IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 419 documents. Displaying 25 entries per page.


Copper distribution in soil leached from full scale decking boards during one year
2010 - IRG/WP 10-50265
The distribution of copper in the soil under exposed decking boards after one year has been analysed. The decking boards were impregnated with copper HDO, copper quat and copper triazoles. The decking boards were pine sapwood and pressure treated in a full cell process, fixed by heating and then dried. The samples were not surface treated. Each decking sample of five boards (0.25 m2) was placed on...
F G Evans


Combined Effect of Boric Acid and Waste Oil Treatment on Boron Leaching
2010 - IRG/WP 10-50268
In this study it was aimed to investigate the boron leaching amounts in Scots pine wood samples treated with boric acid (BA) and waste oil (WO) alone or by dual treatment. The level of water absorption and water repellent efficiency were determined with cyclical wetting tests, total of 336 hours. Wood samples that have both covered and uncovered transversal section were impregnated with 3% boric a...
Ü C Yildiz, E Dizman


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


Sample Origin Influencing the Leachability of Wood Preservatives
2011 - IRG/WP 11-20474
The aim of this study is to see if the raw material influences fixation and leachability of wood preservatives. Moving towards more eco-friendly and –concious society, the wood industries must adjust itself to new rules and regulations. Greener solutions in wood protection are being tested and introduced, older systems are being improved, but questions still arise concerning some elements curren...
K Kängsepp. E Larnøy, P Meier


A Method for Studying Boron Redistribution and Leaching in Timber Framing
2011 - IRG/WP 11-20476
In typical New Zealand timber framed house construction, the timber framing has a vapour permeable building wrap applied to the exterior and a cladding applied over 20 mm battens. An interior lining usually of gypsum plasterboard is then fixed once the timber framing has a moisture content of < 20%. Timber framing within the building envelope is not expected to be wet in-service or exposed to a le...
J A Drysdale, N Marston, M E Hedley


Influence of wood swelling agents on penetration and copper leaching of copper-ethanolamine based wood preservatives
2011 - IRG/WP 11-30556
Copper ethanolamine based preservatives are currently the most important solutions for impregnation of wood in ground contact in Europe. One of the issues related to those and similar water based solutions is insufficient penetration to refractory wood species like Norway spruce. In order to elucidate this issue, commercial copper ethanolamine based solution was supplemented with five different wo...
M Humar, N Thaler, B Lesar


Effect of P/F ratio, PF concentration and treating method on boron leaching from wood treated with PF modified boron compounds
2011 - IRG/WP 11-30559
In order to immobilize boron in wood, three kinds of resol-type phenol-formaldehyde (PF) resin with different P/F ratios were synthesized in laboratory and incorporated with three types of boron compounds to treat wood. The used boron compounds included boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT). The leaching test of boron from wood blocks was performed according to the...
Liping Yu, Jinzhen Cao


Fixed Borates Anyone?
2011 - IRG/WP 11-30563
The quest for a borate based preservative system that resists leaching or is “fixed” has long been a research goal. Boron fixation has been attempted with numerous strategies but there have been problems associated with past methods. This paper discusses new fixation systems based on bio-materials and presents up to five year outdoor exposure testing on full-size decks. Generally, the new f...
C R McIntyre, M A Lake


Treatability variation of scots pine heartwood from Northern Europe
2011 - IRG/WP 11-40563
Scots pine (Pinus sylvestris L.) is one of the most common construction materials for general exterior applications in northern Europe. It has a wide natural geographical distribution, a good availability and it is low-priced compared to other materials. According to EN 350-2 Scots pine heartwood is considered being “untreatable” and having durability class 3. This means that its durability co...
G Behr, E Larnøy, C-T Bues


Characterizing long term leaching behaviour of copper from preservative treated wood in a practical exposure scenario
2011 - IRG/WP 11-50278
To investigate the prediction of the long term emission of copper from preservative treated wood in a Use Class Class 3 scenario, treated boards were exposed vertically above ground to natural weather conditions. The study included two products; an amine copper ACQ-type formulation, air-dried after treatment to a 22 kg/m3 retention, and the same formulation which was hot oil vacuum dried after tre...
T Mark Venås, M Klamer


Copper Migration from Micronized Copper Preservatives Treated Wood in soil contact:
2011 - IRG/WP 11-50280
Emerging formulations of preservatives made with micronized basic copper carbonates with azoles and/or quat to control copper tolerant fungi have been used to replace formulations containing soluble copper to reduce the leaching of copper and the corrosion of metal in contact with wood. This study proposes to use laboratory soil leaching test AWPA standard (E20-08) to estimate the amount of copper...
Lei Wang, D P Kamdem


Extractives in Norwegian-Grown and North American-Grown Western Redcedar and Their Relation to Durability
2012 - IRG/WP 12-10762
The extractives responsible for the natural durability of western redcedar (WRC) are not well understood. Recent work by the Norwegian Institute of Wood Technology and the Norwegian Forest and Landscape Institute has evaluated the natural durability of Norwegian wood species and reference species, including Norwegian-grown WRC and North American-grown WRC, in a series of decay tests. The availabil...
R Stirling, P O Flæte, G Alfredsen, P I Morris


Above Ground Field Evaluation and GC-MS Analysis of Naturally Durable Wood Species
2012 - IRG/WP 12-10764
Nine wood species are being evaluated in above ground field studies in Mississippi and Wisconsin. Candidate naturally durable wood (NDW) species are being rated at yearly intervals for resistance to decay, cupping, and checking. Field ratings after 12 months exposure are presented. To date, Paulownia tomentosa (PAW) and southern yellow pine (SYP) are least durable and cedars are the most durable i...
G T Kirker, A B Blodgett, S T Lebow, C A Clausen


