Increasing the hardness of wood-composite panels by nanosilver
2016 - IRG/WP 16-40715
Effect of silver nanoparticles on hardness in medium-density fiberboard (MDF) was studied here. A 400 ppm aqueous nanosilver suspension was used at three consumption levels of 100, 150, and 200 mL/kg, based on the dry weight of wood fibers; the results were then compared with the control panels. The size range of silver nanoparticles was 30-80 nm. Composite mats were hot-pressed for 6, 8, and 10 m...
H R Taghiyari, J Norton, K Heidarhaee


Investigation of enzymatic effect on pit membranes by light and scanning electron microscopy
2016 - IRG/WP 16-40721
Spruce wood, one of the refractory wood species has pit membranes, which has an influence on the permeability of wood providing liquid flow between the wood cells. However, these membranes tend to close under the fiber saturated point (FSD), which makes impregnation more difficult. In this study spruce sapwood samples were treated with two different commercial enzymes to improve the permeability o...
S Durmaz, Ü C Yildiz, M Öztürk, B Serdar


Resistance of heat treated Ash wood under steam pressure: rot fungi, soil micro-organisms and termites
2016 - IRG/WP 16-40724
Thermal modification processes have been developed to increase the biological durability and dimensional stability of wood. The aim of this paper was to study the influence of ThermoWood® treatment intensity on wood decay resistance improvement against soil-inhabiting micro-organisms, brown/white rots and termite’s exposures. All of the tests were carried out in the laboratory with two differen...
K Candelier, S Hannouz, M-F Thévenon, D Guibal, P Gérardin, M Pétrissans, R Collet


Modifying wood with paraffin wax emulsion impregnation and thermal modification: hydrophobization effect and mechanism of the combined treatment
2016 - IRG/WP 16-40726
The aim of this study was to enhance the water repellency of wood by a combined treatment of paraffin wax emulsion (PWE) impregnation and thermal modification. Two different treating procedures were used to modify the southern pine (pinus spp.). One is first PWE impregnation and then thermal modification, another is first thermal modification and then PWE impregnation. The treated samples were imm...
Wang Wang, Jinzhen Cao, Cong Chen


Combustion and thermal characteristics of Korean wood species
2016 - IRG/WP 16-40727
This study examined the combustion and thermal characteristics of domestic woods in Korea. Wood was confirmed by a cone calorimeter according to the KS F ISO 5660-1 standard. The combustion properties of the wood were measured in terms of the heat release rate (HRR), total heat released (THR), mass lose rate (MLR), and ignition time (time to ignition; TTI). Also, the thermal properties were measur...
Huyun Jeong Seo, Jung-eun Park, Dong Won Son, Won-Joung Hwang


Superhydrophobic treatment of Norway spruce wood for improvement of its resistance against brown rot and moulds
2016 - IRG/WP 16-40734
Water repellence of wood can be increased and its some other properties influenced by introduction of hydrophobic chemicals into and on cell walls without affecting the wood’s bulk density due to lumen filling. Herein, a simple dipping method to insert octadecyltrichlorosilane (OTS) into cell walls and to deposit the self-assembled hydrophobic monolayers (SAMs) of OTS is reported. It was found o...
A Kumar, P Ryparová, P Hajek, B Kričej, M Pavlič, A S Škapin, M Šernek, J Tywoniak, J Žigon, M Petrič


Formation of hydrophobic wood surface by means of thermal treatment and surface modification with alkyl ketene dimer (AKD)
2016 - IRG/WP 16-40738
One of the major shortcomings of wood-based materials compared to technical materials is attributed to their poor dimensional stability in changing climates and in contact with liquid water. Heat treatment induces chemical change with a consequent decreasing of reactivity of the material showing unwanted surface inactivation. Alkyl ketene dimer (AKD) is a widely used sizing agent in papermaking, w...
T Lovaglio, T Meints, L Todaro, W Gindl-Altmutter


Exterior birch plywood: potentiality of the thermo-hydro treatment
2016 - IRG/WP 16-40743
It has been found in the present study that, in laboratory fungi tests after leaching with water (EN 84), exterior birch (Betula spp.) plywood, as birch solid wood, is subjected to degradation by rot fungi. This limits the use of such plywood outdoors or in building structures in high humidity conditions. The possibility to improve the birch plywood fungal resistance was investigated in two ways: ...
B Andersons, I Andersone, A Meija-Feldmane, I Irbe, A Janberga, J Grinins


