Copper distribution in soil leached from full scale decking boards during one year
2010 - IRG/WP 10-50265
The distribution of copper in the soil under exposed decking boards after one year has been analysed. The decking boards were impregnated with copper HDO, copper quat and copper triazoles. The decking boards were pine sapwood and pressure treated in a full cell process, fixed by heating and then dried. The samples were not surface treated. Each decking sample of five boards (0.25 m2) was placed on...
F G Evans


Novel microscopic approaches to visualise chitosan within impregnated wood
2012 - IRG/WP 12-20485
Chitosan, a deacetylated product of an abundant naturally occurring biopolymer chitin, has been used in a range of applications, particularly in food and health areas, as an antimicrobial agent. In the work reported here Pinus radiata wood was impregnated with chitosan as an environmentally compatible organic biocide. It is important to understand micro-distribution of bioprotectants in impregnate...
A Singh, T Singh


Accessibility of Wood Cell Walls to Well-defined Platinum Nanoparticles
2012 - IRG/WP 12-20494
Copper nanoparticles are found in the walls of parenchyma cells in southern pine sapwood treated with a micronised wood preservative, but they are absent from tracheid walls. Hence, we hypothesized that small nanoparticles can penetrate the walls of unlignified parenchyma cells, but are excluded from lignified tracheid walls. This paper tests this hypothesis by treating pine sapwood with an aqueou...
H Matsunaga, Y Kataoka, M Kiguchi, P D Evans


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


Visualization of Copper in the Voids and Cell Walls of Treated Wood using X-Ray Micro-Computed Tomography
2013 - IRG/WP 13-40640
This study extends our observations of the distribution of copper in treated wood. A small wood block was cut from a southern pine batten that had been treated with a particulate-copper preservative and similar sized block was cut from a batten that had been treated with a copper-amine preservative. Both blocks were imaged using X-ray micro-computed tomography. We obtained tomograms of each treate...
P D Evans, A Limaye, H Averdunk, M Turner, T J Senden


COST Action FP0904 – Increasing the Understanding of Thermo-Hydro-Mechanical Wood Behaviour and Processing
2013 - IRG/WP 13-40646
The polymeric components of wood and its porous structure allow its properties to be modified under the combined effects of temperature, moisture and mechanical action – so-called Thermo-Hydro-Mechanical (THM) treatments. Various types of processing techniques, including high temperature steam with or without an applied mechanical force, can be utilised to enhance wood properties, to produce eco...
D Jones, P Navi


Scanning Transmission X-ray Microscopy as a tool for examining chemical changes in wood cell walls due to enzymatic activity
2014 - IRG/WP 14-20556
As development of techniques for examining enzymatic activity on solid, complex biological materials, is considered to be an important factor in further development of enzyme applications and for understanding the decay of plant materials, this study explores applicability of Scanning Transmission X-ray Microscope (STXM) for determining chemical changes in enzymatically treated samples at the cell...
D Jeremic, R Goacher, R Yan, C Karunakaran, E R Master


Full-scale impregnation of wood with siloxane using supercritical carbon dioxide
2014 - IRG/WP 14-40659
Full-scale impregnation of wood with siloxane was carried out using supercritical carbon dioxide as solvent. A batch of 3530 kg of Scots pine sapwood was impregnated to a retention of approximately 1.3% siloxane. The treatment also consisted of a simultaneous impregnation with organic biocides. The performance of the wood was evaluated in terms of capillary water uptake according to a modified EN ...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Measurement of Cell Wall Moisture in Acetylated Radiata Pine Using Low-Field Nuclear Magnetic Resonance
2016 - IRG/WP 16-20583
Understanding the interaction of water with acetylated wood is necessary to explain how the protective mechanism of acetylation functions. Low-field nuclear magnetic resonance is one technique for assessing water in wood. Pinus radiata earlywood sapwood samples were acetylated to various weight percentage gains and then analysed with this method. Increased levels of acetylation showed significantl...
H G Beck, C A S Hill


