Preservative-efficacy of boric acid-triethanol amine solution against wood-decay fungi
1994 - IRG/WP 94-30050
Laboratory preservative-efficacy tests were conducted using boric acid-triethanol amine (BTEA) solution in accordance with the JIS A 9201 (1991) test method excluding the standard weathering process. Sapwood specimens of Picea jezoensis or Fagus crenata to achieve nominal retentions of 0.40-41.2 kg/m³ of boric acid were exposed to Tyromyces palustris, Coriolus versicolor, Serpula lacrymans or Cha...
S Doi, M Mori, Y Mineki


Resistance of various wood species against decay by Coniophora cerebella (Pers) Duby and Lenzites trabea (Pers) Bres
1976 - IRG/WP 142
Both fungi, Coniophora cerebella and Lenzites trabea, are important destroyers of timber. Coniophora often occurs inside buildings and Lenzites trabea has been observed on southern facades of buildings, on balconies and window frames. In most instances that we investigated coniferous timber had been decayed. But both species are known to attack also various hardwoods. For this reason tests similar...
O Wälchli


Preservative ability of wood to be fixed hydroxyl apatite substituted for antimicrobial metals
2001 - IRG/WP 01-30272
We succeeded in forming hydroxy apatite (HAp) in wood. HAp is non-toxicity and safe. Preservative ability of the wood, which substituted one part of Ca of constituent element of this HA p for antibacterial metals was measured. When Ca was substituted for Ag or Zn, mass loss in decay by brown-rot fungus F. palustris was restrained in about 50% (Ag) ~30% (Zn) of value of control specimen. However, w...
Y Haruhiko, I Sumaru


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 6: Report of third inspection (24 months) in Australia
1980 - IRG/WP 456
This report presents the results of the third inspection of the IRG/COIPM International Marine Test specimens installed at the Goat Island Marine Biological Station of the Maritime Services Board of New South Wales, in Sydney Harbour. The inspection was completed on 5th December, 1979, after 24 months exposure. As on previous occasions, this inspection was carried out in conformity with the provis...
J Beesley


Evaluation of bacteria for biological control of wood decay
1990 - IRG/WP 1426
Laboratory soil-block and agar-block tests were carried out to evaluate the efficacy of bacteria as biological control agents against 5 brown-rot and 3 white-rot fungi. Pretreatment of Southern pine and sweetgum with a bacterial solution prevented decay in agar-block tests. However, the bacteria were generally ineffective in preventing decay in Southern pine, Douglas-fir, sweetgum and yellow popla...
R Benko, T L Highley


Evaluation of chlorpyrifos and fungicides alone and in combination for control of insects and fungi in wood and wood composites
1998 - IRG/WP 98-30187
Wood composites are rapidly being adapted for use in exterior applications. The incorporation of a preservative system to prevent fungus and insect attack is necessary with most exterior composites. Research studies were reviewed pertaining to organic preservative systems based on Lentrek* insecticide wood treatment which contains the active ingredient chlorpyrifos alone and in combination with te...
M P Tolley, P E Laks, R Fears


Evaluation of wood durability by laboratory test - A new equation to predict wood durability
2001 - IRG/WP 01-20230
To estimate the wood durability in a short term, periodical weight determination was carried out in a laboratory test. This test provided the results comparable to those of the field test and the fungus cellar test, but it required much more jobs in comparison to the usual accelerated laboratory test. To save the time and jobbing for this method, a new equation was devised from simple two assumpti...
I Momohara, K Yamamoto


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 14: Report of fifth inspection (48 months) in Australia
1982 - IRG/WP 484
This report presents the results of the fifth inspection of the IRG/ COIPM Internatlonal Marine Test specimens installed in Sydney Harbour in December, 1977. This inspection took place on 9th December, 1981, just 48 months after the specimens were installed. Earlier reports have contained full details of the treatment and installation of the specimens as well as results of all previous inspections...
J Beesley


The impact of global warming on the UK distribution of house longhorn beetle Hylotrupes bajulus (L)
2001 - IRG/WP 01-10414
This paper reviews the effects of global warming on insect populations and distribution. The affects of global warming on the spread of Hylotrupes is predicted through a review of research related to the influence of temperature on its life-cycle and flight. Records of Hylotrupes distribution were obtained from published surveys, entomologists and museum collections and were plotted for the UK. Th...
P Oevering, A J Pitman


