Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
Different methods are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring local or global moisture content (MC). Furthermore each measuring metho...
L Meyer, C Brischke, M Kasselmann, C Rösmann


Communities of mold fungi in moisture damaged building materials
2014 - IRG/WP 14-20542
The critical conditions needed for the development of mould and decay fungi have been modelled for different building materials. However, current knowledge of indoor microbes growing on building materials relies on culture-based methods and more advanced molecular biological techniques should be employed to study the complex microbial communities in building materials. In this paper molecular biol...
E Sohlberg, H Viitanen


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Ammoniacal Copper Zinc Arsenate Preservative Treated Wood Ties Their Performance in Testing and Track
2014 - IRG/WP 14-30636
While not a new preservative system, Ammoniacal Copper Zinc Arsenate (ACZA), had not previously been used to protect crossties. Its performance in treating difficult or refractory species of wood has been documented through its wide range of uses approved in AWPA. The establishment of appropriate testing for railroad material use was put in place and includes laboratory, field as well as commercia...
T Carey


Biocidal Products Regulation – Structure and Impact for Product Authorization and Testing in EU
2014 - IRG/WP 14-50308
Since September 2013 the Biocidal Products Regulations (BPR) has been in force in Europe. BPR replaces the Biocidal Products Directive (EC/98/8) and in some respect marks a turning point in the European legislation concerning registration of all types of biocides. BPR introduces some changes both for suppliers of active substances and for companies that produce and place biocide containing wood p...
M Klamer


Development of a rapid screening method to determine the susceptibility to mould growth of novel construction and insulation products
2015 - IRG/WP 15-20562
Wood-based materials are commonly used in building construction/insulation as a replacement for solid timber. However, these materials are susceptible to microbiological growth and different environmental conditions influence the vulnerability of wood-based materials. Moulds are a common problem found within homes and cause aesthetic damage, health problems and can increase material vulnerability ...
B K Stefanowski, S F Curling, E Mansour, G A Ormondroyd


Colonization of treated and untreated decking materials by bacteria, fungi and algae quantified by qPCR
2015 - IRG/WP 15-20568
The use of durable wood species for wood decking in outdoor applications, e.g. garden terrace (use class 3) is gaining more and more interest on the part of consumers and architects. To get detailed information on the practical use of deckings, a project was started in 2010. In total 71 different decking materials (0.03 m²) were installed and evaluated over 30 months. Beside other parameters, the...
E Stoyanova, B Schmöllerl, A Steitz, N Pfabigan, R Gründlinger


Performance of bio-based building materials – viewpoints from the first year of COST Action FP1303
2015 - IRG/WP 15-20572
Maintaining and expanding the market potential for bio-based building products in indoor and outdoor construction uses remains a key activity for industries in the forestry and biotechnological sector, particularly in Europe. Whilst there are ongoing activities within IRG for collecting and populating a database on performance on wood, the performance data for many other (i.e. non-wood) "environme...
D Jones


Above ground field testing: results of experiments in Brazil after one year
2015 - IRG/WP 15-30660
After the development of new products they need to be field-tested to assess their efficacy under diverse conditions of climate, comparing them with a preservative with proven efficacy. In some testing sites, decay occurs very slowly. The solution would be to bring these tests to locations that are conducive to biodeterioration, like tropical climates. Tropical sites provide higher temperature and...
M F Natale, J M Vidal


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Some comments on durability testing of WPC according to EN 15534-1
2015 - IRG/WP 15-40695
The standard EN 15534-1 (2014) gives advice for broad characterization of WPC materials and products. It contains instructions for test procedures concerning different properties e.g. mechanical properties, thermal properties, as well as durability. In this paper some WPC materials from the market were tested for their resistance against brown rot. Furthermore, the water uptake and bending prope...
S Bollmus, A Gellerich, H Militz


How does the test methodology influence the outcome of durability testing of thermally modified wood
2015 - IRG/WP 15-40699
Thermally modified wood is commercially available on the European market since many years. Today, many production units with various production capacities and different modification processes exist. Industrial scale wood heat treatment processes, under the trade name of ThermoWood were developed in Finland. ThermoWood has two standard treatment classes with different target properties, namely Ther...
A Gellerich, S Bollmus, H Militz


Evaluating the Effects of Post Dip-Treatment Laser Marking on Resistance to Feeding by Subterranean Termites
2016 - IRG/WP 16-10854
Dip-treatment of wood packing materials is often used instead of pressure treatment mainly because of issues relating to simplicity and cost. Packaging boxes fabricated for the United States Army are required to be dip-treated for at least one minute in an approved preservative solution prior to use. These boxes are expected to have a service life of up to 20 years in a wide variety of environment...
R A Arango, B Woodward, S Lebow


