Fun with Soil Block Jars: Teaching fungal wood decay in the classroom
2006 - IRG/WP 06-10574
In this world of increasing complexity and technological advancements, it is ever more important to raise scientifically literate children. The National Science Foundation Teaching Fellowship Program (NSF GK-12) at the University of Maine provides an opportunity for advanced graduate students in science, mathematics and engineering to bring their knowledge, as well as the latest equipment, to stud...
C Howell, L Gott, B Meehan


Comparative studies of natural durability of Japanese cedar (Cryptomeria japonica D. Don) among the geographic cultivates
2006 - IRG/WP 06-10592
Variation of natural durability of Japanese cedar (Cryptomeria japonica D. Don) (also known as Sugi) was investigated by accelerated tests for decay (Fomitopsis palustris (Berk. et Curt.) Murr.) and termite (Reticulitermes speratus Kolbe) attacks on 13 clones of Sugi trees from Kyushu-Okinawa Region (Fukuka, Ooita, Saga, Miyazaki, Kagoshima). For this purpose, 57 twenty-five years old Sugi trees o...
I Usta, K Takata, S Doi


Investigation on a Wood Decay Biomarker
2006 - IRG/WP 06-20336
HPLC evolution of beech wood extractives was investigated with or without exposure to Coriolus versicolor during one month. The nature and the quantity of extracts depends on the extraction conditions, but were also strongly influenced by the wood drying temperature and time leading to an important modification for higher drying temperature. After two weeks of exposure to Coriolus versicolor, resu...
S Mounguengui, S Dumarçay, P Gérardin


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


Laboratory methods for assessing the resistance of wood plastic composites to fungal attack.
2006 - IRG/WP 06-20340
Wood plastic composites (WPC’s) have many attractive material features including dimensional stability and resistance to moisture, but the wood in these materials remains susceptible to fungal attack. Assessing WPC decay resistance in laboratory trials has proven difficult because the slow moisture sorption characteristics of this material do not allow for sufficient fungal attack over the trad...
J J Morrell


Testing durability of treated wood according to EN 252. Interpretation of data from Nordic test fields
2006 - IRG/WP 06-20341
To evaluate the effectiveness of new wood preservatives intended for treated wood in ground use there is a European standard, EN 252. The test shall run for five years before any formal interpretation of the results can be made. Due to environmental concerns, the use of wood preservatives based on copper, chromium and arsenic (CCA) has been restricted in recent years. As a consequence of restrict...
M L Edlund, F G Evans, K Henriksen, T Nilsson


L-joint based testing for service life prediction of exterior plywood in out of ground contact conditions
2006 - IRG/WP 06-20342
Good biological performance of several plywood types in exterior conditions is most probably related to altered wood moisture behaviour compared to solid wood. Therefore a test set up was developed, using EN 330 L-joint testing methodology, to facilitate differentiation of plywood for exterior applications. The proposed test set up is an adaptation of an accelerated L-joint method introduced by V...
J De Smet, I De Windt, J Van Acker


Testing biological durability of wood-plastic composites
2006 - IRG/WP 06-20347
Testing biological durability is inherently different for wood-plastic composites (WPC) compared to solid timber. However there is clearly a need for more information on the durability of WPC’s, on the effect of decay on the material properties of WPC’s and on methods for assessing decay of WPC’s. For the emerging European WPC market there has been some discussions on how to work on these to...
J Van Acker


Standard Test Methods for Wood Preservatives by Laboratory Agar-Block Test
2006 - IRG/WP 06-20350
Wood is one of the most valuable and versatile resources for all sorts of constructional purposes. But timber in its various forms is subjected to several types of deterioration. This standard lays down the method for the laboratory determination of threshold value of wood preservatives against fungi. Most chemicals are initially tested for their ability to control decay fungi in agar-block tests....
P K Sarker, M A Rahman, M R Bulbul, T Das, G N M Ilias


