IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 859 documents. Displaying 25 entries per page.


Durability classification of preservative treated and modified wood
2019 - IRG/WP 19-20659
EN 350 (2016) allows formally to determine durability classes (DC) for wood products and wood-based materials, which was previously only possible for untreated wood in the form of natural durability. In a first study, the University of Goettingen carried out the durability classification of chemically modified (modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea, DMDHEU) and preservative-treate...
S Bollmus, L Bachle, C Brischke, H Militz


Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori


Economic and Alternative Preservative Research with an Overview of its Impact on the Dynamics of Wood Tie Markets and Railroads
2019 - IRG/WP 19-30751
This presentation will discuss the Railway Tie Association’s (RTA) efforts in economic research for the North American wood tie industry, along with decades-long research into improving wood preservation processes and its resulting economic impact for railroads. Ongoing research is continuing to expand the knowledge-base by comparing existing standard creosote (C) and borate-creosote (B-C) dual...
J C Gauntt


Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama


The impact of additional interior layers to the moisture dry-out and mould growth risk of CLT walls
2019 - IRG/WP 19-40876
The objective of this study was intended to determine the maximum allowable initial moisture content for CLT walls having both exterior and interior thermal insulation. A laboratory test was conducted, for which four test walls with two different insulation solutions and two different initial moisture contents were built. Based on the test results a simulation model was configured and simulations ...
V Kukk, J Kers, T Kalamees


Wood veneer with high flexible decorated with nanoparticles for highly efficient water treatment
2019 - IRG/WP 19-50347
Natural wood is mainly comprised of numerous long, partially aligned channels (lumens) as well as nanochannels. Wood with these quick and effective passages is suitable for a membrane/separation material. However, a suitable thickness range of wood along its growth direction is essential to effectively separate small molecular, and the wood membrane is too thick to clean easily. In this paper, woo...
S Chang, D Xu, G Liu, J Hu, X Li, Y Liu


Knowledge exchange and transfer from academia to industry in the field of wood protection research – Activities of the IRG-WP Communications Committee
2019 - IRG/WP 19-50354
The International Research Group on Wood Protection (IRG) was founded in 1969 as a structured group of like-minded scientists and technologists focused on generating knowledge of the science of wood deterioration, and novel solutions to provide sustainably and environmentally responsible products for the protection of wood-based materials. The primary function of the IRG is to provide opportunitie...
F Latorre, B Abbott, C Brischke, M Humar, D Jones, E Larnoy, L Nunes, A Preston, T Singh


Performance of bio-based building materials – durability and moisture dynamics
2020 - IRG/WP 20-20666
When exposed to conditions favourable for decay, bio-based building materials can be susceptible to degradation. Their ability to withstand deterioration over time (performance) depends on the intrinsic or enhanced durability of the material as well as its wetting and drying behaviour. The effect of fungicidal components in wood is known since long. Other material characteristics, such as the mate...
L De Ligne, J Caes, S Omar, J Van den Bulcke, J M Baetens, B De Baets, J Van Acker


Future development of durability assessment of wood, according to typical usage of preservative-treated wood and naturally durable wood in Japan
2020 - IRG/WP 20-20675
A market of preserved wood products in Japan has two unique histories. First is the market shift to residential ground sills from utility poles and sleepers; the other is the stop of CCA treatment caused by the new effluent standard. In 2018, around 85% of preserved wood products used for residential ground sills were treated with non-CCA such as Cu-based agents. Since the market of treated wood h...
T Osawa, W Ohmura, H Kurisaki


Performance of resin-treated solid wood and laminated veneer lumber (LVL) under marine conditions
2021 - IRG/WP 21-10973
Wood is a traditional building material in the marine environment, where it is exposed to extremely harsh conditions. Most of the indigenous softwood and hardwood species in Europe are not durable against attack by marine organisms. Recently, wood modification has been considered as an alternative to protect non-durable wood species under use class (UC) 5 (EN 335, 2013) conditions. The present stu...
L Emmerich, C Brischke, S Bicke, H Militz


