IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1432 documents. Displaying 25 entries per page.


Formosan Subterranean Termite Resistance to Heat Treatment of Scots Pine and Norway Spruce
2003 - IRG/WP 03-40264
New challenges to the durability of wood building materials have arisen in the U.S. The Formosan subterranean termite (Coptotermes formosanus Shiraki) now infests sizable portions of the U.S. south and their range is extending. Heat treatments offer a unique opportunity for wood-based composites because many of the process techniques already employ various thermal applications and could be easil...
W R Smith, A O Rapp, C R Welzbacher, J E Winandy


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


Selecting fumigants for treatment of internal decay in wood
1986 - IRG/WP 3370
A number of potential fumigants were screened with respect to their toxicity to decay fungi, (Poria carbonica, and Lentinus lepideus) and their sorption characteristics on Douglas Fir (Pseudotsuga menziesii Mirb. Franco) wood. Wafers of infected wood were exposed to different fumigant concentrations for various times then cultured to determine viability. The lethal concentration X time (ct) factor...
P A Cooper


Collaborative soft rot tests: Specific gravity loss resulting from soft rot
1973 - IRG/WP 227
It was proposed at the 5th meeting of Working Group II of the IRG in June 1973 in Lahti, Finland, that the specific gravity (swollen volume basis) of test blocks used in the IRG Collaborative Soft Rot Tests should be determined on all the blocks at the completion of the exposure period. Specific gravity determined on the basis of the oven dry weight and water swollen volume was selected because (1...
C R Levy


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


Effect of humidity and temperature on fastener withdrawal resistance from CCA and ACZA treated Douglas-fir
2000 - IRG/WP 00-20209
The effects of preservative treatment on fastener withdrawal was investigated in Douglas-fir lumber conditioned to two moisture regimes. In general, conditioning samples to 19% moisture content produced more substantial changes in withdrawal resistance of galvanized fasteners than did conditioning to 12%. Treatment had little or no effect on withdrawal resistance of stainless steel fasteners. With...
Sung-Mo Kang, J J Morrell


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


Pretreatment decay in poles of Pinus sylvestris
1987 - IRG/WP 1329
Storage damage by blue stain and decay in poles before impregnation has been increasingly observed during recent years and there have been reports that salt-impregnated poles today are of lower quality because of incipient decay being increasingly common. The attacks may have started at the time of cutting and then continued during the period of seasoning at the plant, which could be as long as tw...
H Lundström, M-L Edlund


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Antagonism of Gliocladium virens against wood decay fungi
1995 - IRG/WP 95-10102
Antagonistic abilities of a commercial biofungicide, Gliocladium virens (GL-21, Grace) were evaluated against three white-rot fungi, Trametes versicolor, Phlebia brevispora, Irpex lacteus, and three brown-rot fungi, Postia placenta, Neolentinus lepideus, Gloeophyllum trabeum. In dual culture of Gliocladium virens and wood decay fungi, Gliocladium virens rapidly overgrow the decay fungi and killed ...
T L Highley, L Ferge


Biocidal property of the phenolic fraction of ethanol extractives of Hopea parviflora heartwood
1993 - IRG/WP 93-30003
Natural resistance of some species of timber to fungal decay and insect damage (particularly termite) is ascribed toxic nature and quantity of certain chemical substances present in the cell wall of heartwood. These chemical substances generally known to be Phenolic and Polyphenolic compounds (Rao 1982). Earlier investigations on extractives were mainly in relation to resistance of timber to decay...
R V Krishnan, K S Theagarajan, H S Ananthapadmanabha, M Nagaraja Sharma, V V Prabhu, H C Nagaveni


Leaching tests on CCA-treated wood using inorganic salt solutions
1984 - IRG/WP 3310
Pinus radiata sapwood treated to approximately 10 kg/m³ with Tanalith NCA or Tanalith C-type CCA preservatives was ground to a fine powder and samples were then leached with solutions of calcium chloride, calcium nitrate, magnesium nitrate, or a mixture of potassium di-hydrogen orthophosphate and di-potassium hydrogen orthophosphate, at 0.03M-1.00M solution concentrations. Leached wood samples we...
D V Plackett


Antagonistic effects of Dacrymyces stillatus against growth of other fungi
1991 - IRG/WP 2363
The antagonistic effects in dual cultures on malt extract agar of 5 wood decay fungi and the antagonistic effects of Dacrymyces stillatus against 1 mould fungus and 1 blue stain fungus were determined. Dacrymyces stillatus was the only fungus which exhibited clear antagonistic effects. The effects of Dacrymyces stillatus against the different test fungi varied however to a great extent. Dacrymyces...
J Bjurman


A non-destructive testing technique for wood poles
1987 - IRG/WP 2293
A method has been developed to evaluate the stiffness and condition of a wood pole based on structural dynamics. This paper describes the results of tests performed on nearly 200 wood utility poles across Western Canada. A high correlation exists between the dynamic non-destructive test and direct mechanical tests. The need for an accurate non-destructive testing technique is demonstrated by the f...
W M Murphy, D E Franklin, R A Palylyk


A comparison of fatty acid and molecular profiles for identification of wood colonizing basidiomycota
2003 - IRG/WP 03-20278
Two methods that are currently being employed to detect and identify wood decay fungi are Fatty Acid Methyl Ester (FAME) analysis and Restriction Fragment Length Polymorphism (RFLP) analysis. A FAME library and RFLP library for 9 species and up to 10 strains within each species have been developed. The profiles generated by these methods have been compared for each species and strain to test for...
T C McElroy, L Prewitt, S V Diehl


