A comparison of rates of decay and loss in stiffness of radiata pine and Douglas fir framing lumber
2008 - IRG/WP 08-20378
Stiffness loss with time was recorded for untreated radiata pine and Douglas fir framing size lumber and preservative treated radiata pine which dad been pre-inoculated with Oligoporus placenta, a brown rot decay fungus isolated from decaying untreated radiata pine framing. Between stiffness measurements, samples were contained in a plastic tank located outside at ambient temperature. Index of Con...
M Hedley, D Page, J van der Waals


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Accelerated weathering of nine tropical wood species from Cameroon
2009 - IRG/WP 09-10705
The natural durability of tropical species for building components has been a subject of recent concern and questioning, mainly the resistance to weathering. Weathering resistance of nine tropical species from Cameroon, namely Azobe, Bilinga, Bubinga, Teak, Dousie, Moabi, Musanga, Sipo and Padauk were evaluated using an accelerated weatherometer for 2016 hours. Measurement of moisture fluctuation,...
S Pankras, Jinzhen Cao, D P Kamdem


Degradation of wood veneers by Fenton’s reagents: effects of low molecular weight phenolic compounds on hydrogen peroxide decay and tensile strength loss
2009 - IRG/WP 09-20400
Pine wood (Pinus sylvestris) veneers strips were incubated in acetate buffer containing hydrogen peroxide and iron to mimic mechanisms of brown rot decay and assess the degradation of cellulose through analysis of the tensile properties of the decayed wood. The tensile properties of thin wood strips treated with Fenton system reagents or precursors were determined and correlated to weight loss as ...
Yanjun Xie, R Well, Zefang Xiao, B Goodell, J Jellison, H Militz, C Mai


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp


Termite Resistant Properties of Wood and Natural Fiber Plastic Composites - AWPA E1 Test Data
2009 - IRG/WP 09-40466
This paper deals with resistance properties of wood plastic composites against Formosan Subterranean Termites (FSTs) based on the AWPA E1 test standard. Sixteen laboratory WPC formulations, four WPC commercial materials, and southern pine (Pinus sp.) wood control were tested for termite mortality, sample weight loss, and sample damage rating. The results show that FSTs did attack WPC products in ...
Q Wu, T Shupe, J Curole, K Ragon, M Voitier, M Freeman, D Ring


Photostabilization of Wood with Higher Molecular Weight UV Absorbers
2010 - IRG/WP 10-30524
Higher molecular weight UV absorbers were created by reacting the epoxy-functionalized UV absorber 2-hydroxy-4(2,3-epoxypropoxy)-benzophenone (HEPBP) with maleic, phthalic or succinic anhydride. The ability of the UV absorbers to photostabilize wood was then examined. FTIR-spectroscopy confirmed that HEPBP reacted with phthalic anhydride to create a polyester that preserved the UV-absorbing benzop...
P D Evans, M J Chowdhury


TMT–Interlab–Test to establish suitable quality control techniques - Structure and first results
2010 - IRG/WP 10-40503
As a result of growing quality demands from manufacturers and end-consumers of thermally modified timber (TMT) recent scientific research activities are increasingly focussed on modification mechanisms and by this on the development of suitable quality control methods. To deepen the knowledge in modification mechanisms and to obtain a larger variety of scientific data for TMT depending on the trea...
C R Welzbacher


Preliminary Observations of the Photostabilization of Wood Surfaces with Cerium Oxide Nanoparticles
2010 - IRG/WP 10-40504
Reactive transition metal compounds, wood modification and grafting of UV absorbers have all been used to photostabilize wood. Some of these approaches are promising, but the toxicity of certain reactive transition metal compounds and the cost of wood modification and grafting have restricted their commercial applications. Hence, more cost-effective and environmentally friendly methods of protecti...
Chunling Liu, A Ahniyaz, P Evans


Comparative Study of Heat Treatment of Beech Wood in Hot Water and Steam Medium
2010 - IRG/WP 10-40536
Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) in 180ºC were compared in physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated samples. Mechanical properties (MOR, MOE and CS)...
A Talaei, K Yaghoobi, A N Karimi


Wood decay enzymatic ability of Fusarium circinatum
2012 - IRG/WP 12-10777
There exists pathogens that attack standing trees of forests, and do not usually thrive once the tree is felled. However, occasionally they can be present in a latent state in the wood and can spread and affect new areas with economic, ecological and social consequences. Fusarium circinatum is a fungus that causes “pitch canker” in pine species, and is considered a quarantine organism within t...
M T Troya, F Llinares, Y Serrano, M Conde


Treating Bambusa vulgaris with neem seed oil against basidiomycetic biodegradation
2012 - IRG/WP 12-30608
Realising maximum benefits from bamboo stems/culms in Nigeria are presently constrained by their almost non-acceptance for applications in most structural and construction purposes, except in comparatively low quality and some temporary applications, such as scaffolding, owing to their susceptibility to easy destruction by agents of biodegradation as a result of their poor inherent natural durabil...
A A Erakhrumen


Pre-treatment decay and strength loss of railroad ties, and their prevention
2013 - IRG/WP 13-30610
Evidence of fungal decay in air-drying, untreated railway crossties is referred to as ‘stack burn’ in the industry. The deleterious consequences of stack burn on tie mechanical properties was confirmed by evaluating the impact bending toughness of wood samples taken from untreated tie stock air dried in the southern United States. These results suggest that careful consideration should be give...
A M Taylor, B Jordan, J D Lloyd


