Investigations concerning liquid absorption of six heartwood species
2013 - IRG/WP 13-40618
In order to determine the liquid absorption and the penetration different heartwood species were treated with a boric acid containing solution. Heartwood of six wood species (Fir, Spruce, Douglas fir, Scots Pine, Oak and Black locust) were used in these investigations whereby the dimension corresponds to the EN 252 format. One half of the stakes were end sealed before treatment. All stakes were im...
E Melcher, J Zwiefelhofer


Field performance of wood impregnated with siloxanes using supercritical carbon dioxide
2013 - IRG/WP 13-40632
This paper presents preliminary results from a 13-month field test containing pine sapwood samples (Pinus sylvestris) impregnated with a mixture of siloxane and organic biocides using supercritical carbon dioxide as carrier. Samples were exposed above ground at a Danish field test site using matched non-treated sapwood controls for every treated sample. All samples were painted before exposure. Pi...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Comparison of moisture loss and its increment during the rehearsal process based on natural drying and water soaking application with or without sealing the trial discs of Common black poplar (Populus nigra L.)
2013 - IRG/WP 13-40639
This study was subjected to be set up to prove the pattern of moisture loss and moisture increment within the same wood samples prepared as the discs (30x23±3 cm diameter) with or without the bark intact during drying and in the duration of the water soaking application. In this concept, wood was exemplified by Common black poplar (Populus nigra L.) of the five 12 year old trees that are grown in...
I Usta


Effect of bio-resin from cashew nut shell liquid (CNSL) on decay resistance properties of wood
2013 - IRG/WP 13-40649
This study assesses the decay resistance properties of bio-resin modified wood against decay fungi of the Basidiomycota according to the EN 113 protocol. A bio-resin system was developed by ozonolysis process from cashew nut shell liquid (CNSL), a naturally occurring mixture of phenolics. Small wood blocks from sapwood of Scots pine (Pinus sylvestris), Obeche (Triplochiton scleroxylon) and Gmelina...
M Ashaduzzaman, M D Hale, V Tverezovskiy, G A Ormondroyd


Investigating the potential role of creosote oil for the water repellent purposes in fiberboards
2013 - IRG/WP 13-40635
Effect of wood steaming during fiber generation processes and creosote oil on the properties of fiberboard, manufactured from creosote treated solid wood were investigated. Pulp fiber was generated by alkaline pretreatment of waste creosote impregnated wood which being fiberized by laboratory defibrator, atmospherically. These fibers blended with 0, 15, 30, 45 and 100 percent by weight of wood...
M Sheikholeslami


Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
Different methods are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring local or global moisture content (MC). Furthermore each measuring metho...
L Meyer, C Brischke, M Kasselmann, C Rösmann


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Using Commercial Water Repellent Chemicals on Wood Protection
2014 - IRG/WP 14-30656
Lately, researchers have been looking for process and products that use environmental friendly technologies in wood protection. These sorts of innovations on wood protection should be carried out for wood evaluated at outdoor conditions. Using water repelling chemicals is one of those innovations which improve wood durability and dimensional stability by decreasing content of moisture. In this ...
G Köse, A Temiz, S Demirel, O E Özkan


Field performance of wax treated wood
2014 - IRG/WP 14-30649
The durability and outdoor performance of wax treated Scots pine sapwood was investigated in above ground field tests. Therefore wood impregnated with three different waxes was exposed in horizontal lap-joint test which is running since eight years. Durability, wetting resistance and the susceptibility to checking has been investigated. In summary, all wax treated wood performed better compared to...
C Brischke, E Melcher


Hydroponic Phytoremediation of Chromated Copper Arsenate (CCA) and Copper Contaminated Water
2014 - IRG/WP 14-50304
The removal of selected metals by duckweed (Lemna minor) and parrotfeather (Myriophyllum aquaticum) from a simulated aqueous environment contaminated with Chromated Copper Arsenate (CCA) and copper sulfate was studied in a controlled laboratory experiment. The duckweed and parrotfeather’s tissues were analyzed to evaluate the removal of copper (Cu), chromium (Cr), and arsenic (As) from CCA cont...
C Keith, H Borazjani, S Diehl, Y Su, Fengxian Han, B Baldwin


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao


Effect of Nano-Wollastonite on Water Absorption in Particleboard
2014 - IRG/WP 14-40662
Effects of wollastonite nanofibers on physical properties of particleboard were studied. Nano-wollastonite (NW) was applied at 5, 10, 15, and 20 g/kg, based on the dry weight of wood-chips, and compared with control specimens. Two application methods of NW were used: surface application (SA), and internal application (IA). Density was kept constant at 0.68 g/cm3 for all treatments. Tests were carr...
S Karimi, H Reza Taghiyari, A Karimi, P M Tahir, J Abdul Halip


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


The Physical Properties of Heat Treated Fir Wood and Outdoor Durability
2014 - IRG/WP 14-40677
Wood might be easily susceptible to degrade by biotic and abiotic factors. Therefore, wood should be protected from fungi, insects and other degradation factors by applying treatment methods. Especially, for the wood have used in the external environment. Chemical treatment methods have some disadvantages such as use of toxic chemicals (Arsenic and chromium) and treatability of refractory wood spe...
O E Özkan, H Vurdu, A Temiz, G Köse