Resistance of DMDHEU-treated pine wood against termite and fungi attack in field testing according to EN 252. Results after 30 months
2006 - IRG/WP 06-40354
The aim of this study was to determine the effectiveness against decay and termite attack of pine sapwood treated with pure and modified DMDHEU in a field test according to European Standard EN 252. Some of the treatments tested were able to increase, within the period of the test reported (30 months), the resistance of the wood both to micro-organisms and termites. The curing process seems to be ...
S Schaffert, L Nunes, A Krause, H Militz


Biological Protection of Composite Panel from Moulds and Decay
2007 - IRG/WP 07-10612
Composite panels, such as oriented strand board (OSB), are widely used in house construction in North America. These structural panels are normally made of non-durable wood species and are susceptible to moulds and decay when exposed to wet conditions. Building envelope failures due to moulds, decay or poor construction practices can negatively impact the image of wood. To ensure durability of com...
Dian-Qing Yang, Xiang-Ming Wang, Hui Wan


Current state of world standardization in the toxicometric methods for testing of wood preservatives
2007 - IRG/WP 07-20354
The paper presents an outline of the history of forming standardized toxicometric methods for testing of wood preservatives in the world during last 100 years. Numerous studies resulted in three main methods which are currently used for official and basis assessment of biocides: - agar-block method in Europe (EN 113); - soil-block method in the USA and Pacific countries (ASTM D 1413); - modifi...
J Wazny


Detecting fungal DNA in treated and non-treated wood
2007 - IRG/WP 07-10621
Isolating fungi from wood has long involved culturing on selective media followed by identification using various keys. This process can be cumbersome, costly, and, most importantly, not always capable of detecting all of the fungi present. The recent development of molecular methods for isolation and identification of fungi has created tremendous opportunities for expanding our knowledge of the...
C Freitag, M Freitag, J Morrell


Accelerated Above-ground Testing of Wood Preservatives
2007 - IRG/WP 07-20358
The Canadian wood preservation industry is interested the introduction of new preservative formulations, some of which are intended only for above ground uses. Canada’s Pest Management Regulatory Agency requires data from field tests under Canadian conditions but these can take many years to generate results. Forintek has therefore developed an accelerated above ground test, under contract to a ...
P I Morris, S McFarling


Effect of fungal attack on maximum load capacity of simulated wall assemblies
2007 - IRG/WP 07-20363
The effects of moisture intrusion and fungal attack on the maximum load capacity of nailed assemblies was investigated using one white and one brown rot fungus against 4 material combinations over a 20 week period. Wetting significantly reduced the maximum load capacity of all four material combinations, while wetting and autoclaving only affected the OSB sheathing/spruce stud. The white rot fung...
N Melencion, J J Morrell


Lyctine susceptibility testing and dealing with rarely susceptible hardwood species
2007 - IRG/WP 07-10607
This study examined the lyctine susceptibility of 16 timber species or hybrids. Several of the timbers have been placed previously in a ‘rarely susceptible’ category, but for standards and compliance purposes, such in-between ratings are not acceptable. Timber specimens were spot tested for starch content, and exposed to three species of lyctine beetles in an insectary. New criteria were devel...
L J Cookson, J Carr, N Chew, J W Creffield


Growth and succession of mould on commercial paint systems in two field sites
2007 - IRG/WP 07-30421
Discolouring fungi reduce the service life of coated wooden claddings in façades and increase the total cost of ownership due to shorter maintenance intervals. It is of major importance to find paint systems for wood which are durable and have a high resistance to mould growth. A total of 15 paint systems from 9 different manufacturers were exposed on two field sites, Sørkedalen and Birkenes, ...
L Ross Gobakken, K M Jenssen


