Accelerated laboratory soil contact decay test using soil amended with composted wood
2004 - IRG/WP 04-20284
The effect of amending soil with wood compost on the decay rate of wood wafers in contact with the unsterile soil, as measured by radial compression strength loss, was explored. It was found that the addition of composted wood to the soil significantly increased the wood decay rate. The reason for this acceleration in wood decay is not entirely clear, but appears to be at least partially associate...
D D Nicholas, H Borazjani, T Schultz


SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown in wood
1997 - IRG/WP 97-10193
Previous reports have illustrated the involvement of extracellular mucilage (ECM) in wood decay by Basidiomycetes. Its production is investigated in a range of stain, mould and soft rot fungi in Corsican pine, Scots pine and European beech. Fungi examined were: Chaetomium globosum, Ceratocystis coerulescens, Trichoderma harzianum, Ophiostoma piceae, Mucor sp. and Penicillium. sp. The samples were ...
A R Abu, D J Dickinson, R J Murphy


Comparison between agar-block and soil-block methods for wood-destroying Basidiomycetes
1992 - IRG/WP 92-2401
The object of this work is to compare these methods in order to provide some information to help in the choice between them. The comparison was made by a statistical analysis (factorial completely randomized design) and by a discussion about other aspects of each method. An evaluation of some fungi on attacking wood and a comparison between Picnoporus sanguineus isolated from carpophore and decaye...
M B B Monteiro, S Brazolin, G Catanozi


Performance of copper-based wood preservatives in above ground and ground contact tests
1994 - IRG/WP 94-30057
The relative performance of a range of copper-based wood preservatives was compared using above ground and ground contact procedures. The data, accumulated after several years' testing, show that on an equivalent active ingredient basis, differences in performance of the preservative systems tested can vary quite markedly. The contribution of co-biocides to the overall performance of thes...
A F Preston, K J Archer, L Jin, W Metzner, D Seepe


Fungus cellar testing as an evaluation method for performance of treated timber in ground contact
2001 - IRG/WP 01-20227
A fungus cellar method for the accelerated evaluation of performance of treated wood in ground contact is described. The test soil comprised of sandy loam, vermiculite and Japanese horticulture soil "Kanumatsuchi" in a ratio of 6:2:2 by volume. The soil was inoculated with the dominant test fungus isolated with selective medium from decayed wood samples. Pairs of treated and untreated wood specime...
Y Nagano


Valid names for some common decay fungi and their synonyms
1992 - IRG/WP 92-1522
The taxonomy of wood destroying fungi has changed noticeably within the last ten years. New genera and more well defined generic concepts have emerged with concomitant and necessary changes in nomenclature. The following is a revision of a list originally prepared by Kaarik (1979) in collaboration with Professor Dr. C. Jacquiot (France), Mr. J. G. Savory (United Kingdom) and Dr. G. Seehann (Federa...
M J Larsen, R M Rentmeester


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 2: Laboratory fungal bioassays
2000 - IRG/WP 00-20204
Extracts from sawmill residues of the naturally durable white cypress, Callitris glaucophylla were tested for fungicidal activity in a series of laboratory bioassays. The effects of different extraction solvents, techniques and sources of material on the biocidal efficacy of the resultant extracts were evaluated. Soil jar decay tests were used initially however, contractual time constraints necess...
M A Powell, L M Stephens, L Francis, M J Kennedy


The efficacy of remedial treatments for controlling fungal decay in window millwork used in the United States
1987 - IRG/WP 3432
Conventional window millwork was subjected to basidiomycete decay by inoculation and sampled for active growth of the decay fungus before and eight months after remedial preservative treatment with fused disodium octaborate rods (IMPEL) at boric acid levels of 1.5 and 4.0 kg/m³ or liquid bifluoride injections (IMPROSOL) at 1 kg/m³. The elimination of decay fungus after remedial treatment was nea...
M G Dietz, E L Schmidt


