IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 469 documents. Displaying 25 entries per page.


A comparative field test of the effectiveness of anti-sapstain treatments on radiata pine roundwood
1986 - IRG/WP 3376
Peeled radiata pine posts were sprayed with one of six antisapstain formulations, with and without a wax water-repellent additive, to evaluate the protection given by each treatment. After 3 months' outside storage the best treatments tested were 4% product Busan 30, 2% product Busan 1009, and 2% active sodium pentachlorophenoxide (NaPCP) with 1.5% borax. After 6 months' storage ...
J A Drysdale, R M Keirle


Studies on the biological improvement of permeability in New Zealand grown Douglas fir
1983 - IRG/WP 3231
This report outlines progress towards optimizing conditions for water storage of New Zealand grown Douglas fir with the aim of improving permeability to water-borne preservatives, in particular CCA. Small scale laboratory tests are in progress but the need to scale up to potential commercial applications is being considered. Mixed populations of bacteria isolated from 10 week water sprinkled Dougl...
K J Archer


Experimental test site to prevent maritime pine logs from bluestaining: water-spraying and water-immersion methods
2003 - IRG/WP 03-10497
Following a storm which led to windfall wood, a research project was launched to develop preservation methods with a low environmental impact for maritime pine logs. These preservation methods are intended to be suitable for large-scale storage areas of maritime pine. In addition the aim was to maintain wood quality during long term storage. An experimental field test with 1 900 m3 of maritime pin...
I Le Bayon, H Callot, D Reuling, C Brunet, P Castéra


The rate of redistribution and loss of leachable preservatives under service conditions
1993 - IRG/WP 93-30026
This paper describes experiments carried out to determine patterns of preservative redistribution and any associated losses which occur when wood containing unfixed water-soluble wood preservatives is exposed to service conditions where leaching is possible. Scots pine sapwood treated with disodium octaborate was used as a model system. Results are recorded and discussed for trials representing pa...
R J Orsler, G E Holland


The isolation of actinomycetes from wood in ground contact and the sea
1980 - IRG/WP 1110
M S Cavalcante, R A Eaton


Biodegradation of creosote/naphthalene-treated wood in the marine environment
1977 - IRG/WP 428
The present study was undertaken to determine the biodegradability of marine grade creosote and selected components, including naphtalene, and to determine the effectiveness of (up to 40%) creosote in protecting wood from microbial attack. Also, the impact(s) of creosote and naphtalene-enriched creosote on the microbial ecology os estuarine environments was examined....
P A Seesman, R R Colwell, A Zachary, A J Emery


Report on marine borer attack on some timbers treated with CCA wood preservative and exposed for three months in sea-water
1985 - IRG/WP 4112
Destruction of timbers by marine borers has long been a problem for the coastal population of Thailand. The use of heavy durable timbers with frequent maintenance, or total replacement, is the only solution for fishermen with their fishing craft or marine installations, meanwhile wharves or other large scale constructions are usually made by using concrete pilings or concrete casings. In recogniti...
A Rananand, W Yoosukh, U Sittiphuprasert


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


Treatment of particleboard with isocyanate resin to impart improved dimensional stability and water repellency
2000 - IRG/WP 00-40178
Standard particleboard panels (for interior use) of 16 mm nominal thickness were cut into samples measuring 6.4 mm x 78 mm2. The samples were divided into 4 end matched batches. Two batches were treated with isocyanate resin and cured. The other 2 batches were left untreated. One of the treated batched and 1 of the untreated batches were edge sealed with epoxy resin prior to isocyanate resin appli...
K M Filcock, P Vinden


Creosote movement from treated wood immersed in fresh water: Initial PAH migration
2003 - IRG/WP 03-50201
Creosote has a long history of successful use as a wood preservative, but polycyclic aromatic hydrocarbons (PAHs) in this preservative have raised environmental concerns, particularly when creosote-treated wood is used in aquatic environments. A number of models have been developed to predict the risk of creosote use in aquatic environments, but one limitation of these models is a lack of data o...
Sung-Mo Kang, J J Morrell, J Simonsen, S T Lebow


