Effect of densification of Eucalyptus nitens and E. obliqua on moisture uptake, swelling, decay resistance, and fire performance
2022 - IRG/WP 22-40946
Some Australian Eucalyptus species that are abundantly available have low natural durability and poor resistance to fire. These same species are also extremely difficult to treat with preservatives or fire retardants using conventional pressure treatment methods due to a large proportion of refractory heartwood. The aim of this research was to understand whether thermo-mechanical densification had...
B Hassan, J J Morrell, F Wiesner, W Wu, B Belleville, K C Wood


Phenol formaldehyde modification and termite resistance under laboratory testing
2022 - IRG/WP 22-40952
The development of phenol formaldehyde (PF) resins as a means of impregnating solid wood is one that has been explored for several decades, both in terms of conventional impregnation processing (Impreg) or compressional impregnation (Compreg). However, it is only recently with advances in processing conditions that the method truly affords a means of achieving conventional modification for solid t...
L Nunes, A Pitman, M Duarte, B Stefanowski, D Jones


Evaluation of Decay Resistance for the Larch Wood Heat-treated with Superheated Steam
2022 - IRG/WP 22-40956
Heat-treatment of wood is a process that involves applying heat ranging 160–260°C to improve its physico-mechanical properties and resistance against wood rot fungi. The level of the changes in the wood properties by heat-treatment differs depending on the temperature and duration of heat-treatment, as well as the types of heat transfer media used for heat-treatment. The heat-treatment on wood ...
Y Park, S-M Yoon, H Kim, W-J Hwang


A novel method for assessing radial variation in termite resistance of timber
2023 - IRG/WP 23-11005
Australia has many timbers whose heartwood is highly resistant to fungal and termite attack; however, changing public policies have resulted in restricted access to many native forests where these species are found. Plantations of these same species are expected to replace these resources, but there are questions concerning whether timber from these trees will have the same resistance as the nati...
S Kleinschmidt, R McGavin


Assessment of the Material Durability and Structural Integrity of the Wooden Velodrome in Češča vas, Slovenia
2023 - IRG/WP 23-11012
Wood is a widely used material in the construction industry, and it has been utilized for thousands of years to create buildings and other structures. When wooden structures are designed, built, and maintained properly, they can be safe and long-lasting. Sports facilities, which provide athletes with a space to train, compete, and improve their abilities, are crucial in creating a strong and susta...
D Kržišnik, M Humar, B Lesar


Optimisation of accelerated weathering procedure as an alternative to natural weathering
2023 - IRG/WP 23-20693
Comprehensive tests need to be performed to obtain the most accurate data possible on the durability of wood. The most reliable performance tests are field tests. However, since this is very time-consuming, we frequently rely on laboratory tests. To increase the reliability of the laboratory tests, samples are preconditioned with natural or artificially accelerated weathering methods that simulate...
E Keržič, M Humar, V Vek


Resistance of phenol formaldehyde impregnated beech (Fagus sylvativa L.) LVL against biodegradation in soil contact
2023 - IRG/WP 23-40965
Alternatives to preservative impregnation are emphasized in Germany and other European countries. Even though these treatments significantly improve wood's resistance to decay, they often do not have a beneficial impact on the dimensional stability. One alternative product, which may be used in ground contact for items like poles and railway sleepers, could be beech (Fagus sylvatica L.) laminated ...
M Slabohm, C Brischke, S Bicke, H Militz


New wood-modification process based on grafted urethane groups: Durability of carbamamylated Scots pine (Pinus sylvestris L.) wood
2023 - IRG/WP 23-40974
Substituting commonly used toxic preservatives with wood modification treatments can make the wood material less prone to water and moisture uptake. This approach favours a more sustainable protection of wood against biodegradation. In this study, Scots pine sapwood was full-cell impregnated with an aqueous solution of urea (30%), dried at 40°C for 24h, and subsequently heat-treated at 150°C for...
C-F Lin, O Myronycheva, O Karlsson, D Jones, D Sandberg


Evaluation of the effectiveness of soaking of high-temperature plywood in low-temperature oil-based wood
2023 - IRG/WP 23-40991
We conducted a preliminary investigation to determine if soaking high-temperature plywood in a low-temperature preservative solution could achieve deeper penetration of the preservative, even in plywood made with refractory wood species such as Japanese larch. Specimens cut from commercial plywood (Japanese larch) were stored at various temperatures before being soaked in the preservative solution...
T Miyauchi, S Isaji, H Shibui, N Furuta, J Miyazaki, H Matusnaga


