IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 550 documents. Displaying 25 entries per page.


Using X-ray scattering to elucidate the mechanisms behind the moisture and fungal decay resistance of epoxybutene modified wood
2019 - IRG/WP 19-40854
Chemical modification of the hydroxyl groups of wood can improve the properties of wood by providing moisture and biological resistance, as well as dimensional stability. Southern pine solid wood was chemically modified to various weight percentage gains (WPG) with epoxybutene (EpB, 8%-38% WPG). After modification, specimens were extracted with a toluene: ethanol (2:1) solution for 2 hours or wate...
R E Ibach, N Plaza


Development of beech wood thermo-chemical modification treatments based on different vinylic derivatives of glycerol and polyglycerol
2019 - IRG/WP 19-40855
In this study, a combination between chemical and thermal wood modification has been investigated. Seven types of a low concentration of 10% aqueous additive solution of vinylicglycerol [glycerol-maleic anhydride (Gly-MA), glycidyl methacrylate (GM), and Glycerol methacrylate-maleic anhydride (GM/MA(2eq))], vinylicpolyglycerol [polyglycerol-maleic anhydride (PG-MA), polyglycerol methacrylate (PGM...
M Mubarok, S Dumarcay, H Militz, K Candelier, M-F Thevenon, P Gerardin


Dimensional stability and decay resistance of montmorillonite- furfuryl alcohol modified wood
2019 - IRG/WP 19-40856
Poplar (Populus cathayana) wood was impregnated successively by organo-montmorillonite (OMMT; in concentration of 2%) and furfuryl alcohol (FA, in concentrations of 15%, 30% and 50%) in a two-step method to prepare OMMT-FA modified wood. The modified wood samples were characterized using X-ray diffraction (XRD) and field emission scanning electron microscopy (FE-SEM). Moreover, wood physical and a...
L Zhang, J Cao


Thermal performance and fire safety properties of traditional circumferential log-cabin walls
2019 - IRG/WP 19-40872
The paper describes the experiment of fire resistance of a circumferential log-cabin wall fragment using various structural modification of the gap between two log members. The influence of the gap structural modification on the criterion of fire resistance E (envelop integrity) and I (insulation) is evaluated. The evaluating criteria are represented by the development of temperatures measured in ...
S Jochim, L Makovicka Osvaldova, M Zachar, Z Danihelova


The impact of additional interior layers to the moisture dry-out and mould growth risk of CLT walls
2019 - IRG/WP 19-40876
The objective of this study was intended to determine the maximum allowable initial moisture content for CLT walls having both exterior and interior thermal insulation. A laboratory test was conducted, for which four test walls with two different insulation solutions and two different initial moisture contents were built. Based on the test results a simulation model was configured and simulations ...
V Kukk, J Kers, T Kalamees


Novel approaches for improvement of dimensional, photo- and thermal stability of wood through liquefied wood polyols impregnation
2019 - IRG/WP 19-40884
The major problems encountered in both indoor and outdoor utilization of wood are due photo instability and dimensional instability. The modification of Melia dubia wood for ultraviolet resistance and dimensional stability with liquefied wood has been carried out through impregnation method under solvent free conditions. The level of impregnation in modified wood was estimated by weight perc...
A Kumar, A John, T S Mehra


Performance of bio-based building materials – durability and moisture dynamics
2020 - IRG/WP 20-20666
When exposed to conditions favourable for decay, bio-based building materials can be susceptible to degradation. Their ability to withstand deterioration over time (performance) depends on the intrinsic or enhanced durability of the material as well as its wetting and drying behaviour. The effect of fungicidal components in wood is known since long. Other material characteristics, such as the mate...
L De Ligne, J Caes, S Omar, J Van den Bulcke, J M Baetens, B De Baets, J Van Acker


Resistance against marine borers: About the revision of EN 275 and the attempt for a new laboratory standard for Limnoria
2020 - IRG/WP 20-20669
Wood protection technology in the marine environment has changed over the last decades and will continue to do so. New active ingredients, newer formulations, and novel wood-based materials including physically- and chemically-modified wood, together with increasing concerns over environmental impacts of wood preservatives, urgently demand a major revision of EN 275 “Wood preservatives – Deter...
S Palanti, S Cragg, R Plarre


