A preliminary note on the role of moisture absorption rate in durability assessment
2008 - IRG/WP 08-20383
The rate of moisture uptake was studied in 15 wood species using vermiculite at varying moisture levels as the exposure medium. As might be expected, moisture uptake varied widely among the species studied. While some of the more durable wood species were also resistant to moisture uptake, this was not always true. The results are discussed in relation to performance in under varying environmenta...
J J Morrell, L P Francis


Material properties of acetylated beech plywood
2008 - IRG/WP 08-40425
The effect of acetylation process on dimensional stability and mechanical properties of plywood made by Oriental beech layers (Fagus orientalis Lipsky) were studied. The layers cut into sizes of 200×200×2 mm and acetylated in 120°C for 30 and 60 min. Thickness swelling (TS%), water absorption (WA%) and anti-swelling¬ efficiency (ASE%) of specimens were measured. Mechanical properties (MOE, MO...
A Talaei


Fungal decay resistance and durability of wood products made from borax-impregnated wood and bonded with corn starch and tannin adhesive
2009 - IRG/WP 09-30494
At present, the production of wood composites mainly relies on the petrochemical-based and formaldehyde-based adhesives such as phenol formaldehyde (PF) resins and urea formaldehyde (UF) resins, which are non-renewable and therefore ultimately limited in supply. This paper concerns the decay resistance of wood products bonded with a new, environment-friendly adhesive derived from abundant and rene...
A Moubarik, A Pizzi, A Allal, F Charrier, B Charrier


Laboratory and above ground exposure efficacy of silicon-boron treatments
2009 - IRG/WP 09-30510
The study deals with silicon compounds, namely tetraethoxysilane (TEOS), phenyltriethoxysilane (PhTES) and methyltriethoxysilane (MTES) at concentrations of 23, 16 and 10% in combination with 1.2-1.5% boric acid. The aim with the study was to combine the chemical approach with the necessary biological tests of the impregnated wood. The tested silicon-boron combinations ensured mass loss less than ...
N Terziev, D Panov, A Temiz, S Palanti, E Feci, G Daniel


Decay Resistance of Maple (Acer Insigne) Wood Against White Rot
2010 - IRG/WP 10-10740
In this study, the decay resistance of maple (Acer insigne) in natural state and treated with ACC (Acid copper chromate) was investigated against the white rot fungus (Coriolus versicolor). ACC is a kind of water borne preservatives that was used in this study for treating specimens under vacuum and pressure (Bethell procedure) with 3 percent concentration. In conducting mentioned evaluation, koll...
V Tazakor Rezaei


Service life prediction of wooden components – Part 2: Impact of material, exposure and design details
2010 - IRG/WP 10-20440
Dose-response functions permit to estimate the moisture and temperature induced decay potential for any wooden building component and exposure, and thus the service life to be expected. In part 1 of this series dose-response functions were established as a result of double layer field trials carried out at 24 European test sites over up to eight years. Using them makes it no longer necessary to co...
C Brischke, B Lauenstein, M Bilstein, T Bornemann, A O Rapp


Impact of climate change on wood deterioration - Challenges and solutions for cultural heritage
2010 - IRG/WP 10-20441
Deterioration of wood in cultural assets follows the same physiological mechanisms as in modern structures. Therefore rules and data for prediction of service life derived from old wooden structures can be used to model the service life of recent wooden structures and vice versa. The latter is done in this paper: From experimental test set ups in the field spread over Europe, climatic data, wood t...
C Brischke, A O Rapp, M Hasan, R Despot


The Effects of Some Fire Retardant Chemicals on the Decay Resistance of Medium Density Fiberboard (MDF)
2010 - IRG/WP 10-30536
The objective of this study was to determine the decay resistance of Medium Density Fiberboard (MDF) treated with 5% and 10% concentration of various fire retardant (FR) chemicals. Experimental panels were produced using by melamine-urea-formaldehyde (MUF) resins having 10%, 15% and 20% of melamine content. MDF specimens were subjected to decay resistance test performed according to modified EN 11...
D Ustaömer, M Usta, Ü C Yildiz, S Yildiz, E D Tomak


Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5 years’ exposure ( IRG/WP 97-30139), and showed that the resistance of acetylated wood wit...
P Larsson Brelid, M Westin


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Decay resistance of a commercial pistachio twig-plastic composite
2011 - IRG/WP 11-40553
In this research, the decay resistance of commercial extruded pistachio twig flour-plastic composite was investigated against the white-rot fungi Trametes versicolor and the brown-rot fungus Coniophora puteana. The composite specimens containing 60% pistachio twig flour were exposed to a decay test according to modified ASTM standard for 3 months. The results showed that the composite could be d...
M R M Farahani, M Safarzadeh


