IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 337 documents. Displaying 25 entries per page.


Phenol formaldehyde modification and termite resistance under laboratory testing
2022 - IRG/WP 22-40952
The development of phenol formaldehyde (PF) resins as a means of impregnating solid wood is one that has been explored for several decades, both in terms of conventional impregnation processing (Impreg) or compressional impregnation (Compreg). However, it is only recently with advances in processing conditions that the method truly affords a means of achieving conventional modification for solid t...
L Nunes, A Pitman, M Duarte, B Stefanowski, D Jones


Natural durability of 9 tropical species suitable for round wood timber building: fungi and termites laboratory screening tests
2023 - IRG/WP 23-11013
In numerous tropical forest species, wood properties are poorly described and wood is under-valorized. Especially very few is known about small diameter trees although they may be used, directly as round wood, in construction timber building. A selection of abundant species was done and characterization tests were performed to assess their usability as building material. The aim of this work was t...
M Leroy, K Candelier, J Damay, J Bossu, R Lehnebach, M-F Thevenon, J Beauchene, B Clair


Efficacy of a wide-spectrum plant bio-based anti-termite product - Laboratory trials
2023 - IRG/WP 23-11024
Compared to the number of timbers available, the list of wood species resistant to termites is rather limited and largely composed of tropical timbers. In addition, due to climate change and environmental degradation, together with global trade, a significant global expansion of termites is predicted along with the economic losses due to their activities. Therefore, there is a demand to find produ...
M-F Thévenon, F Chopinet, J Vuillemin, A Robert, S Lafay, D Messaoudi


Laboratory durability testing of preservative treated wood products – first attempts and observations
2023 - IRG/WP 23-20697
In the past, durability classes (DC) had been assigned to wood species, sometimes also to homogenously modified wood-based materials such as thermally modified wood. More recently, some standards allow for classifying the biological durability of chemically modified wood, preservative treated wood and wood composites. Even treated products may be subject to durability classification, but necessary...
C Brischke, M Sievert, M Schilling, S Bollmus


Accelerated surface mould testing for exterior wood treatment in Temperate, Tropical and Laboratory environments
2023 - IRG/WP 23-20699
Mould attack is a very common cause of discoloration on wooden surfaces and can subsequently promote development of wood decay by other organisms. Prevention of mould growth is relevant for both pigmented wood paints as well as more transparent systems with a high or low amount of binder. The use of commercial biocides has led to effective microbiological inhibition in many contexts, but the incre...
A Nazeri, J Stenbaek, T R Laursen, A H H Wong, B M Hasnul


Establishing the minimum effective penetration of wood preservatives in the refractory heartwood of E. nitens
2023 - IRG/WP 23-30780
Conventional pressure treatment of many Australian hardwoods results in little to no penetration of heartwood and a non-uniform envelope treatment of <5 mm surrounding a mostly untreated core. This is a major issue for many of the low durability plantation hardwood timbers that are grown in Tasmania, which contain high percentages of heartwood. Long term studies on softwoods such as spruce decking...
J R Vargas, J J Morrell, L Yermán, K C Wood


Performance of treated Malaysian semantang bamboo (Gigantochloa scortechinii) - field and laboratory durability evaluation
2023 - IRG/WP 23-30788
Field performance of sematan bamboo, Gigantochloa scortechinii was evaluated under the Malaysian tropical climate, along with laboratory evaluation to white-rot fungi and mold. Starch was removed from the bamboo by submerging the bamboo in the river for 6-8 weeks, kiln-dried and cut to 300 mm (L) round bamboo and 25 mm (W) x 50 mm (L) stripe for the field and laboratory test respectively. Bamboo w...
S Lipeh, T Khadiran, Z Jalaludin, M K Anwar U


Laboratory evaluation of PA1b, an insecticidal protein extracted from pea seeds (Pisum sativum), as bait active ingredient against the subterranean termite Coptotermes gestroi (Blattodea: Rhinotermitidae) in tropical zones
2024 - IRG/WP 24-11038
Coptotermes gestroi (Wassman 1896) is one of the worst pests in tropic areas, economically. Two types of curative methods are used since decades to eliminate colonies that attack constructions: injection of biocidal treatment solutions on wood, walls and soil, and population control using baits. In application of the current regulations, the first technique can no longer be used in Europe, to lim...
J Vuillemin, D Messaoudi, P da Silva


Laboratory and field evaluations of bio-based termiticide containing Arnica extract from Berkem Biosolutions® against native and Formosan subterranean termites
2024 - IRG/WP 24-11049
Arnica extract from Berkem Biosolutions® is a 100% plant-based ingredient, rich in active molecules, particularly polyphenols, specially adapted to the needs and challenges of termite protection. The efficacy performance of a bio-based termiticide product containing Arnica extract from Berkem Biosolutions® had been evaluated both in soil treatment and in wood protection treatment against native ...
D Messaoudi, J Curole, Q Wu


Studies on the treatability of selected pine species and corresponding efficacies of a new non-biocidal treatment
2024 - IRG/WP 24-20721
Wood decay caused by fungi may reduce the service life of wood in outdoor applications. Since moisture conditions in wood occur as one of the most crucial parameters for fungal decay, chemical modifications, which affect the latter, may increase the resistance of wood against such organisms. Usually, pine sapwood is easier to chemically treat than heartwood, as the former generally shows good perm...
T R da Silva Lins, L Emmerich, H Militz, P H Gonzales de Cademartoni, R J Klizke, M Pereira da Rocha


Phytosanitary heat treatment of wood in a laboratory drying oven and, in a pilot-scale kiln using the house longhorn beetle (Hylotrupes bajulus) larvae as a model
2024 - IRG/WP 24-20722
International trade in wood products brings the risk of the movement of tree pests which can cause devasting ecosystem and economic damage. International phytosanitary guidelines were created to help countries that import wood products. Import requirements intend to minimize pest spreading. Thus, the ISPM 15 (International Standards for Phytosanitary Measures No. 15) which specifies the “Regulat...
B Rubio, C L’Hostis, M Montibus, I Paulmier, C Brunet, L Charron, J-P Gaussorgues, C Guiberteau, V Vlahakis, F-R de Cibon, I Le Bayon


Copper migration from preservative-treated Douglas-fir decking: models vs laboratory leaching data
2024 - IRG/WP 24-50390
The ability of a model to predict copper migration from Douglas-fir treated with organic metallic substances into a freshwater slough was evaluated against data generated through simulated overhead leaching. The model predicted very high loadings of ammoniacal copper zinc arsenate, alkaline copper quaternary or copper azole that had the potential to impact water quality while data from the exper...
M J Konkler, G Presley, J J Morrell, T Singh


Previous Page