The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


The influence of copper (II) chemicals on the weathering of treated wood. Part 1: ACQ treatment of wood on its weathering
1994 - IRG/WP 94-30040
Wood weathering can be accelerated by alkylammonium compound (AAC) treatment, and slowed by ammoniacal copper quat (ACQ) treatment. This study aims at investigating the influence of ACQ treatment of wood, especially the present of copper (II), on its weathering. ACQ, CCA and DDAC treated microtomed sections of southern yellow pine earlywood were prepared and naturally weathered for five periods, t...
Ruiying Liu, J N R Ruddick, L Jin


Thermal modification of non-durable wood species 1. The PLATO technology: thermal modification of wood
1998 - IRG/WP 98-40123
The PLATO technology is an innovative upgrading technology with low environmental impact, which can be applied to fast grown and non-durable wood species. This technology is based on a thermal modification of solid wood without the addition of chemicals (e.g. preservatives), consisting of a hydrothermal treatment, followed by drying and curing. The PLATO technology results in a substantial improve...
M J Boonstra, B F Tjeerdsma, H A C Groeneveld


A serial exposure technique for estimating probable service life of treated timber
1978 - IRG/WP 2111
This paper briefly describes part of our preliminary work aimed at developing a test procedure that culd be adopted as a standard method. A detailed version of the work has been submitted for formal publication. In both papers, the aim is to promote interest in extended laboratory testing of wood preservatives. It is believed that this work may provide the basis of a laboratory test procedure from...
J A Butcher


Fumigant movement in Canadian wood species
1984 - IRG/WP 3296
Pole sections prepared from seven Canadian wood species (Thuja plicata, Thuja occidentalis, Pinus contorta, Pinus resinosa, Pinus banksiana, Pseudotsuga menziesii, southern yellow pine) were fumigated with chloropicrin, methylisothiocyanate and Vapam and the rates of fumigant penetration determined. All three fumigants were applied directly into holes bored radially into the pole sections. Analysi...
J N R Ruddick


Determination of total fluoride and boron in preservative-treated wood fluoride by ion selective electrode without steam distillation, and boron colorimetrically using azornethine-h
1998 - IRG/WP 98-20135
An analytical method was developed to determine total fluoride and boron in wood treated with aqueous or solid diffusing fluoride or borate-fluoride formulations. Ground wood was mixed with 30% sodium hydroxide solution and oven-dried for 2 hours before furnacing at 600° C for 1 hour. The cool fused product was dissolved in hot water, transferred to a plastic beaker and neutralised. Fluoride was ...
P A Collins, M J Kennedy


Environmentally benign biological wood preservatives by Streptomyces rimosus, SC-36
1997 - IRG/WP 97-10196
Microbiocides obtained from mutant culture Streptomyces rimosus SC-36 were evaluated for their abilities to inhibit the growth of brown-rot, soft-rot, white-rot, and sapstain fungi on wood. The test fungi were the brown-rot fungi Antrodia carbonica, Gloeophyllum trabeum, Neolentinus lepideus, and Postia placenta; soft-rot fungi Chaetomium globosum, Paecilomyces variotti, Phialocephala dimorphospor...
S C Croan


A preliminary assessment of the penetration into wood achieved by bodied mayonnaise emulsion wood preservatives
1992 - IRG/WP 92-3725
Five different commercial formulations of bodied mayonnaise emulsions were applied to samples of Scots pine (Pinus sylvestris) sapwood as recommended by the manufacturers. Penetration and loading characteristics were determined by measuring the distribution profiles of the active ingredients after various intervals of time. The changes in the general appearance of the emulsions on the surface of t...
G E Holland, R J Orsler


Termite resistance of Malaysian and exotic woods with plantation potential: Laboratory evaluation
1998 - IRG/WP 98-10280
The resistance of selected Malaysian woods to attack by the representative aggressive subterranean termite Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae) was evaluated in four-week, no-choice laboratory tests. This is part of an ongoing effort between the Forest Research Institute Malaysia and the University of Hawaii to document the termite resistance of Malaysian timber species of po...
J K Grace, A A H Wong, C H M Tome