Limiting Polysaccharide Motion Protects Wood From Decay
2020 - IRG/WP 20-40890
It is well known that chemical modifications to improve decay resistance also reduce the equilibrium moisture content (EMC) of wood. The mechanism of this action, however, has been the subject of much debate. Several groups have suggested that decay resistance is a result of lower diffusion rates of fungal degradation agents through the wood cell wall. A recent paper explained the fundamental prin...
C G Hunt, S L Zelinka, J E Jakes


Biological durability of sapling wood
2020 - IRG/WP 20-10967
Sapling-wood products from different wood species such as willow (Salix spp.) and Common hazel (Corylus avellana) are frequently used for gardening and outdoor decoration purposes. Remaining bark is suggested to provide additional biological durability. Even for temporary outdoor use it seemed questionable that durability of juvenile sapwood can provide acceptably long service lives of horticultur...
C Brischke, L Emmerich, D G B Nienaber, S Bollmus


Impact of fungal decay on the bending properties of wood
2020 - IRG/WP 20-20671
Wood used outdoors is generally prone to fungal degradation, and its impact on the structural integrity of wood is an immanent factor for service life planning with timber. Wood decayed to very small mass losses can suffer from a significant reduction in mechanical strength and elastic properties. Hence, the latter are preferred indicators to detect decay in wood durability studies. Numerous previ...
S Bollmus, P B van Niekerk, C Brischke


Validating a short-term laboratory method to assess the resistance of timber to biodegradation by marine wood-borers
2021 - IRG/WP 21-10975
Novel approaches to protecting wood in coastal and marine environments are needed as the use of traditional broad-spectrum biocides are now restricted. Wood is widely utilised in marine environments where it can be rapidly degraded by wood-boring organisms, causing billions of dollars of damage per annum. Biocidal compounds such as CCA and creosote have been popular treatments for timber products ...
L S Martin, J R Shipway, G P Malyon, S M Cragg


Experience Experience from over 20 years of field trials of resin treated wood – Marine borer resistance of MMF and DMDHEU modified wood
2021 - IRG/WP 21-10976
In 1999 a field test of Scots pine treated with MMF (Methylated Melamine Formaldehyde) resin and acetylated Scots pine post treated with MMF resin was started. Six years later a commissioned full NWPC test for BASF of Belmadur® (DMDHEU resin treated wood) was started at the same site. The testing, according to European Standard EN 275, was done in a bay by Kristineberg Marine Research Station o...
M Westin, P Larsson Brelid, A O Rapp, J Habicht


Marine borer resistance of various wood materials in Japan
2021 - IRG/WP 21-10983
Wood resistance against marine borer was intensively studied in the 1940s in Japan, but the research activities on the subject diminished afterward, as the use of wooden marine structures and ships decreased. Today, however, use of wood as a construction material is officially promoted for its environmental benefits. The author started to immerse some wood materials in the seawater pool at PARI ...
M Yamada


Studies on the material resistance and moisture dynamics of Douglas fir and Sitka spruce from Slovenia
2021 - IRG/WP 21-20677
Wood in outdoor applications is subject to various decomposition factors. Wood degradation can be prevented by construction details, biocide protection of wood, wood modification, or selection of naturally durable wood species. Unfortunately, the majority of timber species in Europe do not have naturally durable wood. Imported tree species represent a new pool from which we can draw wood species w...
M Humar, B Lesar, D Krzisnik, E Kerzic, R Brus


Mechanical and biological durability properties against soft-rot and subterranean termite in the field (grave-yard test) of beech wood impregnated with different derivatives of glycerol or polyglycerol and maleic anhydride followed by thermal modification in an opened or in a closed system
2021 - IRG/WP 21-40917
This paper presents mechanical and biological durability properties in soil beg test (soft-rot test) and field test (grave-yard test) against subterranean termite of the wood modified with an aqueous vinylic derivative of glycerol/polyglycerol or maleic anhydride cured in an opened or in a closed system. Wood modification was performed through impregnation of European beech (Fagus sylvatica) with ...
M Mubarok, H Militz, S Dumarcay, I W Darmawan, Y S Hadi, P Gerardin