The control and pretreatment decay in air seasoning Scots and Corsican pine poles in England
1990 - IRG/WP 1451
Previous work clearly showed that air-seasoned, British grown Scots and Corsican pine poles are subject to serious pretreatment decay. In order to control these infections a range of pretreatments are currently being investigated. One series of treatments is designed not only to control decay but also allow the development of mould and stain fungi in order to achieve the desired increases in poros...
D J Dickinson, A R Zahora, A P Dodson


Production of fungal protoplasts from selected wood-degrading fungi
1991 - IRG/WP 1500
Studies of hyphal morphology and the effects of various chemicals on growth are often difficult to perform on filamentous fungi because of the difficulty of observing the protoplasm through the rigid hyphae wall and because most activity occurs in a limited region near the hyphal tip. As an alternative, hyphae can be reacted with certain cell wall degrading enzymes to remove the cell wall to produ...
C Rui, J J Morrell


Chitin synthetase activity in cellular fractions of wood-decay fungi
1992 - IRG/WP 92-1524
This study was an attempt to explain the variability of in vivo sensitivity of wood decay fungi to the chitin synthetase (CS) inhibitor, polyoxin, by comparing CS distribution in cellular fractions. The five species studied were the brown-rot fungi Coniophora puteana, Gloeophyllum trabeum, Fibuloporia vaillantii, and the white-rot fungi Schizophyllum commune and Ganoderma applanatum. The CS activi...
B R Johnson, S C Croan, B Illman


Decay rates and strength and stiffness loss in foundation beams
1992 - IRG/WP 92-1563
The TNO Centre for Timber Research has executed an extensive research programme into the rate of decay in foundation beams, as a result of lowering of ground water tables. The aim of the research was to develop a method, predicting the decrease in strength and stiffness in beams, due to wood decay during drytime of foundation beams. With the calculated extremes in decay, the damage caused by local...
P Esser, H S Buitenkamp


Influence of fungal exposure on the redistribution of copper in treated spruce wood
2002 - IRG/WP 02-10450
The redistribution of copper in treated wood after exposure to basidiomycete decay fungi is described. The micro-distribution of copper in copper(II) sulphate or copper(II) octanoate/ethanolamine treated Norway spruce wood before and after exposure to 3 different wood decay fungi was studied using transmission electron microscopy with X-ray microanalysis. The copper content of the mycelium and the...
M Humar, F Pohleven, R J Murphy, D J Dickinson, I Moris, M Zupancic, P Kalan, M Petric


Evaluation of fungi isolated from the galleries of the striped ambrosia beetle Xyloterus lineatus (Ol.) (Col., Scolytidae)
1995 - IRG/WP 95-10092
Fungi from the galleries of the striped ambrosia beetle Xyloterus lineatus (Trypodendron lineatum) (Ol.) found in spruce logs were studied. The following fungi were isolated and identified: Trichoderma harzianum Rifai, the yeast Pichia anomale Hansen (Kurzman), the blue-stain fungus Ceratocystis piceae (graphium) (Münch) Bakshi and a fungus closely similar to Ceratocystis araucariae (anamorph). T...
G Babuder,F Pohleven


Questionnaire relating to the occurrence, prevention and repair of Dry Rot attacks in buildings
1989 - IRG/WP 1418
Dry Rot attack in buildings has become an increasing problem in Denmark. The reason is that old multi-storey houses from about 1890-1920 are being renovated and modernised and connected to this well-hidden Dry Rot attacks are detected. The traditional methods for repair used in Denmark are very expensive but with a high degree of confidence when done carefully. There is a big need for development ...
A P Koch


A comparison analysis of eight strains of Serpula lacrymans (Schum. ex Fr.) S.F. Gray
1991 - IRG/WP 2362
Investigations were previously carried out to compare eight strains of Serpula lacrymans (Schum. ex Fr.) S.F. Gray (some used in various countries as standard test strains): FPRL 12C (England), FPRL 12E (Germany), Warsaw III (Poland), HFP 7802 (Japan), DFP 16508, 16509, 16521 and 16522 (Australia). Studies included growth rate and dry mass of mycelium, decay capacity, reduction of compression stre...
J Wazny, J D Thornton


Antagonism of Scytalidium lignicola against wood decay fungi
1989 - IRG/WP 1392
Antagonistic abilities of Scytalidium lignicola against white- and brown-rot wood decay fungi were evaluated. Scytalidium lignicola did not produce inhibition zones but overgrew the decay fungi on a malt-agar medium and in most cases killed them. Pretreatment of Douglas-fir and Southern pine blocks with Scytalidium lignicola prevented decay. Blocks that were heated or treated with propylene oxide ...
T L Highley


Interactions between soft rot fungi and CCA preservatives in Betula verrucosa
1988 - IRG/WP 1367
Ultrastructural investigations were carried out to obtain information on the cell wall distribution of CCA elements during soft rot decay of 4% K33 CCA preservative treated birch (Betula verrucosa) wood. TEM observations on fibres at various stages of S2 cavity formation by mutabilis showed a distinct pattern of electron dense materials to occur within the S2 cell wall region. These materials (gra...
G F Daniel, T Nilsson


Previous Page | Next Page