Toward an assessment of copper bioavailability in treated wood
2010 - IRG/WP 10-20445
Many modern wood preservative systems rely on copper (Cu). Some oxalate-producing fungi detoxify Cu by immobilizing it in crystals, and this may decrease its physiological availability (bioavailability). Cu bioavailability may also decrease during wood treatment. Cu retention in wood, however, is typically measured as a weight-to-volume concentration without an estimate of its bioavailability and ...
J S Schilling, J J Inda


Onset of mould growth – the effect of climate variability and different geographic locations
2010 - IRG/WP 10-20446
This paper presents a study on how climate conditions at numerous locations in Sweden affect the risk of onset of mould on wood sheltered outdoors. The results indicate that the risk is clearly higher in the south compared to the north of Sweden. These differences are mainly explained by colder and dryer winter periods in the north which is unfavorable for development of mould. The results also sh...
M Häglund, T Isaksson, S Thelandersson


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Effect of Nano-silver Treatment on Densified Poplar Wood Properties. Part Two: Spring Back, Compression set, Impact Load Resistance and Hardness
2011 - IRG/WP 11-40568
This paper is the second part of the study of applying nano-silver treatment before densification of poplar wood (Popolus alba). The specimens were prepared in four groups of: 1) nano-silver impregnated 2) water impregnated 3) dried with no impregnation and 4) the control specimens. The impregnation process was done by empty cell process. Then, the groups of 1 to 3 were compressed in a hot press a...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khajeh


Determination of Izod Impact Strength on Wood: A Suitable Method to Detect Fungal Decay in Protective Effectiveness-Screenings of Wood Preservatives
2012 - IRG/WP 12-20484
For testing a large number of different substances regarding fungicide properties, the reduction of the decay test duration is advantageous. In the present paper the suitability of a method for testing plastics using an impact testing machine was examined. The results clearly show that the fungal attack of European beech by the white-rot fungus Trametes versicolor leads to a decrease of izod imp...
H Delenk, M Zauer, A Wagenführ


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


The assessment of biological and mechanical properties of wood treated with ionic liquids – N,N-dimethylamine and 1-decylimidazole derivatives
2012 - IRG/WP 12-40582
This paper presents the results of tests of the effectiveness of action of new imidazolium and bis-ammonium ionic liquids against Basidiomycotina and Ascomycotina wood-destroying fungi. All the investigated ionic liquids showed high fungicidal action against Coniophora puteana. In order to characterize the influence of ionic liquids on mechanical wood properties, the compression strength along the...
W Przybylska


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Development of a quality control assessment method to predict properties of heat treated wood
2012 - IRG/WP 12-40611
Heat treatment has been used to improve properties of non durable European species. Chemical modification of some of the wood components provides improved dimensional stability and biological performance against decay fungi while mechanical properties such as modulus of rupture are reduced. Quality control of commercially made thermally treated wood is one of the major challenges to allow its indu...
M Chaouch, K Candelier, S Dumarcay, A Pétrissans, M Pétrissans, P Gérardin


An assessment of soft rot in preservative-treated poles in two test sites and two network areas in New South Wales
2013 - IRG/WP 13-10801
This document presents an extended summary of recent investigations into soft rot attack of preservative treated power poles from the re-inspection of samples selected from two field sites and two in-service trials located in New South Wales, Australia. The in-ground sapwood of selected poles was assessed by probing and, after core sampling, by microscopy to determine the severity and extent of s...
W D Gardner, M A Powell, C Kirton


The assessment by visual grading, change of color and ergosterol content ratings, the resistance to mould fungi of treated with wood preservative Scots pine sapwood
2013 - IRG/WP 13-20514
The filamentous (mould) fungi belonging to Ascomycetes, Deuteromycetes group are an cosmopolitan organisms which attacks wooden elements disfiguring them, dropping their value and causing environmental and health hazard. The fungi in a short time cause mainly disfigurement of wood does not effect on strength properties of wood, but with strong prolongation of duration of conditions favourable for ...
A Fojutowski, A Koziróg, A Kropacz


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


Application of a model for the prediction of fungal degradation of thermally modified beech timber by Trametes versicolor
2013 - IRG/WP 13-40622
Colour measurement technology is found to be feasible for characterization of the property changes of thermally modified timber (TMT). In opposite to time-consuming and expensive laboratory tests a non-destructive test represents an improvement for the manufacturer of TMT. Therefore the aim of this study was to develop a method which allows sorting the different treatment intensities after the man...
Clauder, L., Richter S., Unger, W., Pfriem, A


Conclusions and Summary Report on an Environmental Life Cycle Assessment of ACQ-Treated Lumber Decking with Comparisons to Wood Plastic Composite Decking
2013 - IRG/WP 13-50295
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of ACQ (alkaline copper quaternary)-treated lumber decking and wood plastic composite decking using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood decking are significant. • Less En...
AquAeTer, Inc.


Conclusions and Summary Report on an Environmental Life Cycle Assessment of Borate-Treated Lumber Structural Framing with Comparisons to Galvanized Steel Framing
2013 - IRG/WP 13-50296
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of borate (disodium octaborate tetrahydrate)-treated lumber structural framing and galvanized steel framing using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood framing are significant....
AquAeTer, Inc.


Conclusions and Summary Report Environmental Life Cycle Assessment of Highway Guard Rail Posts
2013 - IRG/WP 13-50297
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of treated wood and galvanized steel highway guard rail posts using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood guard rail posts are significant. • Less Energy & Resource Use: ...
AquAeTer, Inc.


Conclusions and Summary Report Environmental Life Cycle Assessment of Marine Pilings
2013 - IRG/WP 13-50298
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of treated wood, concrete, galvanized steel, and plastic marine piles using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood piles are significant. • Less Energy & Resource Use: Tre...
AquAeTer, Inc.


Conclusions and Summary Report on an Environmental Life Cycle Assessment of Utility Poles
2013 - IRG/WP 13-50299
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of pentachlorophenol-treated wood, concrete, galvanized steel, and fiber-reinforced composite utility poles using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood poles are significant. ...
AquAeTer, Inc.


Assessment of Scots pine sapwood susceptibility to moulds by determination of fungi growth and ergosterol content in infested wood
2014 - IRG/WP 14-20540
The susceptibility of wood to filamentous fungi (mould) attack is determine mainly by laboratory methods with descriptive grading of fungal growth on the surface of the wood specimens. It is a lot of different grading scale of fungi growth, but determination of the size of fungi growth is many times not easy, not clear and often difficult. Although the filamentous fungi are not included to microor...
A Fojutowski, A Koziróg, A Kropacz


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar


Influence of Exposure Direction on Leaching of a Biocide from Painted Wood Surfaces
2014 - IRG/WP 14-50303
The objective of this project was to investigate the influence different exposure directions – North, East, South and West on the cumulative quantity of a biocide leached from painted wood surfaces due to rainfall and the consequences for the risk assessment. The study included a solvent-borne primer without biocides and a topcoat protected with a biocidal active substance. Both products were a...
M Klamer