Effect of soil parameters on biocide depletion: laboratory and field studies of water- and emulsion-borne preservatives
2000 - IRG/WP 00-30234
Two field test sites with different soils were selected. Soil analysis showed that the soil at the two sites had considerable texture, base saturation, acidity, and cation exchange capacity differences. Five sets of field stakes were treated as follows: three with water-borne CCA to about 0.4 pcf (6.4 kgm-3) retention, one with 0.75% DDAC, and one with 0.75% DDAC:0.25% chlorothalonil. The last two...
T Schultz, D D Nicholas, D E Pettry, M G Kim


Moisture uptake and volumetric swelling as probable factors also affecting leaching in CCA-treated wood. A preliminary study of treated Eucalyptus saligna sapwood
2003 - IRG/WP 03-30318 IRG/WP 03-30318
A number of factors affecting leaching of CCA from treated wood have been variously investigated and discussed. However, the possible effects of moisture movement in treated timbers on leaching have not received attention yet. The present study examines and compares moisture uptake and volumetric swelling in CCA-treated and untreated sapwood of Eucalyptus saligna, and tries to establish a correl...
R Venkatasamy


Effectiveness of copper/chromium salts as wood preservatives against Limnoria tripunctata Menzies in laboratory tests
1977 - IRG/WP 431
During the last joint meeting of IRG and COIPM a co-operative programme of tests with copper/chromium salts as wood preservatives against marine borers was discussed and agreed. In this connection the results of a laboratory test in the BAM with Limnoria tripunctata Menzies will be of interest. But as the respective paper is written in German (H. Kühne; G. Becker: Laboratoriumsversuche über die ...
H Kühne


Development of a turbidity method for the determination of water repellent in CCA treatment solutions
2000 - IRG/WP 00-40177
The use of aqueous water repellent emulsion formulations has increased significantly in the wood treatment industry. These are primarily used to enhance the weathering characteristics of wood products treated with water borne preservatives systems used in exterior above ground exposures. However, they are also used in pole treatments to improve the climbing characteristics and in low VOC millwork ...
P J Walcheski, L Jin


Influence of pre-swelling conditioning on swellometer results for CCA and water repellent additive treated wood
1997 - IRG/WP 97-20125
The pre-test moisture content and conditioning history of wafers cut from wood treated with CCA and an emulsion water repellent additive can dramatically influence swelling curves generated using a standard swellometer apparatus. The rate of water uptake and swelling increased significantly as wafers were dried to lower moisture contents prior to immersion swelling. The pre-swelling conditioning h...
A R Zahora


Investigation on different variation factors in the results of mycological test and means to reduce and avoid them
1986 - IRG/WP 2264
In order to clarify the causes of the dispersion observed in the results obtained with mycological tests made in accordance with standard EN-113, different factors assumed to be sources of the variations were studied. These included the moisture content of the test samples during the test, the influence of certain technological properties of the wood, the virulence of the fungus strains, the metho...
D Dirol


Evaluation of the corrosivity of the treated wood - Laboratory vs field test methodologies
2000 - IRG/WP 00-20211
The corrosivity of treated wood to fasteners has been evaluated using laboratory test procedures, including AWPA Standard E12-94. The standard method was modified in order to allow detailed study of commercial metal fasteners in terms of sample types, installation configuration and exposure conditions. Parallel field tests were also performed. The experimental results generated from these tests su...
L Jin, A F Preston


Service life of pressure treated deckings of spruce in direct contact with the ground
1988 - IRG/WP 3463
For decking outdoors in Sweden, pressure treated Scots pine (Pinus sylvestris L.) is used, on account of its treatability. The feasibility of using instead the refractory Norway spruce (Picea abies Karst.) is tested in a field trial. The spruce decks were treated together with pine decks with an ordinary Bethell process. As yet, after more than four years of exposure, neither in the battens nor in...
J B Boutelje, T Sebring


Evaluating possibilities of leaching of deltamethrin and TCMTB (insecticides and fungicide for protecting wood) by rain water or by soaking in water
1988 - IRG/WP 3464
Deltamethrin and TCMTB have been subjected to several field leaching tests on freshly fallen trees and in the laboratory, using standard EN 84. All the trials gave the same results and confirm that Deltamethrin and TCMTB are not washed out after they have been allowed to penetrate the trunk surface properly. According to the EN 84 standard, less than 1% Deltamethrin and less than 1.7% TCMTB were r...
J S Duguet, V Dartigues


Improvement of some technological and biological properties of poplar wood by impregnation with aqueous macromolecular compounds
1992 - IRG/WP 92-3721
Poplars (Populus spp) belong to the most important tree species in afforestation programs of the Netherlands. Due to their rapid growth, the wood quality is usually low. Therefore, studies were performed to elucidate whether some technological properties and the resistance against fungal attack could be improved by impregnation with water-soluble resins. The results showed that swelling and shrink...
R D Peek, H Militz, J J Kettenis


Treatment of lumber with preservative/water repellent emulsions - The significance of shear stability on penetration
1997 - IRG/WP 97-20124
Currently, the treatment of lumber with a water repellent emulsion and a wood preservative formulation in combination is the most cost effective way to prevent decay and to maintain the appearance of uncoated lumber in service. Water repellents influence the movement of moisture into and out of wood and, by so doing, can decrease checking and splitting significantly. Adequate penetration of the em...
F Cui, K J Archer


