IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 139 documents. Displaying 25 entries per page.


A laboratory evaluation of the susceptibility to biological attack of glued laminated pine timber
1991 - IRG/WP 2387
In the scope of a research programme concerning the use of maritime pine (Pinus pinaster) to produce glued laminated timber structures in Portugal, the natural durability of this material was checked by using laboratory test methods. An European standard, EN 113, was used to test durability against basidiomycetes and a test method developed at LNEC for termites was adapted for this purpose. From t...
L Nunes, H Cruz


Biocide Treatments for Wood Composites - A Review
2006 - IRG/WP 06-40323
This paper reviews the biocidal treatment of wood composites. Included are in-process and post-process treatments. Various biocides are covered as are methods of application. Novel treatments and technologies are also presented....
J W Kirkpatrick, H M Barnes


Preventing fungal attack of freshly sawn lumber using cinnamon extracts
2007 - IRG/WP 07-30432
The potential for using cinnamon oil as an anti-mold and stain compound was investigated on ponderosa pine sapwood. Cinnamon oil was highly effective when used in ethanol, but its activity declined when it was mixed with only water. Attempts to enhance water solubility with surfactants improved solution stability, but had no apparent effect on biological activity. Further studies with other co-so...
Shujun Li, C Freitag, J J Morrell


Migration of Metals from Douglas-fir Lumber Treated with ACZA or Pentachlorophenol Using Best Management Practices: Preliminary Tests
2005 - IRG/WP 05-50224-4
The potential for migration of preservative components from ammoniacal copper zinc arsenate (ACZA) and pentachlorophenol treated Douglas-fir lumber in non-soil contact exposure was assessed in a simulated rainfall device. Metal levels from ACZA treated wood were elevated for the first 30 minutes of rainfall and then declined sharply. Repeated cycles of rainfall led to declines in initial metal l...
J J Morrell, Hua Chen, J Simonsen


Protection of beech veneer for fruit and vegetable boxes
1981 - IRG/WP 3176
In Yugoslavia about 50,000 m³ of low quality beech logs annually are rotary cut into veneer from which boxes are made for transporting fruit and vegetables. Because of steaming before rotary cutting, beech veneer becomes extremely sensitive to mould attack which decreases the quality and commercial value of the final product. To avoid mould attack, veneer sheets are dried to 16% moisture content ...
N Vidovic


Effect of incising depth and density on treatment of Douglas fir, hem fir and spruce-pine-fir lumber with CCA, ACZA or ACQ
1997 - IRG/WP 97-40093
Incising markedly improves both the depth and uniformity of preservative treatment of refractory wood species, but there are few studies directly comparing the effects of incising depth and density on penetration and retention of commonly used waterborne preservatives in wood species from the western United States. The effects of two incision densities (7300 and 8900 incisions/square meter) at two...
M Anderson, J J Morrell, J E Winandy


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Comparative moisture uptake of Douglas fir and radiata pine structural lumber when exposed to rain wetting as an indicator of relative decay resistance
2004 - IRG/WP 04-20285
Trials were undertaken to determine the relative resistance of radiata pine and Douglas-fir to wetting when exposed to the weather. Douglas-fir samples were obtained from one Central North Island and three South Island sources and had a heartwood/sapwood mix typical for each resource. Radiata pine sapwood and heartwood samples were obtained from a Central North Island source. Material was exposed...
M E Hedley, G Durbin, L Wichmann-Hansen, L Knowles


A termite field test with diffusion treated lumber
1991 - IRG/WP 3648
Douglas fir lumber, diffusion treated with concentrated sodium octaborate solutions, was tested against Coptotermes formosanus in an above ground field test wherein the samples were not exposed to a direct leaching hazard during the test period. After 2.5 years exposure, the untreated control samples were almost completely destroyed while poorly treated controls pressure treated with chromated cop...
K J Archer, D A Fowlie, A F Preston, P J Walcheski


Improving the weather resistance of glue-laminated jarrah and karri
1994 - IRG/WP 94-40017
Surface modification and dimensional stabilisation significantly increased the dry and wet shear strength of karri and jarrah lap-shear specimens (laminates) bonded with resorcinol formaldehyde. The combination of surface modification (sanding/sodium hydroxide treatment), and furfurylation produced the highest dry and wet shear strengths. Acetylated laminates had the lowest dry bond strength, but ...
J Balfas, P D Evans


A new technique for testing decay resistance of framing lumber
2002 - IRG/WP 02-20247
Model house frame units (two studs, top and bottom plates and a central “dwang”) were constructed using short (500-600 mm) lengths of framing timber. Constructed frames were impregnated with water using a mild pressure schedule to raise the initial moisture content to 35-40 % mc. The back face of each unit was then covered with black polyethylene. Two locations at the stud/dwang and stud/botto...
M E Hedley, D Page, B E Patterson


Wood-based composites exposed to fungal degradation: Laboratory results
2001 - IRG/WP 01-40215
Oriented strandboard (OSB) and laminated veneer lumber (LVL) are widely used as residential construction materials. The durability of OSB and LVL against biological degradation has not been studied comprehensively. The objective of this research was to investigate the durability of OSB and LVL when exposed to wood decay fungi. Fourteen brown-rot and eight white-rot wood decay fungi were screened f...
V W Yang, B Illman, L A Ferge, R J Ross


Treatment of lumber with preservative/water repellent emulsions - The significance of shear stability on penetration
1997 - IRG/WP 97-20124
Currently, the treatment of lumber with a water repellent emulsion and a wood preservative formulation in combination is the most cost effective way to prevent decay and to maintain the appearance of uncoated lumber in service. Water repellents influence the movement of moisture into and out of wood and, by so doing, can decrease checking and splitting significantly. Adequate penetration of the em...
F Cui, K J Archer


