Preservative performance of copper naphthenate (SANPRESER-OGR) in brush treatment of timber
1991 - IRG/WP 3663
Preservative efficacy of copper naphthenate (SANPRESER-OGR) was evaluated in the laboartory and field trials when timber was treated by brushing. Results of field trial indicated that service life of the brush-treated timber could be approximately 10 years or longer under ground contact conditions, although life span was slightly varied with timber species and test sites. After four years&apos...
Y Sugai, K Hamada, M Kitada, K Tomoi


Generic code of good practices for wood protection facilities. Part 1: Wood protection (antisapstain) facilities
1993 - IRG/WP 93-50003
In general, the potential of high toxicity (aquatic and human) of wood protection (antisapstain) chemicals dictates the need to protect the environment and humans from its harmful effects. This document is a compendium of recommendations for the design and operating practices of wood protection facilities. The suggested recommendations focus on achieving the objectives of protecting the environmen...
G Das, V N P Mathur


An engineering model for the decay of timber in ground contact
2003 - IRG/WP 03-20260
To predict the residual strength of an engineered structure, it is first necessary to predict the effect of decay. A model was developed in which the effective area of structural decay in large section timbers was defined as that area that could be picked out with a pen-knife. Some limited studies indicated that for practical purposes the remaining wood could be assumed to have its full residual s...
R H Leicester, C-H Wang, M N Nguyen, J D Thornton, G Johnson, D Gardner, G C Foliente, C MacKenzie


Development on Damage Functions of Wood Decay for Building Envelope Design
2005 - IRG/WP 05-10556
For the hygrothermal analyses of building envelope systems for insulation design, we tried a natural decay test of wetted wood specimens without any inoculation of fungi. Three principal experimental types: under steady-state conditions (Experiment A), at a cyclic water dripping under Non-steady conditions (Experiment B) and at a cyclic water dipping under-steady conditions (Experiment C), were ca...
H Suzuki, Y Kitadani, K Suzuki, A Iwamae, H Nagai


Canadian code of good practices - Recommendations for design and operation of wood preservation facilities
1990 - IRG/WP 3582
The rationale and procedures for the development of a set of recommendations for design and operation of wood preservation facilities in Canada are discussed. Multi stake holders involvement in problem identification, problem assessment, state of the art knowledge database, implementation and periodic assessment procedures are important considerations for the successful development of a Code of Go...
V N P Mathur, G Das


Serviceability modeling-Predicting and extending the useful service life of FRT-plywood roof sheathing
2000 - IRG/WP 00-20210
One of the most, if not the most, efficient methods of extending our existing forest resource is to prolong the service life of wood currently in-service by using those existing structures to meet our future needs (Hamilton and Winandy 1998). It is currently estimated that over 7 x 109 m3 (3 trillion bd. ft) of wood is currently in service within the United States of America (PATH 1999). Research ...
J E Winandy


Fungus cellar testing as an evaluation method for performance of treated timber in ground contact
2001 - IRG/WP 01-20227
A fungus cellar method for the accelerated evaluation of performance of treated wood in ground contact is described. The test soil comprised of sandy loam, vermiculite and Japanese horticulture soil "Kanumatsuchi" in a ratio of 6:2:2 by volume. The soil was inoculated with the dominant test fungus isolated with selective medium from decayed wood samples. Pairs of treated and untreated wood specime...
Y Nagano


Butt-end incising to improve penetration and retention of creosote in Eucalyptus saligna power transmission poles in Kenya. Preliminary results
2002 - IRG/WP 02-40249
Incising as a possible technique to improve penetration and retention of creosote in the butt end of Eucalyptus saligna power transmission poles in Kenya was investigated. Debarked, butt-end samples from whole poles were seasoned (15% MC), incised using four patterns of incisions, sealed at the top or small diameter end, and pressure treated with a mixture of creosote-furnace oil (60/40 mix) at a...
R Venkatasamy


Service life of pressure treated deckings of spruce in direct contact with the ground
1988 - IRG/WP 3463
For decking outdoors in Sweden, pressure treated Scots pine (Pinus sylvestris L.) is used, on account of its treatability. The feasibility of using instead the refractory Norway spruce (Picea abies Karst.) is tested in a field trial. The spruce decks were treated together with pine decks with an ordinary Bethell process. As yet, after more than four years of exposure, neither in the battens nor in...
J B Boutelje, T Sebring


Commercial potential of the four-cycle method for the impregnation of green beech sleepers in Yugoslavia
1975 - IRG/WP 347
This paper was presented to the Conference on Wood Protection held in Sarajevo (Yugoslavia) in 1973. The paper was based partially on the report prepared by J. Struhar and G. F. Franciosi, who were appointed in 1972 as FAO consultants to demonstrate the new impregnation process for green beech sleepers in Yugoslavia. The so-called 4-cycle method was developed at the State Forest Research Institute...
N Vidovic


Butt-end incising to improve penetration and retention of CCA in Eucalyptus saligna telegraph poles in Kenya: Preliminary results
2002 - IRG/WP 02-40243
Incising to improve penetration and retention of Copper Chrome Arsenate (CCA) in the butt end of Eucalyptus saligna telegraph poles was investigated. Debarked, seasoned (15% MC) butt-end samples from full size telegraph poles were incised using four patterns of incisions, sealed at the top or small diameter end, and pressure treated, together with un-incised samples, with CCA-C (3.0% oxide typ...
R Venkatasamy


A serial exposure technique for estimating probable service life of treated timber
1978 - IRG/WP 2111
This paper briefly describes part of our preliminary work aimed at developing a test procedure that culd be adopted as a standard method. A detailed version of the work has been submitted for formal publication. In both papers, the aim is to promote interest in extended laboratory testing of wood preservatives. It is believed that this work may provide the basis of a laboratory test procedure from...
J A Butcher


