IRG Documents Database and Compendium



Displaying your search results

Your search resulted in 5027 documents. Displaying 25 entries per page.


Variability in durability of some selected South-American wood species
2014 - IRG/WP 14-10831
…one wants to encourage the proper use of lesser known wood species. Therefore the market has to shift from a demand-driven towards a supply-driven market without loss of wood quality. It is generally known that the durability from pith to bark varies thus, affecting the overall durability of wood species.…
I De Windt, P ’t Hooft, J Van den Bulcke, J Van Acker


Assessment of Scots pine sapwood susceptibility to moulds by determination of fungi growth and ergosterol content in infested wood
2014 - IRG/WP 14-20540
The susceptibility of wood to filamentous fungi (mould) attack is determine mainly by laboratory methods with descriptive grading of fungal growth on the surface of the wood specimens. It is a lot of different grading scale of fungi growth, but determination of the size of fungi…
A Fojutowski, A Koziróg, A Kropacz


Performance classification of wood in construction – drafting a user friendly European standard
2014 - IRG/WP 14-20545
The performance classification for wood products in construction is an extremely important topic in Europe and beyond – warranty providers and end users demand service life and performance information in the face of competition with other materials. The European project PerformWOOD has…
E Suttie, C Brischke, L Meyer, J Van Acker, M Kutnik, E Heisel, F Englund, J Jermer, S Thelandersson, M Polášek, D Lorenzo


Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
…are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring…
L Meyer, C Brischke, M Kasselmann, C Rösmann


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of…
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


Colorimetric evaluation of three tropical woods after accelerated weathering
2014 - IRG/WP 14-20541
The use of wood in the furniture industry is directly associated with their physical, mechanical and organoleptic characteristics. The color of the wood is a major factor in the selection of forests species to employ in the furniture projects and is fundamental the…
R Faustino Teles, A Florian da Costa


In vitro fungicidal activity of Tunisian essences extracts against Coriolus versicolor and Coniophora puteana
2014 - IRG/WP 14-20544
…and its phenolic aqueous extract could be tested for wood preservation as a green alternative towards synthetic antifungic molecules.
L Lajnef, N Ayed, B Charrier


Screening method to test efficacy of fumigants against fungi and preliminary data on the efficacy of sulfuryl fluoride
2014 - IRG/WP 14-20551
…in reducing exotic pest establishments via trade in wood products. Efficacy data for established phytosanitary fumigants were mostly developed for arthropods and nematodes, and limited information exists for plant pathogens. Increased interest in developing a fast screening process for fungi has prompted this…
A Uzunovic, A Mukherjee, R Mack, P Elder, S Myers


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few…
S Lipeh, C S Love, J J Morrell


Using Commercial Water Repellent Chemicals on Wood Protection
2014 - IRG/WP 14-30656
…products that use environmental friendly technologies in wood protection. These sorts of innovations on wood protection should be carried out for wood evaluated at outdoor conditions. Using water repelling chemicals is one of those innovations which improve wood durability and dimensional stability by decreasing…
G Köse, A Temiz, S Demirel, O E Özkan


Ammoniacal Copper Zinc Arsenate Preservative Treated Wood Ties Their Performance in Testing and Track
2014 - IRG/WP 14-30636
…performance in treating difficult or refractory species of wood has been documented through its wide range of uses approved in AWPA. The establishment of appropriate testing for railroad material use was put in place and includes laboratory, field as well as commercial treatment and usage, show that ACZA treated wood
T Carey


Cost effective extension of service life of bridge tie (sleepers) - Effectively applying borate during Boulton conditioning and treatment with copper naphthenate
2014 - IRG/WP 14-30637
Current longevity of creosote treated wooden bridge ties in the South Eastern US is about 15 to 25 years, which is well below of the average service life of 33-50 years of railroad ties. Such short service life increases costs associated with maintenance of railroads including bridge down time…
J D Lloyd, T Chambers, J-W Kim


CreoSub – New protection technology to substitute creosote in railway sleepers, timber bridges, and utility poles
2014 - IRG/WP 14-30644
Creosote oil is one of the oldest industrially used wood preservatives. Due to its toxic profile, the European Commission has restricted the use of creosote specific applications, but it is highly controversial within the European Commission. Its approval for use after 2018 is very questionable and may depend…
U Hundhausen, K-C Mahnert, A Gellerich, H Militz


Visualization of gold/silver nanostars in wood by surface enhanced Raman spectroscopy
2014 - IRG/WP 14-30653
…up-to-date technology and ventures expeditiously in the wood preservative market. However, there is still a huge lack of understanding about the interaction and incorporation of nanoparticles (NSs) in wood. Surface-enhanced Raman scattering (SERS) offers unique advantages as an analytical tool with a high…
C Geers, L Rodríguez-Lorenzo, M Placencia Peña, P Brodard, T Volkmer, B Rothen-Rutishauser, A Petri-Fink


