Effects of new fixative additives on leachability of boron wood preservatives
2009 - IRG/WP 09-30507
Borates are well known with their protective capacity against both fungi and insects with low mammalian toxicity and environmental acceptable. However, boron itself does not ensure the appropriate protection for wood in the exterior applications because of their easily depletion from the treated wood under wet conditions. In this study, the potential use of monoglyceride and polyvinyl alcohol prod...
A Mohareb, J Henry, E Wozniak, P Gérardin


New insights from NMR, FTIR, X-ray diffraction and physical chemistry into digestive processes in the wood-boring marine crustacean Limnoria quadripunctata
2010 - IRG/WP 10-10732
This paper summarises preliminary findings of a multi-technique exploration of the degradation of lignocellulose in the marine isopod Limnoria quadripunctata. Scanning electron microscopy revealed connections between the digestive gland and the hindgut that would permit the exchange of fluids between the two organs while the food mass is retained in place within the hindgut. This enables enzymes t...
G P Malyon, S LaBarre, N Kervarec, P Carey, J McGeehan, X Xie, A Klüppel, S M Cragg


Determination of a fixation time of wood preservatives: A discussion paper
2010 - IRG/WP 10-20436
The intention of that paper is to initiate a discussion on the basis of a French method in combination with a German approach regarding the need of a method for the determination of a fixation time and especially to obtain input as well as ideas concerning a possible test design. Since no harmonised European approach exists up to now concerning the determination of a fixation time, CEN TC 38 (2009...
E Raphalen, E Melcher


Effects of polyvinyl alcohol on leachability and efficacy of boron wood preservatives against fungal decay and termites attack
2010 - IRG/WP 10-30526
In this study, the use of polyvinyl alcohol (PVA) as boron fixative agent was investigated. Two levels of PVA (2.5 and 4%) were evaluated with disodium octaborate tetrahydrate (DOT) at three concentrations (1, 2 and 4% boric acid equivalent (BAE) using a double vacuum impregnation processes on Scots pine sapwood specimens. Leaching was performed according to a laboratory leaching procedure. Boron ...
A Mohareb, M F Thévenon, E Wozniak, P Gérardin


A comparison of the chemistry of alkaline copper and micronized copper treated wood
2010 - IRG/WP 10-30528
This paper discusses the chemistry of the reaction of alkaline copper and micronized copper with wood. The objective of this study is to examine the copper species produced in wood during the fixation reaction using electron paramagnetic resonance (EPR) spectroscopy. The initial experiments (phases 1 to 2) were designed to confirm the effect of time of treatment and solution concentration on the s...
Wei Xue, P Kennepohl, J N R Ruddick


Laboratory evaluation of borate amine: Copper derivatives in wood for fungal decay
2010 - IRG/WP 10-30543
The aims of this study were to evaluate borate: amine: copper derivatives in wood for fungal decay protection as well as the permanence of copper and boron in wood. Wood treated with each of four derivatives of borate:amine:copper prevented fungal decay. Disodium tetraborate ecahydrate (Borax):amine:copper derivatives with retentions of 0.61 to 0.63% after water leaching prevented decay by Gloeo...
G Chen


Chapter 13 - Slow fixation of CCA-treated bamboo
2007 - IRG/WP 07-10635-13
Chromated copper arsenate (CCA) leachability tests on full-cell pressure impregnated (with 2-3% CCA solution) and slow dried (six months air-drying under cover) bamboo block of three major bamboo species of Bangladesh revealed initial insignificant leaching of CCA within first week and no leaching in next week. Use of low concentration of CCA, release of particle form of CCA due to exposure ...
A K Lahiry


Chapter 14 - Accelerated fixation of CCA-treated bamboo
2007 - IRG/WP 07-10635-14
Chromated copper arsenate type C (CCA-C) fixation study on impregnated (with adequate w/v 6% CCA solution) then boiled, oven-dried, normal, air-dried and steamed bamboo slices of airdried borakbamboo (Bambusa balcooa Roxb.) of Bangladesh, revealed almost complete fixation in steamed (accelerated fixation) and air-dried (3 weeks, slow fixation) bamboo slices compared to moderate to low fixati...
A K Lahiry


