The performance of CCA treatment in bamboo against decay fungi
1993 - IRG/WP 93-30027
Samples of culm wall material from young (< 6 month age) and mature (> 3 years age) culms of the bamboo, Phyllostachys virideglaucescens were treated to equivalent% w/w retentions of a CCA preservative. After fixation and leaching the treated samples were exposed to decay by Chaetomium globosum FPRL S70K, Coriolus versicolor FPRL 28A and Coniophora puteana FPRL 11E. Thin section samples of u...
O Sulaiman, R J Murphy


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Work programme of CEN/TC 38 (April 1999) and European publications
1999 - IRG/WP 99-20165
Scope of the CEN/TC38: Standardization of the characteristics of natural or conferred durability of wood and its derived materials against biological agents, including the characteristics of protection products and associated processes to obtain this durability. This applies in particular to: - the identification of hazard classes-, - the test methods (wood preservatives and treated wood and wood ...
R Hüe


A Soil Bed Test of the Effect of CCA Penetration on the Performance of Hem-fir Plywood
2004 - IRG/WP 04-30332
An accelerated decay test was set up to compare the performance of CCA-treated Western hemlock/amabilis fir plywood treated to meet the preserved wood foundation (PWF) retention standard with various patterns of preservative penetration. Short lengths of treated plywood and comparable untreated material were installed in a soil bed. After eleven years of exposure, the CCA treatments were all sou...
P I Morris, J K Ingram


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Kinetic of the wood degradation produced by wood decay fung
1993 - IRG/WP 93-20016
The degradation degree of a wooden structure has a direct influence on its loss of mechanical strength. It&apos;s necessary to deepen in non destructive techniques which permit to extrapolate the results obtained in laboratory to structural timber used in the building&apos;s construction. This work studies the relationship existing between the pulse velocity of ultrasonic waves and the wei...
M T De Troya, A M Navarrete, A Sanchez, V Bucur


Screening of lignin peroxidase from white-rot fungi
1998 - IRG/WP 98-10274
Since lignin peroxidase was first found in the ligninolytic culture of Phanerochaete chrysosporium, it has been regarded as an enzyme responsible for the lignin biodegradation and studied comprehensively. As the results of these studies its unique characteristics have been revealed. On the other hand, the features of lignin peroxidase produced by other white-rot fungi have not been studied so much...
I Momohara


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


List of wood-destroying fungi in Iran
1976 - IRG/WP 138
This list gives information on the wood-destroying fungi collected in the Iranian forests and from felled logs and boards in sawmills until now. They are mainly from the region of the Caspian Forests and from the climatically dry region between Teheran and Azarbaidjan, North Iran. It is understood, that this document may help to give more knowledge outside the country about the specific problems o...
P Soleimani


Biological control of sapstain fungi in wood
1996 - IRG/WP 96-10158
Sapstain fungi can cause serious damage to wood and wood products, resulting in a significant economic loss for the wood products industry. The purpose of the present investigation was to determine whether the sapstain in wood caused by sapstain fungi could be biologically controlled. Biological control of sapstain fungi in wood was demonstrated in field trials with nonpigmented isolates of Cerato...
S C Croan


Susceptibility of harvested softwoods to infection by sap-staining fungi
2002 - IRG/WP 02-10435
In the UK a field study programme was carried out to compare the susceptibility of softwood timber from five different commercially important tree species to infection by sap-stain fungi. Logs cut from freshly felled Scots pine (Pinus sylvestris), Lodgepole pine (P. contorta var. latifolia), Sitka spruce (Picea sitchensis), Norway spruce (P. abies) and Japanese larch (Larix leptolepis) were expo...
E J Young, R A Eaton, J F Webber


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980&apos;s against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


Biocontrol and bioprotection of wood decay and sapstain fungi
2003 - IRG/WP 03-10474
The most serious damages caused in the wood industries by decay and sapstain fungi, and the growing international pressures on the use of biocides products with toxic active ingredients harmful to human health and the environment, have made it necessary to search for alternative chemical products to protect the wood, and for the possibility to use micro-organisms as biological controllers. This la...
M T De Troya, F Rubio, M Villarreal, F Arenal, F Llinares, V Rubio, D Muñoz-Mingarro, N Acero


Calculation of preformance index of Bardac 20 (an alkylammonium compound) evaluated in a field stake test
1982 - IRG/WP 3206
Bardac 20 treated stakes have been in test for three years at the Westham Island test site near Vancouver, B.C. The Performance Index for the preservative was calculated and found to be 0.009 which infers that, at the standard retention, Bardac 20 added 0.9 y to the life of the stake. It may be concluded that when tested using a standard field stake test using ponderosa pine (Pinus ponderosa Laws)...
J N R Ruddick


Correlation between different international standard assessment procedures with termites. Part 1: Field exposure
1983 - IRG/WP 1198
Ramin treated with copper-chrome-arsenic (CCA), pentachlorophenate and lindane, each at three retentions, and three other untreated timbers were assessed in the field against Coptotermes lacteus and Nasutitermes exitiosus. Replicate specimens were exposed around five mounds of each termite species over a period of five years in south-eastern Australia. The field results provided the basis for judg...
M Lenz, C D Howick, N Tamblyn, J W Creffield, M Westcott


