Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


Behaviour of some selective Indian species towards treatment with solvent based water repellent preservative
1984 - IRG/WP 3309
This paper discusses a solvent based preservative using PCP and a water repellent for preserving three species of timber commonly used in India for the manufacture of doors and windows. It examines the method of treatment to achieve desired levels of penetration and retention of the preservative-cum-water repellent, and tests made on these timbers to examine the success of the processing methods a...
V R Sonti, B Chatterjee


Reinfestation of consolidated ancient wood by insects
1998 - IRG/WP 98-10290
Wooden artifacts are often attacked by wood-destroying insects. Therefore conservators have to stabilize numerous objects from such attack. Initially we studied the resistance of painting materials and consolidants on unaffected recent wood against wood-destroying insects (IRG/WP 97-10239). Further, we wanted an answer to the question: Are artifacts, formerly destroyed by wood-borers, reinfested b...
W Unger, A Unger, U Schiessl


Effect of boron compounds-furfuryl alcohol treatment of wood on dimensional stability, termite resistance and boron leachability
2001 - IRG/WP 01-40195
Sapwood blocks of Japanese cedar (Cryptomeria japonica) and Caribbean pitch pine (Pinus caribaea) measuring 20 (tangential) x 20 (radial) x 10 (longitudinal) mm were impregnated with furfuryl alcohol (FFA) by a vacuum-diffusion process followed by curing under heating. Boron compounds (boric acid, ammonium borate and ammonium biborate) were mixed in the impregnation solution of FFA. Anti- swelling...
S K Ozaki, M K Yalinkilic, Y Imamura, M F Souza


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


Development of wood retification process at the industrial stage
1998 - IRG/WP 98-50101-16
Wood is a natural composite material which exhibits outstanding properties from the technical as well as from the ecological point of view. However, it is an anisotropic, hygroscopic material sensitive to biological attacks. We have to stabilise and preserve it if we want to ensure its market shares faced with competing synthetic material, whilst taking the new environmental rules into account. T...
P Gohar, R Guyonnet


Optimun storage period for the boron diffusion treatment of rubber wood
1996 - IRG/WP 96-30121
The study determined the maximum thickness of rubber wood that can be diffusion treated and the effect of diffusion storage period on the distribution of chemicals in treated wood of various thicknesses. Wood of thickness up to 50 mm can be easily diffusion treated with 10% boric acid equivalent (BAE) solution to adequate loading of chemicals. The optimum diffusion storage period to get uniform an...
T K Dhamodaran, R Gnanaharan


Kiln drying of poles as a means of solving the problems of pre-treatment decay in poles
1985 - IRG/WP 1263
The concept that pre-treatment decay can cause wide variation in the treatability of wood and especially wood poles has caused much discussion and debate in wood preservation circles. Yet it seem only logical that if decay has effected the strength characteristics of the wood and caused a differential moisture content in the wood the treatment of the end product will be highly variable and the lon...
J A Taylor


Effect of vapour boron treatment on mechanical properties of wood based board materials
1992 - IRG/WP 92-3727
The mechanical properties of Medium density fibre board, Chipboard and Oriented strand board were investigated after treatment to two retention levels of boric acid applied as a vapour phase system. A range of mechanical properties were investigated. The vapour boron treatment does not have any significant effect on most of the mechanical properties of the boards. The exception is a reduction in i...
R Hashim, D J Dickinson, R J Murphy, J Dinwoodie


Acceleration of boric acid uptake into the subterranean termite, Coptotermes formosanus Shiraki using steamed larch wood
2000 - IRG/WP 00-10353
Laboratory tests were done to measure the efficacy of addition of steamed larch (Larix leptolepis (Sieb. et Zucc.) Gord.) heartwood extracts for the uptake of boric acid against the termite, Coptotermes formosanus Shiraki. Paper discs were treated with the water-soluble fraction obtained from hot-water extracts of steamed larch wood (S-Water) with or without 0.01-2.0% boric acid, followed by expos...
W Ohmura, S Doi, S Ohara


A review of incising as a means of improving treatment of sawnwood
1994 - IRG/WP 94-40019
The use of incising, perforation of the wood surface, is increased because of the need to treat refractory wood species. This paper reviews the development of incising and shows how the required incising patterns can be determined and specified. Most of the development has been in the area of toothed-roller incisors because of their rapid throughput. Needle, Laser, drill and water jet incisors hav...
P I Morris, J J Morrell, J N R Ruddick


Treatment of refractory timbers
1993 - IRG/WP 93-40001
Worldover crisis of wood is being felt due to the global environmental problems. Wood preservation technology plays a good role in curtailing the demands of wood for replacement by prolonging the service life of the timber and thus indirectly helps in saving the environment. Some species of timbers which could not be treated to the desired level by virtue of their refractory nature by any of the c...
I Dev, S Kumar


Supercritical fluid treatment: Effects on bending strength of white spruce heartwood
1993 - IRG/WP 93-20008
The effects of supercritical carbon dioxide on wood strength were evaluated using white spruce heartwood, a species known to be especially susceptible to collapse during exposure to higher pressures. The effects of pressures of 2000 or 3600 psig and temperatures of 40 or 80°C were evaluated using 30 or 60 minute exposure periods. No significant differences were noted in modulus of rupture or modu...
S M Smith, J J Morrell, E Sahle-Demessie, K L Levien


