Variation in moisture content in field trials according to use class 3.2 conditions
2016 - IRG/WP 16-20580
Different test methods to determine the durability of wood in use class 3 (EN 335:2013) are available. Fungal degradation of wood requires liquid water. Different Standards (EN 335-1:2006; DIN 68 800:2011) specify the risk for decay with moisture content (mc) of above 20%. EN 335 (2013) does not specify moisture content but rather defined limited wetting conditions (use class 3.1) or prolonged wet...
S Bollmus, A Gellerich, H Militz


Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


Durability of a willow/plastic composite mat
2016 - IRG/WP 16-20592
Developing uses for wood wastes could enhance utilization of low value renewable materials while creating opportunities for rural development. Small diameter willow stems have little use in China, but they could be combined with high density polyethylene to create wood plastic composite mats for decorative applications. These mats could be used in exterior, above ground exposures, but would still ...
Li Yan, Haiyan Duan, Beizhan Quan, J Cappellazzi, J J Morrell


Distribution and penetration of the tung oil in wood studied by high-resolution magnetic resonance imaging
2016 - IRG/WP 16-20593
Water repellents as environment-friendly treatments are gaining their popularity as non-biocidal solutions for wood protection. One of the most important water repellents for wood besides waxes and organosilicon compounds are drying oils. Tung oil is one of the best performing oil. However, tung oil, similarly as other oils, does not penetrate deeply into wood, due to its high viscosity. In order...
M Žlahtič, U Mikac, I Serša, M Merela, M Humar


Evaluation of field test data
2016 - IRG/WP 16-20594
The resistance against fungal decay and insect attack of wood can be highly variable, between boards and even within boards. The variability in durability is not always an issue, but for high demanding applications information about its reliability is required. This comprises the variability of outdoor performance. Durability testing in laboratory and outdoor exposures can provide a good basis to ...
F Bongers, C Brischke, J Van den Bulcke, W Gard, I De Windt, H Militz


Anti-Fungal Activity on Some Wood extracts as a Wood Protectant
2016 - IRG/WP 16-30684
In this study, six different wood barks were used, where obtained bark extracts were blended with potato-agar in order to investigate their antifungal properties. To determine the inhibition effectiveness of extractives, two different fungi; Coniophera puteana and Trametes versicolor were selected. Fungal activity was carefully observed for the duration of seven days. Following biological testing,...
Ö Özgenç, S Durmaz


Screening of fastener resistance in contact with untreated wood using different test designs
2016 - IRG/WP 16-30686
The performance of fasteners in wooden constructions is an important aspect especially regarding corrosion resistance. In an early stage corrosion of fasteners in untreated timber becomes often visible as a discoloration on the surface of the timber resulting in bad appearance of the product followed by complaints. In order to develop an accelerated test for the assessment of fastener performance ...
E Melcher, S Wolf, U Cera


Laboratory and Field evaluation on Resistance of Thiacloprid-treated Pine Species to Termites in Mexico
2016 - IRG/WP 16-30687
The usage of Neonicotinoids for wood preservatives is common practice in several countries. Especially the active ingredient Imidacloprid is well established for this application due to its high efficacy against termites. (2Z)-3-(6-chloro-3-pyridylmethyl)-1,3-thiazolidin-2-ylidene-cyanamide, also known as Thiacloprid showed a good efficacy against Reticulitermes santonensis De Feytaud in efficacy ...
P Meckler, T Jaetsch, I Rodriguez


Resistance of heat treated Ash wood under steam pressure: rot fungi, soil micro-organisms and termites
2016 - IRG/WP 16-40724
Thermal modification processes have been developed to increase the biological durability and dimensional stability of wood. The aim of this paper was to study the influence of ThermoWood® treatment intensity on wood decay resistance improvement against soil-inhabiting micro-organisms, brown/white rots and termite’s exposures. All of the tests were carried out in the laboratory with two differen...
K Candelier, S Hannouz, M-F Thévenon, D Guibal, P Gérardin, M Pétrissans, R Collet


