The Comparison of Fixation and Leachability of Bark, Fruit and Leaf Tannin Extracts with Boron Minerals
2008 - IRG/WP 08-30473
Tannins extracted from several plants have natural durability properties. Due to these properties, some of the researchers have studied them for protecting wood. In this study, Scots pine (Pinus sylvestris) and beech (Fagus orientalis) wood samples were treated with bark, fruit, and leaf extracts as well as water-based wood preservative salts at various concentrations to increase fixation. The pen...
S Sen, C Tascioglu, K Tirak


Thermal treatment of Nigerian-grown Albizzia zygia and Funtumia elastica wood in soy oil medium.
2008 - IRG/WP 08-40413
Thermal treatment in soy oil medium is one of the techniques used as a substitute to the chemical treatment in wood preservation. However, the effects of this technique vary from one species to another and hence the need to investigate the response of individual species to it. Thermal treatment of air-dried Nigerian-grown Albizzia zygia and Funtumia elastica wood was carried out in a vessel contai...
L Awoyemi


The Effect of Heat Treatment on Water Absorption and Dimensional Stability of Anatolian Chestnut (Castanea sativa Mill.) wood
2008 - IRG/WP 08-40407
The heat treatment of wood is an environment-friendly method for wood preservation. This process improves wood’s resistance to decay and its dimensional stability. However, mechanical properties decrease in different ration because of density loss as a result of heat treatment. In this study, the effect of heat treatment on water absorption and dimensional stability at different relative humidit...
G Gunduz, D Aydemir


Effects of Moisture Content and Species on Penetration of Liquid in Laser Incised Lumber by the Passive Impregnation Method
2008 - IRG/WP 08-40408
Penetration of liquid by passive impregnation method for Douglas-fir (Pseudotsuga menziesii Franco), sugi (Cryptomeria japonica D. Don) and Japanese larch (Larix leptolepis Gordon) were studied. Effects of initial moisture content of sugi (16, 43 and 70% moisture content) on liquid penetration by the method were also studied. Dried Douglas-fir and sugi, and green Japanese larch and sugi were treat...
N Hattori, M Nazrul Islam, K Ando, H Yamauchi


Variations of Furfuryl alcohol and Wolmanit CX-8 treatability of pine sapwood within and between trees
2008 - IRG/WP 08-40421
The variations on the ratio of filling (RoF) were investigated on Norwegian grown Scots pine (Pinus sylvestris). The samples were taken from 10 different stands in south-east Norway, and treated with furfuryl alcohol and a copper-containing wood preservative. Both within tree variations, between tree variations and variations between stands were investigated for significant differences. Factors li...
E Larnøy, S Lande, G I Vestøl


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


Mold fungi - Major impediments to cleaning/repairing flood and rain-damaged homes
2008 - IRG/WP 08-40427
Damage to homes by hurricanes that make landfall in the south and southeastern United States, or sub-tropical and tropical regions, during the hot, humid summer months is compounded by the growth of mold fungi on wetted building materials. Most homeowners are better equipped to deal with construction problems associated with storm damage than to control the growth of mold fungi. Following hurrican...
T L Amburgey


Impregnación de durmientes de quebracho blanco (Aspidosperma quebracho blanco) con preservadores cromocuproarsenicales (CCA)
2008 - IRG/WP 08-40428
CCA impregnation of railroad ties is a recent process in Argentina which has not been optimized in a commercial scale. This study analyzed the influence of treatment pressure on final retentions to optimize the impregnation process. Results showed that a 3.2% m/v solution resulted in 10.8 kg/m3 CCA retention. At 1187 kPa (12 kgf/cm2) quebracho blanco wood had an average absorption of 338 l/m3. Als...
D Gherscovic, Z Cataldi, J M Languasco


Dimensional Stability of Nine Tropical Hardwoods from Cameroon
2009 - IRG/WP 09-10687
This study investigated the swelling behavior, rate of swelling and dimensional stability of nine tropical hardwood species from Cameroon, namely ayous (T. scleroxylon), bilinga (N. diderrichii), bubinga (G. tessmannii), iroko (C. excelsa), Makore (M. heckelii), moabi (B. toxisperma), movingui (D. benthamianus), teak (T. grandis) and zingana (M. brazzavillensis). Continuous swelling was monitored ...
S R Shukla, D P Kamdem


Moisture adsorption isotherms of wood studies using a dynamic vapour sorption apparatus
2009 - IRG/WP 09-20398
Five types of wood including two Malaysian hardwoods acacia mangium (Acacia mangium) and sesenduk (Endospermum malaccense), two temperate softwoods, Sitka spruce (Picea sitchensis), radiata pine (Pinus radiata) and Accoya (commercially modified wood) were studied to determine their moisture sorption behaviour using a Dynamic Vapour Sorption (DVS) apparatus. The isotherm plot for each species teste...
J Zaihan, C A S Hill, S Curling


