Copper based wood preservative - A new approach using fixation with resin acids of rosin
2000 - IRG/WP 00-30249
Copper soaps with carboxylic acid groups of resin acids of rosin were shown to be potential long-term wood preservatives. The principle involved is the attachment of copper to the network formed by the inorganic part of the preservative (rosin) through the -COOH groups. The mechanisms of fixation have been studied, and it has been shown that this association could be obtained : (1) by forming the ...
C Roussel, J P Haluk, A Pizzi, M-F Thévenon


Preliminary desk research in the Netherlands on development of a Knowledge Based System for Life Cycle Assessment of wood products
1997 - IRG/WP 97-50093
TNO is currently coordinating an EC-project (LIFE-SYS WOOD) to develop a consistent approach to Life Cycle Assessment (LCA) of wood products. Existing and new LCA-inventory data of six wood products will be evaluated on reliability and consistency. After validation, LCA-results will be made available through a Knowledge Based System (by 1998-1999). The aim of the KBS is to make LCA-results availab...
P Esser, D Robson, R Vanhauten


Feeding response of field populations of Coptotermes species to softwood blocks treated with non-toxic water-proofing and anti-microbial products.
2003 - IRG/WP 03-10487
The feeding response of field populations of the subterranean termite, Coptotermes lacteus, to Pinus radiata wood blocks (50 x 40 x40 mm) treated with various combinations of non-toxic and odourless water-proofing materials based on natural high molecular weight esters (TimberTreatÒ) and a new water insoluble quaternary ammonium compound (‘anti-microbial’) is described. Treated wood blocks we...
J R J French, T Pynsent, M Susic


A technique for determining the efficacy of water diffusible preservative plugs for implanting in joinery in service
1987 - IRG/WP 2291
A technique is described for determining the efficacy of soluble, diffusible preservative plugs for eradicating decay in joinery. It uses blocks of Scots pine sapwood or heartwood adjusted to known moisture contents prior to the establishment of the test fungus Coniophora puteana, from a single longitudinal dowel and the subsequent introduction of the preservative plugs. Prevention of decay, eradi...
J K Carey, A F Bravery


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


Practical considerations of the Formosan subterranean termite in Louisiana: A 50-year-old problem
2000 - IRG/WP 00-10330
In an eleven-year censusing (1989 through 1999) in the French Quarter of New Orleans and surrounding areas, Coptotermes formosanus alate numbers were found to be increasing dramatically in all years but one. Moreover, in parks and neighborhoods in New Orleans and Lake Charles, LA, as well as in Sam Houston Jones State Park near Lake Charles surveyed in 1998, alarmingly high numbers of this exotic ...
G Henderson


Studies on the fungicidal effectiveness of a petroleum derived product as a creosote alternative
1986 - IRG/WP 3384 E
This work, appears first because of the necessity to find out a profitable use for a residual product of the petrol pyrolisis, and second, because the lack of high natural durability wood used until now-a-days to build posts and sleepers in creosote lacking countries. Our main objective was pointed to the characterization of this new product and to find out the effectiveness against the wood-destr...
A M Navarrete, M T De Troya


Permatek IM 30 as a termiticide treatment for veneer-based wood products
2003 - IRG/WP 03-30325
Permatek IM 30 is a termiticide designed for incorporation into wood products during manufacture. Whereas existing approved products in Australia are based predominantly on synthetic pyrethroids carried in solvents, Permatek IM 30 is based on imidacloprid, a neonicotinoid insecticide. The formulation has very low mammalian toxicity, is free of VOCs, and has been successfully tested as a glueline ...
J Doyle, K Webb, W R Rae, A F Siraa, J Malcolm-Black


Durability of some alternatives to preservative treated wood
2004 - IRG/WP 04-30353
The environmental discussion in Sweden has lead to an increasing use of naturally durable domestic wood species and wood treated according to alternative methods for use above ground. A number of these alternatives have been tested according to field- and laboratory tests and compared to wood treated with preservatives for above ground use. Seven untreated wood species, four alternative wood treat...
M-L Edlund


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic applications. Part 1: Laboratory scale investigation
1995 - IRG/WP 95-50046
In order to investigate the applicability of current prestandard leaching test methods, a series of experiments has been performed on CCA impregnated wood dealing with the influence of pH, temperature and agitation of the surrounding water. The leaching method used in this first part of the investigation is the European prestandard drafted by CEN/TC38/WG11, a short term dynamic leaching test under...
G M F Van Eetvelde, R J Orsler, G E Holland, M Stevens


Algal growth resistance of paints for coating of wood; a laboratory study
1997 - IRG/WP 97-10213
Twelve paints were tested for resistance against algae. In addition, one algicidal compound commercially used for remedial treatments of algal growth on paints was tested for its effectiveness for prevention of algal growth. An agar diffusion bioassay was employed in which paint films on filter paper discs were placed on mineral salt medium and sprayed with an algal suspension containing a mixture...
J Bjurman


