IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 371 documents. Displaying 25 entries per page.


Algal growth resistance of paints for coating of wood; a laboratory study
1997 - IRG/WP 97-10213
Twelve paints were tested for resistance against algae. In addition, one algicidal compound commercially used for remedial treatments of algal growth on paints was tested for its effectiveness for prevention of algal growth. An agar diffusion bioassay was employed in which paint films on filter paper discs were placed on mineral salt medium and sprayed with an algal suspension containing a mixture...
J Bjurman


Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston


Laboratory evaluation of AC 217,300 as a termiticidal dust
1983 - IRG/WP 3247
Laboratory bioassays are described with the amidinohydrazone, AC217,300, a candidate termiticide to replace arsenic trioxide in termite control. When used as a dust and topically applied, AC217,300 was toxic to Coptotermes acinaciformis and Mastotermes darwiniensis. Although arsenic trioxide dust causes faster mortality in Coptotermes acinaciformis than AC217,300 dust, the latter has lower mammali...
J R J French, P J Robinson


The use of organic wood preservatives in ground contact and the suitability of laboratory test procedures to determine their efficacy
1999 - IRG/WP 99-20175
Organic fungicides, such as propiconazole, have proven to be highly effective when used as a co-biocide in recently developed wood preservative formulations. They have however been ineffective when used as a stand alone preservative, particularly when used in ground contact (European Hazard class 4). Previous research, using the test methods of ENV 807 (1993), provided conflicting evidence regardi...
I J Herring, D J Dickinson


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


Aggressiveness of Reticulitermes species in laboratory test
1993 - IRG/WP 93-10026
In European Standards concerned with the preventive action of wood preservatives against termites, i.e. EN 117, EN 118 the obligatory test species is Reticulitermes santonensis. It is argued that this species is more aggressive than the second European Reticulitermtes species, Reticulitermes lucifugus. Since Reticulitermes santonensis is confined to certain smaller areas in France and thus not rea...
H Hertel, S Pantos, D Rudolph


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


Methods of testing anti-stain chemicals for protecting sawn timber during storage and transport
1976 - IRG/WP 273
No international standard method for testing anti-stain chemicals for protecting fresh sawn timber exists. The methods used can be divided into three types: a) Rapid screening tests for finding chemicals effective against blue-stain and mould fungi. The chemicals are tested in agar medium, in pieces of filter paper or on small pieces of wood using pure cultures. b) Laboratory tests for evaluating ...
T Vihavainen


Laboratory evaluation of anti-sapstain formulations
1989 - IRG/WP 3510
Four formulations were tested for their efficacy in controlling molds and sapstaining fungi on wood according to the Standard-II of Japan Wood Preserving Association (JWPA). Relative efficacy was compared on the basis of visual rating of the fungal growth on the treated and untreated wood surfaces when the wood specimens were exposed to each monoculture of 5 test fungi at 26±2°C and 70-80% for 4...
K Tsunoda


Laboratory tests on the residual effects of pyrethroids against termites thirteen years after application
1994 - IRG/WP 94-30056
This paper is in continuation to a series of articles published on the work being developed in Brazil regarding the feasibility of using photostabl synthetic pyrethroids against termites. Tests were carried out to compare the efficacy of five synthetic pyrethroids with the traditional organo-chlorinated pesticide, chlordane. Wooden blocks were impregnated with alcohol-based solutions of the above-...
A M F Oliveira


Comparative study on the leaching of wood preservatives between natural exposure and accelerating laboratory conditions
1999 - IRG/WP 99-50134
Impregnated specimens with CCA, ACQ, and BAAC were subjected to leaching tests. Specimens of 2x2x1 cm3 in size were used for the laboratory leaching test for 10 days according to JIS K 1571. Specimens of 25x1 x1 cm3 were used for outdoor leaching test for 6 months. Total leaching amounts of boron per cm3 of specimens treated with BAAC were 325 µg in the laboratory test and 206 µg in the outdoor ...
K Yamamoto, S Motegi, A Inai