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Enhanced uptake of wood modification agents in “bioincised” wood
2009 - IRG/WP 09-40445
The permeability of refractory wood species e.g. Picea abies and Abies alba is reduced resulting in a radial penetration of chemical solutions of only a few millimetres. Exploitation of these wood species is therefore not possible for many applications. A novel biotechnological method (European patent 05027812.6) based on the pre-treatment of wood with the white-rot fungus Physisporinus vitreus si...
F W M R Schwarze, M Schubert


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Differential response of wood to dry air thermal treatment (DATT) and soy oil thermal treatment (SOTT)
2009 - IRG/WP 09-40446
Thermal treatment is an alternative to chemical modification method which has been used to some extent in improving timber quality. In order to get the maximum benefits possible without compromising the various end-use quality requirements of timber, several possibilities have been and are still being investigated in relation to this technique. Clear wood samples (19 x 19 x 150mm) of kiln-dried re...
L Awoyemi


Modification of Wood by a Water-Repellent Compound Used in the Textile Industry: Boron Release and Termite Resistance
2009 - IRG/WP 09-40447
In the study, wood specimens were treated with disodium octoborate tetrahydrate (DOT) and a commercial water and oil repellent compound, FORGUARD M®, a weak cationic emulsion containing dipropylene glycol monomethylether, water and solids in its formulation and used in the textile industry. There were two different processes for preservative treatments: double and single treatments. The leaching ...
S N Kartal, E Terzi, B Erilkun, Y Imamura


Interactions between wood and propiconazole in supercritical carbon dioxide
2009 - IRG/WP 09-40461
Understanding the movement and deposition of biocides in wood is a fundamental aspect of the supercritical wood impregnation process and a key issue in developing the process e.g. to handle wood of larger dimensions. Previous research on supercritical wood impregnation frequently reports of a biocide concentration gradient in impregnated samples i.e. a lower concentration of biocides in the core o...
A W Kjellow, O Henriksen


Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


The brown rot of oak wood submerged for 6 months in the Baltic sea
2010 - IRG/WP 10-10736
The natural wood submerged or partially immersed in sea water is commonly affected by certain microorganisms. The bacteria and marine borers that decay the wood totally submerged in sea water and above sea level other microorganisms as fungi, algae, insects may attacked wood. The sea water may affect and change the properties of wood. We have tried to determine the susceptibility to decay caused b...
A Fojutowski, A Kropacz, I Pomian


Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


Using plant oils as hydrophobic substances for wood protection
2010 - IRG/WP 10-30550
The increased interest to use oils as hydrophobic agents and the current debate about the further use of creosote emphasises the urgent need of better understanding of plant and other oils as wood protectors. The present study sheds light on the hydrophobic properties and distribution of various plant oils in the anatomical structure of Scots pine sapwood. Oil retentions from approximately 70 to 5...
D Panov, N Terziev, G Daniel


Study on the thickness swelling of mould-resistant chemical treated bamboo strand woven outdoor flooring
2010 - IRG/WP 10-40489
To prevent bamboo strand woven flooring from mould, several preservatives were chosen to treat bamboo strand before dipping into adhesives and pressing. The thickness swelling and mould resistant effect of the finished board were studied. Results showed that different preservatives had different influences on the thickness swelling of BSWF, and in order to reduce the thickness swelling of the fini...
Fangli Sun, Binfu Bao, Shenyuan Fu, Anliang Chen


An investigation on some physical properties of oil heat treated poplar wood
2010 - IRG/WP 10-40509
In this study some physical properties of small samples (20×20×20 cm) of poplar wood (Populus nigra var.pyramidalis) after oil heat treatment with linseed oil was investigated. Two time levels (4.5 & 6 hours) and three temperature stages (180,200 & 220°C) were selected. The results of this study showed significant differences in effects of treatment temperature on physical properties of wood....
B Bazyar, D Parsapajouh, H Khademiesalam


Kinetic Water Vapour Sorption of Sitka Spruce at Variable Temperature Using the Parallel Exponential Kinetics Model
2010 - IRG/WP 10-40512
In this study the water vapour sorption of Sitka spruce (Picea sitchensis (Bongard) Carr.) was measured using a Dynamic Vapour Sorption (DVS) apparatus and then analysed using the parallel exponential kinetics (PEK) model. The water vapour sorption rate of wood quickly increased when the relative humidity was changed. With the elapse of time, the sorption rate gradually decreased within any specif...
Yanjun Xie, C Hill


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5 years’ exposure ( IRG/WP 97-30139), and showed that the resistance of acetylated wood wit...
P Larsson Brelid, M Westin