Computerised data acquisitioning, handling and processing in wood preservation studies
1984 - IRG/WP 2218
The computerisation of data acquisitioning, handling and processing in weathering studies on wood treated with protective coatings is discussed. An integrated system comprising a data base, statistical package and a custom written graphical processor is explained. Two treatments are compared and the correctness of a mathematical weathering model is evaluated....
T Rypstra, K Vos


Surface coatings for impregnated wood
1992 - IRG/WP 92-3684
The use of proper surface coatings enhances the aesthetic and protective properties of impregnated wood. Good results with especially water-borne coatings have been obtained for class-A impregnated L-joints and claddings in field tests started in 1982....
L Kotama


The window joinery test hut
1975 - IRG/WP 257
D F Purslow


Collaborative soft rot tests: Proposed amendments to Document No: IRG/WP/208
1973 - IRG/WP 224
J K Carey, J G Savory


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


Examination of timbers from the Mary Rose in storage
1988 - IRG/WP 4149
Timbers from the Tudor ship, Mary Rose, have been examined for the presence of fungal fruiting structures. Wood specimens were also examined for the presence of microbial decay patterns using light and scanning electron microscopy. Structural timbers were surveyed using the Pilodyn for an overall picture of the extent of decay. Mary Rose timbers were predominantly inhabited by marine fungi. Fourte...
R Mouzouras


Technique for monitoring absorption during a vacuum pressure process
1992 - IRG/WP 92-3696
A laboratory technique was developed and an apparatus constructed which allowed for the direct and continuous measurement and observation of volumetric uptake of water-borne preservative into wood samples throughout a controlled vacuum-pressure treatment process. Fractional filling of void space was calculated. Graphing (fractional saturation) against time allows prediction of optimum cycle length...
A J Pendlebury, J A Petty


A comparison between methods for evaluating the water repellency of wood
1989 - IRG/WP 2328
Wood specimens treated with a number of water repellent formulations have been tested for their water repellency according to four laboratory test methods, based on weight increase, swelling and contact angle measurements, in order to assess the degree of agreement between the different methods. Treatments representing formulations with a wide range of water repellent efficiency were tested both i...
R Nussbaum


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


300 years water-logged wood: Treatability with CCA-C
1998 - IRG/WP 98-40103
The treatability of 300 years water-logged and recent wood (Abies bornmülleriana M.) was assessed by dip treatment and vacuum and pressure cycling with CCA-C. Treatment runs were evaluated on the basis of weight gain retention and radial and tangential penetration measurements. The preservative penetration and retention levels in the 300 years water-logged wood were higher than in the recent wood...
S N Kartal, N Yilgör


Leaching tests - A paper for discussion
1973 - IRG/WP 221
J W W Morgan


Improvement of liquid penetration of wood by precompression under appropriate conditions and recovery process
1993 - IRG/WP 93-40014
A new system for enhancing the penetration of liquid into wood using a precompression treatment was designed, and the effects of compressive deformation and recovery on liquid uptake were evaluated. Precompression of up to 60% under appropriate moisture and heat conditions effectively increased the penetration of liquid into refractory wood samples of practical sizes without producing any strength...
I Iida, Y Imamura


Assessment of contamination of soil and water at a CCA treatment plant: A demonstration project
1996 - IRG/WP 96-50067
Soil, sludge, dust and water samples were collected at a copper/chromium/arsenic wood preservation plant. Contamination of soil, sludge, dust and surface water with copper, chromium and arsenic was detected. Levels of contamination were sufficiently high to require remediation. Contamination originated from preservative solution dripping from recently treated wood. Migration of contaminants was vi...
P N Durrant, D C R Sinclair, G M Smith


Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Previous Page | Next Page