IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3169 documents. Displaying 25 entries per page.


Natural resistance of Bamboo (Bambusa sp.) to marine wood-borers in Goa waters (India)
1993 - IRG/WP 93-10032
The paper deals with the natural durability of Bambusa sp. against the attack of marine wood-borers in Goa waters. Test specimens of this species were completely destroyed within a short period of nine months due to severe attack of borers indicating its very low natural resistance. Wood-borers involved were Martesia striata (Linnaeus), Nausitora hedleyi Schepman and Lyrodus pedicellatus (Quatrefa...
L N Santhakumaran, S G Sawant


Comparing the resistance of a number of lesser known species of tropical hardwoods to the marine borer Limnoria using a short term laboratory assay
2003 - IRG/WP 03-10500
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, durability was assessed by measuring the production of faecal pellets by ...
L M S Borges, S M Cragg, J R Williams


Effects of two wood preservatives and one water repellant on the settlement of fouling communities in a tropical marine environment
2002 - IRG/WP 02-30293
Observations made on recruitment of fouling organisms on treated panels exposed at an Indian harbour, Krishnapatnam on the east coast (Lat: 13028’ to 13059’ N; Long: 80010’ to 80016’ E) during November, 1997 to October, 1999 are reported and compared with fouling communities on control panels. Wooden panels of Erythrina variegata, Paraserianthus falcataria, Tetrameles nudiflora an...
B Tarakanadha, K S Rao


Some recent studies on the marine wood-borers of the west coast of India
1982 - IRG/WP 486
Occurrence and distribution of marine wood-borers along the west coast of India from Mangalore to Kandla are presented together with the distribution pattern of all the molluscan and crustacean wood-borers so far reported from India coasts. The survey, conducted for the first time along this coast, revealed the presence of 14 species of Teredinidae, 2 species of Pholadidae, 3 species and one varie...
L N Santhakumaran


Natural resistance of timbers to marine borer attack. A laboratory test with Limnoria tripunctata
1977 - IRG/WP 430
Attack of the timber specimens was much less severe in the laboratory than in some marine localities. This is not surprising. One reason is certainly that wood-boring molluscs (Teredinidae and Pholodidae) which were missing in the laboratory are the most important wood-destroying organisms in the open sea. Another reason is that it is not possible to offer the gribbles optimal environmental condit...
H Kühne


Examination of algal and wood extracts for the control of marine borers
1999 - IRG/WP 99-10306
Extracts obtained from a marine alga and white cypress pine (Callitris glaucophylla J. Thompson & L.J. Johnson) were examined for their ability to control marine borers. In a two week laboratory bioassay, filter papers were soaked in 0-8% extract concentrations, dried, and placed with Limnoria quadripunctata Holthuis in Petri dishes containing seawater. The 8% algal extract virtually prevented...
D Scown, L J Cookson, R De Nys


Natural durability of fifty species of Indian timber in Goa waters against marine wood-borers
1989 - IRG/WP 4150
Results of the investigations on the natural durabilitv of fifty species of Indian timber, based on data collected bv exposing test panels at Betim near Panaji (Goa) continuously for a period of 11 months are presented. The study revealed that none of the timber species tested has any natural resistance at this locality and all the panels were completely destroyed within 11 months. Details on the ...
L N Santhakumaran, S Udaya Bhaskar, J C Jain


Timber deterioration and its prevention in marine environment
2005 - IRG/WP 05-10559
Wood-borer activity is an established fact in Mumbai harbour that leads to severe deterioration of timber. In order to prevent the deterioration caused by wood borers three resin preservatives containing Zinc borate, Organo-copper polymer (4 wt% Cu) and Organo-Tin polymer Copoly(TBTM-MMA) were used for timber treatment. Test panels were treated using standard method and the...
B S Swami, M Udhayakumar, P Kumar, A B Samui


Screening techniques for potential wood preservative chemicals. Proceedings of a special seminar held in association with the 10th Annual Meeting of the IRG, Peebles 1978. Report No 136, 1979
1980 - IRG/WP 2138
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


Ability of chloropicrin, Vorlex, or methylisothiocyante to prevent marine borer attack of Douglas fir piling
1989 - IRG/WP 4153
The preservative-treated shell around Douglas-fir piling is an excellent barrier to attack by marine borers; however, damage to this shell can permit marine borer attack. The feasibility of using fumigants to enhance piling performance was examined by exposing fumigant-treated Douglas-fir sections in marine waters off Newport, OR, or Port Hueneme, CA. The piling were inspected annually and increme...
M A Newbill, J J Morrell


Controlling marine borer attack of timber piles with plastic wraps
1981 - IRG/WP 479
Plastic films 20 to 40 mils thick have been used for many years to wrap creosoted timber piles in service to protect them from attack by marine borers. As long as the wrap remains undamaged, this procedure provides complete protection to the pile. Properly applied, wraps generally provide protection for 25 yeara or longer. Polyvinyl chloride (PVC) and polyethylene (PE) films are specially formulat...
F Steiger, G Horeczko