On the resistance of consolidated ancient wood against Serpula lacrymans (Wulfen: Fr.) Schroeter
2000 - IRG/WP 00-10348
Structural timbers and other wood objects of cultural value in historical buildings and museums are often attacked by wood-destroying fungi. The aim of conservators is to preserve such damaged timbers and prevent further biodeterioration by impregnation with consolidants. There is little knowledge of the resistance of consolidated timber and art objects to a new attack by wood-destroying fungi. Br...
W Unger, A Unger, U Schiessl


Field testing of nootkatone and tetrahydronootkatone wood treatments against Coptotermes formosanus Shiraki
2003 - IRG/WP 03-30308
A component of Alaskan yellow cedar, citrus oil, and vetiver oil, nootkatone, and its derivative, tetrahydronootkatone, were tested for their potential as wood treatments against Coptotermes formosanus. Wood treatments dipped in 1% and 5% nootkatone and tetrahydronootkatone in ethanol or vacuum impregnated (5% only) were tested in a natural setting using termite infested bald cypress trees along t...
K E Nix, G Henderson, R Laine


Heat transfer and wood moisture effects in moderate temperature fixation of CCA treated wood
1994 - IRG/WP 94-40022
Practical aspects of heat transfer and fixation of wood exposed to drying conditions after CCA treatment are considered. The rates of heat transfer and CCA fixation are substantially influenced by the cooling effect of water evaporating from the wood surface when drying occurs during fixation. At least in the early stages of fixation, the wood temperature approaches the wet bulb temperature, rathe...
J Chen, M Kaldas, Y T Ung, P A Cooper


Fundamentals on steam fixation of chromated wood preservatives
1988 - IRG/WP 3483
Weathering of treated wood directly after impregnation leaches up to 2% of copper-chromate-containing wood preservatives. Almost total fixation of Cr+6 is achieved by steaming the treated wood at 100°C to 120°C, preferably 110°C. To initiate such spontaneous fixation 85°C to 90°C inside the wood are essential, which requires heating times ranging from 20 to 80 min, depending on timber species...
R-D Peek, H Willeitner


Modification of wood by graft treatment
2003 - IRG/WP 03-40257
New water-repellent systems for wood are needed to improve the weathering characteristics. This study found that treatment of wood with chemical grafting systems imparted substantial water repellency. Different direct oxidative grafting systems were examined. Specifically, KMnO4, Fe(NH4)(SO4)2·12H2O, Fe2(SO4)3·5H2O, and (NH4)2Ce(NO3)6 were used as initiators and styrene as the monomer. All the...
M M Morshed, D D Nicholas, C Pittman Jr, T Schultz


Need to develop processing technologies (for value addition) of the species evaluated for their properties and uses
2005 - IRG/WP 05-40307
The demand of timber in India for different industrial as well as domestic applications is ever increasing mostly due to urbanization and industrialization. This demand can only be met either from the imported timber or from the plantation resources outside the reserved and natural forests. There are a number of timber species grown under plantation forestry have their heartwood refractory to any ...
S R Shukla, S K Sharma, Y M Dubey, P Kumar, R V Rao, K S Shashidhar


Evaluation of outdoor weathering performance of modified wood
2004 - IRG/WP 04-20296
Interlace treated, oil treated, silicon treated as well as untreated Scots pine samples have been exposed outdoors. For evaluating the samples on their long term performance an internal standard had been developed. Parameters to be determined were the uptake of liquid water (submersion test), weight variation during exposure, crack performance, surface roughness and colour change. This paper disc...
Y Schulte, S Donath, A Krause, H Militz


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


An appraisal of the vertical distribution of attack of untreated and treated wood by warm water sphaeromatids at some tropical sites - A discussion paper
1986 - IRG/WP 4124
Examples of the vertical distribution of burrows of warm water sphaeromatids relative to tide levels and mud line from sites in India, Papua New Guinea and tropical Australia are discussed in detail. These data show clearly that these animals concentrate their attack of resistant natural wood or resistant treated wood in the tidal zone, particularly around Mean Sea Level. Supportive evidence from ...
J E Barnacle, L J Cookson, C N McEvoy


Preservative treatment of wood by diffusion processes - Simulation of commercial treatment processes
1988 - IRG/WP 3498
Spruce (Picea abies), Scots pine (Pinus sylvestris) and birch (Betula pendula) were preservative treated by diffusion with mixtures of copper sulphate and arsenic pentoxide. The preservative was fixed after a suitable diffusion storage period by soaking in ammonia solution. A high standard of treatment could be achieved in spruce sapwood. This was attributed to its low wood density, and high wood ...
P Vinden


Persistance of active ingredients in treated wood
1993 - IRG/WP 93-50001-20
Disposing of chemically protected waste wood implies the distinction between surface and pressure treatment. Considering that barked round-wood merely contains, after 7 months open storage, less than 30 g per ton of bark or 25 mg per ton of sapwood, depending on the type of insecticide, the bark or sapwood shavings may be incinerated normally, according to less severe legal prescriptions than for ...
E Graf, P Manser, S Rezzonico, B Zgraggen


Previous Page | Next Page