Alternatives to CCA for ground contact protection of timber: a perspective from UK on performance and service life expectations
2002 - IRG/WP 02-30289
The proposed amendment to the European Union's Marketing and Use Directive (1976/769/EEC) in respect of arsenic in CCA wood preservatives seeks to restrict the use of CCA across the European Union. CCA is an extremely important wood preservative in the UK from the manufacturing of the product to the extent of use of CCA-treated timber. Based on our experience and judgement on the use of ...
E D Suttie, A F Bravery, T B Dearling


Natural durability, density and extractive contents of 42 wood species of Bangladesh.
2003 - IRG/WP 03-10490
Natural durability, density and major extractive contents of 42 lesser used or unused wood species of Bangladesh have been studied. Correlation analysis between these properties has been performed. It has been shown that natural durability of these species neither explained by water soluble nor by alcohol benzene extractive contents. Density has a weak but significant positive correlation with dur...
S Akhter, K Akhter, S C Das


Premature failure of treated timber in wharfs in Papua New Guinea, attributed to defects in design
1991 - IRG/WP 4158
The performance of timber in wharfs in Papua New Guinea has been monitored for a number of years. Premature failure of wharf structures was found in many cases to be due to defects in design rather than ineffective preservative treatment. Above-water timbers were found to be prone to severe checking followed by decay. Protection for the end grain of pile tops and the limiting of radial checking in...
S M Cragg


Design of Field Trials for Evaluation of Antisapstain Products
2003 - IRG/WP 03-20263
Field trialing is an important phase of antisapstain product development and careful planning is required to ensure trial validity for predicting performance in the industrial situation. Experiences of trialing antisapstain products on lumber over a ten-year period are discussed in this paper. It is not mandatory to source "fresh " wood for trialing and useful information can be generated even...
F W Frazer, N R Edmonds, B J Nairn


Effect of kerfing on performance of Douglas-fir utility poles in the Pacific Northwest
1990 - IRG/WP 3604
Preservative treatment produces an external layer of protection in Douglas-fir poles, but the development of deep checks as the wood dries after treatment can permit entry by fungi and insects. A variety of remedial treatments can arrest this decay; however, it is far more efficient to prevent checking. Kerfing represents one potential method for limiting the development of deep checks. In previou...
J J Morrell


Disodium octaborate tetrahydrate, alone and in conjunction with a selected isolate of Trichoderma viride, reduces decay of fresh felled pine independent of the effect of weathering
1994 - IRG/WP 94-10054
Unpeeled billets of Corsican pine were treated with the following: 5% aqueous disodium octaborate tetrahydrate (DOT) solution; 5% DOT solution with an isolate of Trichoderma viride with a low susceptibility to borate; the Trichoderma viride isolate alone. Half of the billets in each treatment group were also placed in large-diameter plastic pipes to protect the billets from the weather. All three ...
M W Schoeman, D J Dickinson, J F Webber


Integrated protection of freshly sawn lumber using Bacillus subtilis and selected fungicide
1997 - IRG/WP 97-10235
Bioprotection against stain fungi has tremendous potential for reducing discoloration of freshly sawn wood while decreasing chemical consumption. Unfortunately, most bioprotectants appear to be unable to consistently perform under the array of conditions to which freshly sawn wood is exposed. While research is underway to understand the nature of the inconsistent performance, a more pragmatic appr...
M E Mankowski, M Anderson, J J Morrell


Service life of outdoor wooden constructions. Expectations of private house owners in Sweden
2001 - IRG/WP 01-10401
Wood is traditionally used in indoor as well as outdoor applications. However, if not kept dry, wood is easily attacked by wood degrading micro-organisms. Thus the service life is heavily affected by construction design, choice of wood and wood treatment. For most constructions there is an expected service life. The expectations concerning wooden constructions and what kind of wood is chosen to fu...
M-L Edlund, J Jermer


Quality assured wooden sidings - Criteria, performance evaluations and current status
2000 - IRG/WP 00-20216
Quality assured wooden sidings were brought to the Swedish market in 1998. The system was worked out during a six year period in a close cooperation between the sawmill industry and several research institutes. Centuries of use have given a wealth of experience of spruce boards as a siding material, showing that it works well in most cases but also that its longevity is highly variable, depending ...
F Englund, I Johansson, J Ekstedt, R Nussbaum


Recent development in North American industrial wood preservation plants
1988 - IRG/WP 3467
After remaining static for many years there have been a number of changes in plant design and treating cycles in recent years. This has been particularly true in the USA where few restrictions are placed on plant treating cycles by specifications; since only results type specifications are used. It is also important to realize that the AWPA Specifications for Southern Yellow Pine only call for tre...
J F Bridges


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Deterioration of wood viewed from iron nail
1991 - IRG/WP 2368
Deterioration of nail was graded by a five - rank numerical - rating. The rating of nail moisture content and decay of wood were inspected in a mortal-wall of 34-year-old house. The wood was mostly in decay, when the rating of the nail was above about 4, and the moisture content was above about 20%. Nailed wood specimens kept in several humidity room of 20°C for 4 years showed that the rating of ...
H Imamura


Design of a laboratory method for evaluating the effectiveness of soft rot preservatives
1988 - IRG/WP 2312
This purpose of this work was to design a method which makes it possible to evaluate the effectiveness of products which present protect wood against soft rot, using new products·of a different nature, on wood of·Pinus sylvestris L. and Fagus sylvatica L., and which, suitably applied, avoid big economic losses deriving from lack of knowledge of the active principles suitable to present protect w...
M T De Troya, A M Navarrete