The effect of aqueous leaching on moisture uptake by CCA-treated blocks during soil burial
1987 - IRG/WP 2283
Mass loss, moisture content and nitrogen data from two soil burial experiments with untreated and CCA-treated Scots pine (Pinus sylvestris L.), Sitka spruce (Picea sitchensis Carr) and lime (Tilia vulgaris Hayne) are presented. These show that aqueous leaching of CCA-treated wood prior to burial significantly reduces its subsequent moisture uptake from soil. In the case of lime, a reduction in the...
C A Green, G M Smith, B King


Standard and accelerated testing of boron-additive wood protection systems
2005 - IRG/WP 05-30381
The main objective of this research was to determine the effectiveness of boron-additive protection systems for above ground applications by means of field testing. The two field test procedures used are based on the L-joint test described in the European standard EN 330. For the first set up the boron treated timber was coated in accordance with the standard EN 330 system. The second set up is ba...
A Mohareb, J Van Acker, M Stevens


A comparison of the leaching resistance of copper 2-ethanolamine and copper ethylenediamine treated Scots pine
2000 - IRG/WP 00-30233
The depletion of copper from copper 2-ethanolamine and copper ethylenediamine treated Scots pine blocks was investigated. A greater leaching resistance was found for copper 2-ethanolamine, which retained ca. 86% and ca. 50% copper after water and buffer leaching, respectively. Leached amine treated blocks also contained significant residual amine. This was consistent with other observations linked...
Xiao Jiang, J N R Ruddick


Comments on soft rot attack in timbers treated with CCA preservatives: A document for discussion
1982 - IRG/WP 1167
This paper is not based on any particular results but rather on several observations of soft-rot during many years of studies, and on a review of the existing literature. The short time available has unfortunately not permitted a detailed review of the literature. Data and knowledge of important facts are lacking for several aspects of soft-rot attack and for reactions occurring in the wood as a r...
T Nilsson


A quantitative weathering study of wood surfaces modified by chromium VI and iron III compounds
1989 - IRG/WP 2330
Thin veneers of Pinus radiata were treated with dilute aqueous solutions of chromium VI and iron III compounds and exposed to natural weathering for 35 days. Zero-span tensile strength and weight losses of treated veneers were compared with losses observed in untreated specimens In a study designed to demonstrate the applicability of strength and weight loss measurements to the rapid quantitative ...
P D Evans, K J Schmalzl


Co-operative studies on determining toxic values against wood-destroying basidiomycetes: Progress report to April 1990
1990 - IRG/WP 2357
This document reports progress on the co-operative study between nine laboratories, set up following the proposals contained in Document IPG/WP/2316 (1988). Results have been received from eight laboratories. Toxic values data have been established successfully for the test fungus Coniophora puteana with soil, malt agar and vermiculite methods and with the test fungi Gloeophyllum trabeum and Poria...
J K Carey, A F Bravery


Relationship between the bending strength and the degree of termite attacks on western hemlock by Coptotermes formosanus Shiraki
1990 - IRG/WP 1434
For the examination of the relationship between the bending strength and the degree of termite attacks, Western Hemlock (Tsuga heterophylla Sarg.) was used. Sixty specimens (4.5 x 4.5 x 82 cm³) were attacked by termites at the culture room of Coptotermes formosanus Shiraki. The termites were introduced on the central parts (10 cm) of specimens. In the case of the 2 points loading, the bending mom...
K Suzuki, T Tanaka


Wood detection by the marine isopod Limnoria.markup
1995 - IRG/WP 95-10134
The search for alternative control methods for Limnoria, should perhaps focus on the most vulnerable stage during the isopod life cycle - during dispersal when adulls leave their tunnels to find new wood. Dispersal is known to be triggered by environmental conditions, although how Limnoria locate fresh wood is unknown. Literature available on Limnoria dispersal, their sensory capabilities during d...
S M Henderson, S M Cragg, A J Pitman