Eastern redcedar included sapwood: Resistance to mold and termites under laboratory conditions
2012 - IRG/WP 12-10765
The heartwood of eastern redcedar (Juniperus virginiana) frequently contains areas of light-colored wood. This “included sapwood” is considered to be a defect by some manufacturers. In this study, sapwood, included sapwood and heartwood samples from five eastern redcedar trees were exposed to mold fungi or to subterranean termites in a no-choice feeding test. Extractives content was also measu...
C Köse, A M Taylor


Antifungal activity of wood extractives from waste products of steam distillation of Aniba rosaeodora
2012 - IRG/WP 12-10779
Aniba rosaeodora, is a slow growing evergreens of the Lauraceae family which are indigenous over a wide range of the Greater Amazon Region (the Guianas and Venezuela, Brazilian Amazon…). The essential oil obtained from the wood has a characteristic aroma and is a long-established ingredient in the more expensive perfumes. Around the olfactive characteristic of the essential oil is due to the pre...
N Amusant, A Digeon, E Hoüel, J Beauchène


Tannin resin-boron associations: Leaching and biological resistance
2012 - IRG/WP 12-30587
The easy leaching of boron in wood preservation formulations has allowed to use this fungicide only for short term applications. The recently discovered adduct with flavonoids allows boron to resist longer periods of time within wood and consequently extend its life. Two different leaching treatments were compared and the fungal and termite decay was examined. The biological tests have shown extre...
G Tondi, S Wieland, N Lemenager, A Petutschnigg, A Pizzi, M-F Thevenon


Antifungal activities of acetone-soluble Eusideroxylon zwageri and Potoxylon melagangai crude extracts against white rot
2012 - IRG/WP 12-30591
The development of natural wood extracts as a wood preservative is a potentially attractive prospect for the wood preservation industry. This study attempts to evaluate the toxicity of Eusideroxylon zwageri and Potoxylon melagangai extractives as potential wood preservatives. These two species are well-known as among the heaviest and very durable timbers. It has been established that natural durab...
I Jusoh, A Tida Henry, Z Assim, F Badruddin Ahmad, S Ujang


Fixation and leaching characteristics of Malaysian tropical hardwoods treated with CCA-C
2012 - IRG/WP 12-50289
The fixation and leaching characteristics of 8 Malaysian tropical hardwood (MTH) species treated with chromated copper arsenate (CCA-C) wood preservative were examined. The species evaluated were Acacia (Acacia mangium), Bintangor (Calophyllum sp.), Geronggang (Cratoxylon arborescens), Medang (Litsea sp.), Meranti rambai daun (Shorea acuminata), Putat (Planchonia sp.), Ramin (Gonystylus sp.) and S...
S Salim, S Shahomlail, Z Ashaari, Yong-Seok Choi, Gyu-Hyeok Kim


Inhibitory extractives or nutrients? Mould growth on coated heartwood and sapwood of Pinus sylvestris and Gleditsia triacanthos
2013 - IRG/WP 13-10806
Sometimes mould fungi grow over weathered coated sapwood, whereas the coated heartwood is not colonised. Two factors may be responsible for these differences: Either the larger content of nutrients in the sapwood, or the content of biocidal extractives in the heartwood. In this study the factors for the difference in mould growth on coated heartwood and sapwood of Pinus sylvestris (Scots Pine) and...
D Lukowsky, N Buddruhs


Transferable Durability: Enhancing decay resistance of non-durable species with extractives from durable wood species
2013 - IRG/WP 13-10808
Extractive content and composition is a vital component of naturally durable woods; however, variability in extractives can limit their usefulness in the field. Two extractive-free, non-durable wood species were pressure treated with ethanol-toluene extractives from 8 durable wood species. Extracted Southern pine, Paulownia and unextracted Southern pine blocks were treated and challenged in soil b...
G T Kirker, A B Blodgett, S Lebow, C A Clausen


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Preliminary testing of spiroborate esters as wood preservatives
2013 - IRG/WP 13-30614
Fungicide and insecticide properties of boric acid are known since 30’s of the last century, but high solubility and leachability of inorganic borates limit their use for only applications not directly exposed to liquid water. A number of attempts were made to fixate borate salts into the wood structure but this research topic is still up to date and undiscovered. Water insoluble organoboron est...
D Panov, N Terziev


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


The effects of impregnation with secondary metabolite extracted from Ipe on durability of Japanese cedar and beech wood
2013 - IRG/WP 13-30618
Ipe wood is known for its high durability; it has been widely used in exterior structures that are exposed to the weather. In this paper, to increase the durability of less durable wood, Japanese cedar and beech specimens were impregnated with a secondary metabolite from Ipe. In a previous study, secondary metabolites extracted by a Soxhlet extraction method showed antifungal properties. Therefore...
T Iida, R Konuma, K Kawarada


Copper leaching from copper-ethanolamine treated wood during exposure to terrestrial microorganisms
2013 - IRG/WP 13-30621
Copper-ethanolamine based wood preservatives are still the most important solutions for protection of wood in ground applications in Europe. Wood in ground is exposed to variety of organisms, which can act synergistically. In order to simulate these conditions in laboratory, Scots pine (Pinus sylvestris) specimens impregnated with copper-ethanolamine preservative of three different concentrations ...
M Humar, N Thaler, B Lesar


Previous Page | Next Page