Development of a new method for wood hydrophobizing and fixation of copper compounds by chemical hardening of vegetable based modified oils
2016 - IRG/WP 16-40754
Wood products with ground and direct water contact, but without sufficient biological durability, have to be protected against biological degradation by fungi and other microorganisms. Due to European legislation (Biocidal Products Regulation 528/2012), the selection of possible chemical agents, which are still allowed to be used, is diminishing rapidly. The use of previously widely applied, very ...
C Swaboda, M Fischer, K Jacobs


Effect of insitu polymerization on practical properties of heat treated wood
2016 - IRG/WP 16-40763
This research was conducted to investigate the effect of combined modification; heat treatment and impregnation with styrene monomer on physical and mechanical properties of poplar wood (Populus deltoides). Test samples were grouped in six levels of control, wood polymer made from styrene, heat treatment at 170 ºC and 200ºC and combined modification; first hat treated at 170 ºC and 200ºC and t...
M Ghorbani, M Mohseni Shaktaei


Decontamination of sludges, liquids and soils polluted by “class 1, 2 & 3a” and “temporary” wood treatment products from dipping tanks
2016 - IRG/WP 16-50315
Wood is one of the most widely used building materials as it is easy to find and process. As an organic material, time leads to a degradation of its substance, and even more so when it is exposed to pathogens such as fungi, bacteria and insects. In order to try and inhibit this phenomenon, several preservation treatments have been developed and applied thanks to the production of chemical biocides...
A Zaremski, E Wozniak, S Maman, C Zaremski, S Morel


Influence of organosilicon compounds and nanocellulose treatment on dimensional stability of waterlogged elm wood
2017 - IRG/WP 17-10891
Commonly used agents for waterlogged wood consolidation (including the most popular polyethylene glycol) have proved ineffective and even dangerous to the preserved objects, jeopardising their integrity. Finding new, effective alternatives for safe preservation of wooden cultural heritage is therefore of key importance. The future conservation agents should, first and foremost, provide the integri...
M Broda, B Mazela, I Dąbek, A Dutkiewicz, H Maciejewski, R Markiewicz, M Grzeszkowiak, S Jurga


Novel wood treatments improve resistance to the wood-boring marine isopod Limnoria quadripunctata
2017 - IRG/WP 17-10899
The marine isopod Limnoria quadripunctata degrades wooden structures in the sea and causes significant economic damage. Broad-spectrum biocides and naturally resistant tropical hardwoods have failed to prevent feeding by Limnoria and have caused ecological damage. Wood modification is now the favoured method, and resin-based modifications have been effective, while the efficacy of silica-based mod...
H Bowen, M Montibus, M Kutnik, S M Cragg


Possibility of using lichen (Usnea filipendula) and mistletoe (Viscum album L.) extracts as potential natural wood preservative
2017 - IRG/WP 17-30712
Increasing environmental pressures on toxic chemical wood preservatives lead to the development of natural and environmentally friendly wood preservatives. In this study, using possibilities of lichen (Usnea filipendula) and leaves of mistletoe (Viscum album L.) as potential natural wood preservative were researched. Treatment solutions have been prepared with two different solvents, water and met...
Ü C Yildiz, C Kiliç, A Gürgen, S Yildiz


Weathering protection of European hardwoods through double modification
2017 - IRG/WP 17-30715
Beech and poplar were thermally modified, treated with melamine resin and both treatments were combined. The weathering performance (cracks and general appearance) of modified beech and poplar was assessed in natural weathering and correlated to material properties such as work in bending (WB) and Brinell hardness. In addition, the equilibrium moisture content after exposure of 12 months and subse...
G Behr, A Gellerich, S Bollmus, H Militz


Permeability of Eucalyptus wood improved by microwave treatment
2017 - IRG/WP 17-40773
The wood species with low permeability may cause many problems during timber manufacturing. Extreme difficulties take place in fabricating new wood-based composites by impregnating low- permeability timber with functional materials, such as flame retardant, preservatives and resins. Microwave (MW) treatment can increase the permeability of wood both in transverse and longitudinal directions. The e...
Xia He, Xianjun Li, Jie Xie, Xingyang Xiong


Treatability of beechwood railway sleepers with potential creosote substitutes
2017 - IRG/WP 17-40790
Maintenance of an efficient railway infrastructure still requires the use of wooden railway sleepers, particularly because wooden sleepers have more favourable properties for intensified vibrations than concrete or steel sleepers. Creosote, used for decades for the impregnation of railway sleepers, will possibly no longer be available for this application due to European legislation. This reveals ...
N Pfabigan, E Habla, R Gründlinger


Borate and Copper Naphthenate Dual Treatment of Bridge Timbers-Borate movement over time
2017 - IRG/WP 17-40795
Preservative treated wooden bridge ties in the South Eastern USA have a service life of about 15 to 20 years, which falls well below the average service life of 40 years of railroad cross ties (sleepers). It has been shown that cross tie life is significantly extended using borate dual treatment and this is now commercialized in bridge timbers using borate inserts. In previous research, it was dem...
J-W Kim, J D Lloyd


Dual Borate and Copper Naphthenate Treatment of Bridge Timbers:- Potential Performance Enhancements and Cost Savings
2017 - IRG/WP 17-40797
Dual treatment technology combining diffusible preservatives with oil borne preservatives, widely used for crossties in the USA, has now also been commercialized with bridge ties/timbers. In order to understand the implications of these changes, the historic service life of creosote treated bridge timbers in northern and southeastern USA were considered as well as field test data for both creosote...
J Lloyd, C Brischke, R Bennett, A Taylor


Plasma-assisted bleaching of blue-stain from lodgepole pine wood
2017 - IRG/WP 17-40799
We hypothesize that plasma will etch wood and fungal hyphae in blue-stained lodgepole pine, and increase the ability of hypochlorite bleach to remove discolouration from blue-stained wood. Blue-stained lodgepole pine wood was exposed to a glow-discharge plasma derived from water, and the surface wettability, permeability and colour of the treated wood was measured. Plasma-treated wood was dipped i...
A Jamali, P D Evans


The Effects of Pre-Microwave Treatment on Retention Levels And Some Mechanical Properties of Spruce Wood Treated with CCA
2017 - IRG/WP 17-40800
Microwave (MW) treatment of wood has been evaluated in recent years for different purposes by several scientists. Microwave conditioning improves permeability, reduces density and heat conductivity and changes dimensional stability. Furthermore, it could even improve the permeability of refractory wood species such as spruce and Douglas fir. In this study, MW pre-treatment was applied to spruce wo...
E D Gezer, S Kuştaş, S Durmaz


Studying Weathering Performance of Coatings on Thermally Modified Wood
2017 - IRG/WP 17-40805
Thermal modification and degree of improved properties depends on wood species and treatment parameters. Southern pine and spruce are the two common wood species for decking, fences and siding in North America. This study was the first to evaluate coating performance when applied on oil-heat-treated southern pine and spruce wood samples. Water uptake, colour and gloss changes of samples were analy...
M Nejad, M Dadbin, P Cooper


Review on protection of timber bridges in Norway and other countries
2017 - IRG/WP 17-40809
Wood plays a major role in design and construction of modern bridges in Norway. Typical elements of those bridges are double impregnated glued laminated members, stress laminated timber decks, slotted-in steel plates, metal cladding of the surfaces of loadbearing members, and cross girders made of steel. Selected examples of timber bridges in Norway are presented. This review paper gives an overvi...
K-C Mahnert, U Hundhausen


Influence of hygro-thermal treatment temperature and duration on dimensional stabilisation of wood modified with poly(butylene succinate)
2017 - IRG/WP 17-40813
To improve wood properties, especially dimensional stability, a treatment based on poly(butylene succinate) oligomers (OBS) was experimented. After impregnation in wood, a further hygro-thermal treatment (HTT) was carried out in a pressurized reactor at 100% relative humidity (RH) at differing temperatures for differing durations. The aim of HTT is to induce partial swelling of wood cell walls so ...
C Grosse, M Noël, L Rautkari, P Gérardin


Corrosion verification experiment of the screw driven into CLT
2017 - IRG/WP 17-40816
Japan has abundant forest resources, but we depend on import for 70 percent of the consumed timber. Japan has the vision which promotes the timber self-sufficiency rate 30% to 50% by 2020. Therefore CLT attracts attention as a new timber material. Japan has a climate with high temperature and humidity, and wooden buildings are often treated with chemicals as a measure against biological deteriorat...
N Wada, H Ishiyama, S Yamamoto