Comparison of moisture loss and its increment during the rehearsal process based on natural drying and water soaking application with or without sealing the trial discs of Common black poplar (Populus nigra L.)
2013 - IRG/WP 13-40639
This study was subjected to be set up to prove the pattern of moisture loss and moisture increment within the same wood samples prepared as the discs (30x23±3 cm diameter) with or without the bark intact during drying and in the duration of the water soaking application. In this concept, wood was exemplified by Common black poplar (Populus nigra L.) of the five 12 year old trees that are grown in...
I Usta


Effect of Nano-silver and Nano-copper and Nano-zinc oxide on Paulownia wood exposed to white-rot fungus
2013 - IRG/WP 13-30635
Paulownia is known as a fast growing tree and it can be used in several applications. The present study investigated the effect of Nano-silver and Nano-copper and Nano- zinc oxide on resistance of Paulowina (Paulownia fortunei) wood against the white rot fungus (Coriolus versicolor). Wood specimens with a dry density of 0.37g/cm3 were impregnated with a 400 ppm aqueous suspension of micronized na...
M Akhtari, M Ganjipour


Preliminary Investigation into the Natural Decay Resistance of Nigerian Grown Hevea brasiliensis and Mitragyna ciliata wood to Phanerochaete chrysosporium White-Rot Fungus
2018 - IRG/WP 18-10919
Wood is an important and versatile structural building material that finds applications in numerous uses. However, wood is also a biological material vulnerable to degradation by microbial activities; this is especially true in the tropics. Following the scarcity of highly durable species from our natural forests and the introduction of so many lesser used/durable wood species into the booming tim...
J M Owoyemi, U O Emmanuel


Self-Extinguishment Phenomena of Mass Timber in Medium-Scale Compartment Fires
2018 - IRG/WP 18-30729
This paper presents a review of the fire safety risks that mass timber construction may introduce in buildings, with special consideration to medium- and high-rise buildings. These main risks are represented by an effect to the classical fire safety strategy for buildings: (1) Compartmentalisation, to ensure that the fire will not spread farther than the compartment of origin, (2) Preventing verti...
C Gorska, J P Hidalgo


Using X-ray micro-CT to evaluate density loss in anobiid infested wood
2019 - IRG/WP 19-10956
Considering the relevance of wood borers in construction, the present study had as main objective the evaluation of the impact of anobiid damage on timber elements by establishing an empirical correlation between lost material percentage (LM%, consumed by beetles) and apparent density (original – OTD and residual – RTD). Since the beetles’ attack produces a diffuse damage with a set of tunne...
J L Parracha, M F Pereira, A Maurício, P Faria, L Nunes


Validation by micro-computed tomography of an assessment method to measure the residual strength of anobiids infested timber
2019 - IRG/WP 19-20650
In this article a quantitative correlation study of pine timber structural elements, which have been subject to attack by anobiids, is presented. The main objective of the study was to establish a valid empirical correlation between the lost material percentage (consumed by beetles) and original/residual apparent density. Since the beetles’ attack produces a diffuse damage with a set of tunnels ...
J L Parracha, M F Pereira, A Maurício, P Faria, L Nunes


Preservative Treatment of CLT: An Example at Shimojishima Airport
2019 - IRG/WP 19-30748
Cross laminated timber (CLT) is a relatively new construction method that allows multi-storey construction using solid wood instead of concrete or steel. It is a method favoured by progressive architects and recognized for its much lower environmental footprint. Wood is an excellent construction material and is a long-term carbon sink that also performs well in the event of earthquakes and fire....
J Lloyd, N Yamashita, A Taylor


Durability testing of mass timber building elements: a call for a collaborative trial
2019 - IRG/WP 19-40875
Mass timber buildings have captured the imagination of architects and engineers seeking more environmentally friendly building materials. The mass timber movement has tremendous potential to markedly increase timber use in mid-rise to high rise buildings. With great promise, however, comes great risk. Most mass timber structures that have been built or are being planned use no protective treatm...
J J Morrell


Durability of acetylated Radiata pine: Laboratory tests and performance in practice
2020 - IRG/WP 20-40899
Wood acetylation is an established process to enhance biological durability and dimensional stability of lower valuable wood species without the use of biocides. Acetylated Radiata pine (ACCOYA® wood) has been on the market for more than 10 years now, starting in 2007. Numerous lab tests have confirmed the high durability of acetylated Radiata pine. Here, additional data with four Radiata pine ...
K Jacobs, W Scheiding, B Weiß


Significance of the thermal design and the sorption isotherm shape in hygroscopic wood moisture dynamics and service life
2022 - IRG/WP 22-20682
Moisture dynamics are considered important for predicting the service performance of wood in exterior applications. Above a critical moisture content, water acts a softener on the structural polymer matrix of the wood cell wall, enabling the necessary diffusion of molecular species involved in the fungal degradation mechanism of wood. Water may enter solid wood in either liquid form or in vapor fo...
W Willems


Post-layup protection of mass timber elements in above ground protected exposures: 2-year results
2022 - IRG/WP 22-30766
Mass timber has seen increased use as a building material for low and mid-rise construction in recent decades. The durability of mass timber elements has not been fully examined and the effects of wood destroying organisms on this these materials merits attention. The effectiveness of currently labeled soil termiticides and passively applied biocides at post-construction or as remedial agents need...
M E Mankowski, T G Shelton, G T Kirker, J J Morrell


Previous Page | Next Page