Experience Experience from over 20 years of field trials of resin treated wood – Marine borer resistance of MMF and DMDHEU modified wood
2021 - IRG/WP 21-10976
In 1999 a field test of Scots pine treated with MMF (Methylated Melamine Formaldehyde) resin and acetylated Scots pine post treated with MMF resin was started. Six years later a commissioned full NWPC test for BASF of Belmadur® (DMDHEU resin treated wood) was started at the same site. The testing, according to European Standard EN 275, was done in a bay by Kristineberg Marine Research Station o...
M Westin, P Larsson Brelid, A O Rapp, J Habicht


Development of Wooden Fireproof Structures for Mid- and High-rise Buildings in Japan
2021 - IRG/WP 21-30757
When constructing a mid-to-high-rise building more than 4 stories in general in Japan, it is necessary to have a fireproof structure stipulated by the Building Standard Law. The performance required as a fireproof structure in Japan is generally stricter than in other countries, and it is required to be structurally sound after a fire even without fire extinguishing activities. In order to satisfy...
D Kamikawa, M Harada, H Matsunaga, R Takase, N Hattori, Keisuke Ando, M Miyabayashi


Mechanical and biological durability properties against soft-rot and subterranean termite in the field (grave-yard test) of beech wood impregnated with different derivatives of glycerol or polyglycerol and maleic anhydride followed by thermal modification in an opened or in a closed system
2021 - IRG/WP 21-40917
This paper presents mechanical and biological durability properties in soil beg test (soft-rot test) and field test (grave-yard test) against subterranean termite of the wood modified with an aqueous vinylic derivative of glycerol/polyglycerol or maleic anhydride cured in an opened or in a closed system. Wood modification was performed through impregnation of European beech (Fagus sylvatica) with ...
M Mubarok, H Militz, S Dumarcay, I W Darmawan, Y S Hadi, P Gerardin


Evaluation of decay and energy properties from thermally modified biomasses during fungal deterioration by NIR-spectrometry
2021 - IRG/WP 21-40922
This study is focused on the prediction of fungal weight loss (WL) and high heating value (HHV) from raw and torrefied waste lignocellulosic feedstocks, according to their exposure duration to wood-destroying fungi, using near infrared spectroscopy (NIR) and chemometrics models. Sugarcane bagasse, coffee husk, eucalyptus and pine shavings were torrefied at 290 °C in a screw reactor, during 5, 7...
B de Freitas Homem de Faria, P Santana Barbosa, J Valente Roque, A de Cassia Oliveira Carneiro, P Rousset, K Candelier, R F Teofilo


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Introduction to the project ‘Deterioration and decay of wooden cultural heritage in Arctic and Alpine environments’ (ArcticAlpineDecay)
2022 - IRG/WP 22-10997
The Arctic is already affected by climate change, and this is expected to accelerate over the coming decades. Alpine regions in Norway are projected to face similar challenges. Current knowledge on Norwegian wooden cultural heritage in Arctic and Alpine regions is scattered and contains significant knowledge gaps. Historically, - scientists, sectorial governance, tourist trade and commerce have ma...
G Alfredsen, L Ross, A W Hegnes, M S Austigard, J Mattsson, N B Pedersen, A Sinitsyn, V V Martens, A-C Flyen


Evaluation of Decay Resistance of Copper-based Preservatives Treated-Wood exposed to different field test sites in Korea
2022 - IRG/WP 22-20679
In Korea, preservative treated wood is required to have a stamp on the surface which contains information such as wood species, use categories, and the company that treated the wood. Such stamping is necessary to safely and appropriately use the treated wood. Since majority of treated wood is being used outdoor environment, the treated wood must have efficacy against wood decay fungi or termite. I...
W-J Hwang, S-M Yoon, Y Park, Y-S Choi, H-M Lee, J-W Kim