Leaching results of shower test on L-joints with boric acid, bifluoride and TBTO rods
1995 - IRG/WP 95-50051
As part of the EC-project "Improvement of a local preservation process for wood products with reduced environmental impact", TNO has performed a leaching test on L-joints treated with pills with boric acid (Defence corner), bifluorides (Woodpil 55) and TBTO (Woodcap). The L-joints were exposed in an adapted shower test during 10 days, using 70 liters of water per day. The experiment is designed to...
P Esser, M J Boonstra, W L D Suitela, A J Pendlebury


Characterization of tropical wood-decaying fungi by RFLP analysis of PCR amplified rDNA
1998 - IRG/WP 98-10251
Five brown-rot fungi (Tyromyces palustris, Gloeophyllum trabeum, Antrodia sp., Poria placenta, Coniophora puteana) and three white-rot fungi (Coriolus versicolor, Pycnoporus sanguineus, Lentinus squarrosulus) registred as representative wood-decaying fungi for international standards of wood durability tests have been characterized using molecular tools (PCR/RFLP). The Internal Transcribed Spacer ...
A Zaremski, M Ducousso, Y Prin, D Fouquet


Soft rot studies on CCA treated eucalypt power transmission poles
1981 - IRG/WP 1132
Initial results found for sixty CCA treated eucalypt poles, from a soft-rot survey are discussed. Retentions of CCA within above and below ground pole samples were variable. The variation was attributed mostly to biodegradation and effect of soil environment, rather than leaching. Bacterial decay was found in many poles and was severe in some cases. Although found in the presence of soft-rot decay...
L E Leightley


Wood decay of Pinus sylvestris L. by marine fungi
1990 - IRG/WP 1463
Waterlogged wood decay by marine microorganisms represents a major problem for the conservation of wood structures of historic value. It is important to know which kind of decay affects the wood from a conservation point of view. Enzyme activities of 14 marine fungi belonging to several localities were studied. Also, the weight loss and the rot type suffered by the wood at a microscopic level were...
M C Escorial, M T De Troya, J E Garcia de los Rios


Resistance of painted wood to mould fungi. Part 2. The effect of wood substrate and acrylate paint systems on mould growth
1997 - IRG/WP 97-10234
Resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments studied. The efficacy of the treatment systems varie...
H Viitanen, P Ahola


The effect of malt and agar trademarks on growth, decay and stilbene resistance of fungi
2000 - IRG/WP 00-20202
Effects of malt and agar trademarks used in growth media on growth of fungi in cultures, amount of decay they cause in birch samples and their resistance to stilbenes were tested. It was tested also had the conditions where fungus cultures were stored before inoculation of test plates some effect on the results. Fungi used in these tests were white rot fungus Trametes versicolor and brown rot fung...
L Syrjälä, L Paajanen, A Pappinen


A study of decay type variability in variously treated Fagus sylvatica and Pinus radiata field test stakes exposed at a vineyard for 30 - 45 months
1998 - IRG/WP 98-10271
Pinus radiata test stakes were treated with 10 kg/m3 of CCA plus 4 lower retentions in a geometric series of 1.5. Fagus sylvatica was treated with 15 kg/m3 and 2 lower retentions. Both timber species were also treated with equivalent retentions of various new generation preservatives (P. radiata was also treated with creosote). Whilst these stakes were exposed at 11 sites in New Zealand (NZ) and 2...
R N Wakeling, A P Singh


Accelerated laboratory soil contact decay test using soil amended with composted wood
2004 - IRG/WP 04-20284
The effect of amending soil with wood compost on the decay rate of wood wafers in contact with the unsterile soil, as measured by radial compression strength loss, was explored. It was found that the addition of composted wood to the soil significantly increased the wood decay rate. The reason for this acceleration in wood decay is not entirely clear, but appears to be at least partially associate...
D D Nicholas, H Borazjani, T Schultz


Co-operative research project on L-joint testing. Progress report to March 1984
1984 - IRG/WP 2211
Each participant was intended to expose L-joints in the main trial on 1 April 1983 and the first sampling, after 8 months exposure, was to be undertaken on 1 December 1983. Some participants have had to vary this schedule. Results are presented from CTFT (France) and PRL (United Kingdom). These show a greater effectiveness by the double vacuum treatments compared with the 1 minute dip treatments. ...
J K Carey, A F Bravery


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 5: Extensive data from a site where both decay and termites are active. Results from a full-replicated set of heartwood specimens from each of ten myrtaceous hardwoods after 18, 19 and 20 years' exposure - A discussion paper
1988 - IRG/WP 2324
Extensive data are presented on the decay situation, the termite situation and the decay-termite associations; all gathered from a fully-replicated set of heartwood specimens of 10 hardwood timbers after 18, 19 and 20 years&apos; exposure in the ground at a single test site, i.e. a semi-arid steppe site. Sixteen tables are presented in addition to the one table providing the rating data; the l...
J D Thornton, G C Johnson, J W Creffield