Leachability And Decay Resistance of Copper-Treated Wood
2004 - IRG/WP 04-30337
Samples of scots pine sapwood (Pinus sylvestris L.) were treated with solutions of (Copper II sulfat-5 hydro + fluoroboric acid) and (Copper II sulfat-5 hydro + fluoroboric acid + boric acid) in order to determining to leachability and decay resistance against brown rot fungus (Postia placenta) and white rot fungus (Coriolus versicolor). Results indicated that the copper in treated wood is less s...
A Temiz, T Nilsson, I Deemirtas, Ü C Yildiz


Bending properties of TCMTB-treated Southern pine sapwood using supercritical carbon dioxide impregnation process
1997 - IRG/WP 97-40080
The effects of elevated pressure and treatment with thiocyanomethylthiobenzothiazole (TCMTB) on the bending properties of Southern pine sapwood were evaluated at pressures ranging from 1,800 to 3,600 psi. All bending properties were affected to some extent by supercritical fluid treatment. Modulus of elasticity and work to maximum load were not significantly affected by pressure levels. Modulus of...
Gyu-Hyeok Kim, S Kumar, E S Demessie, K L Levien, J J Morrell


Comparative moisture uptake of Douglas fir and radiata pine structural lumber when exposed to rain wetting as an indicator of relative decay resistance
2004 - IRG/WP 04-20285
Trials were undertaken to determine the relative resistance of radiata pine and Douglas-fir to wetting when exposed to the weather. Douglas-fir samples were obtained from one Central North Island and three South Island sources and had a heartwood/sapwood mix typical for each resource. Radiata pine sapwood and heartwood samples were obtained from a Central North Island source. Material was exposed...
M E Hedley, G Durbin, L Wichmann-Hansen, L Knowles


Efficacy of linear chain carboxylic acid anhydrides as wood protection chemicals
2002 - IRG/WP 02-30295
This paper presents an assessment of the effectiveness of linear chain carboxylic acid anhydrides namely, acetic, propionic, butyric, valeric and hexanoic anhydride, in improving the decay resistance of Corsican pine (Pinus nigra Schneid) sapwood. Wood-anhydride bond formation was verified by the increase in sample weight and volume. A brown rot fungus [Coniophora puteana (Schum.:Fr)] was selec...
A N Papadopoulos, M D C Hale, C A S Hill


Serviceability of copper naphthenate-treated poles
2000 - IRG/WP 00-30214
Copper naphthenate-treated poles in service were inspected for deterioration, penetration, retention, and serviceability. The study to date has included poles in all hazard zones in the United States. Poles installed by 12 different utilities and eight different treating companies are included in the survey. Both southern pine and Douglas-fir poles and distribution and transmission poles are inclu...
H M Barnes, M H Freeman, J A Brient, C N Kerr Jr


Termite and decay resistance of particleboard composed of white cypress pine and radiata pine
1997 - IRG/WP 97-10200
Phenol-formaldehyde bonded particleboard was manufactured from blends of non-durable radiate pine (P. radiate) and heartwood of the naturally durable species, white cypress pine (C. glaucophylla). Board specimens were subjected to bioassays using two termite species, M. darwiniensis and C. acinaciformis, and the basidiomycete fungi, C. puteana and P. ostreatus, and the durability of specimens was ...
P D Evans, J W Creffield, J S G Conroy, S C Barry


Attempt for developing a new method for above ground field testing of wood durability
2000 - IRG/WP 00-20199
Field testing remains the most appropriate way for evaluation of wood preservatives or natural durability of wood species. Above ground tests are designed to answer specific questions concerning the outdoor utilisation of wood. Such methods supply additional information and confirm or reject preliminary laboratory results. The European standard (ENV 12037, "lap-joint") for assessment of the durabi...
N Terziev, M-L Edlund


