Gloeophyllum trabeum and Gloeophyllum abietinum, the most frequent brown rot fungi in fir wood joinery
1999 - IRG/WP 99-10319
In Croatia the primary raw material for joinery production is silver fir wood (Abies alba Mill). L-joints made of home-grown fir sapwood and prepared according to EN 330: 1993 were used to establish the infection and colonisation of micro-organisms, particularly wood decay fungi, to compare the performance of untreated and 1% TnBTO treated L-joints. The L-joints were coated with two types of coat,...
R Despot, M Glavas


A direct method for testing plywood and particle boards against fungal decay
1984 - IRG/WP 2214
A method directly inspired from the French standard testing method of the resistance of particle boards against fungal decay (AFNOR N° 51.295 May 1980) is described. But in that experimentation, the infestation is localized and realized in non sterile conditions. Small blocks of Fagus sylvatica (60 x 20 x 10 mm³) used as " inoculates " are infested with basidiomycetes, in Kolle flask for 4 to 6 ...
L N Trong


Decay resistance of wood removed from poles treated with Trichoderma
1989 - IRG/WP 1386
Wood blocks removed from a distribution pole previously treated with a biological control product (Binab FYT pellets) were exposed in soil block tests to selected basidiomycetes. The blocks were removed from regions of poles where Trichoderma colonization had been confirmed by extensive sampling and computer mapping of microbial inhabitants. The results indicate that material from pole interiors c...
A Bruce, B King, T L Highley


Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem


Accelerated ageing of preservatives in treated wood
1988 - IRG/WP 3476
New preservatives are tested in the laboratory and often in field tests before they are used commercially. Some preservatives, however, tested in the laboratory do not show the expected stability when used in service. The differences between laboratory tests and practical use can never be completely eliminated but must be minimized as far as possible by relevant testing methods. Studies of the eff...
M-L Edlund, B Henningsson, B Jensen, C-E Sundman


Contribution to study of the degradation caused in Pinus spp. poles used in field test
1989 - IRG/WP 1417
The study of the degradation produced by soil natural microflora on wood in contact with it in the field, has been going on for several years now. Our contribution to this aim in the present work has dealt with the possible relationship of the microorganisms in the soil. The microscopic visualization of wood colonization by the microorganisms, and the chemical analysis of the degraded wood compare...
M T De Troya, A Garcia, M J Pozuelo, A M Navarrete, A Cabanas


Forest products laboratory methodology for monitoring decay in wood exposed above ground
1995 - IRG/WP 95-20074
Research at the Forest Products Laboratory on the durability of wood in service has included a full complement of laboratory and field tests. In this report, we present a review of past and current methods used to evaluate the condition of preservative-treated wood exposed above ground. Current protocols are described for tests on wood packaging, roofing, and dimension lumber....
R C De Groot, T L Highley


Efficacy of anhydrides as wood protection chemicals - II. Performance against soft rot fungi
1998 - IRG/WP 98-30174
Pine sapwood modified with various anhydrides and with butyl isocyanate was tested for its resistance to soft rot decay. Small stakes were exposed for 20 months in unsterile soil in a fungal cellar test. Wood modified with butyl isocyanate performed better than any of the anhydrides tested, with a threshold level of protection (less than 3% weight loss) at 12% weight percent gain (WPG). Stakes ac...
S C Forster, M D C Hale, G R Williams


Electron microscopic detection and chemical analysis of three-lamellar structures in wood-destroying fungi
1984 - IRG/WP 1240
In the course of transmission electron microscopical investigations of pine wood decay by various brown- and white-rot fungi extracellular three-lamellar structures (TLS) formed by the fungi were found in specimens stained with ruthenium red. These structures occured in the lumen of the wood cell surrounding the hypha at the outermost layer of the fungal cell wall. In the course of the investigati...
R Foisner, K Messner, H Stachelberger, M Röhr