IUFRO rating system compares favourably to weight loss for soil-bed testing
1990 - IRG/WP 2343
The soil-bed/small stake test is commonly used for rapidly evaluating the performance of new, more environmentally acceptable, preservatives. In a 1.5 year experiment with three copper-based waterborne preservatives, visual evaluation and probing using the IUFRO performance rating scale (0-4) gave very similar toxic thresholds to those derived from measurement of weight loss at the end of the expe...
P I Morris


Durability of exterior natural wood finishes in Brazil
1985 - IRG/WP 3343
Wood finishes systems were evaluated in natural weathering conditions during 5 (five) years, over "Parana-pine" (Araucaria angustifolia). Test samples results show that: - Semitransparent wood preservative stains, based on polimerized linseed oil, provided very good protection to the wood, compared with the one based on alkyd varnish; - Solid color wood preservative stains provided good durability...
D R Macedo


Natural durability of fifty species of Indian timber in Goa waters against marine wood-borers
1989 - IRG/WP 4150
Results of the investigations on the natural durabilitv of fifty species of Indian timber, based on data collected bv exposing test panels at Betim near Panaji (Goa) continuously for a period of 11 months are presented. The study revealed that none of the timber species tested has any natural resistance at this locality and all the panels were completely destroyed within 11 months. Details on the ...
L N Santhakumaran, S Udaya Bhaskar, J C Jain


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


Durability of surface coating systems. Mycologg - an accelerated mycological test.
2004 - IRG/WP 04-20301
Field testing and natural aging/degradation of test sample, e.g. coated wooden surfaces is a slow process. Accelerated tests focus on mechanical properties, water uptake or sometimes stain fungi. Artificially weathered coated panels are not easily compared with naturally aged panels, and show the importance of involving the biological component among the degrading facors. It is a need for acce...
L Ross Gobakken, J Mattsson, B Jacobsen, F G Evans


Laboratory evaluation of termite resistance of five lesser-known Malaysian hardwoods used for roof and ceiling construction
2001 - IRG/WP 01-10398
The general laboratory procedure of AWPA E1-97 was used to evaluate the termite resistance of 5 lesser- known species (LKT) of Malaysian hardwoods: Kekatong (Cynometra sp.), Kelat (Eugenia spp.), Mempening (Lithocarpus spp.), Perah (Elateriospermum tapos) and Pauh Kijang (Irvingia malayana) against the subterranean termite Coptotermes curvignathus over 28 days. Kempas (Koompassia malaccensis) and ...
A A H Wong, Kee Suan Cheok, J K Grace


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Occurrence of termite species on decaying heartwood specimens exposed 18 to 23 years at an Australian site
1998 - IRG/WP 98-10270
The occurrence of species of subterranean termites on hardwood and softwood specimens (including preservative-treated), exposed in-ground at a semi-arid site at Walpeup (north-western Victoria), 18 to 23 years after installation, is reported. This paper presents maps of the cumulative occurrence on specimens, after six annual inspections, of the following species: Coptotermes acinaciformis, Hetero...
J W Creffield, J-D Thornton, G C Johnson


Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 18. Report of seventh inspection (72 months) in Australia
1984 - IRG/WP 4108
This report includes the results for the 72 month inspection of the IRG/COIPM International Marine Test installed in Sydney Harbour. Although, overall, attack by teredinid and limnorid borers have been most commonly encountered in test specimens at this site, slight attack, mainly by sphaeromatids, has recently been initiated on some hitherto unattacked treated Alstonia scholaris and Pinus sylvest...
L J Cookson, J E Barnacle


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


The relationship between the electrical resistance and fixation of water-borne CCA salts and pressure-treated wood
1991 - IRG/WP 3657
Two investigations at 22°C and 30°C have been carried out. The electrical resistance in the treated wood and chemical analyses of the remaining amount of unfixed copper, chromium and arsenic were investigated. Samples impregnated with water were used as references. To hold the samples moist during the investigation, each sample was wrapped in a polyethylene plastic foil immediately after impregn...
F G Evans, B Nossen


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel