Decay types observed in small stakes of pine and Alstonia scholaris inserted in different types of unsterile soil
1990 - IRG/WP 1443
The attack of various wood-degrading microorganisms occurring in mini-stakes of pine and Alstonia scholaris buried in various types of unsterile soil was studied. Attacks by white rot, brown rot, soft rot, erosion bacteria, tunnelling bacteria and actinomycetes were found. Soft rot occurred in all soils, whereas attack by white rot and especially brown rot and erosion bacteria was rare. The type o...
T Nilsson, G F Daniel


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


Soft rot decay of Eucalyptus maculata Hook. in different soils from Queensland, Australia
1980 - IRG/WP 1113
In the present work, different Queensland soils were chosen and their gross effects on the decay of treated and untreated Eucalyptus maculata examined. The soils were also amended with various levels of phosphate to study the response of the wood decay mycota to an increasing supply of this nutrient. Phosphate amendment was chosen because of the wide-scale use of superphosphate on Queensland soils...
L E Leightley, I W Russell


Effects of boron treatments on partially decayed oak and pitch pine heartwood
1996 - IRG/WP 96-30106
This paper reports results of borate based preservative treatment and leaching experiments on partially decayed oak and pitch pine heartwood. Previous experiments have shown little damage is caused to sound timber of these types when treated with Polybor and Boracol 20 preservatives. This experiment was carried out to assess the suitability of selected borate based preservatives for use in histori...
S McCutcheon, G M Smith, J W Palfreyman, P Durrant


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Role of cell wall structure in soft rot decay of bamboo
1995 - IRG/WP 95-10133
Models of soft rot hyphal penetration of bamboo cell walls are proposed. Soft rot hyphae show an interesting capability of penetrating the bamboo cell wall in different forms; typical longitudinal penetrating hyphae and tangentially orientated penetrating hyphae. The second form of penetration was found to be different from that normally associated with wood cell walls. The differences can be attr...
O Sulaiman, R J Murphy


Laboratory bioassay on the termiticidal efficacy of two ACQ formulations
1999 - IRG/WP 99-30199
The termiticidal efficacy of two ammoniacal copper quaternary ammonium formulations (ACQ) was evaluated in a laboratory bioassay using two species of subterranean termites, Mastotermes darwiniensis Froggatt and Coptotermes acinaciformis (Froggatt). Five retentions (1.0, 2.0, 4.0, 6.0 and 8.0 kg/m3 of active ingredient) of each ACQ formulation (MitrexACQ and ACQ97) were assessed in sapwood specimen...
J W Creffield, A F Preston, N Chew


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


Modelling the control of decay in freshly felled pine poles
1997 - IRG/WP 97-10206
In a recent study investigating control of decay in freshly felled pine utility poles, it became apparent that the efficacy of different treatment methods was strongly related to the size of the material being treated. A topical application of 5% w/v disodium octaborate tetrahydrate (DOT), brush applied to the cut surfaces of logs with otherwise intact bark was just as effective at excluding white...
M W Schoeman, W Van der Werf, J F Webber, D J Dickinson


An evaluation of CCA, CCB and CCP preservatives using a "sandwich test"
1991 - IRG/WP 2370
The last two years has seen some important changes in standards and preservative types used in Scandinavia, which have led to a wider choice for specifiers. In order to identify those treatments suitable for replacement or reinforcement of decayed constructional timbers, it was felt necessary to modify the standard EN 113 test. Impregnated blocks were sandwiched between two untreated blocks, previ...
A P Koch, L B Sheard


The performance of CCA treatment in bamboo against decay fungi
1993 - IRG/WP 93-30027
Samples of culm wall material from young (< 6 month age) and mature (> 3 years age) culms of the bamboo, Phyllostachys virideglaucescens were treated to equivalent% w/w retentions of a CCA preservative. After fixation and leaching the treated samples were exposed to decay by Chaetomium globosum FPRL S70K, Coriolus versicolor FPRL 28A and Coniophora puteana FPRL 11E. Thin section samples of u...
O Sulaiman, R J Murphy


Movement and persistence of Dazomet and pellected methylisothiocyanate in wrapped Douglas fir and southern pine timbers
1991 - IRG/WP 1496
The movement and persistence of Dazomet (tetrahydro-3,5-dimethyl-2 H-1,3,5 thiadiazine-6-thione) and pelleted methylisothiocyanate (MIT) was evaluated in wrapped Douglas-fir and Southern Pine timbers. MIT pellets did not impart a fungistatic effect to any of the timbers. Failure of MIT was probably due to loss of MIT from pellets prior to application. Fungistatic effect of Dazomet was consistently...
T L Highley


