Soft-rot in Tabebuia sp. wood used in water cooling tower: identification and degradation capacity of the fungi
1998 - IRG/WP 98-10253
Tabebuia sp. (ipe), a native Brazilian wood, is considered of high natural resistance to decaying fungi, and has been used in harsh environments, as cooling towers. Fifty-one fungi, belonging to mitosporic fungi group (Fungi Imperfecti), were isolated from deteriorated Tabebuia sp. wood samples, collected from the mist eliminator and packing of a cooling tower in operation for about 23 years. The ...
S Brazolin, M Tomazello, I H Schoenlein-Crusius


Simulation test of subchronic inhalation toxicity of TBTO vapours in the air
1987 - IRG/WP 3454
The test was carried out in a wainscotted room of a normal size. Wooden panelling had been treated with one coat of basic preserving agent and, after the installation, with 2 coats of stain. Laboratory animals (rats) were kept in this room for 90 days. For the same period a control group of test animals was kept in a room of equal size where there was no panelling. During the test, concentration o...
V Skubic, S Kobal, J Stupar, R Ajlec, J Korošin, G R Pecenko


Screening of modified linseed oils on their applicability in wood protection
2004 - IRG/WP 04-30346
In this study modified linseed oils, rape oil and three waxes were screened on their efficacy as wood protecting agents. By testing all products when impregnated with high retentions in Scots Pine sapwood on water repellence qualities, additionally an accelerated weathering test, drying quality, accelerated brown rot and blue stain test, an indication is formed of the capability of these products ...
A Treu, J Lückers, H Militz


Design of a laboratory method for evaluating the effectiveness of soft rot preservatives
1988 - IRG/WP 2312
This purpose of this work was to design a method which makes it possible to evaluate the effectiveness of products which present protect wood against soft rot, using new products·of a different nature, on wood of·Pinus sylvestris L. and Fagus sylvatica L., and which, suitably applied, avoid big economic losses deriving from lack of knowledge of the active principles suitable to present protect w...
M T De Troya, A M Navarrete


Marine wood-borer test with preservatives on the coasts of Turkey
1995 - IRG/WP 95-10091
Marine wood-borer tests were carried out on the coasts of Turkey (Marmara, Mediterranean Sea and Black Sea). Sapwood blocks of 8 x 15 x 30 cm³ in size from Scots pine, Bornmüller's fir oriental beech and sessile oak were used. The test blocks were treated with CCB-salts by full cell process and coal tar creosote by empty cell process. The test blocks were installed on exposure sites bef...
A Bobat


The efficacy of polymer/preservative treatments in soil-bed exposure
1992 - IRG/WP 92-3729
Southern pine was treated with CCA, CCB, sodium borax/boric acid, or disodiumoctaborate, alone or in combination with an acrylic polymer system containing a water repellent. Treated samples were subjected to an unsterile soil burial test. The addition of polymer reduced the weight loss in borontreated samples at the lower retentions but not at the higher retention. Results with borates indicate th...
R J Murphy, H M Barnes, S M Gray


The effect of of sorbitol on the decay of boric acid treated Scots pine
1991 - IRG/WP 1509
The tetra-hydroxy borate ion is known to undergo complexation with polyols of biological importance and probably protects treated timber by this action. The inhibitory effect of boric acid upon fungal growth and dehydrogenases has been shown to be prevented by the addition of certain polyols. This work was extended, with a study of the effects of a polyol on the performance of boric acid in treate...
J D Lloyd, D J Dickinson, R J Murphy


Preliminary evaluation of the answers to the 2nd IRG/WP-questionnaire on the state of pollution control in the field of wood preservation
1982 - IRG/WP 3209
This preliminary evaluation of the answers to the 2nd IRG/WP-Questionnaire only gives a general survey on those questionnaires which the author received until April 30th, 1982. Details, such as correlations between importance of wood preservation and pollution control, as well as a comparison of the answers with those to the first questionnaire (Doc. IRG/WP/369), could not be considered due to lac...
H Willeitner


Leaching of Boron - more than 3 years of field exposure
1997 - IRG/WP 97-30143
The diffusibility of Boron in wood and thus the ability of its leaching is known since long. Nevertheless quantitative data on this process are only rarely available. To overcome this lack of information field exposure tests were started with beam-segments treated with pure boric acid and poles treated with CCB. In addition some of the beam-segments were surface-treated with a varnish to investiga...
A Peylo, H Willeitner


Assessing the bioresistance conferred to solid wood by chemical modification
1997 - IRG/WP 97-40099
The chemical modification of wood using straight chain alkyl anhydrides can considerably enhance its durability. This paper presents an assessment of the effectiveness of these modifiers in improving the biological resistance of a susceptible softwood when exposed to four different basidiomycete fungi, soft rots and the larvae of the house longhorn beetle (Hylotrupes bajulus). It was clear that so...
E D Suttie, C A S Hill, D Jones, R J Orsler


Environmental consequences of various materials in utility poles - A life cycle analysis
1992 - IRG/WP 92-3726
A model for environmental life cycle analysis, LCA, has been created to compare environmental impact from transmission poles, made alternatively of concrete, steel, aluminium and pine wood treated with CCA type B or creosote. The main pollution sources and energy use are included in the LCA. One pole size, 12 meters long, is presented in the study, a so called "45 kV" pole. Poles of different mate...
M Erlandsson, K Ödeen, M-L Edlund