Lab and field test results for wood treated with polymeric alkylphenol polysulfide
2001 - IRG/WP 01-30268
A new wood preservative based on polymeric alkyphenol polysulfide (PXTS-A) is being evaluated in a series of laboratory and field tests and the results continue to show promise. A modified formulation (PXTS-B), which contains additives to reduce the viscosity, is being evaluated along with the original formulation. Soil block decay tests comparing PXTS-B with CCA-C indicate that PXTS-B is equally ...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Observations on the destruction of fishing craft in India by marine wood-borers with special reference to the West Coast
1981 - IRG/WP 468
The paper highlights the economic importance of the destruction of fishing craft in India by marine wood-destroying agencies. The annual loss involved is to the extent of over 94 million rupees. Thirty-nine spectes and one variety of woodborer have so far been recorded from India, of which Bankia campanellata, Bankia carinata, Bankia rochi, Dicyathifer manni, Lyrodus pedicellatus, Teredo clappi, T...
L N Santhakumaran, J C Jain


Resistance of six timber species, treated with CCA and CCB, against marine borer attack in Goa waters (India)
1991 - IRG/WP 4166
Panels of Lagerstroemia speciosa, Toona ciliata, Olea dioica, Pinus insignis, Acrocarpus fraxinifolius and Borassus flabellifer, pressure-treated with a 6.6% solution of Copper-Chrome-Arsenic (CCA) and 6% solution of Copper-Chrome-Boric (CCB), were exposed along with untreated controls, in triplicate, in Goa waters to, assess their resistance to damage by marine borers. The control panels were all...
L N Santhakumaran, R V Krishnan


A collaborative test to determine the efficacy of polyurethane coatings on wood samples in the marine environment. 3rd Interim Report
1993 - IRG/WP 93-10046
The results of al long-term marine trial to assess the protective effect of polyurethane coatings on wood samples exposed at different sites around the world are reported. The condition of samples exposed in the sea for up to 88 months was generally sound, although instances of marine borer infestation were reported at two sites. At one site, mechanical damage of a non-biological nature is believe...
R A Eaton


Occurrence of wood-boring pholads in Kochi harbour waters (south-west coast of India)
1992 - IRG/WP 92-4175
The paper reports the occurrence of four species of wood-boring pholads (Pholadidae: Martesiinae), namely Martesia (Martesia) striata (Linnaeus), Martesia (Martesia) fragilis Verrill and Bush. Martesia (Particoma) nairi Turner and Santhakumaran and Lignopholas fluminalis (Blanford), in the Kochi back-waters, south-west coast of India. Of these Martesia nairi and Lignopholas fluminalis are now reco...
L N Santhakumaran, M V Rao


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Ten Year Marine Borer Exposure Trial of Chlorothalonil and Emulsified Preservatives in Australia
2003 - IRG/WP 03-30314
Results of a ten-year marine exposure trial at Townsville and Port Stephens are presented. Sawn Pinus radiata and natural round Eucalyptus obliqua specimens were treated with preservatives including creosote (HTC), pigment emulsified creosote (PEC), chlorothalonil, and the oil emulsions of CCA called PROCCA and HYCON. Basic zinc chloride treatment was also exposed at Townsville. Some of the findin...
L J Cookson, D Scown


Trust in the durability of preserved wood during and after the reclamation of the Zuiderzee
1987 - IRG/WP 4134
A firm belief in the durability of preserved wood must have existed during the reclamation of the Zuiderzee, because thousands of m³ have been utilized. The wood is exposed to attacks of marine borers and other organisms in the marine environment. Was this trust right or wrong? A recent examination was made of creosote impregnated pine posts after 65 years service in a dam, near the Barrier Dam a...
H Visscher


New ways of chemical wood preservation
1997 - IRG/WP 97-40087
Synergistic effects pertaining to wood preservation have been investigated by combining different polymerizing agents with modifying chemicals, modifying chemicals with known preservatives and new types of preservative chemicals with each other. One of the investigated methods is the use of impregnating solutions based on furfuryl alcohol (produced from biomass), in which the chemicals polymerizes...
M Westin, T Nilsson, B Ohlsson, R Simonson


Special seminar on screening techniques for potential wood preservative chemicals
1978 - IRG/WP 2113
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


Natural resistance of twenty-five timber species to marine borer attack in Goa waters (India)
1992 - IRG/WP 92-4178
Natural durability of 25 species of Indian timbers has been discussed, based on data collected from test panels exposed in Goa waters (west coast of India. for a period of 7 months. All the timber species, except Cleistanthus collinus, were heavily destroyed within 7 months on account of the combined attack by Martesia striata (Linnaeus) and Lyrodus pedicellatus (Quatrefages). Cleistanthus collinu...
L N Santhakumaran, G Srimannarayana, K Nagaiah


Rubber wood for fishing canoe construction
2005 - IRG/WP 05-40319
The rubber tree (Hevea brasiliensis) is cultivated for its latex and the wood comes as a by-product from the rubber plantations. The highly perishable nature makes it unsuitable for boat building. The Central Institute of Fisheries Technology, Cochin conducted laboratory and field studies with chemical preservative treated rubber wood and found that the durability of the wood increased considerabl...
L Edwin, S N Thomas, B Meenakumari


Fouling organisms as indicators of the environmental impact of marine preservative-treated wood
1995 - IRG/WP 95-50063
This study evaluates the use of fouling organisms (epibiota) to assess the environmental impact of preservative treated wood. This paper presents initial findings from treated panels exposed for 6 months at Sagres, Algarve, Portugal. Panels were treated with CCA, two copper-containing quaternary ammonium (ACQ) formulations and creosote, with nominal retentions from 10 to 40 kg/m³ (creosote 25 pcf...
R M Albuquerque, S M Cragg


Previous Page | Next Page