Natural Durability of Fence Poles from Fourteen Semi-Arid Land Species after Six-Month Exposition
2010 - IRG/WP 10-10724
A sample of thirty fence poles from each of fourteen tree native species from Northeast Mexico were tested in ground contact in a wood-cemetery area located in Linares, Nuevo Leon, Mexico. The samples were submitted to six treatments (control, debarked, chemical treated, used cooking oil, thermal and creosote) and randomly distributed in five blocks. The effectiveness of using a bark gauge tool â€...
A Carrillo, F Garza, V Bustamante, S Sandoval, H VillalĂłn


Structural changes, basidiomycete richness, enzyme activity and proteomic profiling of decay resistant and non-resistant woods over 18 months in soil contact
2010 - IRG/WP 10-10733
Wood decay fungi damage wood by production of enzymes that attack the structural components. The objective of this study was to better understand which suite of decay genes and proteins are expressed during biodeterioration of three different wood types in forest soil over time. Variation in decay genes and proteins were determined for pine (non-resistant), cedar (naturally durable), and ACQ-treat...
Youngmin Kang, S Diehl, L Prewitt, D Nicholas


Natural durability of Mulberry wood from Iran
2010 - IRG/WP 10-10737
Mulberry wood (Morus alba L.) is traditionally used in Iran to manufacture music instruments such as tar and setar. But little is know and contradictory statements are found on the natural durability of Morus alba. Moreover, in many cases, Iranian instrument makers leave freshly cut Mulberry timber into water (cold or hot) for a time period depending on the craftsman habit, without any real knowle...
A Se Golpayegani, M-F Thevenon, J Gril, K Pourtahmasi


Natural durability of African Padauk and Niove. Comparison of new trials and former data from the CIRAD database
2010 - IRG/WP 10-10743
African Padauk (Pterocarpus soyauxii) and Niove (Staudia kamerunensis) were tested in laboratory against Basidiomycetes. The results were calculated according to the requirements of EN 350-1 (1994) and XP CEN/TS 15083-1 (2006). Padauk samples showed a high durability and very small variations between trees and within tree. Niove presented a high durability, but with notable differences according ...
Y N N’Kolo Meze’e, N Leménager, C Baudassé, M-F Thévenon


Glued laminated poles - Progress report after 30 years testing
2010 - IRG/WP 10-20427
In 1979 a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse at Uppsala, at the SimlĂĄngsdalen test field in southern Sweden and in a power lane in Vuollerim in northern Sweden in order to study their resistance against biological degradation. The tests have shown that the best performance will be obtained if each lamination is treated with a water-borne pre...
Ă– Bergman, J Jermer


The Relative Performance of an Organic Preservative System under UC3A and UC3B Conditions using Two Test Methods
2010 - IRG/WP 10-20429
Coated L-joints have been used for decades to evaluate the performance of wood preservatives in protected environments. This study was conducted using matched coated and uncoated L-joints to simulate above ground protected and unprotect exposures. When exposed to constant moisture in a greenhouse environment, coated and uncoated L-joints give very similar performance results. In contrast, exposi...
C F Schauwecker, A Zahora, A F Preston


Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas


Determination of a fixation time of wood preservatives: A discussion paper
2010 - IRG/WP 10-20436
The intention of that paper is to initiate a discussion on the basis of a French method in combination with a German approach regarding the need of a method for the determination of a fixation time and especially to obtain input as well as ideas concerning a possible test design. Since no harmonised European approach exists up to now concerning the determination of a fixation time, CEN TC 38 (2009...
E Raphalen, E Melcher


Diagnosis of failures in wood beams from historical house in Banská Štiavnica – Relations between ultrasonic measurements and bending properties
2010 - IRG/WP 10-20437
Various degrees of rot and other damages in ceiling beams with dimensions of 6500-8800 x 160-200 x 240-310 mm (length x height x width) situated in one historical bourgeois house in the UNESCO town Banská Štiavnica, Slovakia were determined visually and by the PUNDIT-plus ultrasonic device. Subsequently, for seventeen of the most bio-damaged fir (Abies alba Mill.) beams chosen for exchange were ...
L Reinprecht, M Pánek