Fabrication and characterization of MicroPCMs filled wood-plastic composites: Effects of polyethylene glycol on melamine–formaldehyde shell material
2016 - IRG/WP 16-40728
Microencapsulated phase change materials (MicroPCMs) containing dodecanol were fabricated using melamine-formaldehyde (MF) or polyethylene glycol 200 modified melamine-formaldehyde (PMF) resin as the shell materials by in situ polymerization. Wood flour/high-density polyethylene (WF/HDPE) composites with MF shell MicroPCMs (MF-MicroPCMs) or PMF shell MicroPCMs (PMF-MicroPCMs) were prepared, respec...
Xi Guo, Jinzhen Cao


The durability of natural and thermomodified black poplar wood and Scots pine sapwood after two years of external exposition
2016 - IRG/WP 16-40730
Natural biological durability of many European wood species is considered to be relatively small, particularly in a ground contact conditions. This is due to the exposure of the wood to the range of biological and atmospheric destructive factors. This may to limit the scope of application of the wood of these species, particularly in construction. The biocides are often used for wood protection in...
A Fojutowski, A Kropacz, A Noskowiak


Variation in coating hardness during the EN 927-6 weathering test: influence of pigmentation
2016 - IRG/WP 16-40739
The objective of the SERVOWOOD project is to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. Within this project an extensive round robin exercise has been carried out by five partners to establish the repeatability and reproducibility of the EN 927-6 artificial weathering test. This round robin included the exposure of the I...
L Podgorski, L Malassenet, C Reynaud


Durability of Thermally Modified Engineered Wood Products
2016 - IRG/WP 16-40745
In this study, rated plywood, oriented strand board (OSB), laminated strand lumber (LSL), and laminated veneer lumber (LVL) were thermally modified as a post-treatment at 140 °C, 150 °C, 160 °C, 170 °C, and 180 °C using a closed, pressurized treatment method. Eastern larch OSB manufactured from heartwood and sapwood was also thermally modified as a post-treatment at 160 °C and 180°C. All ...
H M Barnes, M D Aro, A Rowlen


The impact of catalyst on the properties of furfurylated beech wood
2016 - IRG/WP 16-40748
European beech (Fagus sylvatica L.) is a major tree species of European forest that is underexploited because of its low dimensional stability and durability. Similarly to what has been developed with radiata pine, furfurylation might be the answer to optimize the utilization of local beech wood. Beech wood furfurylation process was studied using five different catalysts: maleic anhydride, maleic ...
P S Sejati, A Imbert, C Gérardin, S Dumarçay, E Fredon, E Masson, D Nandika, T Priadi, P Gérardin


The influence of log soaking temperature and thermal modification on the properties of birch veneers
2016 - IRG/WP 16-40749
In veneer manufacture the logs are routinely soaked in heated water baths in order to soften the wood prior to peeling. The temperature of the water may vary greatly between batches; however, the influence of log soaking temperature on veneer properties has had little research attention. Uncontrolled moisture is known to cause problems in wood-based materials, while thermal modification offers a m...
S Källbom, K Laine, M S Moghaddam, A Rohumaa, K Segerholm, M Wålinder


Fungal resistance and accelerated weathering of Wood-Plastic composites reinforced with Maritime pine wood flour
2016 - IRG/WP 16-40750
This study evaluates the durability of wood-polymer composites (WPCs) elaborated for use in cladding application from recycled polypropylene (rPP) and wood flour. Local Maritime pine wood flour derived from regional sawmills was used in the study to reduce the environmental impact associated with transport. Different wood-plastic ratios with and without UV stabilizers and biocide were tested. One ...
M Jebrane, T Fournier, N-E El Bounia, F Charrier-El Bouhtoury


Encapsulation of poles to prevent moisture uptake – a laboratory test
2016 - IRG/WP 16-40753
Premature failure of utility poles due to decay in soil contact is the main reason for early removal of utility poles, a measure that implies extra costs for utilities. Remedial treatments and barriers are common methods to prolong the service life of utility poles. The first part of this paper gives an overview of mode of action and commercial application of barrier systems as described in the li...
K-C Mahnert, U Hundhausen