Changes in the degree of decay of lignocellulosic substrate used in a screening test of fungicidal wood preservatives
1977 - IRG/WP 287
This report contains results of investigations aimed at: a) determination of the effect of the kind of substrate and species of test fungus on quantitative changes in used samples prepared from spruce cardboard, and b) comparison of the threshold fungicidal values of come fungicides determined with accelerated method, with values obtained by block method. During performed investigations, the metho...
K Lutomski


Extracellular layers of wood decay fungi and copper tolerance
1983 - IRG/WP 1180
Extracellular layers around the hyphae of brown, white and soft rot fungi have been examined using electron microscopy. These layers were isolated for identification. Particular interest was directed towards the extracellular layers of copper-tolerant soft rot fungi....
D M Francis, L E Leightley


Targeting fungal proteinases to prevent sapstain on wood
1995 - IRG/WP 95-10097
Discoloration of wood, caused by a variety of sapstaining fungi, leads to periodic losses in the Canadian lumber export industry. Proteolytic enzymes are thought to be necessary for retrieval of nitrogen during fungal growth on wood. The major extracellular proteinase of Ophiostoma piceae, a representative sapstaining fungus, was purified to homogeneity and its inhibition pattern characterised. Cl...
L D Abraham, D E Bradshaw, A Byrne, P I Morris, C Breuil


A technique for the quantitative isolation of Actinomycetes from decayed wood
1980 - IRG/WP 1116
A technique combining comminution and high-speed homogenisation has been developed for the preparation of suspensions of micro-organisms in colonised wood. When standard inocula of Streptomyces spores were applied to wood, constant proportions of the inocula were recovered. This method was used in conjunction with selective culture media to isolate actinomycetes from wood which had been buried in ...
A A W Baecker, B King


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


A short note on fungal decay in K33-treated poles
1982 - IRG/WP 1169
Soft rot cavities and erosion of the lumen have been found in K33-treated Pinus sylvestris poles from the years 1956-66 by microscopic studies. Poor treatment quality has been proved for some of these poles. The microscopy showed an unusual pattern of attack, and pre-treatment decay is suspected but not yet proved. Sounding the poles and using the Pilodyn indicated decay, but poking did not. Quant...
H Friis-Hansen


Model questionnaire for preparation of monographic cards for wood-destroying fungi
1972 - IRG/WP 103
C Jacquiot


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Accelerated wood decay in a soil bed test under greenhouse conditions compared with a stake test under field condition
1991 - IRG/WP 2384
The rate of decay of oak, beech, Douglas fir, pine and spruce stakes in an outside test field were compared with the decay rate of the same species in a greenhouse soil-bed test. Strength loss after four and six months respectively was measured by determining the compression strength parallel to the grain. The results show that all species, strength loss in the greenhouse was 2 to 4 times higher t...
J E Polman, S G Michon, H Militz


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


Wood preservation in the Australian beekeeping industry
1988 - IRG/WP 3473
This paper reports the results of a survey of Australian commercial beekeepers working 200 or more hives in June/July 1985. Nine hundred and forty seven apiarists were asked to participate and to provide information on their wood preservation methods, painting procedures and maintenance of bee boxes. Three hundred and eighty-four apiarists returned completed questionnaires (41%). The main wood pre...
P J Robinson, J R J French


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Effect of sterilization method on germination of spores of wood decay fungi observed by contact agar block method
1978 - IRG/WP 2117
Previous studies of germination of spores of wood decay fungi on wood have generally concluded that method of wood sterilization has little significant effect on germination response. This study expands the numbers of test fungi as well as number of sterilization methods employed to determine the influence of sterilization method on spore germination response of decay fungi. Germination was assess...
E L Schmidt, D W French


Non-enzymatic Gloeophyllum trabeum decay mechanisms: Further study
2001 - IRG/WP 01-10395
Information will be presented on the mechanisms involved in, and potential application of, non-enzymatic wood decay by brown rot decay fungi. Specifically, the hypothesized role of low molecular weight phenolate derivatives will be discussed in relation to non-enzymatic degradation of wood. The mechanism of binding of iron by cellulose, and binding and reduction of iron by fungal derivatives and m...
B Goodell, J Jellison