List of fungi in soft-rot tests
1975 - IRG/WP 105
This list gives information on the terrestrial and marine species and strains of fungi tested for soft-rot ability in pure culture with data on their decay activity in untreated wood. An index of the timber species tested is added. The compilation is based on 1) the list of soft-rot fungi of the former OECD Group (Doc.No. 27/DAS/CSI/M/559), Oct. 1968, prepared by R. Rösch and W. Liese, 2) informa...
G Seehann, W Liese, B Kess


Comparative performance of copper azole and copper-chrome-arsenate treated rubber wood in Australian, Malaysian and New Zealand tests sites
2000 - IRG/WP 00-30213
Rubberwood (Hevea brasiliensis) has been used for non-structural products where appearance is important. It has rarely been used for structural uses where preservative treatment is required. In order to evaluate the in-ground durability of preservative-treated rubberwood, test stakes (20 x 20 x 500 mm3) were treated to four retentions of CCA and copper azole (Tanalith® E) and installed in test si...
J A Drysdale, M E Hedley, E Loh, L T Hong


Defining fungal decay types - A proposal for discussion
1985 - IRG/WP 1264
The present definitions of the fungal decay types, white rot, brown rot, and soft rot are somewhat vague. The definitions are based on a mixture of criteria involving morphological and chemical aspects of decay as well as taxonomic affiliation of the responsible fungal species. The present vague definitions have led some fungi being erroneously places in a wrong decay type. Furthermore, some fungi...
T Nilsson


Biological control of sapwood-inhabiting fungi by living bacterial cells of Streptomyces rimosus as a bioprotectant
1992 - IRG/WP 92-1564
The objective of this study is to evaluate the efficacy of antifungal activity of living bacterial cells for the protection of wood against sapwood-inhabiting fungi. The following sapwood-inhabiting fungi were selected: sapstain --Ceratocystis coerulescens, Ceratocystis minor, Ceratocystis pilifera, and Aureobasidum pullulans; mold fungi --Aspergillus niger, Penicillium spp, and Trichoderma spp. L...
S C Croan, T L Highley


Degradation of resin constituents in various wood species by the white rot fungus Bjerkandera sp. strain BOS55
1999 - IRG/WP 99-10301
In previous studies, the white-rot fungus Bjerkandera sp. strain BOS55 was shown to cause extensive degradation of lipophilic extractives (resin) in Scots pine wood. Further research was carried out in order to investigate the ability of Bjerkandera sp. for reducing resinous constituents in various softwood (Douglas fir, larch and spruce) and hardwood species (birch, beech and poplar). The greates...
J Dorado, T A Van Beek, F W Claassen, R Sierra-Alvarez


Effect of fungal degradation on the chemical composition of acetylated beech wood
2003 - IRG/WP 03-40267
This study investigated the impact of fungal attack on the chemical composition of acetylated wood. Beech wood acetylated to different degrees was exposed to decay by the white-rot fungus Trametes versicolor under solid-state fermentation conditions. Laboratory soil-bed assays were also conducted to study the degradation of acetylated wood by soft rot fungi and other soil-inhabiting microorganisms...
H Militz, Dong-won Son, L Gómez-Hernández, R Sierra-Alvarez


A 53-year old field trial to evaluate the performance of a range of chemical treatments on eucalypt poles
1989 - IRG/WP 3526
Hardwood pole stubs of Eucalyptus maculata, Eucalyptus pilularis, Eucalyptus saligna and Eucalyptus paniculata were examined for termite attack and fungal decay after 53 years in ground contact. The trial compared eight different chemical treatments with untreated pole stubs of the four species investigated. Untreated Eucalyptus paniculata, a Class I durability species, performed particularly well...
R S Johnstone, R A Eaton


Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston


Laboratory evaluation of AC 217,300 as a termiticidal dust
1983 - IRG/WP 3247
Laboratory bioassays are described with the amidinohydrazone, AC217,300, a candidate termiticide to replace arsenic trioxide in termite control. When used as a dust and topically applied, AC217,300 was toxic to Coptotermes acinaciformis and Mastotermes darwiniensis. Although arsenic trioxide dust causes faster mortality in Coptotermes acinaciformis than AC217,300 dust, the latter has lower mammali...
J R J French, P J Robinson


Effectiveness of wood preservatives and treatments against marine borers in Philippine waters
1976 - IRG/WP 416
A 5-year exposure test was conducted on the effectiveness of wood preservatives and treatments against marine borers in Philippine waters. Air-dried heartwood samples of apitong (Dipterocarpus grandiflorus) 76.2 x 88.9 x 609.6 mm³ (3 x 3.5 x 24 in³) in size were pressure treated with coal tar creosote and two types of CCA (copper/chrome/arsenic) and CuCZA (copperized chromated zinc arsenate) wat...
F R Siriban, M G Laxamana, P G Mata


