Design of a laboratory method for evaluating the effectiveness of soft rot preservatives
1988 - IRG/WP 2312
This purpose of this work was to design a method which makes it possible to evaluate the effectiveness of products which present protect wood against soft rot, using new products·of a different nature, on wood of·Pinus sylvestris L. and Fagus sylvatica L., and which, suitably applied, avoid big economic losses deriving from lack of knowledge of the active principles suitable to present protect w...
M T De Troya, A M Navarrete


The efficacy of polymer/preservative treatments in soil-bed exposure
1992 - IRG/WP 92-3729
Southern pine was treated with CCA, CCB, sodium borax/boric acid, or disodiumoctaborate, alone or in combination with an acrylic polymer system containing a water repellent. Treated samples were subjected to an unsterile soil burial test. The addition of polymer reduced the weight loss in borontreated samples at the lower retentions but not at the higher retention. Results with borates indicate th...
R J Murphy, H M Barnes, S M Gray


Preliminary evaluation of the answers to the 2nd IRG/WP-questionnaire on the state of pollution control in the field of wood preservation
1982 - IRG/WP 3209
This preliminary evaluation of the answers to the 2nd IRG/WP-Questionnaire only gives a general survey on those questionnaires which the author received until April 30th, 1982. Details, such as correlations between importance of wood preservation and pollution control, as well as a comparison of the answers with those to the first questionnaire (Doc. IRG/WP/369), could not be considered due to lac...
H Willeitner


Improvement in dimensional stability against water of the main Spanish timbers impregnated with water repellent organic protectors
1988 - IRG/WP 3468
The study reported the increase of dimensional stability against water of the main Spanish timbers, both broadleaved and coniferous, after impregnation in the autoclave with organic protector, with contains 33.3% water repellent waxes and resins. The proposed Spanish standard, U.N.E. n° 56541 is used, where dimensional stability of the impregnated wood is expressed as a% of that of the non-impreg...
J A Rodríguez Barreal


New principles for the protection of wood: Impregnation with waterborne resins
1995 - IRG/WP 95-40047
The environmental impact of classical wood preservatives as well as the use of tropical wood species with high natural durability is regarded increasingly critically in the public. Therefore other partially new principles for the protection of wood, like chemical modification, or treatment with resins were examined especially in USA, Japan and in Europe with promising results predominantly in the ...
A O Rapp, R-D Peek


Dura-Treet II, a water dispersible pentachlorophenol
1980 - IRG/WP 3165
During the past several decades, penta petroleum wood treating has become increasingly popular. Penta is an effective chemical compound against wood organisms causing decay and rot, is safe to handle, also clean and easy to use. In terms of preservative cost, it has been and remains by far the least expensive of the three major preservatives. However, when the cost of petroleum carrier is added, t...
D B Hatcher


The effect of a chelator mediated fenton system on activation of TMP fibres and decolorization of synthesized dyes
2004 - IRG/WP 04-50223
The purpose of this work is to improve our current knowledge of the non-enzymatic mechanisms involved in the brown rot degradation of wood, but also to study the potential applications of a chelator-mediated Fenton system in activation of wood fibers and decolorization of synthesized dyes. In this work, Electron Spin Resonance (ESR) spin-trapping techniques were used to study the generation of hyd...
Yuhui Qian, B Goodell, J Jellison


Effect of a water repellent additive on the performance of ACQ treated decks
2000 - IRG/WP 00-40168
The performance of a water repellent (WR) additive formulated for use with ACQ has been evaluated. The water repellency of wood treated with this formulation was studied in laboratory and field tests. The change in moisture content of ACQ/WR treated boards under field exposure conditions is compared with that of CCA/WR treated boards. Although the water repellency of the ACQ/WR system is lower tha...
F Cui, A R Zahora


