Collaborative soft rot tests: Specific gravity loss resulting from soft rot
1973 - IRG/WP 227
It was proposed at the 5th meeting of Working Group II of the IRG in June 1973 in Lahti, Finland, that the specific gravity (swollen volume basis) of test blocks used in the IRG Collaborative Soft Rot Tests should be determined on all the blocks at the completion of the exposure period. Specific gravity determined on the basis of the oven dry weight and water swollen volume was selected because (1...
C R Levy


Leaching of components from CCF treated timber in ground contact
1998 - IRG/WP 98-50108
In order to investigate the depletion of different CCF-salts during service small stakes (10*10*450mm³) were treated with five water-borne wood preservatives and after fixation brought into ground contact for several years. After failing some of the broken down stakes were used to determine the remaining concentration of relevant ions and their distribution in different segments of the stakes. A...
E Melcher


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Pretreatment decay in poles of Pinus sylvestris
1987 - IRG/WP 1329
Storage damage by blue stain and decay in poles before impregnation has been increasingly observed during recent years and there have been reports that salt-impregnated poles today are of lower quality because of incipient decay being increasingly common. The attacks may have started at the time of cutting and then continued during the period of seasoning at the plant, which could be as long as tw...
H Lundström, M-L Edlund


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Antagonism of Gliocladium virens against wood decay fungi
1995 - IRG/WP 95-10102
Antagonistic abilities of a commercial biofungicide, Gliocladium virens (GL-21, Grace) were evaluated against three white-rot fungi, Trametes versicolor, Phlebia brevispora, Irpex lacteus, and three brown-rot fungi, Postia placenta, Neolentinus lepideus, Gloeophyllum trabeum. In dual culture of Gliocladium virens and wood decay fungi, Gliocladium virens rapidly overgrow the decay fungi and killed ...
T L Highley, L Ferge


Leaching tests on CCA-treated wood using inorganic salt solutions
1984 - IRG/WP 3310
Pinus radiata sapwood treated to approximately 10 kg/m³ with Tanalith NCA or Tanalith C-type CCA preservatives was ground to a fine powder and samples were then leached with solutions of calcium chloride, calcium nitrate, magnesium nitrate, or a mixture of potassium di-hydrogen orthophosphate and di-potassium hydrogen orthophosphate, at 0.03M-1.00M solution concentrations. Leached wood samples we...
D V Plackett


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


Antagonistic effects of Dacrymyces stillatus against growth of other fungi
1991 - IRG/WP 2363
The antagonistic effects in dual cultures on malt extract agar of 5 wood decay fungi and the antagonistic effects of Dacrymyces stillatus against 1 mould fungus and 1 blue stain fungus were determined. Dacrymyces stillatus was the only fungus which exhibited clear antagonistic effects. The effects of Dacrymyces stillatus against the different test fungi varied however to a great extent. Dacrymyces...
J Bjurman


A non-destructive testing technique for wood poles
1987 - IRG/WP 2293
A method has been developed to evaluate the stiffness and condition of a wood pole based on structural dynamics. This paper describes the results of tests performed on nearly 200 wood utility poles across Western Canada. A high correlation exists between the dynamic non-destructive test and direct mechanical tests. The need for an accurate non-destructive testing technique is demonstrated by the f...
W M Murphy, D E Franklin, R A Palylyk


Wood cement composites using spent CCA treated wood
1999 - IRG/WP 99-50126
The feasibility of using spent or out-of-service CCA treated wood as a component of wood/cement composites was evaluated. Cold pressed wood particle cement boards were made using CCA treated particles from a red pine (Pinus resinosa Ait.) pole removed from service and from untreated red pine wood from a new pole. Boards were manufactured using a range of wood to cement ratios and water to cement r...
Chen Huang, P A Cooper


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


A comparison of fatty acid and molecular profiles for identification of wood colonizing basidiomycota
2003 - IRG/WP 03-20278
Two methods that are currently being employed to detect and identify wood decay fungi are Fatty Acid Methyl Ester (FAME) analysis and Restriction Fragment Length Polymorphism (RFLP) analysis. A FAME library and RFLP library for 9 species and up to 10 strains within each species have been developed. The profiles generated by these methods have been compared for each species and strain to test for...
T C McElroy, L Prewitt, S V Diehl


The control and pretreatment decay in air seasoning Scots and Corsican pine poles in England
1990 - IRG/WP 1451
Previous work clearly showed that air-seasoned, British grown Scots and Corsican pine poles are subject to serious pretreatment decay. In order to control these infections a range of pretreatments are currently being investigated. One series of treatments is designed not only to control decay but also allow the development of mould and stain fungi in order to achieve the desired increases in poros...
D J Dickinson, A R Zahora, A P Dodson