Global survey on durability variation – on the effect of the reference species
2016 - IRG/WP 16-20573
Climate change due to anthropogenic emissions is the largest environmental challenge of our time. Forest-based value chains play an important role in reducing the accumulation of CO2 in the atmosphere. Maximizing the use of wood to tackle climate change requires improved understanding of the service life of timber products. This information can best be obtained from field testing and while there i...
R Stirling, G Alfredsen, C Brischke, I De Windt, L P Francis, E Frühwald Hansson, M Humar, J Jermer, M Klamer, M Kutnik, P Laks, I Le Bayon, S Metsä-Kortelainen, L Meyer-Veltrup, P I Morris, J Norton, T Singh, J Van Acker, J Van den Bulcke, T M Venås, H Viitanen, A H H Wong


Moisture induced risk and fungal development in various field test set-ups in and above ground
2016 - IRG/WP 16-20577
A high number of studies on the decay performance of wood in outdoor exposure have been conducted in the past. However, no testing methodology for wooden components exposed above ground reflecting the variety of different loads has been established so far. Many test protocols were modified in different ways throughout the years and results were often published in an encoded or incomplete way. This...
L Meyer-Veltrup, C Brischke


Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


Evaluation of field test data
2016 - IRG/WP 16-20594
The resistance against fungal decay and insect attack of wood can be highly variable, between boards and even within boards. The variability in durability is not always an issue, but for high demanding applications information about its reliability is required. This comprises the variability of outdoor performance. Durability testing in laboratory and outdoor exposures can provide a good basis to ...
F Bongers, C Brischke, J Van den Bulcke, W Gard, I De Windt, H Militz


Effects of fungal exposure on air and liquid permeability of nanosilver- and nanozincoxide-impregnated Paulownia wood
2016 - IRG/WP 16-30680
Effects of aqueous dispersion of silver and zinc-oxide nano-particles on air and liquid permeability of Paulownia wood exposed to T. versicolor were studied in the present research project. Specimens were also heat-treated at 100 and 150°C and compared with the control specimens. Permeability values were measured when the moisture content of the specimens was 12%. Results showed significant incre...
H R Taghiyari, A Kalantari, M Ghorbani Kookandeh, F Bavaneghi, M Akhtari


The durability of manufactured structural building materials
2016 - IRG/WP 16-40718
The projected market potential for Engineered Wood Products such as CLT (cross laminated timber) is very positive however, potential prolonged rain leakage or moisture exposure during construction and in-service could pose considerable concern for its durability and reputation. This research was conducted to assess the decay resistance of CLT and OSB (oriented strand board) in an accelerated trial...
T Singh, D Page


Fabrication and characterization of MicroPCMs filled wood-plastic composites: Effects of polyethylene glycol on melamine–formaldehyde shell material
2016 - IRG/WP 16-40728
Microencapsulated phase change materials (MicroPCMs) containing dodecanol were fabricated using melamine-formaldehyde (MF) or polyethylene glycol 200 modified melamine-formaldehyde (PMF) resin as the shell materials by in situ polymerization. Wood flour/high-density polyethylene (WF/HDPE) composites with MF shell MicroPCMs (MF-MicroPCMs) or PMF shell MicroPCMs (PMF-MicroPCMs) were prepared, respec...
Xi Guo, Jinzhen Cao


The Environmental Impact of Timber Products Compared to other Building Materials - A Survey of Published Environmental Product Declarations
2016 - IRG/WP 16-50314
One of the positive aspects of using wood in construction is the environmental benefits that this can potentially bring. However, manufacturers of all construction products and materials make claims about the ‘environmental friendliness’ of their products, making it exceedingly difficult for the end user to make informed choices about the advisability of using one product over another. This st...
C Hill, J Dibdiakova


Lignin-Based Adhesive for Engineered Wood Products
2016 - IRG/WP 16-50319
Lignin as a naturally occurring polyphenolic compound has an excellent potential to replace petroleum-based phenol in formulation of phenol-formaldehyde adhesive that are used in manufacturing of engineered wood products. However, there are three major obstacles in application of polymeric lignin as phenol replacement: 1) low reactivity toward phenol, 2) high molecular weight, and 3) high polydisp...
I Kalami, M Arefmanesh, E Master, M Nejad


Efficacy of lignocellulosic materials for Removal of Cation and Anions from Industrial and Urban Wastewater
2016 - IRG/WP 16-50321
The adsorption of Ca, Zn, Na, Cd (II), Cr (III) and No3 ions from industrial and urban wastewater and aqueous solutions by poplar (Populusnigra) sawdust, cotton linter, zeolite and expanded perlite were examined on the basis of a batch adsorption technique. The results revealed that application of sawdust, cotton linter, perlite and zeolite are effective in improving elimination of Ca, Zn, Na ions...
M Akhtari, M Ghorbani Kohkandeh, H Borazjani


Estimation of wood degradation determined by visual inspection, mechanical testing and DNA characterisation – report after 3 years of exposure
2016 - IRG/WP 16-30700
The influence of two separate treatments, thermal modification and alkaline copper quaternary (ACQ, Silvanolin©) treatment, on fungal decay, visual disfigurement, deterioration in mechanical properties and fungal community structure was assessed on Norway spruce (Picea abies) and compared with the performance of two naturally more resistant tree species native to North America: Douglas fir (Pseud...
N Thaler, T Martinović, M Bajc, D Finžgar, H Kraigher, A Sinha, J J Morrell, M Humar