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 19: Report on the condition of specimens at Sekondi, Ghana after 42 months
1984 - IRG/WP 4109
The results of the first formal inspeation of CCA- and CCB- treated test panels exposed at Sekondi, Ghana, in June 1980, are presented. All untreated control panels of both reference and local species have been destroyed. Of the% CCA- treated specimens, only those of Pinus sylvestris (reference species) and Mitragyna stipulosa (local species) have not been attacked. 3% CCB-treated local species ha...
F F K Ampong


Mobility and bioavailability of wood preservation chemicals in soil - actual field measurements
1998 - IRG/WP 98-50101-11
Wood material intended for outdoor use is often impregnated with chemicals to withstand attack from fungi and bacteria. Both inorganic and organic substances are used to protect the wood, and they are used in a toxic and bioavailable form. At wood preservation facilities severe soil contamination can be encountered due to spills and deposition of sludge, especially at old sites. Two sites, one whe...
S Andersen, G Rasmussen


Health and safety regulations on the use of wood preservatives in Switzerland
1980 - IRG/WP 3148
There is not any doubt that the chemical protection of wood (besides the architectional-constructional wood protection) is of utmost importance for the increase of the durability of technically used timber. The toxic properties of wood preservatives make certain legal regulations necessary for the protection of human beings, animals and the environment. Thereby wood preservatives fall under the po...
O Wälchli


Diffusion and interaction of components of water-borne preservatives in the wood cell wall
1988 - IRG/WP 3474
This study investigates the rates of diffusion and ultimate distributions of copper and arsenate components of wood preservatives in wood cell walls following vacuum treatment. Adsorption studies of copper on red pine (Pinus resinosa) and trembling aspen (Populus tremuloides) wood confirm the importance of cation exchange reactions on the ultimate distribution of copper in the wood substance and i...
P A Cooper


The relationship between basic density and liquid absorption in fast, plantation grown 8 Year Old Eucalyptus pellita and E. Urophylla
2002 - IRG/WP 02-40220
The liquid absorption characteristics of 8 year old Eucalyptus pellita and E. urophylla were studied in order to gain insight into the treatability of this young, fast grown eucalypt plantation resource. The trees were grown in an experimental plantation trial near Innisfail in northeast Queensland. The study demonstrated that average sapwood basic density in young plantation grown E. pellita a...
J Norton, A Muneri


Optimisation of an analytical method for the determination of total fluoride in preservative-contaminated soils using water steam distillation and an ion-selective electrode
1999 - IRG/WP 99-20153
This paper describes a simple modified procedure for the quantitative fluoride determination of different origin in a soil matrix using a water steam distillation and an ion-selective electrode. Distillation methods generally require a preliminary preparation step like fusing. The modified method presented here is based on the direct distillation of fluoride so that no further sample preparation i...
E Melcher


The susceptibility of acetylated Pinus radiata to mould and stain fungi
1992 - IRG/WP 92-1548
The aim of this investigation was to determine the effect of 5, 10, 15 and 20 percent acetylation weight gains on the susceptibility of Pinus radiata sapwood to mould and stain fungi, and to establish if an acrylic paint, an oil-based stain and a water repellant gave superior protection from fungal growth on wood treated to 20% acetylation weight gain, compared to untreated wood. One treatment set...
R N Wakeling, D V Plackett, D R Cronshaw


Biosorption of metals for wood waste effluent clean up
1997 - IRG/WP 97-50090
The common filamentous fungi can sorb metal ions from aqueous solutions. The biosorption of metal ions like copper Cu2+, chromium Cr6+ and arsenic As5+ by dead fungal mycelia was investigated. Two industrial fermentation byproducts are tested: Mucor miehei and Aspergillus oryzae. The adsorption of metal ions depends on parameters such as chemical treatment of fungi before biosorption (acid or basi...
S Legay, G Labat


Recovery of copper, chromium, and arsenic compounds from the waste preservative-treated wood
1991 - IRG/WP 3651
In Japan, about 40 percents of waste wood is incinerated and the residue is dumped into the landfill site. The waste preservative-treated wood, which is mixed in nontreated wood, is incinerated in the same way, too. However, it will cause the serious problems that the gases contained with high concentration arsenic compounds are discharged from the smokestacks of the incineration facilities and th...
A Honda, Y Kanjo, A Kimoto, K Koshii, S Kashiwazaki


