Assessment of the Inhibition of wood decay fungi by volatile organic compounds identified from Trichoderma spp.
1999 - IRG/WP 99-10302
Previous research identified five volatile organic compounds produced by Trichoderma spp. that may be inhibitory to wood decay fungi. The effects of four of these volatile organic compounds, 2-propanone, 2-methyl-1-butanol, heptanal and octanal were tested over a range of concentrations against four selected wood decay fungi. The fungi were incubated in malt extract broth under appropriate conditi...
S N Humphris, R E Wheatley, A Bruce, C Payne


Bestimmung der pilzwidrigen Wirksamkeit von Holzschutzmitteln gegen Moderfäule-Erreger
1977 - IRG/WP 2125
Ziel der vorliegenden Arbeit war der Vergleich der in verschiedenen Ländern zur Bestimmung der pilzwidrigen Wirksamkeit von Holzschutzmitteln gegen Moderfäule-Erreger angewandten Methoden. Als Vergleichsmaterial dienten drei normierte Methoden: die britische (42), skandinavische (45) und die in der DDR angewendete (47) sowie wichtige, von verschiedenen Fachleuten ausgeführte Arbeiten experiment...
J Wazny


Evaluation of a utility pole inspection procedure
1996 - IRG/WP 96-20084
Methods were developed and are currently being utilized to appraise residual strength of utility poles based on visual assessment of increment cores. Strength tests, mycological descriptions and anatomical analyses were performed on eight utility poles taken out of service and one new (never in service) pole. Samples were obtained from increment cores removed from 6 levels in the pole: 2 feet, gro...
S E Anagnost, C J K Wang


Effect of test site, preservative and wood species on decay type Glenbervie pastoral and radiata pine forest sites
2000 - IRG/WP 00-30248
Pinus radiata stakes were treated with 0.8, 1.2, 1.8, 2.7 and 4.1 kg/m3 of CCA and Fagus sylvatica with 2.7, 4.1 and 6.1 kg/m3 of CCA. Both wood species were also treated with equivalent retentions of a copper plus triazole preservative (CT) (0.89, 1.3, 2 and 3 kg/m3 of copper for pine & 2.5 and 4 for beech) and chlorothalonil plus chlorpyriphos in oil (CC) (1.4, 2.1, 3.2 and 4.8 kg/m3 of chlo...
R N Wakeling


Proposing innovative technologies in the control of dry-wood insects
1985 - IRG/WP 1262
This paper discusses the social-economic problems involved in the biological evaluation of dry-wood insects with particular reference to Nigeria. It also discusses prospects of applying non-conventional methods of control against such insects, integrating these with the conventional preservatives as a control strategy. This discussion follows attempts made to identify the major dry-wood insects in...
M O Akanbi


New boron-based biocides for the protection of wood
2002 - IRG/WP 02-30283
Boric acid and other simple inorganic oxides of boron are amongst the oldest wood preservatives currently in use. Their relatively low toxicity and broad-spectrum activity are just some of their desirable characteristics. The primary disadvantage associated with conventional boron-based preservatives is their lack of permanence in exposed applications. A collaborative project between CSIRO and the...
D G Humphrey, P J Duggan, E M Tyndall, J M Carr, L J Cookson


The relationship between the electrical resistance and fixation of water-borne CCA salts and pressure-treated wood
1991 - IRG/WP 3657
Two investigations at 22°C and 30°C have been carried out. The electrical resistance in the treated wood and chemical analyses of the remaining amount of unfixed copper, chromium and arsenic were investigated. Samples impregnated with water were used as references. To hold the samples moist during the investigation, each sample was wrapped in a polyethylene plastic foil immediately after impregn...
F G Evans, B Nossen