An electron spin resonance study of manganese changes in wood decayed by the brown-rot fungus, Postia placenta
1988 - IRG/WP 1359
Electron spin resonance (ESR) spectrometry was used to examine wood decay by the brown-rot fungus, Postia placenta. Wood slivers of Douglas-fir, white fir, redwood, sweetgum and yellow poplar were incubated for 4 weeks in custom-made quartz ESR tubes with or without Postia placenta. In all wood species without fungus, a weak partially resolved signal (about g=2, presumably due to manganese) was de...
B Illman, D C Meinholtz, T L Highley


Some experiences with attack of microorganisms on wooden constructions supporting foundations of houses and bridges
1997 - IRG/WP 97-10232
Reconstructions of bridges and public buildings or damage of houses during the construction of subway lines in Berlin have led to a number of inspections of wooden foundations, mostly pine or spruce piles, representing service lives of between ca. 70 and 140 years. In all cases bacterial attack was found both in wood submerged in ground water and in surface water. The extent of deterioration diffe...
M Grinda


A termite field test with diffusion treated lumber
1991 - IRG/WP 3648
Douglas fir lumber, diffusion treated with concentrated sodium octaborate solutions, was tested against Coptotermes formosanus in an above ground field test wherein the samples were not exposed to a direct leaching hazard during the test period. After 2.5 years exposure, the untreated control samples were almost completely destroyed while poorly treated controls pressure treated with chromated cop...
K J Archer, D A Fowlie, A F Preston, P J Walcheski


Incorporation of phenyl boronic acid treatment with vapor phase formalization
1997 - IRG/WP 97-40083
Phenylboronic acid (PBA) treatment was incorporated with vapor phase formalization (VPF) in order to increase dimensional stability and boron fixation as well as enhancement of biological resistance. Five and ten hours VPF were applied after PBA treatment as 0.34, 0.50, 1.00 and 2.00% concs. aqueous solutions. Anti swelling efficiency (ASE) attended to 71% in specimens impregnated with 0.50% PBA s...
M K Yalinkilic, S Yusuf, T Yoshimura, W-Y Su, K Tsunoda, M Takahashi


Occurrence, prevention and repair of Dry Rot
1990 - IRG/WP 1439
Information about the frequency, detection, identification and repair of Dry Rot attacks (Serpula lacrymans) is summarized from 13 European countries. Based on 28 completed and returned questionnaires it appears that Dry Rot attacks are recognized in all countries participating, and that there is an appreciable similarity in the frequency of attacks and methods of detection and identification. How...
A P Koch


Termite and decay resistance of particleboard composed of white cypress pine and radiata pine
1997 - IRG/WP 97-10200
Phenol-formaldehyde bonded particleboard was manufactured from blends of non-durable radiate pine (P. radiate) and heartwood of the naturally durable species, white cypress pine (C. glaucophylla). Board specimens were subjected to bioassays using two termite species, M. darwiniensis and C. acinaciformis, and the basidiomycete fungi, C. puteana and P. ostreatus, and the durability of specimens was ...
P D Evans, J W Creffield, J S G Conroy, S C Barry


Attempt for developing a new method for above ground field testing of wood durability
2000 - IRG/WP 00-20199
Field testing remains the most appropriate way for evaluation of wood preservatives or natural durability of wood species. Above ground tests are designed to answer specific questions concerning the outdoor utilisation of wood. Such methods supply additional information and confirm or reject preliminary laboratory results. The European standard (ENV 12037, "lap-joint") for assessment of the durabi...
N Terziev, M-L Edlund


International comparison of three field methods for assessing the in-ground termite resistance of materials - highlights after two years
1999 - IRG/WP 99-20157
First-year results of a comparative study, evaluating the in-ground termite resistance of a range of materials, including CCA and ACQ-treated timbers, using the below-ground exposure, ground contact and graveyard methods against diverse termite faunas were provided in IRG/WP/98-20132. Further annual inspections have confirmed early trends and identified notable differences between sites and method...
M Lenz, J W Creffield, A F Preston, B M Kard, C Vongkaluang, Y Sornnuwat


