Relative performances of DNBP and CCA wood preservatives in accelerated decay tests
1988 - IRG/WP 3496
The effectiveness of 2-sec-butyl-4,6-dinitrophenol (DNBP) was compared with that of CCA. Test blocks of Pinus patula and Eucalyptus grandis were impregnated to precisely known retentions of approximately 3, 6, and 10 kg/m³ CCA and solvent-borne DNBP respectively. They were then challenged in decay tests comprising soil burial and exposure to monocultures of Chaetomium globosum, Coriolus versicolo...
W H Schnippenkoetter, L D Abraham, A A W Baecker


Natural resistance of different species of timber to marine borer attack in the Trondheimsfjord (Western Norway)
1978 - IRG/WP 435
Natural resistance of 34 timber species to marine wood-borers has been discussed, based on data collected from panels immersed in selected localities in the Trondheimsfjord during 1977-78. The wood-borers encountered on the panels were Psiloteredo megotara, Xylophaga dorsalis, Xylophaga praestans and Limnoria lignorum. The number of borers present and their growth were taken as the criterion for a...
L N Santhakumaran, J A Sneli


Examining environmental conditions and the biodeterioration of historic waterlogged wood: the Kolding Cog
2002 - IRG/WP 02-10441
Survival of waterlogged wood from thousands and in rare cases millions of years presents scientists with a unique opportunity to examine wood specimens which, due to select properties of the wood itself and/or the depositional environment, have not been completely degraded. This paper discusses the biodeterioration of a submerged shipwreck buried in Kolding Fjord, Denmark for the past 1000 years....
B A Jordan, D J Gregory, E L Schmidt


Movement and persistence of chloropicrin, Vapam, Dazomet and methylisothiocyanate in red and white oak timbers
1992 - IRG/WP 92-3728
This study describes the movement and persistence of four fumigants in sawn red and white oak timbers exposed out of ground contact for 2 years. Chloropicrin moved the furthest from the point of application, and was the most persistent. Vapam was next best, followed by Dazomet. Methylisothiocyanate (MIT), applied as pellets, was not effective, probably because MIT was lost from pellets prior to tr...
T L Highley


The yeast Pichia sp. As a short-term biological control agent to fungal spoilage of sawn softwood timber
2000 - IRG/WP 00-10362
Previous work has found isolates of the yeast Pichia to be a successful biological control agent toward moulding of fruits. An isolate was tested for the ability to protect sapwood of Pinus sylvestris timber against visual degrade by surface growth of moulds and staining fungi. Successful protection of autoclaved wood sprayed with a mixture of common wood moulding fungi was achieved when the yeast...
C Payne, H J Staines, A Bruce


Ten year field test with a copper-borate ground line treatment for poles
1993 - IRG/WP 93-30017
A wood preservative paste consisting of borax and copper naphthenate has been tested to determine its efficiency in protecting wood from decay fungi and insects. The paste was applied to polyethylene-backed wraps that were fastened to the below-ground portions of unseasoned southern pine pole stubs. After 4 years of exposure in Mississippi, the untreated control stubs were completely deteriorated....
T L Amburgey, M H Freeman


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Chemical analyses of IRG/COIPM INTERNATIONAL MARINE TEST (to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water) samples
1987 - IRG/WP 4114
Chemical analysis of CCA and CCB treated timber was carried out after exposure at tropical and temperate marine sites. Results indicated that losses of all elements had occurred. In particular, losses of boron were severe. Arsenic and copper were also lost. The chromium components in both formulations was the most dominant metal remaining. The results suggest that chromium modification was importa...
L E Leightley


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Durability of wood in the area of wood-inhabiting termites in Slovenia
1981 - IRG/WP 1139
This report describes a research dealing with resistance and durability of five different species of wood. The experiment was made in natural conditions in the Slovene area of wood-inhabiting termites. The results of our experimental field, which correspond to the results of the former laboratory experiments, show a very weak resistance of spruce-wood, fir-wood, and beech-wood. They also show thei...
L Kervina


An engineering model for the decay of timber in ground contact
2003 - IRG/WP 03-20260
To predict the residual strength of an engineered structure, it is first necessary to predict the effect of decay. A model was developed in which the effective area of structural decay in large section timbers was defined as that area that could be picked out with a pen-knife. Some limited studies indicated that for practical purposes the remaining wood could be assumed to have its full residual s...
R H Leicester, C-H Wang, M N Nguyen, J D Thornton, G Johnson, D Gardner, G C Foliente, C MacKenzie