Marine Borer Resistance of Acetylated and Furfurylated Wood – Results from up to 16 years of Field Exposure
2016 - IRG/WP 16-40756
Furfurylated and acetylated Scots pine sapwood has been tested since 1999 in a marine field with high marine borer activity. In 2004, two test groups with acetylated southern yellow pine (product later known as Perennial Wood™) were put out and over the whole test period differently furfurylated wood (later marketed as Kebony®) test groups have been started. Furthermore, some combinations of mo...
M Westin, P Larsson Brelid, T Nilsson, A O Rapp, J P Dickerson, S Lande, S Cragg


The Environmental Impact of Timber Products Compared to other Building Materials - A Survey of Published Environmental Product Declarations
2016 - IRG/WP 16-50314
One of the positive aspects of using wood in construction is the environmental benefits that this can potentially bring. However, manufacturers of all construction products and materials make claims about the ‘environmental friendliness’ of their products, making it exceedingly difficult for the end user to make informed choices about the advisability of using one product over another. This st...
C Hill, J Dibdiakova


Estimation of wood degradation determined by visual inspection, mechanical testing and DNA characterisation – report after 3 years of exposure
2016 - IRG/WP 16-30700
The influence of two separate treatments, thermal modification and alkaline copper quaternary (ACQ, Silvanolin©) treatment, on fungal decay, visual disfigurement, deterioration in mechanical properties and fungal community structure was assessed on Norway spruce (Picea abies) and compared with the performance of two naturally more resistant tree species native to North America: Douglas fir (Pseud...
N Thaler, T Martinović, M Bajc, D Finžgar, H Kraigher, A Sinha, J J Morrell, M Humar


Development of Wood Modification – High melting point wax and hot oil treatments
2016 - IRG/WP 16-40768
This study covers an introduction to the projects where new facilities were created for developing wood modification. In this new research environment it is possible to treat wood with versatile equipment. First modifications with this equipment are going to be done in high temperature and pressure using high melting point waxes and hot oils. Earlier studies, tests and commercial products show...
H Turunen, L Linkosalmi, J Peura, O Paajanen


10 year Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2017 - IRG/WP 17-30718
A round robin involving 15 European participants was set up in 2006. The round robin consisted of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. The laboratory test results were reported in an earlier IRG paper (IRG/WP13-20535) but are included also in this paper in order to facilitate the comparison with the field test...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, E Melcher, R Moeller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Durability Testing of a Cattail (Typha spp.) based Insulation Material against Termite Attack
2017 - IRG/WP 17-10879
The use of insulating materials is particularly important in the construction industries, especially with regard to the use of wood and naturally occurring substances. The use and durability of natural materials as insulating materials is of keen interest to many construction experts, and continues to be a topic of intense investigation. It is generally agreed that the use of natural substances ...
M Dass, W Unger, T L Woods


Assessing the natural durability for different tropical timber species using the mini-block test
2017 - IRG/WP 17-10886
The Xylarium in the Royal Museum for Central Africa (RMCA, Tervuren, Belgium) contains over 60,000 wood-samples, comprising over 12,000 species. These samples are of great historical and scientific value yet have a random format, which complicates standard testing. The wood-durability against Coniophora puteana and Trametes versicolor was tested for 36 species. Due to the random sample sizes the s...
V Deklerck, I De Windt, N Defoirdt, J Van den Bulcke, H Beeckman, E Espinoza, J Van Acker


Laboratory test to determine the effect on durability of combining biobased building materials with timber in construction
2017 - IRG/WP 17-20604
The use of Structural Insulated panels is a construction approach that is seeing more abundant use and is becoming a widely available method. Preformed units are usually a composite structure which often include a range of bio-based materials such as timber, wool or straw. Traditional laboratory based wood decay tests do not take into account this combination of biobased materials and it may be po...
S F Curling, G A Ormondroyd


Previous Page | Next Page