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Aspects of the fungal degradation of quaternary ammonium compounds in liquid culture
1997 - IRG/WP 97-30160
Didecyldimethylammonium chloride (DDAC) is a quaternary ammonium compound (QAC) that has found use as an anti-sapstain preservative for the transportation of softwood lumber from Canada to overseas markets. However, its use is limited by the knowledge that certain mould fungi seem capable of degrading it. The aim of this research was to gain knowledge about the fungal degradation of DDAC. The effe...
J W Dubois, J N R Ruddick


Laboratory trial to identify potential in-forest treatments to control fungal pre-infections of radiata pine logs
2000 - IRG/WP 00-30220
Development of fungal infections of radiata pine logs by wood degrading fungi commences immediately after tree felling. In general, subsequent antisapstain treatments are unable to control fungal degrade on logs where the pre-treatment log storage time exceeds 2-5 days. However, use of an in-forest treatment of logs may be advantageous to log exporters to control fungal pre-infections during the p...
D R Eden, B Kreber, R N Wakeling, J G Van der Waals, C M Chittenden


Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel


Water-Borne Copper Naphthenate: An Emerging Wood Preservative
2002 - IRG/WP 02-30280
Waterborne copper naphthenate (WB Cu-N) was used to treat southern yellow pine (Pinus spp) and red maple (Acer rubrum) stakes. The treated stakes were exposed in test sites located in Florida, Michigan and Mississippi for 3 to 6 years. Copper Chromium Arsenate (CCA), Ammoniacal Copper Quat (ACQ) and Oil-borne Copper Naphthenate (OB Cu-N) were also used to treat some stakes for comparison. Results...
P Nzokou, D P Kamdem, M H Freeman


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


A dynamic approach to assess the modulus of elasticity in wood decay testing
1998 - IRG/WP 98-20139
In this study, the changes in elastic behaviour and mass losses of different hardwood and softwood species exposed to decay in a laboratory soil tests were assessed. Wood decay was monitored using different assessment methods, namely: mass loss and changes in elastic behaviours (MOE) determination. Elastic changes were determined by static and dynamic methods, for the latter, acoustic technique wa...
L Machek, H Militz, R Sierra-Alvarez


Susceptibility of CCA treated North American hardwoods to Chaetomium globosum decay
1998 - IRG/WP 98-10278
Seven species of hardwood, Beech (Fagus grandifolia), Basswood (Tilia americana), Maple (Acer rubrum), Oak (Quercus rubra), Trembling Aspen (Populus tremuloides), White birch (Betula papyrifera) and Yellow poplar (Liriodendron tulipifera) were vacuum or pressure impregnated with CCA, at four retention levels. The CCA was allowed to fix in the wood at 35°C. Red pine (Pinus resinosa) was also inclu...
U Srinivasan, Y T Ung, P A Cooper


A non-pressure method of protection based on hurdle theory to control the spectrum of internal environmental factors which affect the decay of poles in soil contact
1993 - IRG/WP 93-20005
A field trial was conducted to establish whether superficial barrier linings on poles in soil contact could function as environmental hurdles against the growth of biological agents and thus provide preventative methodology to preclude premature failure of vineyard poles under flood-irrigation. Assessment after 52 weeks exposure to the prevailing conditions and sub-tropical environment showed that...
A A W Baecker


Factors affecting decay rates in a fungus cellar II
1986 - IRG/WP 2259
Tests were initiated to investigate the influence of various factors on the decay rate in a "Fungus Cellar". Birch and pine stakes treated with chromated copper arsenate and didecyldimethyl ammronium chloride, as well as untreated control stakes, were incubated in two soils in a Fungus Cellar test and installed at two field sites for comparative purposes. The visual rating vs actual stake weight l...
P A McKaig