The natural history of teredinid molluscs and other marine wood borers in Papua New Guinea
1975 - IRG/WP 410
The teredinids, commonly known as teredos or shipworms, are bivalve molluscs adapted to boring into wood. They are most closely related to the Family Pholadidae, or piddocks, which bore into mud, stone and coral. The teredinids have a relatively small, hemi-spherically shaped shell, the elongated body extending beyond the posterior end of the shell valves. The soft body, protected by the wood and ...
S M Rayner


A new type of biocide suitable for use in different fields of wood preservation
1993 - IRG/WP 93-30014
A new type of polymeric biocides was developed containing quaternary ammonium and boron ester groups as active structure elements, to overcome the disadvantages of AAC's in wood preservation use and to utilise their good performance due to a broad efficacy against fungi on the other hand. The new biocides called polymeric betains have been tested in laboratory and field tests and especial...
V Barth, H Härtner


Protection of pile tops using combinations of internal treatments and water shedding caps
1993 - IRG/WP 93-30020
Preservative treatment produces an excellent barrier against fungal, insect, and marine borer attack; however, fabricators often disrupt this barrier during construction, creating avenues for entry of decay agents. This problem is particularly acute in marinas along the coastal United States. Standards recommend the application of a water-shedding cap at the time of installation to prevent pile to...
P Schnieder, M A Newbill, J J Morrell


Production, function and neutralization of oxalic acid produced by the dry rot fungus and other brown rot fungi
1987 - IRG/WP 1330
The formation of oxalic acid by the wood-destroying fungi causing brown rot, is found to be the key which by hydrolysing the hemicellulose brings the cellulose in the tracheid wall in contact with the cellulase enzymes and yeld watersoluble sugars leaving only a lignin skeleton. To control the pH in the substrate the excess oxalic acid is precipitated to water insoluble calcium oxalate by the dry ...
J Bech-Andersen


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 22: Report on the conditions of specimens at Sekondi, Ghana after 60 months
1986 - IRG/WP 4123
The results of the third inspection of CCA and CCB treated test panels exposed at Sekondi, Ghana in June 1980 are presented. None of the panels still in test, i.e. panels of Pinus sylvestris treated with CCA at 3 and 10%, Alstonia scholaris treated with CCA at 10%, Fagus sylvatica treated with CCA at 10%, and Erythrophleum ivorense and Mitragyna stipulosa both treated with CCB at 10%, shows any ex...
F F K Ampong, N Asare-Nyadu


Some fundamental thoughts on the prediction of field performance from lab-testing based on comparison of lab and field test results of some copper-free materials
2003 - IRG/WP 03-20269
In the paper results from lab testing (ENV 807 and EN 113) are compared with field results (EN 252) of differently treated wood. Depending on the type of the organic biocide containing material and depending on type of soil and type of decay differences were found in suitability of the lab methods to predict field performance. The attempt is made to interpret the found differences. Furthermore it ...
A O Rapp, U Augusta


The durability of wood polymer composites against fungi and insects
2000 - IRG/WP 00-40161
New materials such as wood polymer composites are used more in France. These materials are obtained by mixing wood and thermoplastics in different ratios. These kind of material must be considered as new materials and some characteristics such as durability must be evaluated for outdoor applications. On the other hand, some recycled fibers from wood waste could be used as raw materials. Some woodp...
G Labat, I Le Bayon, J Gerard, F Amin


Information from the COIPM Wood Group
1988 - IRG/WP 4146
Abstract from the COIPM minutes: Wood in marine environment: Mrs Gambetta stated that the main item discussed by the Group was the collaborative work to test the durability of heat shrinkable polyolephin sheating materials for the protection of wood against marine organisms. The work began last year when wood samples were sent out to the participants. Three samples of Pinus sylvestris wrapped in ...
A Gambetta