Optimization of furfurylic alcohol/tannin ratio to improve the performance of biosourced thermoset resins for wood protection
2023 - IRG/WP 23-40994
This study concerns the chemical modification of wood with different ratios of tannin and furfuryl alcohol (FA) in the presence of maleic acid as catalyst. Tannins were used not only as cross-linking agents, but also as co-monomers to improve wood durability, while reducing the amount of FA used. Different aqueous formulations were prepared containing decreasing amount of FA (from 45.45% to 0%) an...
E Azadeh, A Pizzi, P Gérardin, C Gérardin-Charbonnier


Do naturally sequestered biocidal metals contribute to the marine borer resistance of turpentine?
2024 - IRG/WP 24-11036
Turpentine wood is renowned for its resistance to attack by molluscan marine borers. This resistance is thought to be due to its high silica content, and possibly the presence of other, as yet unknown, compounds. Silica in turpentine wood is present as particles in rays, but in many plant species silica also occurs in cell walls. We hypothesized that Si is present in cell walls of turpentine, but ...
P D Evans, H Matsunaga, D Feng, M Turner, C Kewish


Intra-species variability of moisture dynamics in wood
2024 - IRG/WP 24-11040
Moisture dynamics of wood and wood-based materials play a major role in wood durability against different decay organisms. Their impact becomes particularly evident when wood is exposed, but not permanently wet. To date, however, this has only been taken into account indirectly and therefore inadequately when testing the durability of wood. While test methods are available, for example to determin...
C Brischke, H Purps, L Emmerich


Exposure tests on railroad ties treated with DOT
2024 - IRG/WP 24-20705
Keruing railroad ties were treated with disodium octaborate tetrahydrate (DOT) to retentions of 0.7 to 1.7% boric acid equivalent (BAE) and selected borate treated ties were subsequently over treated with creosote/diesel fuel mixture. The treated ties were exposed in a simulated railway track test bed in Malaysia. The leaching of borate was measured over 5 years. BAE in the ties after 5 years of e...
L Arthur, J-W Kim


Enhancing UV resistance and decay resistance of wood by nanoparticle dispersed linseed oil nanoemulsion
2024 - IRG/WP 24-20706
Enhancing increasing demand for eco-friendly and cost-effective wood coatings and preservatives has led to the development of water-borne formulations and use of non-toxic and natural materials such as vegetable oils and waxes. The aim of this study was to improve the UV resistance and decay resistance of wood by nanomaterial dispersed linseed oil emulsions. Highly stable nanoemulsions of linseed ...
R Bansal, R Kumar, K K Pandey


Surface treatment of cross-laminated timber to improve water repellency and UV resistance
2024 - IRG/WP 24-20716
Cross-laminated timber (CLT) has emerged as a revolutionary building material, offering a sustainable alternative to traditional construction methods. By layering and bonding multiple layers of wood at right angles, CLT creates a robust and versatile structural element capable of supporting significant loads while promoting eco-friendliness and design flexibility. However, despite its numerous adv...
M Chen, S Uphill, J Hilsenbeck, A Hughes


Comparison of copper leaching from alkaline copper quat and copper compound nanosol-based wood preservative treated wood
2024 - IRG/WP 24-20726
To improve the leaching resistance of copper ion-based wood preservatives, copper compound nanosol-based wood preservatives were developed and its copper leaching characteristics were evaluated. Three types of preservatives (DC1, DC2, DC3) were prepared with different crystallinity and dispersant types of copper compound nanosol, and the copper concentration was adjusted to be the same as that of ...
Y-S Choi, S-M Yoon, J O Kim, J-G Kang, J-G Park


Influence of the substitution of phenol with lignin cleavage products in phenol-formaldehyde impregnation resins for wood modification on the fungal decay resistance and impregnation depth
2024 - IRG/WP 24-30805
The impregnation modification of wood with phenol-formaldehyde (PF) resins increases the woods dimensional stability and resistance against fungal decay. However, to decrease the usage of non-renewable resources, the substitution of phenol has been a topic of scientific interest. Lignin is a currently underutilized resource with a chemical structure that contains phenolic units. For adhesive appli...
J Karthäuser, L Tarentino, A Treu, H Militz, G Alfredsen