Preliminary field and laboratory findings regarding the efficacy of a novel anti-marine wood borer agent
2000 - IRG/WP 00-10380
Blocks of sapwood of Pinus nigra were treated by vacuum impregnation with Biocide A to retentions of 0.5, 1 and 2 kg m-3. Similar blocks were vacuum-pressure impregnated with CCA to retentions of 2, 24 and 38kg m-3. The blocks were exposed subtidally in Mourilyan Harbour (Queensland, Australia). After 5 and 10 months exposure, blocks were removed, examined for superficial signs of attack by wood b...
A Praël, S M Cragg, R A Eaton


Work programme of CEN/TC 38 (April 1999) and European publications
1999 - IRG/WP 99-20165
Scope of the CEN/TC38: Standardization of the characteristics of natural or conferred durability of wood and its derived materials against biological agents, including the characteristics of protection products and associated processes to obtain this durability. This applies in particular to: - the identification of hazard classes-, - the test methods (wood preservatives and treated wood and wood ...
R Hüe


Development on Damage Functions of Wood Decay for Building Envelope Design
2005 - IRG/WP 05-10556
For the hygrothermal analyses of building envelope systems for insulation design, we tried a natural decay test of wetted wood specimens without any inoculation of fungi. Three principal experimental types: under steady-state conditions (Experiment A), at a cyclic water dripping under Non-steady conditions (Experiment B) and at a cyclic water dipping under-steady conditions (Experiment C), were ca...
H Suzuki, Y Kitadani, K Suzuki, A Iwamae, H Nagai


Chemical, physical and biological factors affecting wood decomposition in forest soils
2003 - IRG/WP 03-20281
Organic matter (OM) decomposition is an important variable in determining the potential of forest soils to sequester atmospheric CO2. Studies using OM from a particular location gives site-specific decomposition information, but differences in OM type and quality make it difficult to compare results among soils and forest ecosystems. By using a “standard” OM in decomposition studies, OM qual...
M Jurgensen, P Laks, D Reed, A Collins, D Page-Dumroese, D Crawford


Kinetic of the wood degradation produced by wood decay fung
1993 - IRG/WP 93-20016
The degradation degree of a wooden structure has a direct influence on its loss of mechanical strength. It&apos;s necessary to deepen in non destructive techniques which permit to extrapolate the results obtained in laboratory to structural timber used in the building&apos;s construction. This work studies the relationship existing between the pulse velocity of ultrasonic waves and the wei...
M T De Troya, A M Navarrete, A Sanchez, V Bucur


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


Novel observations on the micromorphology of soft rot attack of wood
1996 - IRG/WP 96-10176
Electron microscopic examinations of decaying Pinus radiata horticultural posts which had been treated with CCA preservative prior to being placed in service about nine years ago showed the presence of soft rot fungi and tunnelling bacteria. Some novel observations on the micromorphology of the soft-rotted areas of tracheid walls are described here. The micromorphology of soft-rotted areas was hig...
A P Singh, R N Wakeling


Biological control of sapstain fungi in wood
1996 - IRG/WP 96-10158
Sapstain fungi can cause serious damage to wood and wood products, resulting in a significant economic loss for the wood products industry. The purpose of the present investigation was to determine whether the sapstain in wood caused by sapstain fungi could be biologically controlled. Biological control of sapstain fungi in wood was demonstrated in field trials with nonpigmented isolates of Cerato...
S C Croan


Laboratory evaluation of chlorothalonil formulation for stain and mold control on rubberwood and maple
1998 - IRG/WP 98-30175
We evaluated the efficacy of several chlorothalonil and carbendazim fungicides (F1 and F2), etc. in the control of mold and stain fungi on rubberwood and maple. The results showed that these formulations effectively inhibited the selected fungal species such as Aspergillus niger, Penicillium sp., Trichoderma sp. (P71H), Aureobasidium pullulans, Ceratocystis minor (C-188), Ceratocystis pilifera (RW...
Mingliang Jiang, T L Highley, L Ferge, T L Woods


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980&apos;s against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


The influence of gaseous oxygen concentration on fungal growth rates, biomass production and wood decay
1998 - IRG/WP 98-10283
The effects of air and several levels of oxygen balanced with nitrogen (% oxygen (v/v) nitrogen to 100%) on growth rates, biomass production and wood decay were investigated. The best technique for measuring daily growth rates in anaerobic jars was found to be by using 40 mm petri dishes which were attached to the walls of the jars. At the end of the test period the same petri dishes were also use...
S M Kazemi, D J Dickinson, R J Murphy


Biocontrol and bioprotection of wood decay and sapstain fungi
2003 - IRG/WP 03-10474
The most serious damages caused in the wood industries by decay and sapstain fungi, and the growing international pressures on the use of biocides products with toxic active ingredients harmful to human health and the environment, have made it necessary to search for alternative chemical products to protect the wood, and for the possibility to use micro-organisms as biological controllers. This la...
M T De Troya, F Rubio, M Villarreal, F Arenal, F Llinares, V Rubio, D Muñoz-Mingarro, N Acero