Decay resistance of Siberian larch wood against brown rot fungus. - Part 3. The variation between plus trees and their grafted clones
2000 - IRG/WP 00-10350
The aim of the study was to estimate the variation in the decay resistance of Siberian larch (Larix sibirica Ledeb.) wood using mature plus trees and their grafted clones. Samples were collected with an increment core borer from 11 original plus trees and their 25-year-old grafted seed orchard clones. A typical brown rot fungus, Coniophora puteana (Schum. ex Fr.) Karst. (BAM Ebw. 15), was used as ...
H Viitanen, L Paajanen, M Venäläinen, A Harju, P Velling


Mould growth at lumber surfaces of pine after kiln and air drying
1994 - IRG/WP 94-40033
Distribution of water soluble substances in green wood and later redistribution during drying is of importance for the colonisation of wood by microorganisms. According to literature the availability of nitrogenous materials is probably a major limiting factor to the microbial colonisation of wood. King et al. (1974) and Oxley et al. (1976) have shown correlation between surface nutrient concentra...
N Terziev, J Bjurman, J B Boutelje


New principles for the protection of wood: Impregnation with waterborne resins
1995 - IRG/WP 95-40047
The environmental impact of classical wood preservatives as well as the use of tropical wood species with high natural durability is regarded increasingly critically in the public. Therefore other partially new principles for the protection of wood, like chemical modification, or treatment with resins were examined especially in USA, Japan and in Europe with promising results predominantly in the ...
A O Rapp, R-D Peek


Dura-Treet II, a water dispersible pentachlorophenol
1980 - IRG/WP 3165
During the past several decades, penta petroleum wood treating has become increasingly popular. Penta is an effective chemical compound against wood organisms causing decay and rot, is safe to handle, also clean and easy to use. In terms of preservative cost, it has been and remains by far the least expensive of the three major preservatives. However, when the cost of petroleum carrier is added, t...
D B Hatcher


The effect of a chelator mediated fenton system on activation of TMP fibres and decolorization of synthesized dyes
2004 - IRG/WP 04-50223
The purpose of this work is to improve our current knowledge of the non-enzymatic mechanisms involved in the brown rot degradation of wood, but also to study the potential applications of a chelator-mediated Fenton system in activation of wood fibers and decolorization of synthesized dyes. In this work, Electron Spin Resonance (ESR) spin-trapping techniques were used to study the generation of hyd...
Yuhui Qian, B Goodell, J Jellison


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


New ways of chemical wood preservation
1997 - IRG/WP 97-40087
Synergistic effects pertaining to wood preservation have been investigated by combining different polymerizing agents with modifying chemicals, modifying chemicals with known preservatives and new types of preservative chemicals with each other. One of the investigated methods is the use of impregnating solutions based on furfuryl alcohol (produced from biomass), in which the chemicals polymerizes...
M Westin, T Nilsson, B Ohlsson, R Simonson


Penetration as Key Factor for Determining the Performance of Wood Preservatives
2004 - IRG/WP 04-20293
Stakes of Scots pine sapwood with a dimension of 4 x 4 x 75 cm³ were impregnated with preservatives containing 2 % of propiconazole which had passed the EN 113 test criteria without any problems. The penetration of the colourless preservative was determined successfully by a fungal screening test described by Sutter (1978). The test revealed the insufficient penetration behaviour within the gi...
H Leithoff, I Stephan, R-D Peek


Effect of a water repellent additive on the performance of ACQ treated decks
2000 - IRG/WP 00-40168
The performance of a water repellent (WR) additive formulated for use with ACQ has been evaluated. The water repellency of wood treated with this formulation was studied in laboratory and field tests. The change in moisture content of ACQ/WR treated boards under field exposure conditions is compared with that of CCA/WR treated boards. Although the water repellency of the ACQ/WR system is lower tha...
F Cui, A R Zahora


Variations in the virulence of test strains of Coniophora puteana (Schum ex Fr) Karst
1982 - IRG/WP 2185
In laboratory experiments using petri-dishes and small wood blocks (30 x 10 x 5 mm³) 6 different isolates of Coniophora puteana strain BAM 15 were compared with strain FPRL 11E for growth rate and decay capability. Only the recently received strain from EMPA was suitably active giving 24% weight loss after 6 weeks compared with 38.1% for 11E. Collation of data from standard test records revealed ...
A F Bravery, J K Carey, W Worley


Mobility of zinc borate wood composite preservative
1997 - IRG/WP 97-30153
Zinc borate (ZB) is being used as an antifungal and insecticidal wood preservative for flake/strand-based composites. Data is reported on the laboratory and field leaching behavior of ZB when contained in apen flake composites. In general, the performance results correlate with leaching hazard. Although the boron in ZB is more resistant to depletion than in sodium borates, the ZB boron will deplet...
P E Laks, M J Manning


In-house accelerated method for testing decay resistance of treated wood
2004 - IRG/WP 04-20286
Fungicidal compounds often change their effectiveness when they are incorporated into candidate formulations. For this reason fungistatic effectiveness needs to be re-evaluated as many times as the formula has been modified for better performance. To avoid multiple expenses, in-house fungistatic tests are essential. Our goal was to develop in-house usable, simple but reliable and reproductive proc...
N Vidovic


Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica. In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut


Effectiveness of wood preservatives by IUFRO's method
1984 - IRG/WP 3305
Pinus elliottii and Eucalyptus saligna stakes treated with 4.9; 6.9; 9.6 and 13.5 kg/m³ of CCA-A, CCA-C and CCB and with 30-50; 60-80; 90-110 and 120-140 kg/m³ of Benzotar and CNSL (cashew-nut shell liquid) were exposed in seven test sites in Sao Paulo State, Brazil. After 4 years it was concluded that the mean useful life of untreated Pinus elliottii stakes was 8 months and of untreated Eucalyp...
G A C Lopez, E S Lepage, O B Neto