Presteaming radiata pine heartwood to improve treatability
1983 - IRG/WP 3239
Steaming and holding before preservative treatment by the Bethell process greatly improved the treatment of radiata pine heartwood. Maximum penetration of preservative for the shortest holding period was obtained by the use of steam vacuum but the difference between this and steam venting was small when compared with the standard of treatment of air dried samples. A holding period of one day was s...
A J Bergervoet


The efficacy of Sentry® as a treatment for the control of sapstain in pre-infected radiata pine
2001 - IRG/WP 01-30260
Experiments were conducted to determine the efficacy of Sentry® when used to control sapstain fungi on radiata pine branch billets stored under high fungal hazard conditions. Prior to antisapstain treatment, the billets were pre-infected with a mixed inoculum of staining fungi and held from zero to 10 days at 25°C and 75% relative humidity. This was done to produce billets with different degrees...
C Chittenden, J G van der Waals, B Kreber, R N Wakeling


An evaluation of chemical treatments for the protection of radiata pine logs from fungal degrade
1986 - IRG/WP 3377
Busan 30, Busan 1009, Mitrol PQ375. and sodium pentachlorophenoxide (NaPCP) plus have been evaluated as antisapstain treatments for the long-term protection of debarked radiata pine logs. After 3 months' winter-spring storage, treated debarked logs had less surface and internal sapstain than 'control' logs. After 6 months' storage all logs had internal sapstain ...
J A Drysdale, M E Hedley, J A Butcher


Field tests of preservative-treated radiata pine in Japan
1995 - IRG/WP 95-30083
Test stakes of radiata pine treated with various alkyl ammonium compound (AAC) formulations and with copper-chrome-arsenate (CCA) as reference preservative were installed in 3 test sites in Japan in 1981-82. When inspected in 1995, CCA-treated stakes showed less decay at all three sites than stakes treated with other formulations. Ammoniacal copper quaternary (ACQ)- treatment was only slightly les...
M E Hedley, K Tsunoda, K Suzuki


Effect of mobile fungicides on fungal pre-infection in radiata pine billets.
1999 - IRG/WP 99-30191
In New Zealand, fungal infection of logs begins directly after felling and whilst severe degrade can be prevented if antisapstain-treated within 24 hours, such short turn-around times of logs are not always practicable. However, conventional antisapstain formulations in use only provide an envelope of protection on the log surface but are unable to control pre-infections below the surface. The obj...
D R Eden, T Singh, B Kreber


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


Effect of angle of exposure on degradation of radiata pine during weathering trials
1988 - IRG/WP 2301
The importance of angle of exposure on the degree of weathering of materials has not been adequately resolved. In conventional tests, specimens are exposed at an angle of 45° facing the equator, but more recently experiments on polymeric materials have suggested that an angle of 0° may be preferable since this angle maximises levels of received ultra-violet radiation. In this paper the degradati...
P D Evans


The influence of copper (II) chemicals on the weathering of treated wood. Part 1: ACQ treatment of wood on its weathering
1994 - IRG/WP 94-30040
Wood weathering can be accelerated by alkylammonium compound (AAC) treatment, and slowed by ammoniacal copper quat (ACQ) treatment. This study aims at investigating the influence of ACQ treatment of wood, especially the present of copper (II), on its weathering. ACQ, CCA and DDAC treated microtomed sections of southern yellow pine earlywood were prepared and naturally weathered for five periods, t...
Ruiying Liu, J N R Ruddick, L Jin


Effect of Scytalidium lignicola on decay resistance and strength of wood
1994 - IRG/WP 94-10061
We reported previously that in laboratory tests, pretreatment of Douglas-fir and Southern Pine blocks with Scytalidium lignicola prevented decay. In the present work, we determined 1) the ability of Scytalidium lignicola to colonize and survive in wood exposed in the field, 2) the decay resistance of blocks removed from previously treated Scytalidium lignicola wood and 3) the effect of Scytalidium...
T L Highley