Copper and chromium leaching from wood impregnated with chromium-copper containing preservatives: Results of different studies
2014 - IRG/WP 14-50300
Copper and chromium based wood preservatives remained one of the most important ingredients for wood protection solutions for protection of wood in demanding applications all-over the world. Leaching of heavy metals from treated wood is important from two different aspects; firstly…
M Humar, N Thaler, E Melcher


Potential for migration of boron from fused boron rods used as internal remedial treatments of utility poles
2014 - IRG/WP 14-50301
…application of fused boron rods. Boron levels in the wood never reached the levels that might be predicted if diffusion were to produce a uniform chemical distribution, nor did levels in the soil suggest that boron was becoming more concentrated. The results suggest the need for further studies to better…
M Konkler, C Freitag, C S Love, J J Morrell, J Renfroe


Migration of copper from copper naphthenate treated Douglas-fir poles during storage
2014 - IRG/WP 14-50302
Preservative migration from treated wood products has raised concerns among regulators, especially when the biocides move into surface waters. In most cases, chemical levels are well below the acceptable minimum level, but can become a concern if large quantities of treated wood are stored in…
C S Love, C M Freitag, J J Morrell


Influence of Exposure Direction on Leaching of a Biocide from Painted Wood Surfaces
2014 - IRG/WP 14-50303
…the cumulative quantity of a biocide leached from painted wood surfaces due to rainfall and the consequences for the risk assessment. The study included a solvent-borne primer without biocides and a topcoat protected with a biocidal active substance. Both products were applied by brushing at DTI in Denmark.…
M Klamer


VOC-free remedial treatment agent on organic solvent basis with surface cleaning by photocatalysis using titanium dioxide
2014 - IRG/WP 14-40651
…is introduced including a potential method to clean up the wooden surface of remaining biocides after a remedial treatment using photocatalysis.
H Ahl, J Fromm, P Jüngel, E Melcher, M Pallaske


Nano-Zycosil in MDF. Part I: Gas and Liquid Permeability
2014 - IRG/WP 14-40652
…at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. The obtained results indicated that the addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the nanozycosil-treated…
H Reza Taghiyari, A Karimi, P M D Tahir, O Schmidt, E Bari, P Nouri , A Jahangiri


Evaluation of vessel features on physical and mechanical properties of wood of Common black poplar (Populus nigra L.) grown at different elevations in the region with a continental climate
2014 - IRG/WP 14-40656
…properties of Common black poplar (Populus nigra L.) wood. The scope of the study was to observe the variability of vessel element features on physical and mechanical properties of Common black poplar (Populus nigra L.) in relation to habitat at different elevations. For this purpose, the twelve 12 year old…
I Usta


Thermal durability and biodegradation of tannin lignin adhesives
2014 - IRG/WP 14-40657
Mimosa tannins and lignosulfonates were used in wood adhesives formulation to substitute resins based on formaldehyde. Mimosa tannins were mixed with either glyoxalated sodium lignosulfonates or glyoxalated ammonium lignosulfonates. The ratios of mimosa tannins and sodium lignosulfonates varied from 20%…
L Chupin, B Charrier, A Pizzi, F Charrier


Full-scale impregnation of wood with siloxane using supercritical carbon dioxide
2014 - IRG/WP 14-40659
Full-scale impregnation of wood with siloxane was carried out using supercritical carbon dioxide as solvent. A batch of 3530 kg of Scots pine sapwood was impregnated to a retention of approximately 1.3% siloxane. The treatment also consisted of a simultaneous impregnation with organic…
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Termite resistance of wood modified with short- and long-chain siloxanes
2014 - IRG/WP 14-40660
Scots pine (Pinus sylvestris L.) sapwood specimens modified with short- and long-chain amino-functional siloxane emulsions were exposed to subterranean termites (Reticulitermes flavipes Kollar). Laboratory choice and no-choice tests following the standard EN 117 (2013) were conducted for 8…
P Gascón-Garrido, M-F Thévenon, H Militz, C Mai


Effect of Nano-Wollastonite on Water Absorption in Particleboard
2014 - IRG/WP 14-40662
…at 5, 10, 15, and 20 g/kg, based on the dry weight of wood-chips, and compared with control specimens. Two application methods of NW were used: surface application (SA), and internal application (IA). Density was kept constant at 0.68 g/cm3 for all treatments. Tests were carried out in accordance with ASTM…
S Karimi, H Reza Taghiyari, A Karimi, P M Tahir, J Abdul Halip