Reaction of osmium tetroxide with a diphenolic compound as a model substance for demethylated lignin
1986 - IRG/WP 1303
By using caffeic acid as a model substance for diphenolic moieties of demethylated lignin it was found that electron dense particles called by the authors "osmiophilic particles" in former papers are reaction products of OsO4 with the model substance. By these products it is possible to indicate the enzymatic demethylation of lignin taking place during wood decay. The appearance of the electron de...
K Messner, E Srebotnik


Natural decay resistance of some lesser-used tropical hardwoods from Ghana
2002 - IRG/WP 02-10438
Ghana is a tropical African country that is rich in diverse timber species. In order to reduce over-exploitation of the popular timber species and increase the resource base for the wood industry, lesser-used or lesser-known timber species are being promoted locally and for export. To do this successfully, it is essential to determine the physical, mechanical and biological properties of these tim...
S A Amartey, F R Hanson


The effect of hemicellulose degradation on the mechanical properties of wood during brown rot decay
2001 - IRG/WP 01-20219
Incipient decay of wood by brown rot fungi causes measurable strength losses in wood before measurable weight loss occurs. Previous studies have shown that the high levels of strength loss that occur during incipient brown rot decay may be related to loss in hemicellulose. This paper investigates the effect of decay on hemicellulose composition and the relationship to the mechanical properties of ...
S F Curling, C A Clausen, J E Winandy


Susceptibility of CCB treated wood to fungal colonization
2003 - IRG/WP 03-10492
CCB treated wood is generally resistant to all wood decay fungi. However, like CCA impregnated wood, susceptibility of CCB treated wood to copper tolerant fungi have been observed. The ability of various brown rot fungal hyphae to penetrate and overgrow the wood samples was investigated. Samples made of Norway spruce (Picea abies) were impregnated with 5 % CCB solution according to the EN 113 proc...
F Pohleven, U Andoljsek, P Karabegovic, C Tavzes, S A Amartey, M Humar


Chemical and biological studies of organotin treated and painted wood stakes after outdoor exposure
1987 - IRG/WP 3419
Organotin based wood preservatives containing tributyltin oxide (TBTO) or tributyltin naphthenate (TBTN) are used in Sweden mainly for double-vacuum treatments of window joinery of Pinus sylvestris. After impregnation the joinery is painted or stained in different colours. To evaluate this effect (different colours on the degree of degradation of TBTO and TBTN, effected by different temperatures i...
M-L Edlund, B Henningsson


Field stake test assessment with the Pilodyn
1980 - IRG/WP 2136
The Pilodyn, which was originally developed to estimate the degree of soft rot in wooden poles, was thought to have potential for giving a quantitative measure of the extent or depth of decay in field test stakes. In the present work a 2-joule Pilodyn with 2.0-mm diameter pin was used in an attempt to limit depth of pin penetration (to 10-15 mm) without reducing scale sensitivity. The results show...
M E Hedley, R W Naish


Co-operative work on the performance of treated timber in ground contact
1975 - IRG/WP 344
At the 6th meeting of The International Research Group on Wood Preservation in Vienna, it was decided to approach all interested parties in order to: collate available information, set up collaborative work and to stimulate research on the performance of treated timber, especially hardwoods, in ground contact. In recent years, considerable concern has been expressed about the performance of preser...
D J Dickinson, J F Levy


Some data on the activity of alternative fungicides for wood preservation
1985 - IRG/WP 3333
Data from laboratory tests against basidiomycete fungi are presented for 9 alternative fungicides in organic solvent formulations and also in water for one product. Results are compared with data for reference preservatives, tributyltin oxide, copper and zinc naphthenates and pentachlorophenol. Of special interest is the apparently better than additive effect of mixing tributyltin naphthenate and ...
A F Bravery, J K Carey


Above-ground field tests undertaken in New Zealand
1995 - IRG/WP 95-20063
In addition to "standard" L-joints, above-ground test material exposed at the NZ FRI test site includes treated and untreated decking units, Y-joints, fence battens and weatherboards either with or without additional protection from surface coatings. The latter tests bridge the gap between "model" test assemblies, such as L-joints, and services tests. Most tests are of preservative-treated radiata...
M E Hedley, D R Page, J B Foster, B E Patterson