Comparison of Temporal Changes in Metal Leaching and Aquatic Toxicity from Wood Treated with CCA and Alternative Preservatives
2005 - IRG/WP 05-50236
This study compares the temporal variation of chemical leaching and aquatic toxicity of wood treated with chromated copper arsenate (CCA) and other copper-based wood preservatives (alkaline copper quaternary (ACQ), copper boron azole (CBA), copper citrate (CC) and copper dimethyldithiocarbamate (CDDC)). Treated wood blocks were leached for 21 days and the leachate collected was analyzed for prese...
B Dubey, T G Townsend, G Bitton, H M Solo-Gabriele


Electrochemical deterioration of wood in sea-water
1981 - IRG/WP 464
In the specialistic literature only few items can be found dealing with the specific kind of wood deterioration called electrochemical corrosion of wood. This deterioration occurs predominantly on marine vessels, yachts, and other marine craft where wood is jointed by means of various metal connectors. Up to date information demonstrates that in wood surrounding copper connectors, when in proximit...
J Raczkowski


Weathering trials on natural wood finishes in New Zealand
1986 - IRG/WP 3383
The weathering properties of various transparent and semi-transparent exterior finishes for New Zealand-grown radiata pine are currently being examined. After 12 to 16 months' weathering, unpigmented water repellents have failed to provide satisfactory protection from weathering under field test conditions. With the exception of two formulations, penetrating oil-based stains are already s...
D V Plackett, C M Chittenden


Copper based water-borne preservatives: Copper adsorption in relation to performance against soft rot
1987 - IRG/WP 3452
As part of a fundamental study concerned with the performance of copper based water-borne preservatives the adsorption of copper from aqueous solutions by 4 hardwood and 1 softwood species has been studied. Experiments were conducted to determine the influence of solution pH, solution concentration and solution temperature. The results obtained were consistent with an acid form ion-exchange mechan...
P M S Rennie, S M Gray, D J Dickinson


Remediation of wood treatment sites in Finland
1999 - IRG/WP 99-50139
Finnish legislation in connection with soil contamination are firstly waste management legislation and secondly public health legislation and water legislation. There is no separate legislation concerning soil protection or remediation. The Ministry of the Environment has published a proposal for official contaminant guideline values to be used both as criteria for contamination and clean-up targe...
S Salonen


A report of the Technical Recommendations documents for the Canadian Wood Protection and Preservation Facilities and an environmental study of storm water runoff from anti-sapstain treatment plants
1988 - IRG/WP 3478
With the completion of the Final draft of the Technical Recommendations (TR) documents for the Wood Preservation and Wood Protection Industry, there are naturally questions on what is expected from these documents and how Environment Canada and Provincial regulatory agencies may interact with the wood preservation industry. In general, it is expected that the Canadian Wood Preservation and Protect...
G Das, V N P Mathur


Preservative treatment of green timber by soaking in ammoniacal copper borate
1984 - IRG/WP 3292
Freshly sawn boards of radiata pine sapwood were preservative treated by soaking in ammoniacal copper borate. Optimum schedules were obtained by partially seasoning the boards for one week prior to treatment. This aided the absorption of preservative and reduced the required soaking time to approximately 2 hours. Complete boron penetration was obtained after one week of block storage under cover a...
P Vinden, A J McQuire


Mechanical properties of CCA-treated southern pine after post-treatment kiln drying
1989 - IRG/WP 3543
This report reviews current research dealing with the effects of waterborne preservative treatment and redrying on the mechanical properties of wood. In general, waterborne preservative treatments reduce average mechanical properties. This effect is exaggerated when treated wood is kiln-dried after treatment, especially at elevated temperatures. For lumber, recently completed research at the Missi...
H M Barnes, J E Winandy