Aiming for eco-friendly log production and wooden construction!
2021 - IRG/WP 21-50365
In order to reduce greenhouse gas (GHG) emissions to zero by 2050 in the fields of forest and forest products, it is necessary to promote appropriate management and renewal of planted forests, and development of wooden building materials and the wooden construction of mid-to-high-rise buildings with lower GHG emissions. Unless we also try to reduce the environmental loads other than GHG for such d...
N Hattori


Application of suberin fatty acids extracted from birch bark for wood coating
2021 - IRG/WP 21-40914
It is well known that chemical modifications to improve decay resistance also reduce the equilibrium moisture content (EMC) of wood. The mechanism of this action, however, has been the subject of much debate. Several groups have suggested that decay resistance is a result of lower diffusion rates of fungal degradation agents through the wood cell wall. A recent paper explained the fundamental prin...
A Kumar, Risto Korpinen, Veikko Möttönen


The effect of sapwood and heartwood differences on durability of short rotation teak wood
2022 - IRG/WP 22-10991
Short rotation teak has been developed to overcome the limited supply of long rotation teak. The aim of this study was to investigate the effect of sapwood and heartwood differences on durability of short rotation teak. The following basic properties were studied: extractive content, dimensional stability (volumetric swelling and water uptake), decay resistance, and termite resistance. The result...
R Martha, M Mubarok, F O Akong, B George, C Gérardin, S Dumarçay, I S Rahayu, I Batubara, W Darmawan, P Gérardin


Results of the resistance of acetylated wood against marine borers at three Italian sites after five years of sea immersion
2022 - IRG/WP 22-10994
The aim of this research was the determination of resistance of acetylated wood against marine decay in use class 5 (EN 335) in temperate sea waters. The resistance of acetylated Pinus radiata (radiate pine) in solid and medium density fibreboard (MDF) panels is compared with that of the untreated Scots pine, radiata pine and other untreated wood of European species such as Fagus sylvatica (Europe...
S Palanti, F Stefani, M Andrenacci, M Faimali, I Guarneri, M Sigovini, D Tagliapietra


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Introduction to the project ‘Deterioration and decay of wooden cultural heritage in Arctic and Alpine environments’ (ArcticAlpineDecay)
2022 - IRG/WP 22-10997
The Arctic is already affected by climate change, and this is expected to accelerate over the coming decades. Alpine regions in Norway are projected to face similar challenges. Current knowledge on Norwegian wooden cultural heritage in Arctic and Alpine regions is scattered and contains significant knowledge gaps. Historically, - scientists, sectorial governance, tourist trade and commerce have ma...
G Alfredsen, L Ross, A W Hegnes, M S Austigard, J Mattsson, N B Pedersen, A Sinitsyn, V V Martens, A-C Flyen


Evaluation of Decay Resistance of Copper-based Preservatives Treated-Wood exposed to different field test sites in Korea
2022 - IRG/WP 22-20679
In Korea, preservative treated wood is required to have a stamp on the surface which contains information such as wood species, use categories, and the company that treated the wood. Such stamping is necessary to safely and appropriately use the treated wood. Since majority of treated wood is being used outdoor environment, the treated wood must have efficacy against wood decay fungi or termite. I...
W-J Hwang, S-M Yoon, Y Park, Y-S Choi, H-M Lee, J-W Kim


Above-Ground Termite Resistance of Naturally Durable Species in Ontario and Mississippi
2022 - IRG/WP 22-30767
A collaborative above-ground protected termite field test was initiated by FPInnovations and the USDA Forest Service at sites in Ontario and Mississippi. The aims of the experiment were to compare the rate of attack in protected, above-ground exposures by the subterranean termite species, Reticulitermes flavipes, between northern (Ontario) and southern (Mississippi) test sites and to generate perf...
R Stirling, M Mankowski


Impact of wetting agents on polyelectrolyte complex impregnation for wood fire-retardancy
2022 - IRG/WP 22-30768
Wood fire performance is a great concern in interior finishing due to the high risk of flame spread. To increase the use of wood in high building while ensuring the safety of building occupants, fire retardant (FR) treatments are required. Traditionally, two fireproofing strategies are employed: impregnation and coatings. They have been widely studied but they, respectively, are time and chemicals...
M Soula, J B Grenier, S Duquesne, F Samyn, V Landry


Previous Page | Next Page