Experiences with an industrial system for controlled thermal wood modification in pressurized unsaturated steam
2014 - IRG/WP 14-40678
Thermal wood modification in pressurized reactors has a long history, but these processes are to date industrially scarcely used, because of the relatively complicated process equipment, compared to the more common high-temperature processes in kilns at atmospheric pressure. However, based on our practical experience with the FirmoLin® process, supported by recent scientific findings, it is foun...
W Willems


Lignin Modification to Produce Sustainable Polyurethane Resin for Wood Coatings
2014 - IRG/WP 14-40682
The use of lignin as the most abundant aromatic natural polymer has been evaluated for use in the production of lignin-based polyurethane resin for coating applications. Coatings are made of resins (ca. 50%), which today are mainly derived from petroleum-based polymers. This study is focused on the development of an environmentally friendly method of modifying lignin to be used as source of natura...
M Nejad, M Arefmanesh, S Chandra, J Mostaghimi, E Master


Leachability and Dimensional Stability of Nanosilver-Steamed Densified Poplar
2014 - IRG/WP 14-40684
This study was aimed to investigate leachability and dimensional stability of nanosilver impregnated poplar (Popolus alba), steamed before hot compression. Wood samples were impregnated with nanosilver suspension (200 and 400 ppm) under pressure of 4 bar for 20 minutes. Steam treatment was carried out at 150°C for 2 hours. Then samples were compressed (33%) radially in a hot press at 170°C for 3...
G Rassam, A Talaei, A Ahmadi


Development of a rapid screening method to determine the susceptibility to mould growth of novel construction and insulation products
2015 - IRG/WP 15-20562
Wood-based materials are commonly used in building construction/insulation as a replacement for solid timber. However, these materials are susceptible to microbiological growth and different environmental conditions influence the vulnerability of wood-based materials. Moulds are a common problem found within homes and cause aesthetic damage, health problems and can increase material vulnerability ...
B K Stefanowski, S F Curling, E Mansour, G A Ormondroyd


Some comments on durability testing of WPC according to EN 15534-1
2015 - IRG/WP 15-40695
The standard EN 15534-1 (2014) gives advice for broad characterization of WPC materials and products. It contains instructions for test procedures concerning different properties e.g. mechanical properties, thermal properties, as well as durability. In this paper some WPC materials from the market were tested for their resistance against brown rot. Furthermore, the water uptake and bending prope...
S Bollmus, A Gellerich, H Militz


Buffered Amine Oxide Treatment Systems for Imparting Water Based Azoles/Insecticides in Douglas Fir and Eucalyptus
2015 - IRG/WP 15-40707
In today’s world, wood remains the most versatile, practical and sustainable building material. In contemporary countries, wood is a well-managed renewable resource that has a remarkably small carbon footprint compared to those of steel, aluminium, composites, and concrete. These alternative materials have continued to emerge as viable building materials given the durability issues of untreate...
R W Clawson Jr


Outcomes deal to impregnability of Eucalyptus globolus L. wood after microwave treatment
2015 - IRG/WP 15-40712
Microwave treatment of wood has been used with several aims in many studies as drying, enhancement of pulp properties, angle fibre detecting, density evaluation, etc., and also to improve permeability of wood. Eucalyptus globulus Labill. is a refractory species which is spreading its use as solid wood for construction in Spain. Studies of different ways to improve their impregnability (uptake and ...
A Vega, E Hermoso, M T Troya


Effects of fungal exposure on air and liquid permeability of nanosilver- and nanozincoxide-impregnated Paulownia wood
2016 - IRG/WP 16-30680
Effects of aqueous dispersion of silver and zinc-oxide nano-particles on air and liquid permeability of Paulownia wood exposed to T. versicolor were studied in the present research project. Specimens were also heat-treated at 100 and 150°C and compared with the control specimens. Permeability values were measured when the moisture content of the specimens was 12%. Results showed significant incre...
H R Taghiyari, A Kalantari, M Ghorbani Kookandeh, F Bavaneghi, M Akhtari


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti


A Comparison on Penetration of Silica Sol in Scots pine and Southern pine wood
2016 - IRG/WP 16-40722
Penetration is one of the most important issues to be considered in wood impregnation with various kinds of chemicals in liquid form. Scots pine (Pinus sylvestris) and Southern pine (Pinus spp.) are two frequently used wood species for treatment, such as preservative treatment. With the development of treating systems, some micro- or nano-sized aqueous modifiers are emerging in the market, which p...
Mingyang Sun, Jinzhen Cao


Influence of pressure phase impregnation time on the uptake and distribution of wood preservatives in Scots pine material of diverse treatability
2016 - IRG/WP 16-40752
In spite of the general opinion that Scots pine sapwood is easy to impregnate considerable variations in treatability are reported. In order to study impregnation results of diverse Scots pine sapwood treated with increasing process times, Scots pine sapwood from two different predefined treatability groups was impregnated. A copper solution was used as impregnation agent in ten different vacuum p...
K Zimmer, B Kerfriden


Previous Page | Next Page