and toughness were de...
A Talaei A Karimi, K Yaghoobi, A Talaei


KERUING and APITONG: A Timely Review of the Perfect Choice Wood Species for Crossarms and Brace Arms, Including Data on Copper Naphthenate Treatments
2012 - IRG/WP 12-40603
Apitong or the wood species more commonly known as Keruing is an important tropical hardwood known for its high strength to weight ratio and its reasonable durability and preservative treatability. This wood has been exported from managed permanent forest estates in Malaysia into the United States for over 4 decades for its widespread use in wooden utility industry brace arms and crossarms, yet cu...
A Wong, M Freeman


Improvement of the biological performance and dimensional stability of two tropical woods by thermal modification
2012 - IRG/WP 12-40605
Pink cedar wood and rubberwood were thermally modified at 230°C in air for 4 h or for 8 h, and then subjected to bending, compression and hardness tests to evaluate the effect of the treatment on these mechanical properties. The biological performance of the modified wood was also determined, according to EN113, and the dimensional stability measured by means of the anti-swelling efficiency. The ...
M M González-Peña


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Wood Aging. Characteristics of aged Hinoki wood from Japanese historical buildings
2012 - IRG/WP 12-40610
Wood has always played a major role in Japanese traditional culture. More than 90% of buildings listed as a National property or a nationally important cultural property of Japan are constructed with wood. In the ancient capitals Kyoto and Nara, many traditional wooden buildings were inscribed as World Cultural Heritage of the UNESCO. The most famous and the world’s oldest wooden construction st...
M Yokohama, S Kawai


Differences between heat treated Pinus pinaster heartwood and sapwood
2012 - IRG/WP 12-40617
Heat treatment is a well known process to improve the durability and dimensional stability of less noble woods. The treatment can be applied for heartwood unlike the traditional treatments based on impregnation due to the difficulty of impregnating heartwood. Pure sapwood and pure heartwood samples were treated in an oven at 190ºC and 200ºC for 2h, 4h and 6h. Dimensional stability, measured a...
B Esteves, L Nunes, I Domingos, H Pereira


Pre-treatment decay and strength loss of railroad ties, and their prevention
2013 - IRG/WP 13-30610
Evidence of fungal decay in air-drying, untreated railway crossties is referred to as ‘stack burn’ in the industry. The deleterious consequences of stack burn on tie mechanical properties was confirmed by evaluating the impact bending toughness of wood samples taken from untreated tie stock air dried in the southern United States. These results suggest that careful consideration should be give...
A M Taylor, B Jordan, J D Lloyd


Copper leaching from copper-ethanolamine treated wood during exposure to terrestrial microorganisms
2013 - IRG/WP 13-30621
Copper-ethanolamine based wood preservatives are still the most important solutions for protection of wood in ground applications in Europe. Wood in ground is exposed to variety of organisms, which can act synergistically. In order to simulate these conditions in laboratory, Scots pine (Pinus sylvestris) specimens impregnated with copper-ethanolamine preservative of three different concentrations ...
M Humar, N Thaler, B Lesar


Effect of the nature of the inert atmosphere used during thermal treatment on chemical composition, decay durability and mechanical properties of wood
2013 - IRG/WP 13-40625
Wood heat treatment is an attractive alternative to improve decay resistance of low natural durability wood species. Nowadays, several types of thermal treatments of wood exist. These treatments differ mainly by the nature of the inert atmosphere used to avoid wood combustion which may correspond to: nitrogen, vacuum, steam or oil. Decay resistances as well as mechanical properties are strongly co...
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Combined effects of thermal modification and ACQ-D impregnation on properties of southern yellow pine wood
2013 - IRG/WP 13-40637
In this study, samples of southern yellow pine sapwood were first thermally modified and then treated by the alkaline copper quat-type D (ACQ-D) wood preservative. Two heating temperature (180℃ and 220℃) and two concentrations of ACQ-D solution (0.9% and 1.35%) were used in the experiments. The combined effects of thermal modification and ACQ-D on leaching performance, mechanical prope...
Wang Wang, Yuan Zhu, Jinzhen Cao


Investigation of Nanocopper-Hygrothermally Treated Wood Properties
2013 - IRG/WP 13-40644
Nanometals with high thermal conductivity can be considered as modifiers, especially in thermal modification of wood. This study was aimed to investigate some physical and mechanical properties of nanocopper impregnated Iranian beach (Fagus orientalis Lipsky), which was hygrothermally treated. For this purpose, nanocopper solution (400 ppm) was used for impregnation process. Hygrothermal treatment...
G Rassam, B Jamnani, A Faraji Heris


COST Action FP0904 – Increasing the Understanding of Thermo-Hydro-Mechanical Wood Behaviour and Processing
2013 - IRG/WP 13-40646
The polymeric components of wood and its porous structure allow its properties to be modified under the combined effects of temperature, moisture and mechanical action – so-called Thermo-Hydro-Mechanical (THM) treatments. Various types of processing techniques, including high temperature steam with or without an applied mechanical force, can be utilised to enhance wood properties, to produce eco...
D Jones, P Navi


Glue-bond strength of simul (Bombax ceiba) plywood made of Neem (Azadiracta indica) leaves treated veneers
2013 - IRG/WP 13-40647
The glue-bond qualities of plywood made of treated simul (Bombax ceiba) veneers were investigated. The veneers were treated with cold and hot water solution of neem (Azadiracta indica, A. Juss.) leaves of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated simul plywood ...
K Akhter, M A Hashem, S Akhter


Investigating the potential role of creosote oil for the water repellent purposes in fiberboards
2013 - IRG/WP 13-40635
Effect of wood steaming during fiber generation processes and creosote oil on the properties of fiberboard, manufactured from creosote treated solid wood were investigated. Pulp fiber was generated by alkaline pretreatment of waste creosote impregnated wood which being fiberized by laboratory defibrator, atmospherically. These fibers blended with 0, 15, 30, 45 and 100 percent by weight of wood...
M Sheikholeslami


Performance of recent and old Sweet chestnut (Castanea sativa) wood
2014 - IRG/WP 14-10816
Sweet chestnut (Castanea sativa) hardwood is one of the most durable European wood species. In the present research, various aspects that could potentially influence the durability were elucidated, namely: presence of extractives, ring width, and weathering. Simultaneously, properties of wood, which was in outdoor use for 35 years, were elucidated as well. The results indicate that ring width and ...
M Humar, M Žlahtič, N Thaler


Using Commercial Water Repellent Chemicals on Wood Protection
2014 - IRG/WP 14-30656
Lately, researchers have been looking for process and products that use environmental friendly technologies in wood protection. These sorts of innovations on wood protection should be carried out for wood evaluated at outdoor conditions. Using water repelling chemicals is one of those innovations which improve wood durability and dimensional stability by decreasing content of moisture. In this ...
G Köse, A Temiz, S Demirel, O E Özkan


Dynamic mechanical analysis (DMA) of nano cupric oxide (CuO) modified aqueous phenol formaldehyde (PF) resin
2014 - IRG/WP 14-40654
Phenol formaldehyde (PF) resins, modified by nano CuO incorporating alkane surfactant and polyvinyl alcohol (PVA) 17-99, were analyzed by dynamic mechanical analysis (DMA). The mechanical properties of its bonded plywood including tensile strength, modulus of rupture (MOR), modulus of elasticity (MOE) and shear strength under five test conditions were evaluated. Results indicated that the incorpor...
Wei Gao, Guanben Du