A novel treatment for increasing UV stabuility of wood based on citric acid and urea
2024 - IRG/WP 24-30811
Wood, a fundamental material in the Built Environment, faces challenges related to durability and weathering, notably UV degradation leading to colour changes. This study explored a novel treatment method utilising citric acid and urea to enhance the UV stability of wood. The reaction between these compounds forms fluorescent species and insoluble nanoparticles upon thermal treatment. Two treatmen...
S Jué, A Scharf, C-F Lin, R Moutou Pitti, D Sandberg, D Jones


Outdoor termite resistance performance of zinc borate (Borogard® ZB) treated parallel strand lumber (PSL) – 15 years field test results
2024 - IRG/WP 24-40999
This report discloses the outdoor termite resistance performance of PSL samples treated with zinc borate at a dosage of 0.85% BAE and 1.72% BAE in Wuxi, China. The outdoor field trial lasted for 15 years and observations were made after 6 months, 3 years, 5 years 1 month, 6 years 6 months and 15 years. The retaining rates of B2O3 and ZnO in the final samples were also tested, and the hypothesis wa...
S Shi, E Laval, K Lung, F Ascherl, R Williams, W Li, X Li


Leaching and chemical redistribution of CCA components in refractory heartwood of E. nitens
2024 - IRG/WP 24-41011
Chromated Copper Arsenate (CCA) is a wood preservative widely used to protect against fungal and insect attack. The fixation mechanism of CCA involves complex chemical reactions, including the reduction of chromium (VI) to chromium (III) and the formation of insoluble complexes. Despite fixation efforts, a portion of CCA components tends to leach from treated wood, influenced by factors like wood ...
J R Vargas, L Yermán, K C Wood, T Singh


Durability of Malaysian plybamboo to mold
2024 - IRG/WP 24-41014
Durability of 3-layer plybamboo fabricated from two Malaysian bamboo species, Gigantochloa levis (beting) and Gigantochloa scortechinii (semantan) using three different adhesives - urea formaldehyde (UF), melamine urea formaldehyde (MUF) and phenol resorcinal formaldehyde (PRF) was evaluated in this study. Samples were exposed to the mold, Aspergillus brasiliensis for 4-week following the ASTM D44...
S Lipeh, A Mustapha, A S Yusoh, M K A Uyup


Analysis and performance of spruce alternative species and discarded wood for windows production
2024 - IRG/WP 24-50386
Climate change is having a significant impact on European forestry, particularly on the softwood species used for window frames. This study investigates potential replacement tree species for spruce (Picea abies), the predominant material for window frames. We evaluate Douglas fir (Pseudotsuga menziesii), Scots pine (Pinus sylvestris), thermally modified poplar (Populus nigra) and discarded silver...
B Lesar, J Levanič, M Humar, A Treu


Copper migration from preservative-treated Douglas-fir decking: models vs laboratory leaching data
2024 - IRG/WP 24-50390
The ability of a model to predict copper migration from Douglas-fir treated with organic metallic substances into a freshwater slough was evaluated against data generated through simulated overhead leaching. The model predicted very high loadings of ammoniacal copper zinc arsenate, alkaline copper quaternary or copper azole that had the potential to impact water quality while data from the exper...
M J Konkler, G Presley, J J Morrell, T Singh


Quantifying metal migration from a deck constructed with copper-azole-treated lumber
2024 - IRG/WP 24-50391
Soluble copper or micronized copper wood preservatives are the most common available wood preservative systems for residential applications in the United States. Copper containing wood preservatives have been scrutinized for their potential negative impacts on the environment, across many jurisdictions. Concerns arise from the potential for preservatives to migrate out of treated wood upon water e...
G Presley, M Konkler


Structural health assessment of wood - A comparison of methods for determining the spatial spread of fungal infestation in beams and rafters
2025 - IRG/WP 25-11051
Wood decay in buildings can cause severe economic losses, require comprehensive refurbishment, and removal of decayed wooden elements from the building. The latter aims at restoring the structural integrity of the component or the entire building through replacement, and at preventing the infestation from spreading further. In practice, components are cut out of the structure to such an extent tha...
C Brischke, N Sommerfeld, E Flohr, A K Mayer, S Bollmus


Previous Page | Next Page