Efficacy of Avermectin B1 dust and bait formulations in new simulated and accelerated field tests
1985 - IRG/WP 1257
Avermectin B1 on a silica carrier dust was used in dust and bait formulations whose efficacy against Reticulitermes flavipes was assessed in new simulated and accelerated field tests. A 0.5 mg avermectin/mg dust and a bait with 50 ppm avermectin in paper pulp sandwiched between pieces of corrugated boxboard caused nearly complete mortality in bioassays and suppression of foraging in field tests. T...
G R Esenther


IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...
Anonymous


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


Collaborative soft rot tests: Specific gravity loss resulting from soft rot
1973 - IRG/WP 227
It was proposed at the 5th meeting of Working Group II of the IRG in June 1973 in Lahti, Finland, that the specific gravity (swollen volume basis) of test blocks used in the IRG Collaborative Soft Rot Tests should be determined on all the blocks at the completion of the exposure period. Specific gravity determined on the basis of the oven dry weight and water swollen volume was selected because (1...
C R Levy


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Leaching tests on CCA-treated wood using inorganic salt solutions
1984 - IRG/WP 3310
Pinus radiata sapwood treated to approximately 10 kg/m³ with Tanalith NCA or Tanalith C-type CCA preservatives was ground to a fine powder and samples were then leached with solutions of calcium chloride, calcium nitrate, magnesium nitrate, or a mixture of potassium di-hydrogen orthophosphate and di-potassium hydrogen orthophosphate, at 0.03M-1.00M solution concentrations. Leached wood samples we...
D V Plackett


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


Methods of testing anti-stain chemicals for protecting sawn timber during storage and transport
1976 - IRG/WP 273
No international standard method for testing anti-stain chemicals for protecting fresh sawn timber exists. The methods used can be divided into three types: a) Rapid screening tests for finding chemicals effective against blue-stain and mould fungi. The chemicals are tested in agar medium, in pieces of filter paper or on small pieces of wood using pure cultures. b) Laboratory tests for evaluating ...
T Vihavainen


Sub-group on Basidiomycete tests: Experimental programme and schedule of participants
1980 - IRG/WP 2145
The objectives of this IRG COLLABORATIVE BASIDIOMYCETE TEST are to compare results and assess reproducibility of a miniaturised wood block toxicity test when undertaken by different workers in different laboratories. The co-operative scientists and institutes are: Dr K Messner from Vienna (Austria); Dr R S Smith from Forintek (Canada); Mr J Hansen from Sadolins (Denmark); Mr B Jensen from Gori (De...
A F Bravery


Production of fungal protoplasts from selected wood-degrading fungi
1991 - IRG/WP 1500
Studies of hyphal morphology and the effects of various chemicals on growth are often difficult to perform on filamentous fungi because of the difficulty of observing the protoplasm through the rigid hyphae wall and because most activity occurs in a limited region near the hyphal tip. As an alternative, hyphae can be reacted with certain cell wall degrading enzymes to remove the cell wall to produ...
C Rui, J J Morrell


Upgrading the fungal resistance of OSB
1999 - IRG/WP 99-40138
There is a perception that oriented strand board (OSB) is less resistant to fungl than plywood under conditions of moderate exposure to moisture. Douglas fir-faced plywood (DFP) has been suggested as a benchmark for acceptable durability under such conditions. This project was initiated to determine the minimum level of low-toxicity chemical treatment needed to upgrade the fungal resistance of OSB...
P I Morris, J E Clark, D Minchin, R Wellwood


Decay rates and strength and stiffness loss in foundation beams
1992 - IRG/WP 92-1563
The TNO Centre for Timber Research has executed an extensive research programme into the rate of decay in foundation beams, as a result of lowering of ground water tables. The aim of the research was to develop a method, predicting the decrease in strength and stiffness in beams, due to wood decay during drytime of foundation beams. With the calculated extremes in decay, the damage caused by local...
P Esser, H S Buitenkamp


Influence of fungal exposure on the redistribution of copper in treated spruce wood
2002 - IRG/WP 02-10450
The redistribution of copper in treated wood after exposure to basidiomycete decay fungi is described. The micro-distribution of copper in copper(II) sulphate or copper(II) octanoate/ethanolamine treated Norway spruce wood before and after exposure to 3 different wood decay fungi was studied using transmission electron microscopy with X-ray microanalysis. The copper content of the mycelium and the...
M Humar, F Pohleven, R J Murphy, D J Dickinson, I Moris, M Zupancic, P Kalan, M Petric