Chitin synthetase activity in cellular fractions of wood-decay fungi
1992 - IRG/WP 92-1524
This study was an attempt to explain the variability of in vivo sensitivity of wood decay fungi to the chitin synthetase (CS) inhibitor, polyoxin, by comparing CS distribution in cellular fractions. The five species studied were the brown-rot fungi Coniophora puteana, Gloeophyllum trabeum, Fibuloporia vaillantii, and the white-rot fungi Schizophyllum commune and Ganoderma applanatum. The CS activi...
B R Johnson, S C Croan, B Illman


Decay rates and strength and stiffness loss in foundation beams
1992 - IRG/WP 92-1563
The TNO Centre for Timber Research has executed an extensive research programme into the rate of decay in foundation beams, as a result of lowering of ground water tables. The aim of the research was to develop a method, predicting the decrease in strength and stiffness in beams, due to wood decay during drytime of foundation beams. With the calculated extremes in decay, the damage caused by local...
P Esser, H S Buitenkamp


Laboratory evaluation of anti-sapstain formulations
1989 - IRG/WP 3510
Four formulations were tested for their efficacy in controlling molds and sapstaining fungi on wood according to the Standard-II of Japan Wood Preserving Association (JWPA). Relative efficacy was compared on the basis of visual rating of the fungal growth on the treated and untreated wood surfaces when the wood specimens were exposed to each monoculture of 5 test fungi at 26±2°C and 70-80% for 4...
K Tsunoda


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 17: Report of fifth inspection (4 years) in Italy
1983 - IRG/WP 4103
The wood samples of Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitude 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian coast. The recorded temperature varies from 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 12 ...
A Gambetta, E Orlandi


Evaluation of fungi isolated from the galleries of the striped ambrosia beetle Xyloterus lineatus (Ol.) (Col., Scolytidae)
1995 - IRG/WP 95-10092
Fungi from the galleries of the striped ambrosia beetle Xyloterus lineatus (Trypodendron lineatum) (Ol.) found in spruce logs were studied. The following fungi were isolated and identified: Trichoderma harzianum Rifai, the yeast Pichia anomale Hansen (Kurzman), the blue-stain fungus Ceratocystis piceae (graphium) (Münch) Bakshi and a fungus closely similar to Ceratocystis araucariae (anamorph). T...
G Babuder,F Pohleven


Questionnaire relating to the occurrence, prevention and repair of Dry Rot attacks in buildings
1989 - IRG/WP 1418
Dry Rot attack in buildings has become an increasing problem in Denmark. The reason is that old multi-storey houses from about 1890-1920 are being renovated and modernised and connected to this well-hidden Dry Rot attacks are detected. The traditional methods for repair used in Denmark are very expensive but with a high degree of confidence when done carefully. There is a big need for development ...
A P Koch


A comparison analysis of eight strains of Serpula lacrymans (Schum. ex Fr.) S.F. Gray
1991 - IRG/WP 2362
Investigations were previously carried out to compare eight strains of Serpula lacrymans (Schum. ex Fr.) S.F. Gray (some used in various countries as standard test strains): FPRL 12C (England), FPRL 12E (Germany), Warsaw III (Poland), HFP 7802 (Japan), DFP 16508, 16509, 16521 and 16522 (Australia). Studies included growth rate and dry mass of mycelium, decay capacity, reduction of compression stre...
J Wazny, J D Thornton


Antagonism of Scytalidium lignicola against wood decay fungi
1989 - IRG/WP 1392
Antagonistic abilities of Scytalidium lignicola against white- and brown-rot wood decay fungi were evaluated. Scytalidium lignicola did not produce inhibition zones but overgrew the decay fungi on a malt-agar medium and in most cases killed them. Pretreatment of Douglas-fir and Southern pine blocks with Scytalidium lignicola prevented decay. Blocks that were heated or treated with propylene oxide ...
T L Highley


Interactions between soft rot fungi and CCA preservatives in Betula verrucosa
1988 - IRG/WP 1367
Ultrastructural investigations were carried out to obtain information on the cell wall distribution of CCA elements during soft rot decay of 4% K33 CCA preservative treated birch (Betula verrucosa) wood. TEM observations on fibres at various stages of S2 cavity formation by mutabilis showed a distinct pattern of electron dense materials to occur within the S2 cell wall region. These materials (gra...
G F Daniel, T Nilsson


The critical timing of inspections for field testing of natural durability
1994 - IRG/WP 94-20018
An overestimation of performance will almost always result if the condition of a specimen is considered to be attained at the precise time that an inspection is carried out. The time at which the condition is actually attained, referred to in this document as the "Condition time", is best considered to be halfway between two successive inspections. The requirement to obtain data that is relevant t...
J D Thornton