A prototypical needle-incisor for refractory timber
1995 - IRG/WP 95-40041
A needle-incisor was manufactured for trial. This machine has an incising mechanism that a set of needles held by a rotary plate incises timber which is moved toward the front simultaneously, and then another set of needles incises a new part of the timber. Timber is incised by recycling the process. Timber incised of 4400 incisons/m² with the depth of 56 mm by 2.8 mm-diameter needles on all the ...
A Yakuwa, H Endoh, M Mori, S Doi


Essais de collage de bois traités pour la réalisation d'éléments de charpente lamellées. (+ abstract dated September 1971, Influence du traitement de préservation sur le collage d'éléments de charpente lamellés collés et efficacité vis-a-vis de larves néonates)
1971 - IRG/WP 203
Le but du travail est de vérifier les propriétés générales d'une poutre lamellée collée après traitement des éléments la composant au moyen de formulations insecticides et fongicides commerciales à solvant clair dans les conditions les plus usuelles de fabrication. Les essences utilisées ont été: Epicéa - Pin sylvestre - Sapin de Douglas en planches rabotées de 80 cm de lo...
J Guillemain-Thévenot


Sentry®, a new antisapstain formulation for protecting logs and lumber. - Part 2: protection of lumber
1999 - IRG/WP 99-30189
Recent research conducted by Forest Research, Chemcolour Industries (NZ) Ltd. and Fletcher Challenge Forest Ltd. has resulted in the development of antisapstain formulations that meet the efficacy requirements of the New Zealand Forest industry for export logs. One treatment, called Sentry®, is now poised for commercial use in New Zealand for treating export logs, having undergone an extensive su...
R N Wakeling, D R Eden, C M Chittenden, J G Van der Waals, B Carpenter, I Dorset, R Kuluz, J Wakeman


Remedial treatments of glulam = diffusion of active ingredients through glue lines from solid wood diffusable preservatives
1996 - IRG/WP 96-30117
Diffusable preservatives are very suitable for use in remedial treatments of laminated beams in which too high moisture content involves the development of wood destroying fungi. The diffusion of active ingredients (boric acid, disodium octoborate, bifluoride) is well observed in solid wood but in a composite wood, the glue lines may appear not only as a barrier for the diffusion but also, may be ...
D Dirol, S Mouras


Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown


Characterization of checks and cracks on the surface of weathered wood
2000 - IRG/WP 00-40153
The surface roughness of unweathered and untreated pine; unweathered copper chromium arsenate type C (CCA) - treated pine; weathered CCA-treated pine; and weathered CCA-plus-water-repellent (WR) - treated pine was evaluated by a stylus tracing method. Surface roughness parameters Ra, Rz, Rmax, Rk, Rpk, and Rvk were measured. Ra, Rpk, and Rvk were the most appropriate parameters for describing modi...
D P Kamdem, Jun Zhang


Termite attack on susceptible lumber above naturally durable support posts
2000 - IRG/WP 00-10370
A multi-year field study was designed to simulate the use of naturally durable sill plates (dodai) and floor support posts in Japanese housing construction and test whether Formosan subterranean termites (Coptotermes formosanus) would tunnel over or through these resistant timbers to attack susceptible Japanese red pine (Pinus densiflora) lumber placed above them. This test was intended to explici...
J K Grace


Borate diffusion in wood from rods and liquid product. Application to laminated beams
1988 - IRG/WP 3482
In the aim to use borate preservatives (fused rods and boracol) in fields of building construction other than external joineries, tests of diffusion of borate rods and secondary boracol, were carried out on different species of woods exposed to different moisture conditions. Tests were also applied on laminated beams very often subjected to high moisture contents and thus decay of rot fungi. Diffu...
D Dirol


Oxine copper (NYTEK® GD) for the control of mould and sapstain on lumber in North America
1989 - IRG/WP 3517
NYTEK® GD is a new, water-based, micro-dispersible formulation of oxine copper registered in the United States and Canada for control of mold and sapstain-causing fungi. NYTEK GD is noncorrosive and of low hazard to applicators and people handling treated lumber, when used according to the label. The product is an effective wood protectant applied as a dip or spray treatment at concentrations of ...
D F Myers, J M Fyler, C H Palmer, G D Rosebery


Dimensional lumber model demonstrates the sensitivity of the particle capture immunoassay in early detection of brown-rot fungi
1995 - IRG/WP 95-20058
A dimensional lumber model was designed to test the sensitivity of the particle capture immunoassay (PCI) compared to traditional methods of culturing and microscopic examination for detection of brown-rot fungi. Southern yellow pine 2 x 4's (5.1x10.2 cm²), and 86.4 cm in length, were inoculated on one end with the brown-rot fungus, Postia placenta, and tested over the full length of the...
C A Clausen, L Ferge


Integrated protection of freshly sawn lumber using Bacillus subtilis and selected fungicide
1997 - IRG/WP 97-10235
Bioprotection against stain fungi has tremendous potential for reducing discoloration of freshly sawn wood while decreasing chemical consumption. Unfortunately, most bioprotectants appear to be unable to consistently perform under the array of conditions to which freshly sawn wood is exposed. While research is underway to understand the nature of the inconsistent performance, a more pragmatic appr...
M E Mankowski, M Anderson, J J Morrell


Effect of climate, species, preservative concentration and water repellent on leaching from CCA-treated lumber exposed above ground
2001 - IRG/WP 01-50178
Few studies have examined leaching of chromated copper arsenate (CCA) from treated wood in above ground exposures due to the assumption that leaching is less severe compared to wood in continuous contact with soil or water. However, a significant portion of CCA treated wood is used for above ground applications, exposing considerable volumes of the preservative to precipitation and potential leach...
J L Taylor, P A Cooper


Previous Page | Next Page