Wood surface pretreatments with metal tannates
1989 - IRG/WP 3552
The sequential application of aqueous solutions of tannins derived from radiata pine bark and water-soluble metal salts was examined as a means of improving the water repellency of wood surfaces. Nine metal salts were screened in combination with tannin solutions and, based on water repellency of pretreated filter paper, four were selected for further study. The two-step application of tannin solu...
D V Plackett, D R Cronshaw


Screening of the efficacy of tall oils against wood decaying fungi
2004 - IRG/WP 04-30354
Tall oil is a by-product in pulping of resinous wood by the sulphate process. Tall oil contains a complex mixture of wood extractives. Some of these extractives act as natural protection against wood decaying fungi while other serve as nutrition for the fungi. This report describes a screening of the efficacy of four refined tall oils with different chemical composition on wood decaying fungi. ...
G Alfredsen, P O Flæte, A Temiz, M Eikenes, H Militz


Assessing the leachability of chlorothalonil and methylene bis thiocyanate from antisapstain treated radiata pine
1998 - IRG/WP 98-30176
Rain wash-off and leaching of antisapstain fungicides from wood may cause pollution of waterways and may also lead to a decrease in the efficacy of a formulation against fungal degrade as chemicals deplete from the timber surface. In the current study, the leachability of chlorothalonil (CTL) and methylene bis thiocyanate (MBT), the active ingredients of a commercial antisapstain formulation, was...
B Kreber, T L Woods


Influence of carboxylic acids on LEACHING of copper amine based preservatives
2005 - IRG/WP 05-30365
The importance of chromium free preservatives is increasing. Leaching of copper from wood preserved with such solutions is still higher compared to leaching from wood impregnated with copper chromium ones. In order to decrease leaching, different carboxylic acids (octanoic, 2-etilheksanoic, decanoic) were added to copper/amine/boron aqueous solutions. Experiment of leaching of copper from Norway s...
M Humar, P Kalan, F Pohleven


Status of Work on OECD Test Guidelines for Emissions of Wood Preservatives to the Environment
2005 - IRG/WP 05-50224-3
In April, 2003, OECD published an ESD on wood preservatives that provides guidance on how to estimate emissions: 1) during the wood preservative application processes and storage of treated wood prior to shipment; and 2) from treated wood-in-service. The ad hoc Expert Group that developed the wood preservatives ESD identified the need to develop Test Guidelines to estimate the amount of biocides ...
W Jakob


An environmental aspect relating to leachability of CCA from hardwood and softwood poles in Bangladesh
2001 - IRG/WP 01-50167
Leachability of CCA and the service performance of 8 softwood and 5 heartwood poles in service after 5 to 17 years in Bangladesh have been studied. The study included determination of retention of CCA-C in outer 6 mm zones at groundline (GL) and above groundline (AGL) along with the observation of decay and conditions of soils. The mean leaching of CCA-C derived from retention differential at GL a...
A K Lahiry


Laboratory studies of CCA-C-leaching: influence of wood and soil properties on extent of arsenic and copper depletion
2002 - IRG/WP 02-50186
The extent which a wood preservative leaches is important for efficacy studies and environmental concerns. However, little information exists on the effect soil properties have on leaching. This study investigated leaching of stakelets which had been cut from five different southern yellow pine (SYP) sapwood boards then treated with CCA-C to a target retention of 6.4 kgm-3 (0.4 pcf). All stakel...
D Crawford, R F Fox, D P Kamden, S T Lebow, D D Nicholas, D Pettry, T Schultz, L Sites, R J Ziobro


Leaching of preservative components from pine decking treated with CCA and copper azole, and interactions of leachates with soils
2001 - IRG/WP 01-50171
Radiata pine decking was treated with CCA and copper azole preservatives to Australian H3 retention using conventional and modified Bethel schedules, and air-dried. Treated decking boards and durable hardwood controls were subjected to leaching in weather-exposed decks, and matching 19mm cubes were leached in extended AWPA E11-97 lab tests. Deck runoff and E11 leachate water was analysed after rai...
M J Kennedy, P A Collins


Five years leaching of Boron
1999 - IRG/WP 99-30195
The diffusibility of Boron in wood and thus its leaching behaviour in water contact is known since long. Nevertheless quantitative data on the long-term leaching behaviour are rare. Consequently, field exposure tests were started with beam-segments treated with pure boric acid and with poles treated with CCB. Detailed data of more than five years of field exposure are now available. Pure boron tre...
A Peylo, H Willeitner


Experiences with the OECD guideline proposals for the estimation of emissions from preservative-treated wood in the environment
2004 - IRG/WP 04-50209
The practicability of 2 CEN proposals for OECD guidelines on the estimation of emissions from preservative treated wood by laboratory methods for either wood held in storage after treatment and for wooden commodities that are not covered, and are not in contact with ground (guideline 1) or wooden commodities that are not covered and are in contact with ground, fresh water or seawater (guideline 2...
U Schoknecht, R Wegner, E Melcher


Interactions between water-borne preservatives and emulsion additives that influence the water repellency of wood
1991 - IRG/WP 2374
Incorporation of non-polar additives into water-borne treatments through of emulsion technology can greatly improve the physical characteristics of wood in service. Of specific interest with these emulsions is their effectiveness in reducing the rate of wood swelling. We have observed that the presence or absence of preservatives can often significantly influence the resultant effectiveness of the...
A R Zahora


Reduction of preservatives leaching from wood by the application of animal proteins
2005 - IRG/WP 05-30387
The investigations consisted in the estimation of the effectiveness of protein borates and protein propionates in wood preservation against Coniophora puteana. The estimation was made on the basis of mass losses caused by the test fungus action against treated wood which was subjected to leaching with water. The investigations were performed for Scots pine wood (Pinus sylvestris L.) treated with p...
B Mazela, I Ratajczak, M Bartkowiak


