Sapstain development on Jack pine logs in Eastern Canada
2000 - IRG/WP 00-10358
During 1998-99, a study was initiated to investigate the influence of seasons, log types and storage time on the sapstain development on jack pine logs at two sites in Eastern Canada. Jack pine trees (Pinus banksiana) were harvested into whole-tree and cut-to-length logs in spring and in autumn. Sapstain development was examined in these logs at 2 to 4 week intervals after felling. The mean stain ...
Dian-Qing Yang, R Beauregard


Protection of buildings, other structures and materials in ground contact from attack by subterranean termites with a physical barrier - a fine mesh of high grade stainless stee
1993 - IRG/WP 93-10014
A new type of physical barrier for the prevention of attack by subterranean termites on buildings, other structures and materials in ground contact - a fine mesh of highalloy (originally 304, now 316) stainless steel - has recently been developed and patented worldwide by industry in Australia. The termite resistance of the material was assessed by CSIRO in laboratory and field trials. In the labo...
M Lenz, S Runko


Regulation of hyphal sheath formation iron-chelator production by the brown rot fungi Gloeophyllum trabeum and Postia placenta
1994 - IRG/WP 94-10074
Hyphal sheath formation and iron-chelator production by liquid cultures of the brown rot fungi Gloeophyllum trabeum and Postia placenta were monitored over time. The effects of incubation at various temperatures, pH's and concentrations of iron, manganese and nitrogen were determined. Hyphal sheath production was observed microscopically and quantified with JAVA video analysis. The hyphal...
Y Chen, J Jellison


Bacterial degradation of Pinus radiata compression wood
1996 - IRG/WP 96-10153
An inspection of twelve year old, CCA-treated Pinus radiata wood from an industrial cooling tower showed extensive surface decay of wood. Electron microscopic examination of decaying compression wood indicated that compression wood cells were attacked exclusively by bacteria, which were of erosion and tunnelling types. As compared to the normal wood, compression wood appeared to be more resistance...
A P Singh, R N Wakeling


Breakdown of cellulose derivatives by cellulolytic enzymes. I. Action of fungal ß-glucosidases toward substituted PNP ß-D-glucopyranosides
1998 - IRG/WP 98-10281
The action of fungal ß-glucosidases on the methyl derivatives of p-nitrophenyl (PNP) ß-D-glucopyranoside, which were regioselectively substituted at 0-2, 0-3, 0-4 and 0-6 positions was studied. Several ß-glucosidases from brown-rot, white-rot, and soft-rot fungi and almond were used for the study. These ß-glucosidases did not act on the 2, 3, and 4-0-methyl derivatives, while the 6-0-methyl on...
T Nishimura, I Momohara, M Ishihara


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


The suitability of isothiazolone microemulsions as long term wood preservatives
1997 - IRG/WP 97-30150
Microemulsion formulations of 4,5 dichloro-2-n-octyl-4-isothiazolin-3-one were investigated to determine the leaching potential of these formulation types as well as their efficacy against decay fungi. These patented low leaching formulations exhibited good anti fungal efficacy in standard tests combined with minimal leaching of the active ingredient from the wood. The data suggests that the excel...
B M Hegarty, Bing Yu, L E Leightley


Artificial weathering exposure as an alternative for standard ageing according to EN 84 (leaching) and EN 73 (evaporation)
2002 - IRG/WP 02-20254
In order to verify potential weaknesses of wood preservatives fungal tests are carried out after ageing of wood preservative treated test blocks. The European standard EN 599 as a framework for efficacy assessment of wood preservatives includes the use of two ageing methods prior to fungal testing, namely a leaching method (EN 84) and an evaporation method (EN 73). The European research project "F...
J Van Acker, M Grinda, D J Dickinson


Effect of origin and orientation of Radiata pine substrates on the development of fungal degrade
2000 - IRG/WP 00-30221
The objective of this study was to determine the influence of different radiata pine substrates on colonisation by sapstain fungi. Freshly-cut branch wood, stem wood and sawn lumber were used to prepare test samples with the largest wood surface area showing a transverse, radial or tangential face. Test samples were evaluated against sapstain fungi using a rapid laboratory antisapstain screening m...
B Kreber, D R Eden, C M Chittenden, B Carpenter, J G Van der Waals