Effect of Nano-silver Treatment on Densified Poplar Wood Properties. Part Two: Spring Back, Compression set, Impact Load Resistance and Hardness
2011 - IRG/WP 11-40568
This paper is the second part of the study of applying nano-silver treatment before densification of poplar wood (Popolus alba). The specimens were prepared in four groups of: 1) nano-silver impregnated 2) water impregnated 3) dried with no impregnation and 4) the control specimens. The impregnation process was done by empty cell process. Then, the groups of 1 to 3 were compressed in a hot press a...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khajeh


Coconut lumber for wood decks (Cocos nucifera L.): decay resistance against Basidiomycetes fungi
2012 - IRG/WP 12-10784
Since a couple of years, manufactured products of coconut wood for outdoor uses like wood decks have been proposed on the European market. These are presented as an alternative for traditional tropical timbers. In the past, coconut wood was neglected and burned for sanitary reasons and lack of interest at industrial scale. Plantation coconut trees at end of production of copra constitute a renewab...
B Jourez, C Verheyen, J Van Acker


Durability of timber products – Part 2: Proposal for an IRGWP - Durability Database
2012 - IRG/WP 12-20497
A proposal for a web-based platform for scientific exchange of test data in the field of wood durability and wood protection has been made. The overall aim of the durability data base is to improve the usability of existing test data and to create an added value for durability research and service life prediction. The database allows for test results from standardized and non-standardized laborat...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis


Durability of timber products –Part 1: Inventory and evaluation of above ground data
2012 - IRG/WP12-20498
The material-inherent resistance of wood is one of the most important qualities influencing the durability of timber. Hence, it has also a major effect on the service life to be expected from a timber construction. In addition, design details and the respective climatic conditions determine durability and make it impossible to treat wood durability as an absolute value. Moreover, the reference mag...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis, P O Flæte, P Larsson Brelid


Biological performance of wood- and bamboo-polypropylene composites: Effects of particle content, particle size and Zn borate
2012 - IRG/WP 12-40577
Particle content and size of wood material in wood plastic composites (WPCs) can affect efficacy of WPCs against fungi and termites. This study evaluated fungal and termite resistance of WPCs manufactured by using two different levels of particle content (50 and 70%) and three different particle sizes (30, 60, and 100 mesh). In fungal resistance tests, Tyromyces palustris, a standardized test fung...
S N Kartal, S Aysal, E Terzi, T Yoshimura, K Tsunoda


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


Classifying white rot decay resistance of some hardwoods from Sarawak and Peninsular Malaysia and correlations with their tropical in-ground durability
2012 - IRG/WP 12-10788
White rot wood decay under Malaysian (humid tropical) terrestrial conditions pose more serious threats to the in-ground service life of hardwoods than other common fungal decay types. A study is made on decay resistance variation for a total combined list of 30 Peninsular Malaysian and Sarawak timber species (plus 6 exotic reference temperate commercial woods for comparison) using the laboratory s...
A H H Wong, J M E Jem, Lai Jiew Kok


Resistance of WPC against wood destroying fungi
2013 - IRG/WP 13-40627
The investigation of biological durability is a fundamental topic to assess the performance of Wood Plastic Composites (WPC) particularly for outdoor applications. In the last years, different test setups based on existing standards on the field of wood as well as the field of plastics were used for WPC. But the test methodologies give different information about the durability of the tested mater...
A Gellerich, S Bollmus, A Krause


Variability in durability of some selected South-American wood species
2014 - IRG/WP 14-10831
Within the scope of sustainable forest management one wants to encourage the proper use of lesser known wood species. Therefore the market has to shift from a demand-driven towards a supply-driven market without loss of wood quality. It is generally known that the durability from pith to bark varies thus, affecting the overall durability of wood species. Consequently, a detailed analysis is necess...
I De Windt, P ’t Hooft, J Van den Bulcke, J Van Acker


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of wood. The moisture performance of wood and wood-based products has been recognized as key...
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


The Physical Properties of Heat Treated Fir Wood and Outdoor Durability
2014 - IRG/WP 14-40677
Wood might be easily susceptible to degrade by biotic and abiotic factors. Therefore, wood should be protected from fungi, insects and other degradation factors by applying treatment methods. Especially, for the wood have used in the external environment. Chemical treatment methods have some disadvantages such as use of toxic chemicals (Arsenic and chromium) and treatability of refractory wood spe...
O E Özkan, H Vurdu, A Temiz, G Köse