Leaching of active components from preservative-treated timber. Stages 2 & 3: Laboratory testing and comparison with semi-field testing
2004 - IRG/WP 04-20303
This part of the project is focussed on leaching from preservative-treated wood obtained by the laboratory test method CEN/OECD draft guideline, February 2003 ”OECD guideline for the testing of chemicals proposal for new guideline XXX. Estimation of Emissions from Preservative-treated Wood to the Environment: Laboratory Method for wood held in the storage yard after treatment and for wooden comm...
N Morsing, B Lindegaard


Laboratory Evaluation and Field Trial of Chlorothalonil and Copper-based Preservatives and Leaching Performance of Copper in Copper Treated Wood
2002 - IRG/WP 02-30279
Soil block test and field trial of some Chinese plantation wood species pine and poplar treated with chlorothalonil formulations and copper-based preservatives such as ACQ-B and copper citrate (CC) were conducted. The results of soil block test indicated that chlorothalonil formulations and ACQ-B as well as CC are very effective for controlling the 2 fungi species Corious versicolor and Poria plac...
Mingliang Jiang, Ping Wang, Chungen Piao, Zhaobang Li, Quan Lu, Lei Liu


Creosote losses due to ageing methods prior to laboratory efficacy testing
2002 - IRG/WP 02-20256
Laboratory efficacy testing of creosote is affected by the impact of volatile components on the fungal growth. European test methods for assessing efficacy against Basidiomycetes and soft rot fungi is based on two standard methods, EN 113 and ENV 807 respectively. Combined with both fungal tests two pre-treatment methods are commonly used, namely EN 84 (leaching) and EN 73 (evaporation). Within th...
J Van Acker, K Ghekiere, M Stevens


Influence of hydrophobic agents on the leachability of boron
1995 - IRG/WP 95-30064
Besides its low mammalian toxicity and a broad range of activity towards both fungi and insects, boron shows a high diffusibility, encouraging it to treat wood species of low permeability. However, its difussibility is at the same time responsible for a high risk of leaching, known since long. Nevertheless quantitative data about this process are only rarely available. Therefore, the leaching of b...
A Peylo, H Willeitner


Diffusion modeling of inorganic wood preservative leaching in service
2005 - IRG/WP 05-50224-5
To evaluate the potential environmental and health implications of leaching of inorganic wood preservatives in service under different conditions, there is a need for a predictive model that provides estimates of the rate and extent of leaching over a wide range of product dimensions and exposure conditions. In this paper, we show that the leaching behavior of inorganic preservative components fr...
L Waldron, P A Cooper, Y T Ung


Artificial weathering exposure as an alternative for standard ageing according to EN 84 (leaching) and EN 73 (evaporation)
2002 - IRG/WP 02-20254
In order to verify potential weaknesses of wood preservatives fungal tests are carried out after ageing of wood preservative treated test blocks. The European standard EN 599 as a framework for efficacy assessment of wood preservatives includes the use of two ageing methods prior to fungal testing, namely a leaching method (EN 84) and an evaporation method (EN 73). The European research project "F...
J Van Acker, M Grinda, D J Dickinson


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Determination of the amine to copper ratio remaining in wood after leaching
2002 - IRG/WP 02-30285
The effectiveness of the protection and the environmental impact of the treated wood are two of the most important aspects that need to be understood for all preservatives. Both are particularly influenced by the loss of biocidal components from treated wood. For amine copper preservatives, copper fixation determines the leaching resistance of the copper and amine compounds formed in wood. Previou...
N Lucas, J N R Ruddick


Utilization of coconut timber from north Sulawesi, Indonesia. Part 2: Treatability
1994 - IRG/WP 94-40025
Under tropical conditions coconut wood is quickly degraded by mold and blue stain fungi. Low density wood in ground contact is commonly decomposed by wood destroying fungi within a period of only a few months, higher density wood from the outer stem regions within 24 to 30 months (MOSTEIRO, CASIN, SERIBAN 1976; McQUIRE 1975). Moreover, according to McQUIRE (1975) green wood of lower density is hig...
R-D Peek


Decay and termite resistance of wood treated with boron-containing quaternary ammonia compound, didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin
2004 - IRG/WP 04-30334
This study evaluates the decay and termite resistance of surface-treated wood with didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin emulsion. DBF is a quaternary ammonia compound and contains boric tetrafluoride (BF4-) as a counter ion in its chemical structure. In the study, DBF was incorporated with an acryl-silicon type resin to increase water-resista...
S N Kartal, W J Hwang, K Shinoda, Y Imamura


Leaching of arsenic, copper and chrome from preservative-treated timber in playground equipment
1984 - IRG/WP 3149
Samples were taken from CCA-treated timber in sand play boxes and other play ground equipment. Sand was also sampled. Sand and wood samples were analysed for copper, chrome and arsenic by AAS. About 20-25% of the arsenic had leached from the timber after 2-4 year's exposure in the playgrounds. Very little of the copper and chrome had been leached. Sand collected in the close vicinity of t...
B Henningsson, B Carlsson


Fixation of CCA preservatives in cocos-, oil- and rattan-palm
1986 - IRG/WP 3371
In previous tests with jubaea-palm almost no fixation of a CCA-preservative Type B could be achieved, consequently, further leaching tests were carried out with samples of 1 cocos-, 1 oil- and 2 rattan-palms from Malaysia. A good fixation of chromium and copper took place in cocos-palm after 4 weeks storage at 28°C. Nevertheless the fixation was slower than in pine-wood and demanded an elevated t...