Practical experiments with Boracol 10 Rh used as a fungicide in the repair process after attack by the dry rot fungus (Serpula lacrymans)
1987 - IRG/WP 3458
The test is carried out in an old house in Nyhavn, Copenhagen. The roof and the walls close to were heavily attacked by dry rot fungus (Serpula lacrymans) because damage to the zinc covering the frontspice were letting in water to the wood and wall construction. An attack by the dry rot fungus is more complicated to repair compared with other wood destroying fungi because beside the damage on wood...
J Bech-Andersen


Make ready of a detection system for insect attack by acoustical method
1996 - IRG/WP 96-10183
A contract CRAFT of European research allowed to build a detector prototype able to diagnose on site the presence of Hylotrupes bajulus and termites, even during the first stages of infestation when no sign of activity is visible. Based on non destructive control technics, the device picks up the acoustical waves emitted by the insects in the wood fibers. The amplification and the filtering of the...
M Hyvernaud, F Wiest, M-M Serment, M Angulo, O Winkel


Natural resistance of twenty-five timber species to marine borer attack in Goa waters (India)
1992 - IRG/WP 92-4178
Natural durability of 25 species of Indian timbers has been discussed, based on data collected from test panels exposed in Goa waters (west coast of India. for a period of 7 months. All the timber species, except Cleistanthus collinus, were heavily destroyed within 7 months on account of the combined attack by Martesia striata (Linnaeus) and Lyrodus pedicellatus (Quatrefages). Cleistanthus collinu...
L N Santhakumaran, G Srimannarayana, K Nagaiah


Effects of air-seasoning on fungal colonization and wood strength of Douglas fir poles
1987 - IRG/WP 1315
Air seasoning economically reduces the moisture content of Douglas fir poles before pressure treatment with preservatives. Advanced decay in poles in service has resulted when decay fungi (Basidiomycetes) colonized poles during air-seasoning and survived the treatment process. These problems have led to recommendations to severely limit this practice. To determine the role of these fungi in peeled...
J J Morrell, M E Corden, R D Graham, B L Kropp, P Przybylowicz, S M Smith, C A Sexton


A study on the effectiveness of didecyldimethylammonium chloride to protect wood from attack by termites
1993 - IRG/WP 93-30009
A laboratory bioassay was conducted on the ability of didecyldimethylammonium chloride (DDAC) to protect Pinus radiata D.Don wood specimens from attack by two of Australia's most economically important species of subterranean termite, Mastotermes darwiniensis Froggatt and Coptotermes acinaciformis (Froggatt). Sapwood specimens of Pinus radiata, treated to achieve nominal retentions of 0.5...
J W Creffield


The influence of staining fungi on the decay resistance of wood treated with alkylammonium compounds
1984 - IRG/WP 3308
Although found to be very effective in laboratory tests, alkylammonium compounds (AAC's) have failed to perform as well in field stake tests. Examination of leachability showed that this was not the cause. The present study investigated the possibility that staining fungi, (which have been observed to rapidly infect the field stakes), degrade the AAC wood preservative. Soil-blocks were tr...
J N R Ruddick


Comparison of the in-ground performance of pigment emulsified creosote (PEC) and high temperature creosote (HTC)
2000 - IRG/WP 00-30217
A long-term field trial was conducted in Australia to compare the in-ground performance of two oil-borne preservative formulations, conventional high temperature creosote (HTC) and a modified creosote formulation, pigment emulsified creosote (PEC). Three retentions (50, 100 and 200 kg/m³) were targeted for each formulation. An additional retention of PEC formulation (308 kg/m³), which contained ...
J W Creffield, H Greaves, N Chew, N K Nguyen


The effects of preservative treatment and exposure to wood degrading fungi on fiber reinforced polymer (FRP) materials used for structural wood reinforcement
2001 - IRG/WP 01-40204
Glass fiber reinforced phenolic (GFRP) composite materials are becoming increasingly accepted for use in the construction industry because they combine advantages of both wood and advanced polymeric materials. Addition of only 1-3% FRP in the tension zone, for example, can typically improve the strength of the hybrid system by 200%. As more applications are found for wood/FRP hybrids, (e.g. lamina...
C Tascioglu, B Goodell


