IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1432 documents. Displaying 25 entries per page.


Protection of buildings, other structures and materials in ground contact from attack by subterranean termites with a physical barrier - a fine mesh of high grade stainless stee
1993 - IRG/WP 93-10014
A new type of physical barrier for the prevention of attack by subterranean termites on buildings, other structures and materials in ground contact - a fine mesh of highalloy (originally 304, now 316) stainless steel - has recently been developed and patented worldwide by industry in Australia. The termite resistance of the material was assessed by CSIRO in laboratory and field trials. In the labo...
M Lenz, S Runko


Regulation of hyphal sheath formation iron-chelator production by the brown rot fungi Gloeophyllum trabeum and Postia placenta
1994 - IRG/WP 94-10074
Hyphal sheath formation and iron-chelator production by liquid cultures of the brown rot fungi Gloeophyllum trabeum and Postia placenta were monitored over time. The effects of incubation at various temperatures, pH's and concentrations of iron, manganese and nitrogen were determined. Hyphal sheath production was observed microscopically and quantified with JAVA video analysis. The hyphal...
Y Chen, J Jellison


Laboratory Evaluation of the Formosan Subterranean Termite Resistance of Borate-treated Rubberwood Chipboard
2004 - IRG/WP 04-30359
Both no-choice and two-choice 4-week AWPA laboratory tests were performed to evaluate the resistance of borate-treated rubberwood (Hevea brasiliensis) chipboard prepared from a commercial mill run, against the Formosan subterranean termite Coptotermes formosanus. Boric acid (technical granular) was incorporated into the boards during manufacture to achieve loadings of 1.0% or 1.1% boric acid equiv...
A H H Wong, J K Grace


Efficacy of fumigants in the eradication of decay fungi implanted in southern pine timbers
1986 - IRG/WP 3365
Southern pine timbers (15.2 cm x 15.2 cm x 4.26 m) were fumigated at midlength to evaluate the effectiveness of the fumigants chloropicrin, Vapam, Diazomet, Busan 40, Vanicide 51, Vanicide TH, sodium bisulfite, and ethanolamine in eradication of decay fungi. The fumigants were introduced into 2.54 cm holes which were closed immediately with rubber stoppers. Movement and persistence of lethal conce...
T L Highley, W E Eslyn


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Nasutitermes exitiosus and wood-rotting fungi in Eucalyptus regnans, E. acmenioides, E. wandoo, and E. marginata: force-feeding, laboratory study
1985 - IRG/WP 1231
Under a force-feeding regime, the termitid Nasutitermes exitiosus was fed on four eucalypt timbers infested with several fungal species to investigate the influence of such fungus-infested timbers on mass of wood lost, termite biomass, fat content and water content. The results showed that wood mass losses were markedly affected by species of fungi and timber. The interaction of fungi and timbers ...
D B A Ruyooka


Properties of cellulose degraded by the brown rot fungus, Postia placenta
1988 - IRG/WP 1350
To gain further understanding of the nature of the cellulose depolymerizing agent or agents of brown-rot fungi, brown-rotted cellulose was chemically and physically characterized. Various culture conditions, such as low nitrogen and elevated oxygen levels, did not induce degradation of cellulose by Postia placenta in liquid cultures. Therefore, brown-rotted cellulose for analysis was prepared by a...
T L Highley, R E Ibach, T K Kirk


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


Biological control of wood decay
1992 - IRG/WP 92-1531
This paper provides a general discussion of the principles underlying the concept of using biological control agents for the protection of wooden materials from decay. The rationale for the current upsurge in interest in biological control is discussed and a critical appraisal of the technology compared with the use of chemical wood preservatives is included. The advantages and limitations associa...
A Bruce


Breakdown of cellulose derivatives by cellulolytic enzymes. I. Action of fungal ß-glucosidases toward substituted PNP ß-D-glucopyranosides
1998 - IRG/WP 98-10281
The action of fungal ß-glucosidases on the methyl derivatives of p-nitrophenyl (PNP) ß-D-glucopyranoside, which were regioselectively substituted at 0-2, 0-3, 0-4 and 0-6 positions was studied. Several ß-glucosidases from brown-rot, white-rot, and soft-rot fungi and almond were used for the study. These ß-glucosidases did not act on the 2, 3, and 4-0-methyl derivatives, while the 6-0-methyl on...
T Nishimura, I Momohara, M Ishihara


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Investigation of extracellular mucilaginous material in some wood decay fungi
1996 - IRG/WP 96-10188
The external morphology of the extracellular mucilagenous material (ECM) produced by Coriolus versicolor and Coniophora puteana during colonization of Scots pine and beech was studies using SEM. Specimens were examined in the frozen hydrated, freeze-dried and critical point dried state. All technics produced artefacts but the ECM was best preserved when examined the frozen hydated state. Critical ...
A R Abu, D J Dickinson, R J Murphy


Remedial treatment of creosoted railway sleepers of redwood by selective application of boric acid
1980 - IRG/WP 3134
An ideal preservative for remedial treatment must primarily be characterized by two requirements. First, it must have an ability to diffuse and distribut evenly into the wood and secondly, it must be fixed properly so that it does not leach out too fast. However, these two characteristics conflict with each other, and the choice of preservative must of necessity be a compromise. Wood preservatives...
C Bechgaard, L Borup, B Henningsson, J Jermer