Durability of some alternatives to preservative-treated wood. Progress report 2: Results from field tests after 5 years’exposure
2007 - IRG/WP 07-30442
A number of alternatives to preservative-treated wood have been tested according to EN 252 (stake test) and a specially designed ground-proximity field test, the latter in Sweden as well as in Hawaii, USA. Seven untreated wood species and four alternative wood treatments labelled as environmentally friendly (acetylation, linseed oil, heat treatment, vinyl polymer) were included in the study. Four ...
M-L Edlund, J Jermer


Detection of Anti-Fungal Sapwood Extractives in Non-Durable Scots Pine (Pinus sylvestris), Rubberwood (Hevea brasiliensis) and Jelutong (Dyera costulata)
2007 - IRG/WP 07-10634
A general laboratory bioassay method of Woodward and Pearce (1985) was adopted to detect anti-fungal activity of sapwood or heartwood extractives of 5 Malaysian hardwoods [dark red meranti heartwood (Shorea spp.), red balau heartwood (Shorea spp.), kulim heartwood (Scorodocarpus borneensis), jelutong sapwood (Dyera costulata) and rubberwood sapwood (Hevea brasiliensis), including the temperate Pin...
A H H Wong, R B Pearce


A step towards a better understanding of fungal colonization of modified wood - QRT-PCR studies
2008 - IRG/WP 08-10653
The area of wood protection is in a period of change. New wood protection systems have been developed while their mode of action remains insufficiently understood. The development of molecular methods provides potential tools to investigate the interaction between modified wood and decay fungi. One small step to tackle some of the unsolved questions about the mode of action of modified wood is tak...
G Alfredsen, A Pilgård, A Hietala


Validity of above ground testing according to ENV 12037
2008 - IRG/WP 08-20379
The standard ENV 12037 for testing of treated and untreated wood (lap-joint) exposed above ground was issued in 1996 by The European Committee for Standardization. A draft for the development of the standard was presented by CEN-TC 38/WG 25/DOC N 076 in 2002. For a test to become valid the median rating of decay for untreated control replicates (Scots pine sapwood) must be equal or greater than ...
Ö Bergman, U Råberg, N Terziev


Development of a Weatherometer to Accelerate the Surface Checking of Wood
2008 - IRG/WP 08-20388
There is significant interest in developing preservatives that are better at preventing wood from checking. Currently, however, there is no accepted test methodology for accelerating the development of checks in wood samples so information on the effectiveness of treatments at restricting checking can be obtained more quickly. This paper describes the development of a new type of weatherometer (Ac...
R Ratu, P D Evans


Effect of amphiphilic antioxidant alkyl ammonium ascorbate on inhibition of fungal growth: Application to wood preservatives formulation
2008 - IRG/WP 08-30466
Amphiphilic surfactants were synthesized from ascorbic acid and different fatty amines and evaluated for formulation of wood preservation products. Characterization of physicochemical properties of the new compounds indicated classical behavior of cationic surfactants. Antioxidant properties, estimated using methyl linoleate oxidation inhibition method, were similar to that of ascorbic acid teste...
C Gérardin , T Koumbi Mounanga, P Gérardin


Improvement of the Fungal Resistance of Japanese Cedar by the ThermoWood Process
2008 - IRG/WP 08-40422
The effect of the ThermoWood Process on sapwood of the Japanese cedar, Cryptomeria japonica, was investigated. Seven matched specimens were cut from a sapwood board of Japanese cedar and subjected to thermal treatments according to the ThermoWood Process. The decay resistance and chemical and physical properties of the treated specimens and untreated specimen were investigated. The decay test wa...
I Momohara, T Morita, S Shouho, A Yamaguchi


The Effects of Solar Radiation on the Fungal Colonization and Color of Weathered Wood
2008 - IRG/WP 08-10676
Solar radiation rapidly depolymerizes lignin at wood surfaces exposed outdoors producing a suite of low molecular weight aromatic compounds within weathered wood. Fungi colonizing weathered wood are able to metabolize these aromatic compounds, and many of them also contain high levels of melanin to protect themselves from the harmful effects of UV radiation. Both of these adaptations suggest that ...