Fixed Borates Anyone?
2011 - IRG/WP 11-30563
The quest for a borate based preservative system that resists leaching or is “fixed” has long been a research goal. Boron fixation has been attempted with numerous strategies but there have been problems associated with past methods. This paper discusses new fixation systems based on bio-materials and presents up to five year outdoor exposure testing on full-size decks. Generally, the new f...
C R McIntyre, M A Lake


Tannin resin-boron associations: Leaching and biological resistance
2012 - IRG/WP 12-30587
The easy leaching of boron in wood preservation formulations has allowed to use this fungicide only for short term applications. The recently discovered adduct with flavonoids allows boron to resist longer periods of time within wood and consequently extend its life. Two different leaching treatments were compared and the fungal and termite decay was examined. The biological tests have shown extre...
G Tondi, S Wieland, N Lemenager, A Petutschnigg, A Pizzi, M-F Thevenon


Fixation and leaching characteristics of Malaysian tropical hardwoods treated with CCA-C
2012 - IRG/WP 12-50289
The fixation and leaching characteristics of 8 Malaysian tropical hardwood (MTH) species treated with chromated copper arsenate (CCA-C) wood preservative were examined. The species evaluated were Acacia (Acacia mangium), Bintangor (Calophyllum sp.), Geronggang (Cratoxylon arborescens), Medang (Litsea sp.), Meranti rambai daun (Shorea acuminata), Putat (Planchonia sp.), Ramin (Gonystylus sp.) and S...
S Salim, S Shahomlail, Z Ashaari, Yong-Seok Choi, Gyu-Hyeok Kim


The chemistry of wood degradation by Basidiomycetes studied in a van Krevelen diagram
2013 - IRG/WP 13-10805
The atomic composition ratios of decayed wood by Basidiomycetes are mapped in a van Krevelen diagram. It is shown that the wood residue after decay is chemically reduced, rather than oxidized. A previously developed and verified theoretical model for thermal wood modification, relating atomic composition ratios to moisture sorption and fungal resistance properties has tentatively been applied to w...
W Willems, H Militz


Preliminary testing of spiroborate esters as wood preservatives
2013 - IRG/WP 13-30614
Fungicide and insecticide properties of boric acid are known since 30’s of the last century, but high solubility and leachability of inorganic borates limit their use for only applications not directly exposed to liquid water. A number of attempts were made to fixate borate salts into the wood structure but this research topic is still up to date and undiscovered. Water insoluble organoboron est...
D Panov, N Terziev


The Chelator Mediated Fenton System in the Brown Rot Fungi: Details of the Mechanism, and Reasons Why it has Been Ineffective as a Biomimetic Treatment in some Biomass Applications – a Review
2014 - IRG/WP 14-10828
The chelator-mediated Fenton (CMF) reaction requires the action of two types of chelating compounds. The first chelator, oxalate, solubilizes and then sequesters iron, and the second chelator reduces iron. Iron reduction must be controlled near the fungal hyphae to prevent damaging Fenton chemistry from occurring in that location. Similarly, iron reduction must be promoted within the wood/plant ce...
B S Goodell, M Nakamura, J Jellison


The potential of 2D NIR imaging for wood protection research
2015 - IRG/WP 15-20566
Investigating wood and wood-based materials using infrared spectroscopy has since long been explored. Recently, image-based systems have been developed that are used in food and pharmaceutical industries for rapid screening. Such hyperspectral cameras are able to collect spatial and spectral information simultaneously, resulting in a volume with a spectral profile for each pixel of the image. We p...
J Van den Bulcke, N Defoirdt, W Li, J Van Acker


Evidence for a role for precipitated copper on the chemistry of micronized copper treatments
2016 - IRG/WP 16-30690
Micronized copper preservative treatments of softwoods, result in mobile copper being formed by reaction of the basic copper carbonate (BCC) with the carboxylic acid functional groups in hemicellulose and pectic substances present in wood. Typically, the amount of reacted copper formed is approximately 0.3% Cu m/m. In this paper, two examples are discussed where remaining unreacted basic copper ca...
Wei Xue, P Kennepohl, J N R Ruddick