Inhibition of the biodegradation of coniferous and broadleaved wood by new imidazolium salts
2003 - IRG/WP 03-30320
Studies were carried out on fungicidal values of fourteen potential wood preservatives – modified quaternary heteroaromatic compounds using the screening agar-block. The vacuum treated blocks (22mm x 17mm x 12mm) of Scots pine (Pinus sylvestris L.), spruce (Picea excelsa L.), beech (Fagus silvatica L.) and birch (Betula verrucosa Ehrh.) with testing compounds were exposed to Coniophota puteana a...
J Zabielska-Matejuk, J Pernak, W Wieczorek


Changes in transverse wood permeability during the drying of rimu and radiata pine
1990 - IRG/WP 3636
When softwoods are dried and subsequently impregnated with waterborne preservatives two problems frequently occur, preservative screening of multi-salt preservatives and difficult re-drying. To study the causes, the permeability of rimu and radiata pine wood has been measured along the three principal directions. The radial and tangential permeabilities of the green sapwood of the two species were...
R E Booker


Implications for comparability of laboratory experiments revealed in studies on the effects of population density on the vigour in groups of Coptotermes lacteus (Froggatt) and Nasutitermes exitiosus(Hill) (Isoptera: Rhinotermitidae, Termitidae)
1983 - IRG/WP 1197
(Summary of paper 1194) The vigour - survival and wood consumption - of groups of Coptotermes lacteus and Nasutitermes exitiosus was measured when termites were kept at different population densities (g termites/ mL) by changing group size and/or volume of the holding container. A characteristic pattern emerged. At low population densities (< 0,01 g/mL) performance of termites improved with an increase in group size; at higher population densities it tended to decline. The impact of altering group size and container volume on termite vigour was most pronounced at low densities; at higher population densities, performance tended to be more stable but declined markedly when termites became overcrowded. In most jar-type experiments on termites, especially those conducted in Europe and the U.S.A., small groups of termites are housed in disproportionately large jars, resulting in very low, sub-optimal population densities. Suggestions are made for improvements in experimental design that would lead to an enhancement of the comparability of results from different laboratories.
M Lenz, R A Barrett, E R Williams


Efficacy of a novel copper-based organic solvent preservative in laboratory and fungus cellar tests
1995 - IRG/WP 95-30071
The efficacy of Chemicca 4, a novel copper-based organic solvent preservative, was compared with that of other LOSP in pure culture laboratory decay tests and with that of CCA and TBTO in a fungus cellar exposure. It was markedly superior to copper and zinc naphthenates at equivalent metal retentions in laboratory decay tests, and similar in activity to TBTO. After 60 months&apos; fungus cella...
M E Hedley, P N Maynard


Laboratory evaluation of disodium octaborate tetrahydrate (TIM-BORÒ ) as a wood preservative or a bait-toxicant against the Formosan and eastern subterranean termites (Isoptera: Rhinotermitidae)
1991 - IRG/WP 1513
A no-choice bioassay indicated that termite feeding was significantly reduced when wood was treated with TIM-BORÒ at retentions of >3600 ppm and >900 ppm (w/w) for Coptotermes formosanus and Reticulitermes flavipes, respectively, and thus these wood preservative retention rates may be considered for these termite species. Results of a choice bioassay suggested retention rates of 450-1800 pp...
N-Y Su, R H Scheffrahn


The effect of high and low boron soils on foraging termite behaviour and their metabolic systems
2007 - IRG/WP 07-10602
The highest concentrations of boron are found in ground water and soils of some of the driest climate areas (arid and semi arid regions) in the world. This present study examined the various concentrations of boron levels on filter papers against the subterranean termite species Coptotermes from different provenances and different boron soil levels. The termites were presented with no-choice bioas...
B M Ahmed, J R J French, P Vinden


Laboratory Evaluation of Soft Rot Resistance of Non-Durable Lesser-Known Malaysian Hardwoods
2006 - IRG/WP 06-10582
Resistance of six non-durable lesser-known Malaysian hardwoods, Pulai (Alstonia spp.), Rubberwood (Hevea brasiliensis), Ludai (Sapium spp.), Jelutong (Dyera costulata), Gaham Badak (Blumeodendron tokbrai) and Kayu arang (Diospyros spp.) compared with temperate Scots pine sapwood (Pinus sylvestris), were evaluated using the unsterile soil burial (mixed with Chaetomium globosum) versus vermiculite-b...
A H H Wong