Laboratory determination of the natural decay resistance of some lesser-utilized timbers from Tanzania against wood decay fungi
2004 - IRG/WP 04-10517
Four lesser known/utilized timber species (sap and heartwoods) from Tanzania, namely Albizia lebbeck, Zanthoxylum gilletii, Faurea saligna and Parinari curatellifolia were exposed to the brown rot fungi (Gloeophyllum trabeum and Coniophora puteana) and the white rot fungus (Coriolus versicolor) to determine their natural decay resistance according to the EN 113 standard procedure. The timbers were...
P R Gillah, R C Ishengoma, E Julias, S A Amartey, D H Kitojo


Fluoride woodpill
1987 - IRG/WP 3431
Decay problems of spruce joinery in the Netherlands in the 1960's and 1970's led to the introduction of preservative treatment. Because of the known penetration difficulties with Spruce, the results of the treatments were not always successful. The fact that the decay was found only in the joints led to development of the philosophy of "local preservation" of the joints in remedi...
J W P T Van der Drift, K J M Bonsen


Information from the COIPM Wood Group
1986 - IRG/WP 4130
The Chairman outlined the progress of the co-operative work "testing the resistance to marine borers of heat shrinkable polyolefin sheathings and of wood treated by vacuum/pressure with polymers (polystyrene)". The first part of the work has been started: the samples of wood wrapped with shrinkable polyolefin sheathings have been prepared and sent to the stations participating. The second part of ...
A Gambetta


Decay types observed in small stakes of pine and Alstonia scholaris inserted in different types of unsterile soil
1990 - IRG/WP 1443
The attack of various wood-degrading microorganisms occurring in mini-stakes of pine and Alstonia scholaris buried in various types of unsterile soil was studied. Attacks by white rot, brown rot, soft rot, erosion bacteria, tunnelling bacteria and actinomycetes were found. Soft rot occurred in all soils, whereas attack by white rot and especially brown rot and erosion bacteria was rare. The type o...
T Nilsson, G F Daniel


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


Soft rot decay of Eucalyptus maculata Hook. in different soils from Queensland, Australia
1980 - IRG/WP 1113
In the present work, different Queensland soils were chosen and their gross effects on the decay of treated and untreated Eucalyptus maculata examined. The soils were also amended with various levels of phosphate to study the response of the wood decay mycota to an increasing supply of this nutrient. Phosphate amendment was chosen because of the wide-scale use of superphosphate on Queensland soils...
L E Leightley, I W Russell


Effects of boron treatments on partially decayed oak and pitch pine heartwood
1996 - IRG/WP 96-30106
This paper reports results of borate based preservative treatment and leaching experiments on partially decayed oak and pitch pine heartwood. Previous experiments have shown little damage is caused to sound timber of these types when treated with Polybor and Boracol 20 preservatives. This experiment was carried out to assess the suitability of selected borate based preservatives for use in histori...
S McCutcheon, G M Smith, J W Palfreyman, P Durrant


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Role of cell wall structure in soft rot decay of bamboo
1995 - IRG/WP 95-10133
Models of soft rot hyphal penetration of bamboo cell walls are proposed. Soft rot hyphae show an interesting capability of penetrating the bamboo cell wall in different forms; typical longitudinal penetrating hyphae and tangentially orientated penetrating hyphae. The second form of penetration was found to be different from that normally associated with wood cell walls. The differences can be attr...
O Sulaiman, R J Murphy


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


Modelling the control of decay in freshly felled pine poles
1997 - IRG/WP 97-10206
In a recent study investigating control of decay in freshly felled pine utility poles, it became apparent that the efficacy of different treatment methods was strongly related to the size of the material being treated. A topical application of 5% w/v disodium octaborate tetrahydrate (DOT), brush applied to the cut surfaces of logs with otherwise intact bark was just as effective at excluding white...
M W Schoeman, W Van der Werf, J F Webber, D J Dickinson


Investigation of microwave as a means of eradicating dry rot attack in buildings
1992 - IRG/WP 92-1545
A microwave-apparatus developed for treatment of building-structures infested by dry rot was tested in the laboratory. The test-conditions simulated treatment of either infested timber or infested brickwork. Sawdust samples, both wet and dry, infested by viable mycelium of Serpula lacrymans were packed in glass-tubes. The tubes were then placed in the middle of either 20 cm thick wooden beams or 3...
C Kjerulf-Jensen, A P Koch


An evaluation of CCA, CCB and CCP preservatives using a "sandwich test"
1991 - IRG/WP 2370
The last two years has seen some important changes in standards and preservative types used in Scandinavia, which have led to a wider choice for specifiers. In order to identify those treatments suitable for replacement or reinforcement of decayed constructional timbers, it was felt necessary to modify the standard EN 113 test. Impregnated blocks were sandwiched between two untreated blocks, previ...
A P Koch, L B Sheard


Previous Page | Next Page