State of Nanocopper Fixation by Steam-Densification
2016 - IRG/WP 16-40723
This study was aimed to investigate the effect of steam treatment before densification on leachability and dimensional stability of nanocopper impregnated poplar (Popolus alba). Wood samples were impregnated with nanocopper suspension (200 and 400 ppm) for 20 minutes under 4 bar pressure. Steaming process was done before densification at 150°C for 2 hour. Radial densification (33%) was done conse...
G Rassam, A Talaei, A Ahmadi


Development of a new method for wood hydrophobizing and fixation of copper compounds by chemical hardening of vegetable based modified oils
2016 - IRG/WP 16-40754
Wood products with ground and direct water contact, but without sufficient biological durability, have to be protected against biological degradation by fungi and other microorganisms. Due to European legislation (Biocidal Products Regulation 528/2012), the selection of possible chemical agents, which are still allowed to be used, is diminishing rapidly. The use of previously widely applied, very ...
C Swaboda, M Fischer, K Jacobs


Enhancing Our Understanding of Brown Rot Mechanisms through Catalytic Pretreatment and Cellulase Cocktail
2018 - IRG/WP 18-10909
A catalytic mechanism, described as the “chelator-mediated Fenton” (CMF) mechanism, is proposed to mimic the non-enzymatic action of brown rot fungi. A CMF treatment was used together with an enzymatic cocktail to study how wood was deconstructed and solubilized. This was done in-part to determine if the treatment mimicked the action of brown rot fungi, but also to explore improved treatment p...
S Tabor, L Orjuela, D Contreras, G Alfredsen, J Jellison, S Renneckar, B Goodell


Wood chemistry completes natural durability as criteria for shorting best provenances in the improvement of teakwood quality: case of five provenances from Ivorian Séguié’s trial
2018 - IRG/WP 18-10920
In order to determine the best provenance for continuing breeding program in Côte d’Ivoire, five provenances of teak planted in 1970 at Séguié’s trial (Agboville, in the south of Côte d’Ivoire), were compared. Fifteen trees (three trees per provenance) composed the sample. Decay resistance and the chemical content especially, non-structural carbohydrates, total phenolics and quinone comp...
F B Niamke, N Amusant, A A Adima, A A Kadio, G Chaix, C Jay-Allemand


Performance of bio-based building materials – durability and moisture dynamics
2020 - IRG/WP 20-20666
When exposed to conditions favourable for decay, bio-based building materials can be susceptible to degradation. Their ability to withstand deterioration over time (performance) depends on the intrinsic or enhanced durability of the material as well as its wetting and drying behaviour. The effect of fungicidal components in wood is known since long. Other material characteristics, such as the mate...
L De Ligne, J Caes, S Omar, J Van den Bulcke, J M Baetens, B De Baets, J Van Acker


Decay capacity and degradation patterns of Xylaria hypoxylon on different wood species
2022 - IRG/WP 22-10985
A host of physical and environmental factors may influence fungal decay including the wood substrate, temperature, moisture, oxygen, light, pH, and nitrogen. Understanding the effects of these factors on fungal decay is important for the effective utilization of wood decay fungi in biotechnological processes and for understanding the role of these organisms in global carbon cycling. The ascomycete...
E Bari, G Daniel, A Singh, J J Morrell


Geopolymer as a fixation method for tannin-based wood preservatives
2023 - IRG/WP 23-30774
This study aims to test if a second step impregnation with a geopolymer solution can fix Colatan GT10, a commercial extract rich in tannins, to wood, reducing their leaching and improving their performance as wood preservatives. Scots pine sapwood specimens of 40×10×5 mm3 were impregnated with Colatan GT10 tannin mix, geopolymer, and as combined treatment Colatan GT10 with subsequent geopolymer ...
Y M López-Gómez, A Barbero-López, A Haapala


Leaching and chemical redistribution of CCA components in refractory heartwood of E. nitens
2024 - IRG/WP 24-41011
Chromated Copper Arsenate (CCA) is a wood preservative widely used to protect against fungal and insect attack. The fixation mechanism of CCA involves complex chemical reactions, including the reduction of chromium (VI) to chromium (III) and the formation of insoluble complexes. Despite fixation efforts, a portion of CCA components tends to leach from treated wood, influenced by factors like wood ...
J R Vargas, L Yermán, K C Wood, T Singh


Previous Page