Role of cell wall specific moisture content on the brown-rot fungal attack on wood
2016 - IRG/WP 16-40736
Wood is a hydroscopic resource because the cell wall polymers contain hydroxyl and other oxygen-containing groups that attract moisture through hydrogen bonding. Moisture content varies with changing moisture content in its environment. The moisture content in wood is responsible for many of the performance properties we observe. The strength properties of wood are dependent on the moisture con...
R M Rowell


Hydrolytic stabilization of chemically modified Bambusa vulgaris Shrad ex JC Wendl
2018 - IRG/WP 18-40830
The main drawback which greatly limit the utilisation of bamboos is their high moisture intake, biodegradation and physical properties changes with environmental variations. To prevent excessive dimensional changes and improve moisture properties of bamboo, Bambusa vulgaris was chemically treated with acetic-anhydride without co-solvent. To evaluate the influence of acetylation on the moisture pro...
N A Sadiku, S M Akintayo


The influence of chemical compounds on wood cell wall to surface cracks
2020 - IRG/WP 20-40908
Degradation due to cracking and dimensional changes caused by drying, have a significantly negative impact on the preservation and durability of wood. Therefore, the prevention of surface cracking, which tends to occur during the drying process, is vital. High temperature set drying is one of the most effective methods for preventing wood surface cracking. It begins with softening the wood at a hi...
R Suzuki, Y Mori, K Yoshihiro, K Yamashita, M Kiguchi


Decay capacity and degradation patterns of Xylaria hypoxylon on different wood species
2022 - IRG/WP 22-10985
A host of physical and environmental factors may influence fungal decay including the wood substrate, temperature, moisture, oxygen, light, pH, and nitrogen. Understanding the effects of these factors on fungal decay is important for the effective utilization of wood decay fungi in biotechnological processes and for understanding the role of these organisms in global carbon cycling. The ascomycete...
E Bari, G Daniel, A Singh, J J Morrell


Morphological observation of wood at the early stages of decay in brown rot and white rot
2023 - IRG/WP 23-11020
Wood rotting fungi, the fungal species causing biodeterioration for wood building, are generally classified into white-rot, brown-rot and soft-rot fungi based on their decay modes. Since white-rot and brown-rot fungi are known to reduce wood strength significantly, it is important to clarify the mechanisms of their wood degradation. White-rot fungi reduce wood strength as the decay progress and de...
R Tsukida, T Hatano, Y Kojima, Y Horikawa, S Nakaba, R Funada, M Yoshida


Field durability testing of wood above ground - Part 2: The full guideline of the Bundle method
2023 - IRG/WP 23-20696
To determine the biological durability of wood above ground, numerous approaches for test methods have been pursued and tried out in the field in the past. So far, no method has managed to find its way into a European standard. During the last 15 years, experience with the Bundle method has been gained. As described in Part 1 of this paper, the method is recommended as a suitable tool for determin...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Characterization of cell wall morphology and water-soluble extractives in Japanese larch decayed by white-pocket-rot fungi
2024 - IRG/WP 24-11034
Porodaedalea chrysoloma (Fr.) Fiasson & Niemelä is a basidiomycete that can cause white-rot decay in Japanese larch (Larix kaempferi) heartwood. P. chrysoloma is a white-rot fungus with a unique pattern that causes white-pocket-rot in the xylem of Japanese larch. However, the mechanism by which P. chrysoloma yields the pattern of white-pocket-rot in Japanese larch heartwood remains unclear. Thus,...
Y Mori, H Arai, T Ito, H Hashitani, K Yamashita, Y Ota, M Kiguchi


Field test method for wood in above ground situation - The full CEN/TC 38 guideline for the Sandwich method. Part 1 - Determining the relative protective effectiveness of a wood preservative
2024 - IRG/WP 24-41013
The attached draft CEN Technical Specification (i.e. pre-EN standard) has been drafted in order to become an alternative to the Lap-Joint test method (EN 12037:23) for testing of wood in above ground situation and the draft CEN/TS Part 1 is specifically intended for determining the relative protective effectiveness of a wood preservative. The new draft CEN/TS is based on a test method developed by...
M Westin, R Ringman, A Christof, F Friese


Previous Page