Effects of soil physical and chemical characteristics on adsorption of leached CCA and ACQ preservative components
2003 - IRG/WP 03-50200
The objective of this study was to examine the effect of soil characteristics on adsorption of wood preservative components from CCA and ACQ preservative systems. Adsorption of leached CCA and ACQ preservative components in soils with different characteristics were studied. Three soils (clay, sandy and organic) were investigated using different concentrations of leach water of CCA and ACQ wood pr...
S Stefanovic, P A Cooper


Evaluation of the protective means of some wood preservatives by means of accelerated tests
1973 - IRG/WP 232
In site conditions of the eastern site in the forest-steppe part of the Krasnovarsk region, the relative effectiveness of a series of wood preservatives was obtained by means of field tests. To obtain a more accurate evaluation of the protective qualities of these accelerated tests were carried out in laboratory conditions. In 9 boxes filled with non-sterile soil taken from the site, 72 samples of...
I A Petrenko


The effect of acid rain on CCA treated timber
1990 - IRG/WP 3579
The effect of acid precipitation on the leaching of copper, chromium and arsenic from timber treated with different CCA preservatives was studied in the presence of three types of soil under simulated field conditions. Pine sapwood, embedded in soil, was subjected to simulated rainfall at three different levels of acidity. The CCA preservative formulations tested were:- American Wood Preservers&am...
R J Murphy, D J Dickinson


Determination of fungitoxic value of preservatives in laboratory wood-block tests. Part 2: Statistical estimation
1989 - IRG/WP 2327
Laboratory modified agar-block tests were made to determine the fungitoxic value of the wood preservative CCA against the test fungus Serpula lacrymans using statistical methods. With the aid of statistical computer programmes based on the least square method. the regression equation was found for the dependence between sample mass loss and preservative retention both in terms of percentage and fo...
J Wazny, J D Thornton, K J Krajewski


Development and Implementation of a DNA – RFLP Database for Wood Decay and Wood Associated Fungi
2004 - IRG/WP 04-10527
We are developing Restriction Fragment Length Polymorphism (RFLP) and Internal Transcribed Spacer (ITS) sequence databases for wood decay basidiomycetes and other fungi associated with wood. These databases currently house information for 39 fungal species consisting of 9 brown-rot basidiomycetes, 12 white rot basidiomycetes, 1 soft rot, 1 stain fungi, and 16 molds or other ascomycetes or imperfe...
S V Diehl, T C McElroy, M L Prewitt


Metal plate fasteners in trussed rafters treated with preservatives or flame retardants - corrosion risks
1977 - IRG/WP 3104
In designing roof trusses employing metal plate fasteners it is generally assumed that the roof will remain dry in service. Whilst this is generally true, damp conditions do arise under some circumstances, although it is not possible to quantify the extent of the risk. It is only possible, therefore, to give general recommendations which must be interpreted in the light of local experience of serv...
R A Laidlaw, L C Pinion


Wood durability in the light of recent trends and research on the durability of building materials and components
2000 - IRG/WP 00-20195
Building-related research of today demonstrates a clear shift in focus from the design and production phases to usage and to the entire life time. A consequence is that the performance criteria of materials, components and of the entire building must be regarded over the life time rather than at the time of production or delivery. As one example can be mentioned the Building Construction Directive...
K Ödeen


End grain sealing by polymer impregnation
1992 - IRG/WP 92-3708
The solution and dispersion characteristics of several hydrophobic derivatives of cellulose have been studied and the abilities of these polymers to afford effective end grain sealing of Corsican pine have been examined. Both solution and dispersion treatments with ethyl cellulose imparted good water repellency and end grain sealing to wood samples, however, the disperse systems possessed lower vi...
J M Lawther, W B Banks, D G Anderson, J A Cornfield


Tool wear for vapor boron-treated composites
2001 - IRG/WP 01-40209
A series of composites, including oriented strandboard and medium density fiberboard, were treated via vapor boron technology. Treated samples were compared to untreated composites using a tool force measuring technique. Tool forces measured with a dynamometer indicated a positive effect of boron addition. Visual and SEM examination indicated a wider wear zone on the rake face of the tool for the ...
W A Jones, H M Barnes, H A Stewart, R J Murphy