Service life prediction of wooden components – Part 1: Determination of dose-response functions for above ground decay
2010 - IRG/WP 10-20439
Scots pine sapwood (Pinus sylvestris L.) and Douglas fir heartwood (Pseudotsuga menziesii Franco) specimens were exposed in double layer field trials at 24 different European test sites under different exposure conditions (in total 28 test sets). The material climate in terms of wood moisture content (MC) and wood temperature was automatically recorded over a period of up to eight years and compar...
C Brischke, A O Rapp


Profiling fungal community in wood decay ecosystem by Denaturing High-Performance Liquid Chromatography
2010 - IRG/WP 10-20443
A DNA-based fingerprinting technique, Denaturing High Performance Liquid Chromatography (DHPLC) was developed to profile fungal communities colonizing indoor timber. Molecular fungal diversity was assessed using amplification based on the Internal Transcribed Spacer (ITS1) rDNA of 74 wood samples collected from infected buildings in France. Due to its high sensitivity, the PCR-DHPLC technique was ...
S Maurice, G Le Floch, M Le Bras-Quéré, J P Rioult, G Barbier


Stress wave and visual analysis of treated and non treated fence posts after 15 years in field test
2010 - IRG/WP 10-20449
Wood preservation may play an important role in protecting tropical rain forest. Basically, it can reduce pressure on natural resources by increasing wood durability. Field tests are conducted to simulate final use of woods under different environmental conditions. Visual analysis, non destructive testing, and non destructive evaluation techniques were applied to assess wood resistance and chemica...
A Florian da Costa, R Faustino Teles, J Costa Gonçalves


Development of microbiological test methods for the wooden packaging of foodstuffs
2010 - IRG/WP 10-20453
Whereas different sampling methods already exist for analysing contaminated surfaces or packaging made of plastic or paper, there is no methodology that enables the sampling and quantification of microorganisms in packaging made of wood. The objective of this study was to compare the most commonly used microbiological methods and to develop a reliable quality control test adapted to wooden packagi...
I Le Bayon, H Callot, M Kutnik, C Denis, A-M Revol-Junelles, J-B Millière, M Giraud, M Gabillé, N Passédat


Comparison of Bifenthrin Formulations for Their Skin and Eye Irritation Potential Using the Pollen Tube Growth Test
2010 - IRG/WP 10-30521
The Pollen Tube Growth Test (PTGT) is an effective screening method for measuring the potential of a chemical formulation to affect living cells. The PTGT has been compared against other types of testing, and it shows a good correlation with, for example, the Draize rabbit eye test and the human skin patch assay. It measures the EC50, which is the effective concentration at which 50% growth is o...
S Millward, P Lobb


Evaluation of ACQ-D treated Chinese fir and Mongolian Scots pine with different post-treatments after 20 months of exposure
2010 - IRG/WP 10-30530
The performance of alkaline copper quat-type D (ACQ-D) treated Chinese fir (Cunninghamia lanceolata Hook.) and Mongolian Scots pine (Pinus sylvestris Linn. var. mongolica Litv.) stakes after 20 months exposure in Chengdu and Guangzhou of southern China were evaluated according to AWPA standard E07-07. The ACQ-D treatments used two concentration levels (0.5 and 1.0%) and four different post-treatme...
Lili Yu, Jinzhen Cao, Wei Gao, Haitao Su


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ăś C Yildiz, A Can


A Comparison of the Performance of Related Copper Based Preservatives against Soft Rot
2010 - IRG/WP 10-30540
The performance of pine and beech wood treated with either a soluble copper + quat (ACQ type D) preservative system or a particulate copper + quat system was evaluated in unsterile soil using the European standard ENV 807 soft rot decay test procedure. In addition, to compare soft rot performance of soluble and particulate copper directly without the influence of co-biocides, beech and pine test...
M Ray, D Dickinson, K Archer