BRE Experience in monitoring decay in out-of-ground exposure trials
1995 - IRG/WP 95-20077
The outdoor field trial has always been regarded as the ultimate test of performance for assessing the effectiveness of a wood preservative. For this reason, the Building Research Establishment (BRE) has invested much effort in such trials over many years. Emphasis in early trials was on ground contact tests which were the basis both for assessing the likely performance of a preservative in protec...
J K Carey, R J Orsler


Fungal associates of Buprestis langi Mannerheim colonizing stored douglas-fir logs
1997 - IRG/WP 97-10220
Buprestid beetles are important colonizers of dead and dying conifers. The larvae of these beetles initially mine a gallery beneath the bark, then tunnel deep within the log. These beetles can cause extensive damage to wood, but it is their frequent association with internal fungal decay that causes the greatest concern. Many insects are capable of vectoring fungi that enhance their prospects for ...
C M Garcia, M Y Giron, J J Morrell


Using AE monitoring for detecting economically important species of termites in California
1991 - IRG/WP 2375
Acoustic emission (AE) monitoring was conducted on wooden samples containing three economically important species of termites in California (dampwood termite, Zootermopsis nevadensis, Western drywood termite, Incisitermes minor, and Western subterranean termite, Reticulitermes hesperus). Laboratory AE studies included varying termite species, as well as 7 day studies exploring the periodicity of t...
V R Lewis, R L Lemaster, F C Beall, D L Wood


Will political initiatives stop the use of preservative-treated wood in Sweden?
1990 - IRG/WP 3578
The Swedish government has initiated several investigations on how to reduce the use of different chemicals. Among these chemicals are creosote, arsenic, chromium and organotin. A special investigation was carried out concerning wood preservatives resulting in different proposals on how to reduce the use of preservatives and preservative treated wood. The most important proposals were an "environm...
J Jermer, M-L Edlund


Towards harmonisation of regional approaches for an International Standard for the approval of wood preservatives
1997 - IRG/WP 97-20122
Recent proposals from the European Standards body (CEN) for an ISO Standard on wood preservatives has initiated debate on whether there is any prospect of an acceptable common approach among ISO member countries, to a harmonised framework of hazard classes, with agreed supporting biological tests, leading to a unified rationale for demonstrating compliance with minimum performance standards for sp...
A F Preston, A F Bravery


In situ timber treatments by spraying. Distribution of preservative in wood
1991 - IRG/WP 3678
This study was carried out in order to make the Pest Control Operators able to achieve correct treatments and enhance their efficacy. It was carried out in two steps: 1) in laboratory, to learn the influence of various parameters like spraying pressure, use of repeated applications, distance from nozzle to wood; 2) in situ on roof timber of five buildings. In this case, the applications of the pre...
C Defoin, G Dupont, M Lamour, H Sageot, M-M Serment


Long-term efficacy of wood dip-treated with multicomponent biocides
2005 - IRG/WP 05-30379
Biocides designed for prevention of indoor mold growth on wood-based materials need to provide long-term protection under conditions of high humidity. Specimens of kiln-dried southern pine and unseasoned southern pine, aspen, and Douglas-fir were dip-treated with borate-dimethylcocoamine (DMCA) supplemented with voriconazole, thiabendazole, or thujaplicin and evaluated at 4-week intervals for inhi...
C A Clausen, V W Yang


Technical viability of deltamethrin as a pre-treatment wood preservative
1993 - IRG/WP 93-30012
This paper presents the results of tests conducted on freshly-cut logs and lumber during the seasoning period to verify the effectiveness of Deltamethrin on insect control. The tests were carried out in Quedas do Iguaçú, Paraná (southern region of Brazil) and Breves, Pará (northern region of Brazil) during the-dry and rainy seasons, and used different species of wood and insecticide/fungicide ...
A M F Oliveira, S Milano, J L A Bahia, F Teleginski