The suitability of isothiazolone microemulsions as long term wood preservatives
1997 - IRG/WP 97-30150
Microemulsion formulations of 4,5 dichloro-2-n-octyl-4-isothiazolin-3-one were investigated to determine the leaching potential of these formulation types as well as their efficacy against decay fungi. These patented low leaching formulations exhibited good anti fungal efficacy in standard tests combined with minimal leaching of the active ingredient from the wood. The data suggests that the excel...
B M Hegarty, Bing Yu, L E Leightley


Evaluation of the insecticidal efficacy of deltamethrin and the fungicidal efficacy of its association with TCMTB + MBT in the field of wood preservation
1986 - IRG/WP 1289 E
Deltamethrin possesses many advantages for the insecticidal protection of wood: relatively low toxicity, very reduced evaporation, very prolonged retention in the wood, very slight leaching after having penetrated the wood, and absence of odour. Its association with other active agents or solvents is being studied with regard to chemical compatibility. Compatibility studies have proved positive fo...
J S Duguet


Artificial weathering exposure as an alternative for standard ageing according to EN 84 (leaching) and EN 73 (evaporation)
2002 - IRG/WP 02-20254
In order to verify potential weaknesses of wood preservatives fungal tests are carried out after ageing of wood preservative treated test blocks. The European standard EN 599 as a framework for efficacy assessment of wood preservatives includes the use of two ageing methods prior to fungal testing, namely a leaching method (EN 84) and an evaporation method (EN 73). The European research project "F...
J Van Acker, M Grinda, D J Dickinson


Termite resistance of twenty-eight Indonesian timbers
1982 - IRG/WP 1150
A comparative study of termite resistance of 28 Indonesian wood species has been conducted using small samples measuring 5 x 10 x 20 mm³. The drywood termite Cryptotermes cynocephallus (Kalotermitidae) and the subterranean termite Coptotermes curvignathus (Rhinotermitidae) were used in the study. A resistance classification was derived on the basis of cluster analysis. The result reveals that Alb...
Nana Supriana, P E Howse


The nature of osmiophilic particles and their distribution during different stages of brown and white rot decay
1983 - IRG/WP 1213
The distribution of osmiophilic particles during the course of brown and white rot decay was investigated by applying transmission electron microscopic (TEM) methods. It was found that it correlates with the brown and white rot pattern.The osmiophilic particles are produced by the fungus and are supposed to be wood rotting enzymes....
K Messner, H Stachelberger


Targeted inhibition of wood decay fungi: degradation of cotton cellulose
1999 - IRG/WP 99-10321
Brown-rot decay is responsible for 80% of the damage and replacement of wood in service. For nearly thirty years, researchers have postulated a one-electron oxidase system combining Fe+2 oxalic acid, and H2O2 in the production of hydroxy radicals which ultimately oxidize cellulose in situ. Recently, researchers have been investigating antioxicants, in combination with biocides (Schultz, et al.,199...
F Green III, T A Kuster


Influence of variable lignin content amongst hardwoods on soft-rot susceptibility and performance of CCA preservative
1982 - IRG/WP 1151
This paper presents the outline of an argument, based on both new and established data, which relates varying lignin content to variation of soft-rot susceptibility between hardwood species and of performance of CCA preservatives in controlling soft-rot. Although more data need to be generated to prove this relationship, sufficient evidence exists for the hypothesis to be given close attention, pa...
J A Butcher, T Nilsson


Effect of moisture and cellulosic substrate on decay of hardwoods by soft-rot fungi
1982 - IRG/WP 2173
The development by Forintek Canada Corp. of standard test procedures for laboratory preservative evaluations using soft-rot fungi was requested by the American Wood Preservers' Association. In Europe, through cooperative studies in the International Research Group on Wood Preservation, several attempts have been made to produce a standard procedure, but variability in results obtained bet...
A Byrne, R S Smith


Proposal for a simple methodology for the evaluation of the preventive effectiveness of protectors applied in superficial treatments against basidiomycetes fungi
1999 - IRG/WP 99-20167
Due to the considerable effect that the relation between the lateral surface and the volume of wood blocks has on superficial treatments, this work has attempted to determine the ideal size which allows to evaluate the effectiveness of a preservative in the shortest possible time. Three wood blocks of different dimensions were tested. In addition, as it is necessary to neutralise the effect of the...
M T De Troya, A Navarrete, F Rubio, M Yuste, C Rodríguez-Borrajo, D Muñoz-Mingarro, F Llinares


Electricity pole treatments - Wedding Bells State Forest. Inspection September 1983
1985 - IRG/WP 3334
A survey to study the extent of soft rot in hardwood poles in N.S.W. was commenced in 1975. The results of the survey, published in 1982, indicated that a number of factors contributed towards soft rot attack on poles in service. A detailed rest on pole treatments and maintenance procedures was established in 1976, at a site in Wedding Bells State Forest near Coffs Harbour. The site selected was k...
R S Johnstone, R H Eldridge


Effect of origin and orientation of Radiata pine substrates on the development of fungal degrade
2000 - IRG/WP 00-30221
The objective of this study was to determine the influence of different radiata pine substrates on colonisation by sapstain fungi. Freshly-cut branch wood, stem wood and sawn lumber were used to prepare test samples with the largest wood surface area showing a transverse, radial or tangential face. Test samples were evaluated against sapstain fungi using a rapid laboratory antisapstain screening m...
B Kreber, D R Eden, C M Chittenden, B Carpenter, J G Van der Waals


Previous Page | Next Page