Combining MRI and X-ray CT to monitor fungal decay of plywood and OSB in a lab test
2022 - IRG/WP 22-20683
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, T Núñez Guitar, C Vanhove, J Van Acker, J Van den Bulcke


Copper-octanoate - a potential reference preservative replacement for CCA in field test standards?
2022 - IRG/WP 22-20688
Finding a CCA reference replacement for use in standardised test methods is of high priority since this chemical is being phased out and may in the near future be banned also for experimental and approval purposes. In this paper we assess the possibility to replace CCA reference preservative with an historical copper octanoate product. There is a huge amount of lab and field test data available fo...
R Ringman, M Westin, M Klamer, A Christof, F Friese


Post-layup protection of mass timber elements in above ground protected exposures: 2-year results
2022 - IRG/WP 22-30766
Mass timber has seen increased use as a building material for low and mid-rise construction in recent decades. The durability of mass timber elements has not been fully examined and the effects of wood destroying organisms on this these materials merits attention. The effectiveness of currently labeled soil termiticides and passively applied biocides at post-construction or as remedial agents need...
M E Mankowski, T G Shelton, G T Kirker, J J Morrell


Impact of wetting agents on polyelectrolyte complex impregnation for wood fire-retardancy
2022 - IRG/WP 22-30768
Wood fire performance is a great concern in interior finishing due to the high risk of flame spread. To increase the use of wood in high building while ensuring the safety of building occupants, fire retardant (FR) treatments are required. Traditionally, two fireproofing strategies are employed: impregnation and coatings. They have been widely studied but they, respectively, are time and chemicals...
M Soula, J B Grenier, S Duquesne, F Samyn, V Landry


Copper Naphthenate – A Data and Capability Update
2022 - IRG/WP 22-30771
The efficacy of copper naphthenate against wood decay fungi and wood destroying organisms has been well documented from international field tests as well as decades of commercial service. The use of copper naphthenate has been dramatically expanded due to its proven performance, non-restricted use, minimal environmental impact, and superior end of life options. Extensive demand and interest has al...
J-W Kim, J D Lloyd


Field tests of different tropical wood species in sea water
2022 - IRG/WP 22-30773
A number of tropical timbers have been tested according to EN 275 at Kristineberg Marine Research Station in Sweden since 1999. Most of these tests have started during the last 5-8 years. Wood species included have been Lophira alata (Azobé/Ekki), Minquartia guianensis (Manwood/Acaria), Chlorocardium rodiei (Greenheart), Cyclodiscus gabonensis (Okan/Denya), Shorea spp. (Bankirai), Dicorynia guia...
M Westin, P Larsson Brelid


Steam Pre-conditioning Treatment Prior to Acetylation: Impact on Dimensional Stability, Moisture Response Behaviour, and White-Rot Fungal Resistance of Hevea brasiliensis and Mitragyna ciliata Wood
2022 - IRG/WP 22-40930
The effect of steam pre-conditioning treatment on the dimensional stability, moisture response behaviour, and durability against white-rot fungus P. chrysosporium of acetylated Hevea brasiliensis and Mitragyna ciliata wood species were assessed. Defect-free specimens of both species from the top, middle, and base positions were selected, prepared according to ASTM D143-09 & ASTM D-2017 standards a...
E Uchechukwu Opara, J Mayowa Owoyemi, J Adeola Fuwape


Effect of nano-particle characteristics and concentration on UV protection of timber: A field exposure test
2022 - IRG/WP 22-40941
Wood has a well-known susceptibility to ultra-violet light degradation, leading to premature replacement. A variety of products have been developed to protect against this damage, but most provide less than 12 months of protection and must be regularly reapplied. Developing improved coatings would help reduce wood losses and reduce maintenance costs. Nano-particles have a variety of attractive pro...
T Yi, J J Morrell


Previous Page | Next Page