The “wire-loop slicing technique” for the rapid field collection of large numbers of Coptotermes acinaciformis termites from above-ground mound colonies
2006 - IRG/WP 06-10583
This technique of rapidly slicing through an above-ground C. acinaciformis mound colony with a steel wire-loop attached to a vehicle allows the collection of large numbers of termites. The sliced mound topples onto a tarpaulin arranged on the ground, the outer wall layers break away in large segments, and the carton materials incorporating the termites are readily collected and transferred to larg...
B M Ahmed, J R J French


Effects of chlorothalonil (CTN) and butylated hydroxytoluene (BHT) on microbial communities involved in the deterioration of wood using T-RFLP I: Accelerated laboratory decay study
2006 - IRG/WP 06-20332
The effects of Chlorothalonil (CTN) and Butylated Hydroxy Toluene (BHT) on microbial species diversity in wood and the surrounding soil are being assessed by Terminal Restriction Fragment Length Polymorphism (T-RFLP). CTN was selected as a trial organic wood preservative, and BHT is being evaluated for its synergistic effects with CTN. Results from an accelerated decay test will be presented. The...
G T Kirker, M L Prewitt, S V Diehl


The Use of Modulus of Elasticity and Modulus of Rupture to Assess Wood Decay in Laboratory Soil-Bed Test
2006 - IRG/WP 06-20338
The efficacy of wood preservatives were determined in a soil-bed test. Samples of alder wood sapwood (Alnus glutinosa subsp. barbata) (5x10x100 mm) were treated with Solutions of CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Modulus of Elasticity, modulus of rupture, mass loss and decay rate according to AWPA E7 wer...
A Temiz, Ü C Yildiz


Laboratory methods for assessing the resistance of wood plastic composites to fungal attack.
2006 - IRG/WP 06-20340
Wood plastic composites (WPC’s) have many attractive material features including dimensional stability and resistance to moisture, but the wood in these materials remains susceptible to fungal attack. Assessing WPC decay resistance in laboratory trials has proven difficult because the slow moisture sorption characteristics of this material do not allow for sufficient fungal attack over the trad...
J J Morrell


Standard Test Methods for Wood Preservatives by Laboratory Agar-Block Test
2006 - IRG/WP 06-20350
Wood is one of the most valuable and versatile resources for all sorts of constructional purposes. But timber in its various forms is subjected to several types of deterioration. This standard lays down the method for the laboratory determination of threshold value of wood preservatives against fungi. Most chemicals are initially tested for their ability to control decay fungi in agar-block tests....
P K Sarker, M A Rahman, M R Bulbul, T Das, G N M Ilias


Preliminary screening of a boron based wood preservative for biological efficacy (fungicidal) in treated timber
2006 - IRG/WP 06-30396
The resistance of Pinus radiata D.Don sapwood blocks, treated with a boron based preservative, to attack by five wood destroying fungi (Fomitopsis lilacino-gilva, Coniophora olivacea, Gloeophyllum abietinum (boron resistant), Serpula lacrymans and Perenniporia tephropora) was investigated. A phenyl pyrazole termiticide (fipronil) was also incorporated into the formulation to examine if its presen...
S R Przewloka, J A Hann, P Vinden


Laboratory bioassay and field trial on imidacloprid and cypermethrin as glueline treatments for softwood plywood
2006 - IRG/WP 06-30405
The effectiveness of imidacloprid and cypermethrin as glueline treatments for protecting phenol formaldehyde (PF)-bonded Pinus radiata (radiata pine) plywood from attack by subterranean termites was evaluated both in the laboratory and field. Imidacloprid was evaluated in two plywood constructions (19 ply x 1.6 mm-thick veneers and 5 ply x 3.2 mm-thick veneers) whereas cypermethrin was evaluated i...
J W Creffield, D K Scown


Previous Page | Next Page