Penetration and absorption of water-borne preservatives in conifers from the Western United States: A preliminary report
1988 - IRG/WP 3475
The treatment of most softwoods from the western United States with waterborne chemicals poses a major challenge. Although many of these species are commercially treated with waterbornes, there is considerable debate about their treatability. At present, there is little or no information on the treatability of western wood species with waterborne chemicals. The lack of accurate treatability inform...
S Kumar, J J Morrell


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens


PCP in aquatic environments arising from historic contamination at wood processing and preservation sites
1995 - IRG/WP 95-50040-14
Three different studies are reported that assess the impacts of Pentachlorophenol (PCP) in aquatic environments arising from its historic use at sawmilling and wood preservation sites. These studies involved New Zealand wood processing facilities, and collectively they aimed to measure the transport of PCP from sawmill sites into the aquatic environment, determine the background environmental conc...
J S Gifford, P N McFarlane, M C Judd, S M Anderson


A model for attack at a distance from the hyphae based on studies with the brown rot Coniophora puteana
1995 - IRG/WP 95-10104
In timber infested by brown rot fungi, a rapid loss in strength is attributed to production of hydroxyl radicals (HO·) at a distance from the hyphae. The immediate precursor is Fenton's reagent (Fe(II)/H2O2), but the pathways leading to Fe(II) and H2O2 have remained unclear. Cellobiose dehydrogenase, purified from cultures of Coniophora puteana, will couple oxidation of cellodextrins to ...
S M Hyde, P M Wood


Influence of water soluble extractives on CCA fixation and leaching performance of red maple and red oak
1997 - IRG/WP 97-30133
We have observed several peculiarities in relation to CCA fixation in red maple and red oak woods such as high variability in fixation rates and leaching performance in maple and precipitate formation in solutions expressed from CCA treated red oak wood blocks at different stages of fixation. We have postulated that the extractives could be the factor of influence, as this has already been reporte...
T Stevanovic-Janezic, P A Cooper, Y T Ung


IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...
Anonymous


Leaching Characteristics of Alder Wood Treated with Copper Based Wood Preservatives
2005 - IRG/WP 05-50225
In this study, it was designed for determining leaching characteristics of CCA and alternatives wood preservatives. Alder wood blocks were treated with CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Leaching studies were conducted according to AWPA E11-97. Copper analyses of leachate were determined Atomic absorption...
A Temiz, Ü C Yildiz, E D Gezer, S Yildiz, E Dizman


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


The future for chromium in wood preservation
1985 - IRG/WP 3332
Most water-borne preservatives contain CrVI compounds, originally to reduce corrosion although now also to improve toxicant fixation. Chromium contributes to preservation and this is recognised in, for example, New Zealand and USA where chromium contents are included in calculations of overall preservative activity of CCA formulations, but chromium may also have anti-stain and joinery (millwork) p...
B A Richardson, T R G Cox


The effect of oil-borne preservative treatments on the shear strength of FRP/wood composite adhesive bonds
2003 - IRG/WP 03-40265
Reinforcement of structural wood components with Fiber Reinforced Polymer (FRP) will enhance the beam’s strength, but actual data on long-term durability is sparse, not well documented or not readily accessible. In this study, bond properties of FRP-wood composite materials were investigated following treatment with creosote or copper naphthenate preservatives. The properties investigated inclu...
B Herzog, B Goodell, R Lopez-Anido


Prevention of sapstain in logs using water barriers
1997 - IRG/WP 97-30147
Placing logs in ponds or under water sprinklers to keep moisture levels high enough to prevent oxygen tensions rising above inhibitory levels, is a proven method of preventing sapstain. The objective of this experiment was to determine if water barriers significantly reduce the rate of sapstain penetration into logs by maintaining moisture contents, and consequently oxygen tensions, at inhibitory ...
R N Wakeling, D R Eden, C M Chittenden, B Carpenter, I Dorset, J Wakeman, R Kuluz


Leaching of components from CCF treated timber in ground contact
1998 - IRG/WP 98-50108
In order to investigate the depletion of different CCF-salts during service small stakes (10*10*450mm³) were treated with five water-borne wood preservatives and after fixation brought into ground contact for several years. After failing some of the broken down stakes were used to determine the remaining concentration of relevant ions and their distribution in different segments of the stakes. A...
E Melcher


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Potential use of an emulsified tar oil fraction as a wood preservative: Preliminary technological and environmental assessment
1994 - IRG/WP 94-50028
In order to meet the recent environmental concern specifications of creosote are altered, the B[a]P content is limited and restrictions on the emission of volatile organic compounds (VOC) and higher polyaromatic hydrocarbons (PAH) are expected in some countries. Research has been conducted on an emulsion of a selected tar oil fraction. Using a waterborne formulation opens new perspectives for targ...
G M F Van Eetvelde, R Leegwater, M Stevens