Copper nanoparticles in southern pine wood treated with a micronised preservative: Can nanoparticles penetrate the cell walls of tracheids and ray parenchyma?
2010 - IRG/WP 10-30547
This study tests the hypothesis that copper nanoparticles can penetrate the cell walls of southern pine wood treated with a micronised preservative. We examined the nanodistribution of particles in tracheid and ray parenchyma cell walls using state-of-the-art HR (High Resolution)-TEM and HR-STEM (Scanning Transmission Electron Microscope)-EDX. These devices are capable of atomic-scale resolution. ...
H Matsunaga, Y Kataoka, M Kiguchi, P Evans


Field trials of wood preservatives in UC3 retention. Part 1. Durability results after 13 years in and above ground
2010 - IRG/WP 10-30548
In 1996 an extensive field trial program was set up in order to obtain more data on wood treated with chromium and arsenic free preservatives in Use Class 3 retention. Apart from durability in and above ground, other features were also assessed, e.g. discoloration by staining fungi, depletion of active ingredients, weathering and corrosion of fasteners in con¬tact with the treated wood. Wood spec...
M Westin, J Jermer, M-L Edlund, P Larsson Brelid, I Johansson


Studies on Effect of pH on Copper Availability in Copper-Based Preservatives
2010 - IRG/WP 10-30549
Laboratory methods have been employed to investigate the pH effect on the copper solubility of basic copper carbonate. The pH was controlled using two different approaches. One was with the adjustment of pH of the solutions by acid or base using sulfuric acid or sodium hydroxide until the solution equilibriums were obtained for each defined pH. A second approach was to control pH with buffer sol...
L Jin, P Walcheski, A F Preston


Analysis of phenolic extractives from various Tunisian species trees -Study of its potential valorisation
2010 - IRG/WP 10-30552
Phenol extractives are naturally synthesized compounds taken from several trees. It is well demonstrated that the presence of phenol compounds is positively correlated with the durability of wood. This property is very interesting for outdoor uses of wood with a limited treatment. Phenol compounds may also be used in the formulation of glue. In the aim to improve the knowledge on Mediterranean tr...
I Oueslati, F Charrier, K Seffah, A Moubarik, N Ayed, A Zerizer, B Charrier


The Effects of Natural Weathering on the Properties of Heat Treated Alder Wood
2010 - IRG/WP 10-40484
Heat treatment is an effective method to improve the dimensional stability and biological durability of wood. The heat treatment technology and the heat treated wood products were recently introduced to Turkey. However, only a few studies have been reported on the effect of natural weathering on the properties of heat treated wood in both Turkey and the world. In this study, heat treated alder (Al...
S Yildiz, Ăś C Yildiz, E D Tomak


Decay and termite resistance of particleboard and MDF panels made from pinecones
2010 - IRG/WP 10-40493
Particleboard and medium density fiberboard (MDF) panels were produced by using pinecone from stone pine (Pinus pinea L.) tress and wood particles from pine and beech wood at various ratios. Specimens from the panels were subjected to slightly modified soil-block tests according to AWPA E10-06 standard method by using two brown-rot fungi, Gloeophyllum trabeum and Postia placenta and two white rot ...
C Köse, E Terzi, Ăś BĂĽyĂĽksar, Erkan Avcı, Nadir Ayrılmış, S Nami Kartal, Y Imamura


Hydrothermal modification for upgrading the durability properties of soft deciduous wood
2010 - IRG/WP 10-40494
To extend the application potentialities of soft deciduous wood, upgrading the durability properties, hydrothermal modification (HTM) of aspen alder and birch wood was investigated. The treatment was conducted in a multifunctional laboratory device WTT. In the previous cases it has been found that the treatment at 160oC improves the durability insufficiently. The modification at 180oC ensured a hi...
B Andersons, I Andersone, V Biziks, I Irbe, J Chirkova, E Sansonetti, J Grinins, H Militz


Development of markers to predict decay durability of heat treated wood
2010 - IRG/WP 10-40496
Effect of heat treatment temperature on elemental composition of Scots pine sapwood (Pinus sylvestris) has been investigated in the range of temperatures between 220 and 250°C. Results revealed an important increase of carbon content, while oxygen content significantly decreases. Independently of the heat treatment temperature, elemental composition is strongly correlated with the mass losses due...
Ž Šušteršic, A Mohareb, M Chaouch, M Pétrissans, M Petric, P Gérardin


Previous Page | Next Page