Comparative study of the degradative ability of autochthonous and standardized strains of wood decay fungi
1996 - IRG/WP 96-10178
This study is intended to assess the biomass, the extracellular protein production, and the carbohydrate degradating ability of three standarized (Chaetomium globosum, Trametes versicolor and Gloeophyllum trabeum) and six autochthonous wood decay fungi strains, with unknown degradating effects. The carbohydrate sources used were those that are usually found in wood cells (glucose, galactose, manos...
F Llinares, D Muñoz-Mingarro, J E Garcia de los Rios, M T De Troya, M Yuste, F Rubio, F Alvarez, P Jiménez, C Rodríguez-Borrajo, A M Navarrete


Targeted inhibition of wood decay (Using everything but the kitchen sink)
1997 - IRG/WP 97-10203
Low molecular weight oxidative decay agents have been implicated in the degradation of wood by brown-rot decay as evidenced by chemical analysis of brown-rotted wood and detection of oxalic acid and hydroxy radicals. Fenton chemistry (H2O2 / Fe++) is often proposed as the mechanism for generating hydroxy radicals. Previous authors have shown iron to enhance the brown-rot hydrolysis of wood, while ...
F Green III, T A Kuster, T L Highley


Detection of wood decay fungi in wood using a PCR-based analysis
1998 - IRG/WP 98-10279
We have developed a DNA-based assay to reliably detect brown rot and white rot fungi in wood at different stages of decay. DNA, isolated by a series of CTAB and organic extractions, was amplified by the polymerase chain reaction using published universal primers and basidiomycete-specific primers derived from ribosomal DNA sequences. We have surveyed 7 species of brown rot fungi, 7 species of whit...
C Jasalavich, A Ostrofsky, J Jellison


Aboveground Microbial Decay Test of Biocide Treated and Untreated Wood Exposed to Danish and Humid Tropical Climates
2004 - IRG/WP 04-20306
A co-operative study was initiated to compare the aboveground field decay test of untreated and preservative-treated timbers under Nordic (Danish) and a representative humid tropical (Malaysian) environment according to CEN standard method. Matched specimens of untreated and both preservative-impregnated and surface-treated wood were simultaneously exposed at The Danish Technological Institute (DT...
A H H Wong, N Morsing, K H Henriksen, S Ujang


Screening of the efficacy of tall oils against wood decaying fungi
2004 - IRG/WP 04-30354
Tall oil is a by-product in pulping of resinous wood by the sulphate process. Tall oil contains a complex mixture of wood extractives. Some of these extractives act as natural protection against wood decaying fungi while other serve as nutrition for the fungi. This report describes a screening of the efficacy of four refined tall oils with different chemical composition on wood decaying fungi. ...
G Alfredsen, P O Flæte, A Temiz, M Eikenes, H Militz


Comparative natural resistance of eighty-two timber species to damage by marine borers at Goa (India)
1996 - IRG/WP 96-10139
Natural bioresistance of eighty-two species of Indian timbers to attack by marine wood-borers has been presented based on data collected from test panels exposed in Goa waters (west coast of India) for periods ranging from five to thirteen months. All the timber species, except Artocarpus gomeziana and Pterocarpus santalinus, were completely destroyed within a short period of three to six months. ...
L N Santhakumaran


Termite resistance of Malaysian and exotic woods with plantation potential: Field evaluation
1998 - IRG/WP 98-10289
An in-ground resistance of selected Malaysian and exotic timbers to attack by a representative aggressive subterranean Coptotermes termite was evaluated as part of an on-going collaborative research between the Forest Research Institute of Malaysia and the University of Hawaii on termite control of building timbers under humid tropical conditions. A test site at FRIM, highly susceptible to the sub...
A H H Wong, J K Grace, L H Kirton


Computer-assisted ranking of potential biocontrol fungi based on data from laboratory screening trials
1993 - IRG/WP 93-10023
Forty two fungal isolates were screened for antibiotic activity. In these sceering tests inhibition of target wood decay fungi was expressed as a series of numerical scores for each isolate. These scores, along with values for 5 other charactetistics, were used to assess the isolates. Using selection indices, isolates were judged on the basis of all the characteristics combined and, ranked in orde...