Creosote for wood preservation
1971 - IRG/WP 36
By creosote one usually means coal tar creosote, although there are creosotes of other origin. For example, wood tar creosote is a product of wood distillation. It is, in fact, in this connection that the word 'creosote' was first used. Early in the nineteenth century the oily product obtained by distilling wood was said to have an odour which resembled 'smoked meat&...
Anonymous


A novel device for detecting internal defects in wooden poles
1989 - IRG/WP 2329
The diagnosis of internal defects caused by termites and decay in hardwood transmission poles has been investigated using a novel Automatic Feed Drill (AFD) pole testing device. Internal defects were recognised by changes in drill feed-rate as the automatic air-driven drill traversed its 100 mm working stroke. The instrument is portable, simple to operate and recognises defects instantaneously. Te...
R A Eaton, R S Johnstone


Distinguishing isolates of Aureobasidium on the basis of their ability to utilise lignin breakdown products as a sole carbon source
1996 - IRG/WP 96-10151
Wild isolates of Aureobasidium were obtained by dilution plating from a ca 20 year old painted pine window frame. Four isolates were obtained from the paint/wood interface region and four isolated from regions deep in the wood. The isolates were then used to inoculate liquid cultures containing ferulic acid, a lignin breakdown product, present as the sole carbon source. Ability of the isolates to ...
M W Schoeman, D J Dickinson


Chemical evaluation of borate treated pine sapwood attacked by the subterranean termite Coptotermes acinaciformis
1993 - IRG/WP 93-20003
Sapwood of hoop (Araucaria cunninghamii Ait. ex D. Don) and slash (Pinus elliottii Englem.) pines were treated by Vacuum Pressure Impregnation (VPI) to provide test specimens. The concentration of boron was defined by chemical analyses of the timber, in the zone of primary attack by the termite being bioassayed. A common method of definition of preservative retention, weight uptake of preservative...
A R Moffat, B C Peters


A below-ground exposure method for determining the resistance of woody and non-woody materials to attack by subterranean termites
1993 - IRG/WP 93-10012
With existing field test procedures, in which specimens are installed vertically to some of their length into the ground and spaced out from each other ("grave-yard" tests), variations in the rate of contact by termites between replicates can be common. Mechanical damage to specimens during inspection and re-installation may also be difficult to avoid. A new field test method, evaluated in Austral...
M Lenz, J W Creffield


Biochemical aspects of white-rot and brown-rot decay
1987 - IRG/WP 1319
This paper presents an overview of the decomposition of wood by white- and brown-rot fungi - the most important and potent of known wood-decay fungi. These organisms are unique among cellulose destroyers because of their strong capability to enzymatically degrade lignified material. Special emphasis is given to the following aspects of wood decomposition by white- and brown-rot fungi: (1) effects...
T L Highley


Influence of concentration, catalyst, and temperature on dimensional stability of DMDHEU modified scots pine
1998 - IRG/WP 98-40119
Dimethyloldihydroxyethyleneurea (DMDHEU) is being used in textile industry to improve wrinkle recovery. Trials on solid wood have been performed to minimise swelling of the wood. This paper focuses on the effect of various types and concentrations of catalyst and reaction temperature on the dimensional stability of Scots pine. Three different catalysts, NKS (based on magnesium chloride), 3282 (bas...
M Van der Zee, E P J Beckers, H Militz


Field testing of alkylammonium wood preservatives
1983 - IRG/WP 3248
The field test performance of five alkylammonium wood preservatives is described. The relative effectiveness of three unmodified formulations was determined by calculation of a Performance Index. Of the three, didecyldimethylammonium chloride was found to be superior to octyldecyldimethylammonium chloride, and both were more effective than alkyltrimethylammonium chloride. However, none were consid...
J N R Ruddick


Previous Page | Next Page