The effect of water-repellent additives on the leaching of CCA from simulated southern Yellow pine decks
2000 - IRG/WP 00-50158
End-matched SYP boards were pressure-treated with CCA or CCA in combination with commercial water repellent additives. After fixation and drying, the boards were placed in plastic boxes and exposed outside in Harrisburg, NC. Plastic supports were used to keep the boards above the water collected. Over a period of five months, rain run-off water from 14 natural rainfalls were collected and analyzed...
F Cui, P J Walcheski


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


MDF manufactured from blends of cypress pine and radiata pine shows enhanced resistance to subterranean termite attack
2001 - IRG/WP 01-40214
Medium density fibreboards consisting of blends of the naturally durable wood species white cypress pine (Callitris glaucophylla) and non-durable wood species were manufactured in a commercial plant and subjected to a bioassay using the subterranean termite species, Coptotermes lacteus. A board composed of 30% cypress pine, 30% slash pine (Pinus elliottii) and 40% of the naturally durable hardwood...
P D Evans, S Dimitriades, C Donnelly, R B Cunningham


Chemical evaluation of borate treated pine sapwood attacked by the subterranean termite Coptotermes acinaciformis
1993 - IRG/WP 93-20003
Sapwood of hoop (Araucaria cunninghamii Ait. ex D. Don) and slash (Pinus elliottii Englem.) pines were treated by Vacuum Pressure Impregnation (VPI) to provide test specimens. The concentration of boron was defined by chemical analyses of the timber, in the zone of primary attack by the termite being bioassayed. A common method of definition of preservative retention, weight uptake of preservative...
A R Moffat, B C Peters


Influence of concentration, catalyst, and temperature on dimensional stability of DMDHEU modified scots pine
1998 - IRG/WP 98-40119
Dimethyloldihydroxyethyleneurea (DMDHEU) is being used in textile industry to improve wrinkle recovery. Trials on solid wood have been performed to minimise swelling of the wood. This paper focuses on the effect of various types and concentrations of catalyst and reaction temperature on the dimensional stability of Scots pine. Three different catalysts, NKS (based on magnesium chloride), 3282 (bas...
M Van der Zee, E P J Beckers, H Militz


A light and electron microscopic study of decayed CCA-treated radiata pine (Pinus radiata) wood from a cooling tower
1994 - IRG/WP 94-10056
An inspection of an industrial cooling tower in New Zealand showed surface decay of 12 year old Pinus radiata wood panels treated with CCA preservative to a retention of around 15 kg/m³ of salt. Wood decay micromorphology typical of that caused by soft rot fungi, white rot fungi, 'stripy' and 'v-shaped' erosion bacteria and cavitation bacteria were all commonly...
A P Singh, R N Wakeling, D R Page


Termite-tunnels formation on the surface of termite-resistant wood species in field sites
2001 - IRG/WP 01-10400
In this report, termite-tunnels formation by the subterranean termite, Coptotermes formosanus Shiraki on the surface of termite-resistant wood species, namely, Hinoki (Chamaecyparis abtsu), Yoshino Hinoki (Chamaecyparis abtsu), Miyazaki Hinoki (Chamaecyparis abtsu), Hiba (Chamaecyparis abtsu) and Japanese cedar (Cryptomeria japonica) was conducted in field sites. Westernhemlock (Tsuga heterophylla...
Y Kadekaru, K Kinjo, S Yaga


Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


Soft rot decay in acetylated wood. Chemical and anatomical changes in decayed wood
2002 - IRG/WP 02-40231
Acetylated Beech (Fagus sylvatica) and Scots Pine (Pinus sylvestris) wood were studied in soil beds under laboratory conditions for longer periods. High mass losses and dynamic MOE losses were measured in non-acetylated wood and at lower weight percent gains (WPG). Rapid losses of lignin, holocellulose and ?-cellulose occurred in non-acetylated beech wood and no losses were detected at the highest...
B Mohebby, H Militz


Previous Page | Next Page