Properties of hot oil treated wood and the possible chemical reactions between wood and soybean oil during heat treatment
2005 - IRG/WP 05-40304
Thermal treatment with hot oil as the heating media based on the original idea from oil-heat treatment in Germany was investigated. The treatment was mainly carried out at 200ºC and 220ºC for 2 hours and 4 hours, and the wood species were mainly spruce and fir. This paper focuses on the difference between soybean oil and palm oil and the possible chemical reactions between wood and soybean oil. ...
Jieying Wang, P A Cooper


Fungicidal activity of some new water borne copper octanoate based formulations
1999 - IRG/WP 99-30198
Four new water borne formulations for preservation of wood were prepared: the composition of Cu(II) octanoate, 2-aminoethanol (ethanolamine) and water; the composition of complex of Cu(II) octanoate with nicotinamide, 2-aminoethanol and water; the one of Cu(II) octanoate, organic boron complex, 2-aminoethanol, dimethyl sulfoxide and water and finally, the mixture of Cu(II) octanoate, diazene, 2-am...
M Petric, M Pavlic, F Pohleven, P Segedin, B Kozlevcar, S Polanc, B Stefane, R Lenarsic


The effect of different concentrations of polesaver rods on the survival of selected decay fungi in liquid culture
1998 - IRG/WP 98-30166
An in-vitro method was developed to determine the effect of solutions of Polesaver Rods on the survival of selected decay fungi. Polesaver Rods are a diffusing preservative treatment containing fluorine and boron designed for the internal remedial treatment of power poles. Two white-rot fungi, Perenniporia tephropora and Trametes versicolor, and two brown-rot fungi, Polyporus verecundus and Gloeo...
M A Powell, T Deldot, C McEvoy


The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


Evaluating the performance of preservative/water repellent emulsion systems
1997 - IRG/WP 97-20127
Water repellent emulsions are being combined with wood preservatives to improve the weathering properties of treated wood in service. Unfortunately, few standard procedures are available to objectively compare the performance of these systems and as a result quality issues are almost completely neglected. The value of swellometer tests, water immersion tests and accelerated weathering regimes in t...
K J Archer, F Cui


Some factors affecting the treatability of spruce roundwood with ammoniacal preservative solutions
1976 - IRG/WP 371
Permeable wood species for use in preservative-treated commodities are becoming depleted in Canada. Spruce can be a convenient replacement for them from local resources provided it can be treated to levels adequate for protection of commodities in ground contact. Basically, two approaches were taken to improve treatability of difficult-to-penetrate softwood species; first, to improve the permeabil...
J Rak


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 1: Treatment of reference samples
1977 - IRG/WP 426
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying samples of the reference timbers treated w...
R Cockcroft, T B Dearling, W O Schulz, H V Borck


Preliminary results of the treatment of wood with chlorosilanes
1981 - IRG/WP 3172
It is clear from the initial data reported here that the treatment of pine sapwood with chlorosilanes under the reaction conditions employed did not significantly reduce the decay by both white rot and brown rot fungi. Only the dichlorosilane compounds showed to possess some protective action against fungal attack. Before drawing conclusions on the application of organosilicon compounds as potenti...
M Stevens


The effect of water-repellent additives on the leaching of CCA from simulated southern Yellow pine decks
2000 - IRG/WP 00-50158
End-matched SYP boards were pressure-treated with CCA or CCA in combination with commercial water repellent additives. After fixation and drying, the boards were placed in plastic boxes and exposed outside in Harrisburg, NC. Plastic supports were used to keep the boards above the water collected. Over a period of five months, rain run-off water from 14 natural rainfalls were collected and analyzed...
F Cui, P J Walcheski


Effects of seed origin and site on both wood density and longitudinal fluid uptake of Sitka spruce (Picea sitchensis (Bong.) Carr.) with height in the tree grown in the United Kingdom
2002 - IRG/WP 02-40226
The variation in density and longitudinal fluid uptake was investigated in short specimens of wood taken from eight seed origins of Sitka spruce trees grown at two sites in the UK. Five trees of each seed origin at each site were sampled at three heights (1, 2 and 3 m above ground level). The density of the samples decreased with increasing height within the stem. This corresponded with increasin...
I Usta, M D C Hale


Determination of absorption, accumulation and transport of copper in mycelium of some wood decay fungi
1999 - IRG/WP 99-10323
Copper compounds are common wood preservatives. However, tolerance of some wood decay fungi to copper compounds has been observed recently. Therefore, we tried to elucidate possible causes of this phenomenon. We investigated uptake, accumulation and secretion of copper in the mycelium of potentially copper tolerant fungi (Antrodia sp.) and non tolerant fungus Trametes versicolor. We observed that ...
F Pohleven, S Breznikar, P Kalan, M Petric


Selective chromate elimination from the storage-drainage-water of a wood impregnation plant
1980 - IRG/WP 3153
With the Enviro-Chrom-Ex process it is possible to eliminate ecologically and economically hexavalent chromium (chromate) from water selectively. The process which is based on the principle of selective ion exchange works with different chromate concentrations and under the presence of other ions, irrespective of the water hardness. The values of water-offtake reach 0.1 mg CrVI at maximum, causing...
O Wälchli, R Ott, R Hugener, E Graf, B Lieberherr


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp