Termite Response to Oil-Heat-Treated Norway spruce, Scots Pine and Eucalyptus Wood
2006 - IRG/WP 06-20325
The work here presented focused on the behaviour of subterranean termites (Reticulitermes grassei Clément) towards Oil-Heat-Treated (OHT) Norway spruce (Picea abies L.), Scots pine (Pinus sylvestris L.) and eucalyptus (Eucalyptus globulus Labill) wood, with a particular interest in the development of simple methods adequate to study the resistence of these materials to termite attack. Small test ...
L Nunes, T Nobre, C Welzbacher, A O Rapp


Identification of fungi colonising coated and modified wood exposed outdoors using sequencing and T-RFLP profiling
2006 - IRG/WP 06-20326
Wood decay and staining fungi are known to colonize coated and modified wood. Rapid and reliable ways of identifying fungi on coated and modified wood may improve diagnostics and product development. In this work nine fungi growing in painted wood panels exposed outdoors at a test field in Uppsala, Sweden, were identified using sequencing and T-RFLP (Terminal Restriction Fragment Length Polymorphi...
U Råberg, J Bijelovic, C J Land, S Bardage, N Terziev


Heat treatment of less-valuable Nigerian-grown Ceiba pentandra wood for improved properties
2006 - IRG/WP 06-40332
The hardwood Ceiba pentandra locally known as “ araba “ in Nigeria is rarely used for structural and construction works due to its high dimensional instability, low strength and durability values. Samples (10 x 10 x 150mm) were removed from four green boards (25 x 200 x 3000mm) of this species originating from a natural forest stand in Nigeria and subjected to 2-hour heat treatment at 160°C a...
L Awoyemi


Improvement of Grevillea robusta durability using heat treatment
2006 - IRG/WP 06-40333
Heat treatment of Grevillea robusta was carried-out under inert conditions to improve its durability. Resistance of heat treated samples was evaluated by malt agar block tests after three months of exposure to several wood rotting fungi. Results showed that the fungal durability was greatly improved after treatment. There was a good correlation between fungal resistance and mass loss which is a fa...
F Mburu, S Dumarçay, F Huber, M Petrissans, P Gérardin


Wood plastic composites from modified wood; Part 1 - Conceptual idea, mechanical and physical properties
2006 - IRG/WP 06-40338
Wood plastic composites, WPCs, are rapidly taking shares from preservative treated wood on the decking market. However, the long term performance of the WPC products in this application is uncertain. Therefore, in an attempt to increase the long term performance and durability, the substitution of the unmodified wood component with modified wood has been studied in the work presented in this paper...
P Larsson Brelid, B K Segerholm, M Westin, M E P Wålinder


The Effect of Flavonoids on Colour and Spectral Changes of the Wood Surface Caused by Heat Treatment or Ultra-violet Irradiation
2006 - IRG/WP 06-40341
Both heat treatment and UV irradiation can cause discolouration and change in the spectral properties of wood surface. Some of the characteristic flavonols have significant role on colour and spectral changes, despite of their relative small quantities in wood. Colour changes and spectral properties of natural and extracted black locust (Robinia pseudoacacia L.) and poplar (Populus nigra L.) were...
R Csonka-Rákosa, L Molnár-Hamvas, E Börcsök, J Molnár, K Németh


Assessment of the Envelope Effect of Three Hot Oil Treatments: Resistance to Decay by Coniophora puteana and Postia placenta
2006 - IRG/WP 06-40344
Timber of Corsican pine (Pinus nigra var. maritima) and Norway spruce (Picea abies) was treated in hot linseed oil, rapeseed oil and a proprietary resin derived from linseed oil. The samples were immersed in oil or resin under reduced pressure at temperatures of 180°C and 200°C. Very high uptakes of the oils or resin were recorded for pine, while spruce showed lower weight percent gains, below...
M J Spear, C A S Hill, S F Curling, D Jones, M D C Hale


Wood plastic composites from modified wood. Part 2 - Durability in laboratory decay tests
2006 - IRG/WP 06-40353
The decay resistance of wood plastic composites, WPCs, was tested according to modified versions of AWPA E10 (soil-block test) and ENV 807 (tests in three un-sterile soils, terrestrial microcosms, TMCs). The WPC materials were conically extruded profiles with 30% polypropylene content. The 70% wood content was untreated Scots pine sapwood, acetylated pine and heat treated Norway spruce, respective...
M Westin, P Larsson Brelid, M L Edlund, G Alfredsen


Effects of heat treatments on decay resistance and material properties of ponderosa pine and yellow poplar
2007 - IRG/WP 07-40374
The potential for using heat treatment to improve the properties of North American fenestration species was evaluated on ponderosa pine (Pinus ponderosa L) and yellow poplar (Liriodendron tulipifera L) treated using the ThermoWood process at various treatment temperatures and times. Soil block tests using Gloeophyllum trabeum, Postia placenta, or Trametes versicolor showed that durability was enh...
C Vidrine, C Freitag, J Nicholson, J J Morrell


Copper fixation in ACQ-D treated Chinese fir at various temperature and relative humidity conditions
2007 - IRG/WP 07-30436
In this study, the effect of different conditions of temperature, relative humidity, and duration of post-treatments on accelerating copper fixation in ACQ-D treated Chinese fir wood blocks was investigated. The conditions include the combination of three temperatures (21, 50, and 70?) and two relative humidity levels (20% and 80%), also include four temperatures (50, 70, 90, and 110?) without con...
Jinzhen Cao, Lili Yu


Natural Weathering of Coated Oil Heat Treated Wood
2007 - IRG/WP 07-30440
Oil heat-treated (thermally modified) pine wood was coated with 9 different types of solvent- or water-borne exterior finishes. The systems with modified wood substrate as well as unpainted and painted non-modified controls were exposed to weathering (EN 927-3) on two locations with sub-alpine and alpine climate. The influence of natural ageing on surface systems was evaluated after one year of ex...
M Petric, B Kricej, M Pavlic, A Rapp


Mold resistance of heat-treated wood
2007 - IRG/WP 07-40358
The resistance of heat-treated sugi sapwood against three mold fungi was evaluated. Wood specimens were first subjected to heat treatments at 180 and 220ºC for 2 and 4 hours. Mold growth on the surface of the specimens was measured 1, 2, 4 and 6 weeks after the inoculation with the fungi in laboratory conditions. Laboratory decay tests were performed using two brown and white-rot fungi along with...
S N Kartal


Multivariate analysis of infrared spectra for the prediction of the mechanical performance and dimensional stability of thermally modified wood
2007 - IRG/WP 07-40367
The use of calibrated mid-infrared Fourier transform (FTIR) spectroscopy for predicting the main bending strength parameters of thermally modified wood is described for the first time. The analysis is based on the handling of OSC-filtered FTIR data from control and treated wood samples, using partial least squares (PLS) regression. Sets of Norway spruce, Scots pine and Beech wood samples were th...
M M González-Peña, M D C Hale


Treatment of Green Logs infested by Exotic Pest: Case Study of the Emerald Ash Borer: Agrilus planipennis Fairmaire
2007 - IRG/WP 07-10628
Invasive alien insect species periodically infest forests in the United States causing the destruction of plant species and decimating populations, resulting in significant economic and ecological losses for areas involved. The Emerald Ash Borer (EAB) was first discovered on North American soil in the summer of 2002 near Detroit, Michigan and has since spread to several other Midwestern states and...
P Nzokou, S Tourtellot, D P Kamdem


Do insects infest wood packing material with bark following heat-treatment?
2007 - IRG/WP 07-10633
As a result of international trade, many bark- and wood-infesting insects are inadvertently transported in wood packing materials (WPM) such as crating, dunnage, and pallets. WPM is suspected as the likely pathway for most of these borers, although the exact mode of entry into the USA is unknown for all 25 borers. The top 10 countries of origin were, in decreasing order, Italy, Germany, China, Spa...
R A Haack, T R Petrice, P Nzokou, D P Kamdem


Fire Safety of Wood Floor Assembly: Model and Full-scale Test
2007 - IRG/WP 07-20375
The present paper describes the model for the prediction of fire safety of wood floor assemblies. The model includes heat transfer model for the calculation of the flow of heat in floor assembly and structural model for the analysis of the mechanical performance of wood joists. The floor assemblies considered in this paper are constructed with nominal 2x10 (38x241mm) wood joists lined by Type X ...
H Takeda


Durability of some alternatives to preservative-treated wood. Progress report 2: Results from field tests after 5 years’exposure
2007 - IRG/WP 07-30442
A number of alternatives to preservative-treated wood have been tested according to EN 252 (stake test) and a specially designed ground-proximity field test, the latter in Sweden as well as in Hawaii, USA. Seven untreated wood species and four alternative wood treatments labelled as environmentally friendly (acetylation, linseed oil, heat treatment, vinyl polymer) were included in the study. Four ...
M-L Edlund, J Jermer


Difficulties applying Heat Treatment according to ISPM No. 15, when fast growth species are used
2007 - IRG/WP 07-40386
In 2002, the Interim Commission on Phytosanitary Measures (ICPM) adopted the International Standard for Phytosanitary Measures (ISPM) No. 15 (Guidelines for regulating wood packaging material in international trade). Two treatments are recognized: Heat Treatment (HT), in which wood must be heated to a core temperature of 56°C for 30 minutes, and fumigation with methyl bromide. As the last treatme...
O Encinas, J. I Briceño


A preliminary note on the role of moisture absorption rate in durability assessment
2008 - IRG/WP 08-20383
The rate of moisture uptake was studied in 15 wood species using vermiculite at varying moisture levels as the exposure medium. As might be expected, moisture uptake varied widely among the species studied. While some of the more durable wood species were also resistant to moisture uptake, this was not always true. The results are discussed in relation to performance in under varying environmenta...
J J Morrell, L P Francis


Primary Study on Compressed Preservative-treated Wood (CPW) for Outdoor Applications
2008 - IRG/WP 08-40412
In this study, the compressed wood samples pre-treated with hot water bath or water spraying were immersed in the ammoniacal copper quat –type D (ACQ-D) preservative solution to get compressed preservative-treated wood (CPW). The liquid absorption and the recovery rate of compression deformation of the compressed wood was determined, as well as the surface hardness, the distribution of density a...
Jinzhen Cao, Jia Mao


Effect of wood polymers degradation during heat treatment on extracellular enzymatic activities involved in beech degradation by Trametes versicolor
2008 - IRG/WP 08-40392
Effect of heat treatment on extracellular enzymes involved in wood degradation by Trametes versicolor was investigated. Heat-treated and untreated beech blocks were exposed to T. versicolor on malt agar medium and extracellular enzymatic activities investigated. A strong ABTS oxidizing activity has been detected during the first stage of colonization in both cases, while cellulase activities are m...
S Lekounougou, G Nguila Inari, M Pétrissans, S Dumarçay, J P Jacquot, E Gelhaye, P Gérardin


Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III


Heat treatment, thermal treatment, thermal degradation of wood, carbon nanotubes and Damascus steel swords. What do they all have in common?
2008 - IRG/WP 08-40399
Thermal degradation of wood is a well known phenomenon. Yet heat-treatment of wood can also provide protection for wood against certain environmental hazards. This paper explores some of the aspects of thermal degradation of wood fiber at relatively low temperatures with a surprising result. Carbon nanotubes (CNTs) were produced when a specific heating regime was used to carbonize the wood fiber. ...
Xinfeng Xie, B Goodell, Yuhui Qian, G Daniel


The Effect of Heat Treatment on Water Absorption and Dimensional Stability of Anatolian Chestnut (Castanea sativa Mill.) wood
2008 - IRG/WP 08-40407
The heat treatment of wood is an environment-friendly method for wood preservation. This process improves wood’s resistance to decay and its dimensional stability. However, mechanical properties decrease in different ration because of density loss as a result of heat treatment. In this study, the effect of heat treatment on water absorption and dimensional stability at different relative humidit...
G Gunduz, D Aydemir


The effect of treatments in boron steaming medium on boron leaching and strength properties of wood
2008 - IRG/WP 08-40409
The combined effect of boric acid impregnation together with boron steaming and steaming heat treatments were evaluated in this study. Boric acid pre-treated wood samples and untreated ones subjected to steaming heat and direct steaming treatment in a close reactor at 13 bar pressure and 180 ºC for 30 minutes. Compression strength parallel to grain of wood samples, leaching test and pH measuremen...
E D Tomak, Ü C Yildiz, S Yildiz, E Pesman