Fungal detoxification of organotin biocides
1985 - IRG/WP 1258
The ability of a range of wood decaying fungi to inactivate bis(tri-n-butyltin) oxide (TnBTO) in the extracellular growth medium, in stationary liquid culture was determined. A distinction between the ability to tolerate the fungicide and to inactivate it was made: the white-rot organism Coriolus versicolor being the most efficient inactivator. In an attempt to determine the extracellular agents r...
P S Belford, D J Dickinson


Possible durability transfer from durable to non durable wood species. The study case of teak wood
2001 - IRG/WP 01-10392
Teakwood is well known for its excellent natural durability, mostly due to its high proportion of extracts. Amongst these extracts, quinones, and more precisely some naphtoquinones (such as lapachol) and anthraquinones (such as tectoquinone) appear to play a crucial role in the resistance to wood decay organisms. At a laboratory scale, sawdust from malaysian teak heartwood has been extracted under...
M-F Thévenon, C Roussel, J-P Haluk


Comparison of the anti-fungal efficacy of Cobra with drill perforation on oscillating pressure treated spruce transmission poles -Laboratory test
1988 - IRG/WP 3469
A laboratory method for measuring the depth of penetration of the fungicidal concentrations effective against basidiomycetes (brown rot) was developed. The tests on CCB oscillating pressure treated spruce transmission poles have shown that the depth of salt penetration can be increased by about 10 mm by a drill perforation before the impregnation. An even better penetration is reached, however, if...
E Graf, B Zgraggen


A study of fungal biodeterioration in unseasoned, packaged hem-fir lumber
1978 - IRG/WP 2116
This study was undertaken to determine the extent of biodeterioration that could occur within British Columbia (BC) prior to the export of packaged Canadian Lumber Standard Hem-Fir (Tsuga heterophylla, Abies amabilis and small amounts of Abies grandis). By examining the anti-stain treatments received by the lumber and identifying and characterizing the organisms responsible for the biodeterioratio...
P W Perrin, A J Cserjesi


Effects of chemicals used for ground-line protection of hardwood poles on termite attack
1988 - IRG/WP 1356
The majority of chemicals formulatet to protect the groundline of hardwood poles in Australia have been fungicides. Nine products were tested against Coptotermes lacteus attack to determine their value in preventing attack by subterranean termites. Results indicated that Busan, high temperature creosote, pigment emulsified creosote, copper naphthenate gel and "Blue 7" had a repellent effect on Cop...
R S Johnstone, R H Eldridge


The natural durability of five Indonesian timber species against marine borers - A field test in Indonesia
1981 - IRG/WP 474
This paper presents results of a natural durability field test using five species of Indonesian timbers against marine borers. An attempt is also made to assess any difference in durability between the lower and upper part of the trunks. Results of marine fungal identification, soft-rot assessment, and marine-borer assessment of CCA-treated test blocks will be reported in separate papers...
Suhirman, R A Eaton


Resistance of acrylic paints on wood against growth of the rot fungus Dacrymyces stillatus
1990 - IRG/WP 2345
In the last few years the presence of the rot fungus Dacrymyces stillatus has been repeatedly confirmed in external wood panels, particularly from wood painted with water based paints. A laboratory method for testing of the fungal resistance of paint films on wood has been developed.This method has been used to test the efficacy of the fungicides Parmetol DF 18 and Parmetol HF 25 against attack by...
J Bjurman


Occurrence and importance of various types of fungal and bacterial decay in CCA-treated horticultural pine posts in New Zealand
1984 - IRG/WP 1234
A detailed microscopical examination has been carried out on samples taken from CCA-treated pine posts exposed in horticultural soils. The following decay types were observed: white rot, brown rot, soft rot, tunnelling bacteria, cavitation bacteria, and bacterial erosion. The occurrence and importance of the various decay types between different regions, and plots within a specific region, varied ...
T Nilsson